Synthesis of Low Molecular-weight Poly (Propylene Carbonate)-Poly (Ethylene Glycol) Block Copolymers through $CO_2$/Propylene Oxide Copolymerization (이산화탄소/프로필렌 옥사이드 공중합을 통한 저분자량 폴리(프로필렌 카보네이트)-폴리(에틸렌 글리콜) 블록 공중합체의 합성)

  • Lee, Sang-Hwan;Cyriac, Anish;Jeon, Jong-Yeob;Lee, Bun-Yeoul
    • Clean Technology
    • /
    • v.17 no.3
    • /
    • pp.244-249
    • /
    • 2011
  • We synthesized low molecular-weight polymers bearing hydrophobic and hydrophilic parts in a chain through $CO_2$/propylene oxide copolymerization. When hydrophilic poly (ethylene glycol) bearing -OH group (s) at the end group (s) was added as a chain transfer agent in the $CO_2$/propylene oxide copolymerization catalyzed by a highly active catalyst, block polymers were formed. If poly (ethylene glycol) (PEG) bearing -OH group only at an end was fed, PEG-block-PPC diblock copolymer was obtained. When PEG bearing -OH group at both ends was fed, PPC-block-PEG-block-PPC triblock copolymer was obtained. We confirmed formation of block copolymers by $^1H$-NMR spectroscopy and GPC studies.

Preparation and Release Behavior of Methoxy poly(ethylene glycol)- poly(L-lactide-co-glycolide) Wafer Containing Albumin (알부민을 함유한 메톡시 폴리(에틸렌 글리콜)- 폴리(L-락타이드-co-글리콜라이드) 웨이퍼의 제조 및 방출거동)

  • 서광수;김문석;김경자;조선행;이해방;강길선
    • Polymer(Korea)
    • /
    • v.28 no.4
    • /
    • pp.328-334
    • /
    • 2004
  • A series of methoxy poly(ethylene glycol) (MPEG)-poly(L-lactide-co-glycolide) (PLGA) diblock copolymers were synthesized by ring-opening polymerization of L-lactide and glycolide with carbitol (134 g/mole) or different molecular weights of MPEG (550, 2000, and 5000 g/mole) as an initiator in presence of Sn(Oct)$_2$. The properties of diblock copolymers were characterized by using $^1$H-NMR, GPC, and XRD. After uniform mixing of block copolymers and 1% albumin bovine-fluorescein isothiocyanate(FITC-BSA) with a freeze miller, the wafers loaded FITC-BSA were fabricated by using a mold with a dimensions of 3 mm${\times}$1mm diameter. The release profiles of FITC-BSA and the pH changes of wafer were examined using pH 7.4 PBS for 30 days at 37$^{\circ}C$. The release profiles of albumin showed fast initial burst as the molecular weights of MPEG increased. As a result of this study, the release behavior of BSA was controlled with introducing MPEG in the block copolymers.

Preparation of Polystyrene Particles Containing Poly(ethylene glycol) Groups and Their Surface Charge Characterization in Dielectric Medium (폴리(에틸렌 글리콜)기를 갖는 폴리스티렌 입자의 제조와 유전 매질내에서의 표면 전하 특성)

  • 김성훈;김배중;권대익;박기홍
    • Polymer(Korea)
    • /
    • v.28 no.6
    • /
    • pp.524-530
    • /
    • 2004
  • Polystyrene particles (PS) with poly(ethylene glycol) units on surface were formed by an emulsifier-free emulsion polymerization using styrene, poly(ethylene glycol) methacrylate (PEG-MMA) or poly(ethylene glycol) dimethacrylate (PEG-diMMA) at pH 7, and followed by freeze-drying to give the corresponding powders. The structures of PS particles were confirmed by FT-IR spectroscopy, and the particle size and distribution the PS particle were observed by scanning electron microscopy and particle analyzer. Monodisperse polymer particles were obtained at a concentration of PEG-MMA 2∼5 mol% or PEG-diMMA 1 mol% relative to styrene. The highest zeta potential of polymer surface was measured to be 183 mV at a polymer of PEG-MMA 5 mol%, which was measured in dielectric medium by means of ELS-8000 dynamic light scattering.

An analysis of influence on chemical additives in gas hydrate formation (하이드레이트 제조시 다양한 화학물질 첨가에 의한 영향 분석)

  • Lee Young-Chul;Mo Yong-Gi;Cho Byoung-Hak;Baek Young-Soon
    • Journal of the Korean Institute of Gas
    • /
    • v.8 no.4 s.25
    • /
    • pp.23-29
    • /
    • 2004
  • This work carried out experiment to change characteristics of hydrate formation using various chemicals which are acetone, dimethylbutane, polyvinylalcohol, methanol and ethlyene glycol as additives in gas hydrate formation. Gas storage ability of formed hydrate with acetone, firnethylbuthane and polyvinylalcohol in gas hydrate formation increased higher than that obtained with pure water. Among them polyvinylalcohol showed best gas storage ability, so it is a more useful promoter Methanol and Ethylene gl?col in using additives showed the characteristics of inhibitor and methanol is lower gas storage ability than ethylene gl)rcol as a inhibitor in hydrate formation, so it is a more useful inhibitor. But, low concentration of methanol and ethylene glycol showed considerably higher gas storage ability of hydrate than that obtained with Pure water and showed the characteristics of promoter in gas hydrate formation.

  • PDF

Thermosensitive Sol-gel Phase Transition Behavior of Methoxy poly(ethylene glycol)-b-poly($\varepsilon$-caprolactone) Diblock Copolymers (메톡시 폴리(에틸렌 글리콜)-폴리($\varepsilon$-카프로락톤) 공중합체의 온도감응성 솔-젤 전이 거동)

  • 서광수;박종수;김문석;조선행;이해방;강길선
    • Polymer(Korea)
    • /
    • v.28 no.4
    • /
    • pp.344-351
    • /
    • 2004
  • Poly(ethylene glycol)-based diblock and triblock polyester copolymers stimulating to temperature were studied as injectable biomaterials in drug delivery system because of their nontoxicity, biocompatibility and biodegradability. We synthesized the diblock copolymers consisting of methoxy poly(ethylene glycol) (MPEG) (M$_{n}$=750 g/mole) and poly($\varepsilon$-caprolactone) (PCL) by ring opening polymerization of $\varepsilon$-CL with MPEG as an initiator in the presence of HCl . Et$_2$O. The aqueous solution of synthesized diblock copolymers represented sol phase at room temperature and a sol to gel phase transition as the temperature increased from room temperature to body temperature. To confirm the in vivo gel formation, we observed the formation of gel in the mice body after injection of 20 wt% aqueous solution of each block copolymer. After 2 months, we observed the maintenance of gel without dispersion in mice. In this study, we synthesized diblock copolymers exhibiting sol-gel phase transition and confirmed the feasibility as biomaterials of injectable implantation.n.

Depolymerization of Polycarbonate Waste by Ethylene Glycol (에틸렌글리콜을 이용한 폐폴리카보네이트 해중합 특성)

  • Kim, Dongpil;Kim, Bo-kyung;Cho, Youngmin;Han, Myungwan;Kim, Beom-Sik
    • Korean Chemical Engineering Research
    • /
    • v.46 no.5
    • /
    • pp.875-879
    • /
    • 2008
  • A method for the depolymerization of polycarbonate waste by glycolysis using ethylene glycol without catalyst was explored in order to get the monomer bisphenol A (BPA). The effect of operation variables such as reaction time, reaction temperature, EG/PC weight ratio and the kinetic of glycolysis were studied. It was found that the polymerization reaction has two different activation energies depending on the reaction temperature. A drop in activation energy with temperature indicates that the reaction mechanism has shifted from one of a succession of elementary steps to another in the series. The maximum yield of BPA of 95.6% was achieved at reaction temperature $220^{\circ}C$ for 85min with EG/PC weight ratio 4.

Synthesis of Methoxy Poly(ethylene glycol)-b-poly($\varepsilon$-caprolactone) Diblock Copolymers and Release Behavior of Albumin for Implantable Protein Carriers (이식형 단백질 전달체로서 메톡시 폴리(에틸렌 글리콜)/폴리카프로락톤 블록 공중합체의 합성 및 알부민의 방출 거동)

  • 서광수;전세강;김문석;조선행;이해방;강길선
    • Polymer(Korea)
    • /
    • v.28 no.3
    • /
    • pp.232-238
    • /
    • 2004
  • MPEG-PCL diblock copolymers consisting of methoxy poly(ethylene glycol) (MPEG) and $\varepsilon$-caprolactone (CL) as drug carriers were synthesized by ring-opening polymerization MPEG-PCL diblock copolymers were characterized by X-ray diffraction and differential scanning calorimetry. After freeze milling of block copolymers and albumin bovine-fluorescein isothiocyanate (FITC-BSA) as model protein, the wafers loaded FITC-BSA were fabricated by direct compression method. The release profiles of FITC-BSA were examined using pH 7.4 PBS for 14 days at 37$^{\circ}C$. The release amount was determined by fluorescence intensity by using the fluorescence spectrophotometer. The morphological change of wafers was observed by digital camera and scanning electron microscope. The release rate and initial burst of BSA increased with increasing PEG molecular weights and decreasing PCL molecular weights in the segments of MPEG -PCL diblock copolymers.

Dimensional Stability of Poly(ethylene/propylene naphthalate) as a Flexible Substrate Application (유연 기판 소재로 응용을 위한 폴리(에틸렌/프로필렌 나프탈레이트)의 치수안정성 연구)

  • Kim, Jae-Hyun;Heo, Hye-Young;Jung, Tae-Houng;Han, Joon-Hee;Kang, Ho-Jong
    • Polymer(Korea)
    • /
    • v.33 no.4
    • /
    • pp.371-376
    • /
    • 2009
  • The 1,3-propane diol has been introduced as a co-monomer with ethylene glycol to polymerize the poly(ethylene/propylene naphthalate) in order to improve the dimensional stability of poly(ethylene naphthalate) for a possible flexible substrate material. Based on $^1H$-NMR results, it was found that poly (ethylene/propylene naphthalate) has been synthesised successfully. Introducing 1,3-propane diol resulted in the amorphous state in polyester as well as lowering of glass transition and thermal degradation temperature. Coexisting relatively longer propylene segment compared with ethylene in synthesized polyester caused less orientation behavior and reducing thermal expansion coefficient. This is a promising result for poly (ethylene/propylene naphthalate) to apply a flexible substrate.

Synthesis of Thermosensitive and Biodegradable Methoxy Poly(ethylene glycol)-Polycaprolactone and Methoxy Poly(ethylene glycol)-Poly(lactic acid) Block Copolymers (온도감응 및 생분해성 폴리에틸렌 글리콜-폴리카프로락톤과 폴리에틸렌 글리콜-폴리락타이드 공중합체의 합성)

  • 서광수;박종수;김문석;조선행;이해방;강길선
    • Polymer(Korea)
    • /
    • v.28 no.3
    • /
    • pp.211-217
    • /
    • 2004
  • The sol to gel transition of aqueous solution of block copolymers consisting of methoxy poly (ethylene glycol) (MPEG) and biodegradable polyesters such as $\varepsilon$-caprolactone and L-lactide was investigated as a function of temperature. MPEG-PCL was prepared by ring opening polymerization of $\varepsilon$-caprolactone in the presence of HClㆍEt$_2$O as monomer activator at room temperature. Also, MPEG-PLLA was prepared by ring opening polymerization of L-lactide in the presence of stannous octoate at 115$^{\circ}C$. The properties of block copolymers were investigated by $^1$H-NMR, IR, and GPC as well as the observation of thermo sensitive phase transition in aqueous solution. As the hydrophobic block length increased, the sol to gel transition temperature increased and curve of that steepen to lower concentration. To confirm the gel formation at body temperature, we observed the formation of gel in the mice body after injection of 20 wt% aqueous solution of each block copolymer. After surging, we investigated the gelation in mice. The results obtained in this study confirmed the feasibility as biomaterials of injectable implantation for controlled release of drug and protein delivery.

Depolymerization of Polycarbonate Using Glycolysis/Methanolysis Hybrid Process (폴리카보네이트의 글리콜첨가분해/메탄올첨가분해 복합 해중합)

  • Kim, D.P.;Kim, B.K.;Cho, Y.M.;Kim, B.S.;Han, M.
    • Clean Technology
    • /
    • v.13 no.4
    • /
    • pp.251-256
    • /
    • 2007
  • Several studies regarding depolymerization of polycarbonate waste to get the essential monomer, bisphenol A, have been reported in recent years. However, those methods have some environmental safety problems of using highly toxic organic solvents as well as product separation problem due to the use of alkali catalyst. In this study, we proposed the combination of glycolysis and methanolysis to depolymerize the polycarbonate waste. Glycolysis reaction reached at the reaction equilibrium after about 180 minat 473.15K and dissolution of the polycarbonate was found to be a rate controlling step of the reaction. The yield of BPA was improved with the aid of combination of glycolysis and methanolysis. The methanolysis was carried out at a temperature range of $303.15K{\sim}363.15K$ and MeOH/PC molar ratio $0.5{\sim}3$. The yield of BPA had a maximum at 1.0 MeOH/PC molar ratio and increased with the reaction temperature.