Improvement of long-time creep life prediction of steam turbine rotor steel (증기 터빈축 강재의 장시간 크리프 수명 예측법 개선)

  • 오세규;정순억;전태언
    • Journal of Ocean Engineering and Technology
    • /
    • v.10 no.1
    • /
    • pp.47-52
    • /
    • 1996
  • This paper deals with a study on improvement of long-time creep life prediction of steam turbine rotor steels by using initial strain method as a new approach at high temperatures of 500 to 70$0^{\circ}C$ . The main result shows that the inital strain method could be reliably utilized to predict and evaluate the long-time creep life as creep rupture strength and that the predicting equation for long-time creep life under a certain creep stress at a certain high temperature could be empirically derived out from each initial instantaneous strain measured.

  • PDF

Creep-Fatigue Life Design with Various Stress and Temperature Conditions on the Basis of Lethargy Coefficient (응력 및 온도 변화시 무기력계수를 이용한 크리프-피로 수명설계)

  • Park, Jung-Eun;Yang, Sung-Mo;Han, Jae-Hee;Yu, Hyo-Sun
    • Transactions of the Korean Society of Mechanical Engineers A
    • /
    • v.35 no.2
    • /
    • pp.157-162
    • /
    • 2011
  • High temperature and stress are encounted in power plants and vehicle engines. Therefore, determination of the creep-fatigue life of a material is necessary prior to fabricating equipments. In this study, life design was determined on the basis of the lethargy coefficient for different temperatures, stress and rupture times. SP-Creep test data was compared with computed data. The SP-Creep test was performed to obtain the rupture time for X20CrMoV121 steel. The integration life equation was considered for three cases with various load, temperature and load-temperature. First, the lethargy coefficient was calculated by using the obtained rupture stress and the rupture time that were determined by carrying out the SP-Creep test. Next, life was predicted on the basis of the temperature condition. Finally, it was observed that life decreases considerably due to the coupling effect that results when fatigue and creep occur simultaneously.

Variability of Short Term Creep Rupture Time and Life Prediction in Stainless Steels (스테인리스 강의 단시간 크리프 파단시간의 변동성과 수명예측)

  • Jung, Won-Taek;Kong, Yu-Sik;Kim, Seon-Jin
    • Journal of Ocean Engineering and Technology
    • /
    • v.24 no.6
    • /
    • pp.97-102
    • /
    • 2010
  • This paper deals with the variability of short term creep rupture time based on previous creep rupture tests and the statistical methodology of the creep life prediction. The results of creep tests performed using constant uniaxial stresses at 600, 650, and $700^{\circ}C$ elevated temperatures were used for a statistical analysis of the inter-specimen variability of the short term creep rupture time. Even under carefully controlled identical testing conditions, the observed short-term creep rupture time showed obvious inter-specimen variability. The statistical aspect of the short term creep rupture time was analyzed using a Weibull statistical analysis. The effect of creep stress on the variability of the creep rupture time was decreased with an increase in the stress level. The effect of the temperature on the variability also decreased with increasing temperature. A long term creep life prediction method that considers this statistical variability is presented. The presented method is in good agreement with the Lason-Miller Parameter (LMP) life prediction method.

ISM에 의한 발전용 고온 배관재료 2.25Cr1Mo강의 고온 크리프 수명 예측에 관한 연구

  • Lee, Sang-Guk;Jeong, Min-Hwa;O, Se-Gyu;Song, Jeong-Geun
    • Journal of Ocean Engineering and Technology
    • /
    • v.12 no.2 s.28
    • /
    • pp.71-78
    • /
    • 1998
  • In this report for the assessment of creep properties of high-temperature tube materials in power plants, the long-time($10^4$~105h) creep life prediction by ISM for 2.25Cr1Mo steel was studied. It was clarified experimentally and quantitatively that the newly developed long-time creep life prediction equation was very coincident with the actual experimental data with high confidence, and the model was $t_r=\alpha\varepsilon_0^{\beta}\sigma^{-1}$.

  • PDF

New Considerations on Variability of Creep Rupture Data and Life Prediction (크리프 파단 데이터의 변동성에 대한 새로운 고찰과 수명예측)

  • Jung, Won-Taek;Kong, Yu-Sik;Kim, Seon-Jin
    • Transactions of the Korean Society of Mechanical Engineers A
    • /
    • v.33 no.10
    • /
    • pp.1119-1124
    • /
    • 2009
  • This paper deals with the variability analysis of short term creep rupture test data based on the previous creep rupture tests and the possibility of the creep life prediction. From creep tests performed by constant uniaxial stresses at 600, 650 and $700^{\circ}C$ elevated temperature, in order to investigate the variability of short-term creep rupture data, the creep curves were analyzed for normalized creep strain divided by initial strain. There are some variability in the creep rupture data. And, the difference between general creep curves and normalized creep curves were obtained. The effects of the creep rupture time (RT) and steady state creep rate (SSCR) on the Weibull distribution parameters were investigated. There were good relation between normal Weibull parameters and normalized Weibull parameters. Finally, the predicted creep life were compared with the Monkman-Grant model.

Creep Properties of Aircraft Gas Turbine Materials in relation to Heat Treatment (항공기용 가스터빈 재료의 열처리에 따른 크리프 특성)

  • Kong, Yu-Sik;Oh, Sae-Kyoo;Park, No-Kwang
    • Journal of Ocean Engineering and Technology
    • /
    • v.13 no.4 s.35
    • /
    • pp.112-117
    • /
    • 1999
  • In this paper, the creep properties and creep life prediction by Larson-Miller Parameter method for Udimet 720 to be used for aircraft gas turbine engines or other high temperature components were presented at the elevated temperatures of 538, 649 and $704^{\circ}C$. It was confirmed experimentally and quantitatively that a creep life predictive equation at such various high temperatures was well derived by LMP.

  • PDF

Creep Property Assessment and Creep Life Estimation for High-Temperature Tube Material(2.25Cr1Mo Steel) in Power Plants by LMP (발전용 고온 배관재료 2.25Cr1Mo 강의 크리프 특성과 LMP에 의한 크리프 수명의 예측)

  • Lee, Sang-Guk;Jeong, Min-Hwa;O, Se-Gyu;Song, Jeong-Geun
    • Journal of Ocean Engineering and Technology
    • /
    • v.12 no.2 s.28
    • /
    • pp.65-70
    • /
    • 1998
  • In this report, the creep properties and creep life estimation by Larson-Miller Parameter(LMP) Method for 2.25Cr1Mo steel to be used as power plant tubes or other components were presented at the high temperatures of 500, 550, and $600^{\circ}C$. It was confirmed experimentally and quantitatively that a creep life estimation equation at such various high temperatures was well derived by LMP and could be used very effectively within the creep life of 10$^3$ hours, but very unreliable and even dangerous for design in a long term of creep life such as 10$^4$ or $10^5$ hours.

  • PDF

Taylor Series-Based Long-Term Creep-Life Prediction of Alloy 617 (Taylor 급수를 이용한 617 합금의 장시간 크리프 수명 예측)

  • Yin, Song-Nan;Kim, Woo-Gon;Park, Jae-Young;Kim, Soen-Jin;Kim, Yong-Wan
    • Transactions of the Korean Society of Mechanical Engineers A
    • /
    • v.34 no.4
    • /
    • pp.457-465
    • /
    • 2010
  • In this study, a Taylor series (T-S) model based on the Arrhenius, McVetty, and Monkman-Grant equations was developed using a mathematical analysis. In order to reduce fitting errors, the McVetty equation was transformed by considering the first three terms of the Taylor series equation. The model parameters were accurately determined by a statistical technique of maximum likelihood estimation, and this model was applied to the creep data of alloy 617. The T-S model results showed better agreement with the experimental data than other models such as the Eno, exponential, and L-M models. In particular, the T-S model was converted into an isothermal Taylor series (IT-S) model that can predict the creep strength at a given temperature. It was identified that the estimations obtained using the converted ITS model was better than that obtained using the T-S model for predicting the long-term creep life of alloy 617.

Microstructural Evolution and Magnetic Property of Creep-Fatigued Ferritic 9Cr Heat-Resisting Steel (크리프-피로 손상된 페라이트기 9Cr 내열강의 미세조직 발달과 자기적 특성)

  • Kim, Chung-Seok;Kwun, S.I.;Park, Ik-Keun
    • Journal of the Korean Society for Nondestructive Testing
    • /
    • v.27 no.5
    • /
    • pp.417-425
    • /
    • 2007
  • The ferritic 9Cr-1Mo-V-Nb heat-resisting steel was experimentally studied in order to characterize its microstructural evolution during creep-fatigue by coercivity measurement. The creep-fatigue test was conducted at $550\;^{\circ}C$ with the tensile holding time of 60s and 600s, respectively. The coercivity decreased until the failure and the hardness monotonously decreased for the whole fatigue life. As the life fraction of creep-fatigue increased, the $M_{23}C_6$ carbide coarsened following the Ostwald ripening mechanism. However, the MX carbonitrides did not grow during creep-fatigue due to so stable at $550\;^{\circ}C$. The width of martensite lath increased because of the dislocation recovery at the lath boundaries. The magnetic coercivity has an influence on the microstructural properties such as dislocation, precipitates and martensite lath boundaries, which interpreted in relation to microstructural changes. Consequently, this study proposes a magnetic coercivity to quantify the level of damage and microstructural change during the creep-fatigue of ferritic 9Cr-1Mo-V-Nb steel.

Creep Life Prediction of Type 316LN Steel Using Minimum Commitment Method (최소구속법을 이용한 Type 316LN 강의 크리프 수명 예측)

  • Kim W.G.;Yoon S.N.;Ryu W.S.;Yi W.
    • Proceedings of the Korean Society of Precision Engineering Conference
    • /
    • 2005.10a
    • /
    • pp.295-298
    • /
    • 2005
  • A minimum commitment method (MCM) was applied to predict the creep rupture life of type 316LN SS. For this purpose, a number of the creep rupture data for the type 316LN SS were collected through literature survey and experimental data of KAERl, Using the short-term creep rupture data under 2000 hr, the long-term creep rupture life above $10^5$ hour was predicted by means of the MCM. An optimum value of A, P and G function, used in the MCM equation, was determined respectively, and the creep rupture life with the A values in different temperatures was compared with the experimental data and the predicted curves.