• Title/Summary/Keyword: 타이타늄

Search Result 299, Processing Time 0.019 seconds

Marginal and internal fit of all ceramic crown using the replica technique and the triple-scan protocol (Replica technique과 Triple-scan protocol을 이용한 지르코니아 전부도재관의 변연 및 내면 적합도에 관한 비교 연구)

  • Shin, Mi-Sun;Lee, Jang-Hoon
    • The Journal of Korean Academy of Prosthodontics
    • /
    • v.55 no.4
    • /
    • pp.372-380
    • /
    • 2017
  • This study was conducted to compare the marginal and internal fit of all ceramic crown using the replica technique and the triple-scan protocol. Materials and methods: Twenty zirconia ceramic crowns were fabricated using titanium abutment model. All crowns were divided into two groups of 10 each, depending on the replica technique and the triple-scan protocol. The internal and marginal fit of 10 zirconia ceramic crowns were measured at 17 points for each specimen using the replica technique. The other 10 ceramic crowns were measured using the triple-scan protocol. Statistical analysis was performed by t-test (${\alpha}=.05$). Results: The mean and standard deviation of marginal and internal fit were significantly different between the replica technique ($49.86{\pm}29.69{\mu}m$) and triple-scan protocol ($75.35{\pm}64.73{\mu}m$, P<.001). The mean and standard deviation of internal fit except marginal fit were $58.38{\pm}31.77{\mu}m$ and $64.00{\pm}46.43{\mu}m$, respectively (P>.343). Conclusion: There was a statistically significant difference in the marginal fit measured by the two methods. However, there was no statistically significant difference in the internal fit between the two methods.

MECHANICAL PROPERTIES OF TITANIUM CONNECTORS TREATED BY VARIOUS WELDING TECHNIQUES (용접방법에 의한 타이타늄 연결부의 기계적 성질에 관한 연구)

  • Lee, Soo-Young;Chang, Ik-Tae;Heo, Seong-Joo;Yim, Soon-Ho
    • The Journal of Korean Academy of Prosthodontics
    • /
    • v.37 no.5
    • /
    • pp.545-566
    • /
    • 1999
  • The use of pure titanium and titanium alloys have been increased recently in fixed, removable prosthodontics and implant fields as a framework. But when they were used for superstructures of implant or metal framework of removable prosthesis, welding is necessary to reconnect the fracture site to control the casting distortions. To overcome the difficulties in soldering the titanium due to high oxidation property, much effort have been devoted. In this study, some of mechanical properties were compared between pure titanium and Ti-6Al-4V alloy by using after welding, electron beam welding technique and tungsten arc welding. Mechanical properties such as tensile strength, yield strength, elongation and microhardness were measured. And, in order to compare the effect of welding site and surrounding metal tissue according to the welding condition, SEM photographs were taken and element distribution was observed by Wave Dispersion Spectroscopy. Through analyses of the data, following results were obtained; 1. In items such as tensile strength, yield strength and elongation according to the welding techniques of pure titanium, only tungsten arc welded group showed significant lower value than other groups(P<0.05). 2. In items such as tensile strength and yield strength according to the welding techniques of Ti-6Al-4V alloy, control group and tungsten arc welded group showed significant difference among all the groups(P<0.05). 3. Ti-6Al-4V alloy exhibited significantly greater elongation than control group when the laser welding method and electron beam welding method were used, and elongation showed increasing tendency. 4. Pure titanium specimens exhibited increasing tendency of microhardness regardless of the weld-ing technique applied, and especially tungsten arc welded group demonstrated a great increase of microhardness than parent metal. 5. There was no hardness change in laser welded group and electron beam welded group of Ti-6Al-4V alloy, but in tungsten arc welded group, hardness changed greatly from parent metal to weld seam. 6. Through the metallographic examination and scanning electron microscopy, laser welding caused central fusion and recristallizations were formed and tungsten arc welding caused localized fusion to 0.3-0.7mm from the surface.

  • PDF

The Effect of Alkali- and Heat-Treated Titanium Surfaces on Differentiation of Osteoblast (티타니움 표면의 알칼리-열처리가 골모세포의 분화에 미치는 영향)

  • Kang, Choong Hee;Vang, Mong-Sook;Yang, Hong-so;Park, Sang-Won;Lim, Hyun-Pil
    • Journal of Dental Rehabilitation and Applied Science
    • /
    • v.25 no.3
    • /
    • pp.293-306
    • /
    • 2009
  • In this study, the biological response of fetal rat calvarial cells on alkali- and heat-treated titanium was assessed. The results were as follows; Cell proliferation on alkali- and heat-treated surfaces showed significantly higher level than on the titanium-6aluminum-4vanadium (weight percentage: 6 % aluminum, 4 % vanadium, Ti-6Al-4V) surface (p<0.01). In ELISA analysis, concentration of $IL-1{\beta}$ and IL-6 were raised when the cells were grown to day 7. Pre-treatment with herbimycin, a known tyrosine kinase inhibitor, suppressed the production of IL-6 (p<0.01). In comparison to commercially pure titanium (grade II, cp-Ti) and Ti-6Al-4V alloy, alkali- and heat-treated titanium enhanced alkaline phosphatase activity (p<0.001). In RT-PCR analysis, alkaline phosphatase, bone sialoprotein, receptor activated nuclear factor ligand mRNA expression was increased alkali- and heat-treated titanium. Herbimycin and SB203580, p38 MAPK inhibitor, were repressed of $IL-1{\beta}-induced$ IL-6 mRNA expression. These results suggest that alkali- and heat-treated titanium stimulate osteoblasts differentiation and facilitate bone remodeling.

Comparative study of two CAD software programs on consistency between custom abutment design and the output (두 가지 CAD software의 맞춤형 지대주 디자인과 출력물 일치도 비교)

  • Lim, Hyun-Mi;Lee, Kyu-Bok;Lee, Wan-Sun;Son, KeunBaDa
    • Journal of Dental Rehabilitation and Applied Science
    • /
    • v.34 no.3
    • /
    • pp.157-166
    • /
    • 2018
  • Purpose: This study was aimed to compare the consistency between the custom abutment design and the output in two CAD software programs. Materials and Methods: Customized abutments were designed by using 3Shape Dental System CAD software and Delta9 CAD software on a plaster model with implants (CRM STL file). After milling of the designed abutments, the abutments were scanned with a contact method scanner (Test STL file). We overlaid the Test STL file with each CRM STL file by using inspection software, and then compared the milling reproducibility by measuring the output error of the specimens from each CAD software program. Results: The Delta9 showed better milling reproducibility than 3Shape when comparing the milling errors obtained with a full scan of all specimens (P < .05) and also when comparing the axial wall region specifically according to the axial angle. With 0.9 mm marginal radius, the Delta9 showed better consistency between the design and the output than 3Shape (P < .05). While, anti-rotation form had no significant difference in error between the two systems. When cumulative errors were compared, the Delta9 showed better milling reproducibility in almost cases (P < .05). Conclusion: Delta9 showed a significantly smaller error for most of the abutment design options. This means that it is possible to facilitate generation of printouts with reliable reproducibility and high precision with respect to the planned design.

A HISTOLOGIC STUDY OF THE OSSEOINTEGRATION PROCESS TO THE TITANIUM TOOTH ROOT IMPLANT (타이타늄 치근형 매식체에 대한 골유착 과정에 관한 조직학적 연구)

  • Ahn, Chang Young;Kim, Yung Soo
    • The Journal of Korean Academy of Prosthodontics
    • /
    • v.28 no.2
    • /
    • pp.1-28
    • /
    • 1990
  • The severe atrophic edentulism with poor neuromuscular control militates against successful conventional denture therapy. To such situation, a prescribing of dental implant treatment has been considered with some probability. Implant materials used as a trial for dental implants includes metals, plastic polymers and ceramics. The purpose of this study was to observe histologic response in osseointegration process at titanium implant-tissue interface based on biocompatibility at specific period of sequential natures which were divided into a half month, one, month, two months, three months and immediate as a base line. In this study, unilateral lower left premolar and molar teeth were extraced in three dogs. After allowing to heal for 6 months, three kinds of osseointegrated implant, $Br{\aa}nemark$, Corevent and kimplant(a prototype of SNU implant study)were inserted in each dog respectively according to the above sequence from front to back. The specimens were taken from those dogs at the same time since implant were inserted quite reverse order of the specified periods, and decalcified and processed for histologic examination for the light microscopy and the electron microscopy. The microscopic histologic findings at the interface between titanium implants and tissue were interpretated as follows : A. Light microscopic findings : a. Immediate : Implant were surrounded by compact bone and spongy bone. Microcrak was observed in the superficial bone tissue. Osteocytes were disappeared and bone lacunae were observed as a vacant space in some parts. In the contacting with the spongy bone, bone trabeculae and bone marrow were in contact with the implant. b. A half Month : Osteoblasts exist as a monolayer in th inner bone trabeculae and do bone additiocn. Osteoblasts&inflammatory cells were observed in some parts. c. One Month : The presence of osteoclasts decreased. Osteoblasts did active bone fromation, and bone marrow was in contact with the implant in the many places. d. Two Months : Bone formation was advanced in comparison with the b and c. The presence of osteoclsts was not observed. e. Three Months : The superficial bone tissue contacted with the implants was entirely composed by the compact bone. B. Electron microscopic findings : a. A half month and one month group : In the parts of the active bone formation, osteoblasts with the well developed endoplasmic reticulum and Golgi apparatus were arranged in the monolayer. In the parts of the bone resorption, ruffled border was well developed and many osteoclasts with the well-developed golgi apparatus, mitochondria, vacuole, vesicle and lysosome were existed. b. Three months group : No osteoblasts were observed in the superficial bone tissue. Bone matrix with collaen fiber was observed. c. No significant dirrerence in the histologic findings was observed in $Br{\aa}nemark$, Core-vent and kimplant.

  • PDF

Wettability of titanium implants depending upon surface properties (타이타늄 표면 처리 특성에 따른 젖음성에 관한 연구)

  • Han, Young-Soo;Shin, Sang-Wan
    • The Journal of Korean Academy of Prosthodontics
    • /
    • v.47 no.1
    • /
    • pp.12-20
    • /
    • 2009
  • Statement of problem: When an implant is fixed, a fixture comes into contact with a tissue fluid. Adhesion of a tissue fluid to a surface of implant is various case by case. Purpose: The ultimate goal of this work is to analyze a correlation between a surface roughness and wettability of implant specimens. A measurement for wettability is performed considering 4 types of specimen implant with surface treatments different from each other to investigate the change of wettability with the elapse of time. Material and methods: Firstly, 20 specimens of titanium were prepared. The specimen were made of a commercial Titanium Grade IV with the diameter of 10 mm and the thickness of 1 mm. According to the method of surface treatment, the specimens were classified into 4 groups of 5 specimens per group. Group A: Machined Surface Group B: Anodized surface Group C: RBM (HA blasting) surface Group D: CMP (calcium methaphosphate) coating surface. Surface roughness of specimen was measured using SV-3000S4 (Mituyoto, Japan). The measurement was based on the standard of JIS1994. Sessile drop method was used to measure the wettability, which measures contact angle between implant disc and saline with the time interval of 5, 10, and 15 seconds. SPSS 11.0 was used to analyze the collected data. In order to analyze the difference of wettability and surface roughness according to implant surface treatment method. The statistical significance was tested with the confidence level of 95%. Pearson's correlation coefficient was used to evaluate the correlation of surface roughness and wettability. Results: The difference of surface roughness was statistically significant in the order of Group C ($1.69{\pm}0.26$), Group D ($1.58{\pm}0.16$), Group B ($0.78{\pm}0.14$) Group A ($0.18{\pm}0.05$). The wettability has also a statistically significant difference, which was in the order of group B ($17.70{\pm}2.66$), Group C ($27.86{\pm}4.52$), Group D ($66.28{\pm}3.70$) Group A ($70.52{\pm}8.00$). There was no difference in wettability with the passage of time. Conclusions: 1. The surface roughness was high in the order of RBM, CMP, Anodized, Machined group (P<.05). 2. The wettability was high in the order of Anodized, RBM, CMP, Machined group (P<.05). 3. There was no statistical significance in the correlation of surface roughness and wettability.

The success rate of Mg-incorporated oxidized implants in partially edentulous patients: a prospective clinical study (부분 무치악 환자에서 마그네슘 이온주입 임플란트의 성공률에 대한 전향적 임상연구)

  • Choi, Su-Jung;Yoo, Jung-Ho;Lee, Ku-Bok;Kim, Jin-Wook
    • The Journal of Korean Academy of Prosthodontics
    • /
    • v.50 no.3
    • /
    • pp.176-183
    • /
    • 2012
  • Purpose: This study examined the clinical success rate of Mg titanate implants (M Implant system, Shinhung, Korea), which employ a Mg coating method, by evaluating the marginal bone loss and implant stability using radiographs and Osstell$^{(R)}$, over a 1 year. Materials and methods: The locations of the implants placement were divided into 4 areas; the maxillary and mandibular premolars and molars. In the maxilla, 8 and 9 implants were inserted in the premolar and molar areas, respectively. In the mandible, 11 and 51 implants were inserted in the premolar and molar areas. Marginal bone loss and ISQ of all implants (79) were measured after insertion, mounting the prosthetic appliance, and 1, 3, 6, and 12 months after loading. The marginal bone loss was measured from the radiograph using XCP bite, which was customized, and the implant stability measured using Osstell$^{(R)}$. Fisher's exact test (${\alpha}$=.05) was used to compare the success rates of each region. Results: The mean marginal bone loss for the upper and lower jaws were 1.537 mm and 1.172 mm. The mobility showed a non-significant reduction or increase according with time. The success rates were accounted for 94.12% and 98.39% in the upper and lower jaws; the premolars and molars were accounted for 100% and 96.67%. The two cases of early failure resulted from failure of primary stability during implant insertion. The late failures were not observed for 1 year after adding a loading to the implants. Conclusion: The Mg titanate implant showed good primary stability and good clinical results in both healing and function.

Microstructures and Mechanical Properties of Friction Stir Welded 1925hMo stainless steel (마찰교반접합된 1925 hMo 스테인리스강의 미세 조직 및 기계적 특성에 관한 연구)

  • Ahn, Byung-Wook;Choi, Don-Hyun;Song, Keun;Yeon, Yun-Mo;Jung, Seung-Boo
    • Proceedings of the KWS Conference
    • /
    • 2010.05a
    • /
    • pp.23-23
    • /
    • 2010
  • 마찰교반접합(Friction Stir Welding)은 1991년 영국 TWI에서 개발된 접합 법으로서 일정한 속도로 회전하는 툴이 재료내부에 삽입 되면서 툴과 재료사이에서 마찰열이 발생하여 연화된 재료와 접합 툴 사이에서의 기계적 교반에 의해 소성변형이 일어남과 동시에 접합이 이루어진다. 마찰교반접합은 동적 재결정에 의한 접합부의 미세한 결정립 형성으로 인하여 기계적 특성이 향상되며 보호 가스가 필요 없어 친환경적임과 동시에 용융 용접 법에 비해 접합 시 에너지 소모가 적다는 장점이 있다. 마찰교반접합은 기존의 저융점 재료에 관한 접합을 넘어서 최근에는 철계 합금, 타이타늄 합금, 니켈계 합금 등 고융점 재료에서의 적용에 관한 연구가 이루어지고 있다. 하지만 마찰교반접합을 이용하여 위와 같은 강한 재료를 접합하기 위해서는 내구성이 갖추어진 툴이 반드시 수반된다. 슈퍼 오스테나이트계 스테인리스강은 염화물의 농도가 높은 부식 환경에 적용되는 소재로서, 공식(pitting corrosion) 및 틈부식 (crevice corrosion)에 대한 내식성을 높이기 위하여 Mo의 함량을 6%로 낮추고 20~25% Cr과 Ni을 첨가하여 사용된다. 이러한 고합금의 슈퍼 오스테나이트계 스테인리스강은 여타 내식성 합금에 비하여 내식성이 매우 우수한 것으로 알려져 있다. 최근 SO2 배출에 대하여 규제가 강화되면서 화력 발전소용 탈황 설비 중 일부 장비에서 6% Mo가 첨가된 슈퍼 오스테나이트계 스테인리스강의 사용이 늘어나고 있다. 본 연구에서는 $Si_3N_4$ 툴을 사용하여 Mo이 6% 첨가된 슈퍼 오스테나이트계 스테인리스강인 1925hMo강을 마찰교반접합하였다. 툴 회전속도 (200rpm, 300rpm, 460rpm, 700rpm)를 변수로 하여 접합을 실시하였다. 접합 후 외관상태를 점검하였으며 광학현미경 (optical microscope)과 주사전자현미경 (scanning electron microscope)을 사용하여 미세조직 관찰을 하였으며 경도 및 인장강도 측정 등의 실험을 통하여 접합부의 기계적 특성을 평가하였다. 그 후 이러한 결과를 통하여 미세조직과 기계적 특성과의 관련성을 조사하였다.

  • PDF

Study on microstructure and mechanical properties of friction stir welded duplex stainless steel (마찰교반접합된 이상 스테인리스강의 미세조직 및 기계적 특성에 관한 연구)

  • Choi, Don-Hyun;Ahn, Byung-Wook;Yeon, Yun-Mo;Song, Keun;Jung, Seung-Boo
    • Proceedings of the KWS Conference
    • /
    • 2010.05a
    • /
    • pp.24-24
    • /
    • 2010
  • 마찰교반접합법은 특정한 회전수로 회전하는 용접 툴을 이용하여 접합하고자 하는 피접합재의 맞댄면에 삽입시킨 후 툴을 이동시키거나 혹은 시편을 견고하게 고정시킨 장치(backing plate)가 움직여 고상 상태에서 접합이 이루어진다. 알루미늄, 마그네슘 등 비교적 융점이 낮은 저융점 재료의 재료에 처음 적용이 되어 많은 연구가 활발히 진행되었고 타 용접방법에 비해 우수한 접합특성을 나타내었다. 최근 이러한 마찰교반접합은 이러한 저융점 재료를 넘어서 스틸, 타이타늄, 니켈 등과 같은 고융점 재료 등에 대한 적용이 늘어나고 있다. 마찰교반접합을 이용하여 이러한 고융점 재료의 접합 경우 내마모성 및 내열성 등의 내구성이 갖추어진 툴과 이러한 툴을 냉각시킬 수 있는 냉각 장치 등이 필요로 하나 경제적 측면이나 접합부의 우수한 특성 등을 고려 할 때 그 적용 및 발전 가능성이 매우 높다고 볼 수 있다. 2상 스테인레스 강은 금속 조직적으로 페라이트와 오스테나이트 상이 거의 1:1의 동등한 비율로 매우 미세하게 결합된 구조를 가지고 있다. 또한 이상 스테인레스 강은 각상의 개개의 특성에 기인하여 염소 분위기에서 응력부식 저항성이 우수하고, 공식과 틈부식에 대한 저항성이 매우 뛰어나다. 그리고 이상 스테인레스 강은 비교적 고가인 Ni이 일반 오스테나이트 스테인리스 강의 약 1/2의 수준으로 적게 포함이 되어 경제적인 이점을 지니고 있으며 또한 용접성이 좋아 산업계의 수요는 현재 점차 증가하고 있는 상황이다. 하지만 이러한 이상 스테인리스 강은 용접 후 페라이트 상의 조대화, 그리고 페라이트 상의 분율이 오스테나이트 상의 분율보다 높아지게 되어 용접부에서의 저온 인성 감소 및 내식성 저하 등의 문제가 발생하게 된다. 그리하여 용접 시 이러한 문제점을 해결하기 위해서는 입열량의 조절이 가장 필요로 하는 것으로 알려져 있다. 본 연구에서는 마찰교반용접을 이용하여 두께 3mm의 대표적인 이상 스테인리스 강인 SAF2205 스테인리스 강에 대해 맞대기 마찰교반접합을 실시하였다. 툴 회전속도를 변수로 하여 접합을 실시하였으며 접합 시 툴은 $Si_3N_4$ 툴을 사용하였다. 접합 후 외관상태 점검, 미세조직 관찰, 경도 및 인장강도 측정 등의 실험을 실시하였고, 이러한 결과를 이용하여 미세조직과 기계적 특성과의 관련성을 조사하였다.

  • PDF

TiO2 Nanotubular Formation on Grade II Pure Titanium by Short Anodization Processing (Grade II 순수 타이타늄의 단시간 양극산화에 의한 TiO2 나노튜브 형성)

  • Lee, Kwangmin;Kim, Yongjae;Kang, Kyungho;Yoon, Duhyeon;Rho, Sanghyun;Kang, Seokil;Yoo, Daeheung;Lim, Hyunpil;Yun, Kwiduk;Park, Sangwon;Kim, Hyun Seung
    • Korean Journal of Materials Research
    • /
    • v.23 no.4
    • /
    • pp.240-245
    • /
    • 2013
  • Electrochemical surface treatment is commonly used to form a thin, rough, and porous oxidation layer on the surface of titanium. The purpose of this study was to investigate the formation of nanotubular titanium oxide arrays during short anodization processing. The specimen used in this study was 99.9% pure cp-Ti (ASTM Grade II) in the form of a disc with diameter of 15 mm and a thickness of 1 mm. A DC power supplier was used with the anodizing apparatus, and the titanium specimen and the platinum plate ($3mm{\times}4mm{\times}0.1mm$) were connected to an anode and cathode, respectively. The progressive formation of $TiO_2$ nanotubes was observed with FE-SEM (Field Emission Scanning Electron Microscopy). Highly ordered $TiO_2$ nanotubes were formed at a potential of 20 V in a solution of 1M $H_3PO_4$ + 1.5 wt.% HF for 10 minutes, corresponding with steady state processing. The diameters and the closed ends of $TiO_2$ nanotubes measured at a value of 50 cumulative percent were 100 nm and 120 nm, respectively. The $TiO_2$ nanotubes had lengths of 500 nm. As the anodization processing reached 10 minutes, the frequency distribution for the diameters and the closed ends of the $TiO_2$ nanotubes was gradually reduced. Short anodization processing for $TiO_2$ nanotubes of within 10 minutes was established.