• Title/Summary/Keyword: 치과용 레진

Search Result 278, Processing Time 0.028 seconds

A NEW METHOD TO MEASURE THE LINEAR POLYMERIZATION SHRINKAGE OF COMPOSITES USING A PARTICLE TRACKING METHOD WITH COMPUTER VISION (컴퓨터 시각과 입자 추적 방법을 이용한 복합레진의 선형중합수축 측정의 새로운 방법)

  • Lee, In-Bog;Min, Sun-Hong;Seo, Deog-Gyu;Kim, Sun-Young;Kwon, Young-Chul
    • Restorative Dentistry and Endodontics
    • /
    • v.35 no.3
    • /
    • pp.180-187
    • /
    • 2010
  • Since the introduction of restorative dental composites, their physical properties have been significantly improved. However, polymerization shrinkage is still a major drawback. Many efforts have been made to develop a low shrinking composite, and silorane-based composites have recently been introduced into the market. In addition, many different methods have been developed to measure the polymerization shrinkage. In this study, we developed a new method to measure the linear polymerization shrinkage of composites without direct contact to a specimen using a particle tracking method with computer vision. The shrinkage kinetics of a commercial silorane-based composite (P90) and two conventional methacrylate-based composites (Z250 and Z350) were investigated and compared. The results were as follows: 1. The linear shrinkage of composites was 0.33-1.41%. Shrinkage was lowest for the silorane-based (P90) composite, and highest for the flowable Z350 composite. 2. The new instrument was able to measure the true linear shrinkage of composites in real time without sensitivity to the specimen preparation and geometry.

The influence of moisture control on bond strength of composite resin treated with self-etching adhesive system (Self-etching adhesive system에서 수분 조절이 레진의 치질접착강도에 미치는 영향)

  • Jin, Myoung-Uk;Kim, Young-Kyung;Park, Jeong-Won
    • Restorative Dentistry and Endodontics
    • /
    • v.27 no.4
    • /
    • pp.363-369
    • /
    • 2002
  • 최근에 많이 사용되어지고 있는 치과용 접착제는 산 부식 후 수분이 있는 상태에서 적용하는 wet-bonding 술식을 많이 추천하고 있다. 하지만 self-etching primer의 경우 산부식과 priming 과정이 동시에 시행되고, 제조자들은 건조된 치아표면에 적용할 것을 추천하고 있다. 그러나 건조된 정도에 대하여서는 별다른 추천사항이 없으며. 수분이 self-etching primer에 어떤 영향을 미치는지에 대하여서는 별다른 연구가 이루어져 있지 않은 상태이다. 이에 본 연구에서는 치질 삭제 후 남아있는 수분이 self-etching primer의 레진 접착 강도에 어떤 영향을 미치는 지를 알아보고자 하였다. 발거한 대구치 96개를 이용하여 물기가 있는 상태에서 #600 사포로 표면을 연마하고, 법랑질 면을 노출시킨 군과 상아질을 노출시킨 군으로 분류 후, 30분 공기 중 방치 군 (1군), 5초 공기 건조 군 (2군), 1초 공기 건조 군 (3군), 솜으로 약간의 물기를 제거한 군(blot dry) (4군) 등 총 8개의 군으로 나누었다. Self-etching adhesive system인 Clearfil SE Bond primer를 20초간 적용하고, bonding제 도포 후 10초간 광중합 시행하였다. 접착제 처리한 치아면에 몰드를 고정한 후 Clearfil AP-X 복합레진을 2mm 충전하고, 40초간 광중합을 시행하였다. 24시간 후 전단 응력 결합강도를 측정하였으며, 그 결과는 다음과 같이 나타났다. 법랑질과 상아질 모두에서, 30분 건조군과 5초 공기건조군이 1초와 blot drying 군보다 높은 결합강도를 보였으며 통계학적으로 유의한 차이를 보였다(p<0.05). 본 실험 결과에 의하면 self-etching adhesive system을 사용함에 있어서 법랑질과 상아질군 공히 건조된 상태에서 사용하여야 하며 수분의 존재시 치아와의 결합력이 감소하는 것으로 나타났다. 따라서 임상에서 접착제의 적용시 수분의 조절에 주의하여야 할 것으로 사료된다.

MICROLEAKAGE OF THE EXPERIMENTAL COMPOSITE RESIN WITH THREE COMPONENT PHOTOINITIATOR SYSTEMS (3종 광중합개시제를 함유한 실험용 복합레진의 미세누출도)

  • Kim, Ji-Hoon;Shin, Dong-Hoon
    • Restorative Dentistry and Endodontics
    • /
    • v.34 no.4
    • /
    • pp.333-339
    • /
    • 2009
  • This study was done to determine if there is any difference in microleakage between experimental composite resins, in which various proportions of three component photoinitiators (Camphoroquinone, OPPI, Amine) were included. Four kinds of experimental composite resin were made by mixing 3.2% silanated barium glass (78 wt.%, average size; 1 ${\mu}m$) with each monomer system including variously proportioned photoinitiator systems used for photoinitiating BisGMA/BisEMA/TEGDMA monomer blend (37.5:37.5:25 wt.%). The weight percentage of each component were as follows (in sequence Camphoroquinone, OPPI, Amine): Group A - 0.5%, 0%, 1% / Group B - 2%, 0.2%, 2% / Group C - 0.2%, 1%, 0.2% / Group D - 1%, 1%, 2%. Each composite resin was used as a filling material for round class V cavities (diameter: 2/3 of mesiodistal width; depth: 1.5 mm) made on extracted human premolars and they were polymerized using curing light unit (XL 2500, 3M ESPE) for 40 s with an intensity of 600 mW/$cm^2$. Teeth were thermocycled fivehundred times between $50^{\circ}C$and $550^{\circ}C$for 30s at each temperature. Electrical conductivity (${\mu}A$) was recorded two times (just after thermocycling and after three-month storage in saline solution) by electrochemical method. Microleakage scores of each group according to evaluation time were as follows [Group: at first record / at second record; unit (${\mu}A$)]: A: 3.80 (0.69) / 13.22 (4.48), B: 3.42 (1.33) / 18.84 (5.53), C: 4.18 (2.55) / 28.08 (7.75), D: 4.12 (1.86) / 7.41 (3.41). Just after thermocycling, there was no difference in microleakage between groups, however, group C showed the largest score after three-month storage. Although there seems to be no difference in microleakage between groups just after thermocycling, composite resin with highly concentrated initiation system or classical design (Camphoroquinone and Amine system) would be more desirable for minimizing microleakage after three-month storage.

HARDNESS OF COMPOSITE RESIN CURED BY HIGH INTENSITY HALOGEN LIGHT (고강도 할로겐광으로 중합한 복합레진 수복재의 경도)

  • Park, Jong-Seok;Lee, Kwang-Hee;Kim, Dae-Eup;Kim, Seong-Hyeong;Ahn, Ho-Young
    • Journal of the korean academy of Pediatric Dentistry
    • /
    • v.28 no.3
    • /
    • pp.471-479
    • /
    • 2001
  • The purpose of this study was to compare the effect of the high intensity halogen light $(850\sim1000mW/cm^2)$ with that of the conventional halogen light $(400mW/cm^2)$ on the hardness of composite resin. Three resin composites (Z-100, 3M, U.S.A. : Tetric Ceram, Vivadent, Liechtenstein; SureFil, Dentsply, U.S.A.) were filed in the stainless steel moulds which were 4mm in diameter and 2, 3, 4, and 5mm in depth, respectively. They were cured under the four different modes : (1) conventional mode, 40 seconds at $400mW/cm^2$; (2) 'ramp' mode, 10 seconds at 100 to $1000mW/cm^2$ plus 10 seconds at $1000mW/cm^2$; (3) 'boost' mode, 10 seconds at $1000mW/cm^2$; and (4) 'standard' mode, 20 seconds at $850mW/cm^2$. The surface hardnesses of the top and the bottom of the resin samples were measured with a microhardness tester (MXT70, Matsuzawa, Japan). The top surface hardness was not significantly different among the curing modes. The bottom surface hardness was generally the highest in the conventional mode and the lowest in the high intensity boost mode. There was no significant difference in the bottom surface hardness between the conventional mode and the high intensity standard mode in 2mm depth. The results suggest that the curing time of the high intensity halogen light $(850mW/cm^2)$ should be at least 20 seconds to produce the equal level of the bottom surface hardness of 2mm resin composite as compared to the hardness produced by the conventional halogen light $(400mW/cm^2)$.

  • PDF

Fracture and Wear Behavior of Dental Composite Resins Containing Prepolymerized Particle Fillers (유기복합필러를 함유하는 차과용 컴퍼짓 레진의 파괴와 마멸거동)

  • Kim, Yeong-Bin;Kim, Gyo-Han;Kim, Seok-Sam;Im, Jeong-Il
    • Transactions of the Korean Society of Mechanical Engineers A
    • /
    • v.24 no.2 s.173
    • /
    • pp.464-471
    • /
    • 2000
  • The fracture and wear behavior of dental composite resins containing prepolymerized particle fillers were investigated. Composite resins such as Metafil, Silux Plus, Heliomolar and Palfique Estelite were selected as specimens and contents of filler in specimens in order to evaluate the effect of prepolymerized particle fillers in fracture and wear characteristics. Ball on flat wear tester was used for the wear test at room temperature. The friction coefficient of Metafil was quite high relatively, and the wear resistances of Silux Plus and Palfique Estelite were better than those of Metafil and Heliomolar at the same experimental condition. It was found that the main wear mechanism was abrasive wear containing of plastic deformation of dental material.

MECHANICAL PROPERTIES AND ACOUSTIC EMISSION CHARACTERISTICS OF DENTAL COMPOSITE RESINS (치과용 복합레진의 기계적 성질과 AE특성)

  • Kim, Kyo-Han;Park, Jin-Hoon
    • Proceedings of the KOSOMBE Conference
    • /
    • v.1990 no.11
    • /
    • pp.64-67
    • /
    • 1990
  • Bending strength, bending elastic modulus ,and fracture toughness of different types of dental composite resins were deter mined. The relationship between bending strength, fracture toughness and filler volume fraction of dental composite resin was understood. In Acoustic Emission(AE) behavior during fracture toughness test, characteristic generation patterns of each type were understood. The fracture toughness values, AE generation patterns, and the nature of fracture surface were analyzed to understand fracture behavior of dental composite resin.

  • PDF

ESTHETIC RESTORATION OF FRACTURED IMMATURE PERMANENT INCISORS (파절된 미성숙 영구 전치의 수복)

  • Lee, In-Young;Kim, Hyun-Jung;Kim, Young-Jin;Nam, Sun-Hyun
    • Journal of the korean academy of Pediatric Dentistry
    • /
    • v.36 no.1
    • /
    • pp.126-132
    • /
    • 2009
  • Injuries of permanent teeth by trauma occur frequently in childhood and adolescence. Crown fractures are as frequent as 25-76% and especially maxillary incisors are prone to fractures. There have been numerous efforts to achieve both aesthetically and functionally satisfying restoration. When a mature tooth is fractured, porcelain crown or laminate veneer could be a choice of prosthodontic treatment. However, in a case of immature permanent incisor fracture, prosthodontic treatment is more complicated due to the immaturity of the tooth. Moreover, if endodontic treatment is accompanied with the prosthodontic treatment, the treatment period is prolonged. In the past, restoration using an orthodontic band, a ready-made crown, or glass ionomer cement did not exhibit esthetically satisfying result. As restorational materials have been improved, now more esthetic restoration is possible by reattaching fractured fragments or light-curing composite resin restoration. We reports cases of patients with fractured maxillary incisors and their successful treatment results through reattachment of fractured fragments and composite resin restoration.

  • PDF

A CLINICAL STUDY ON THE MAINTENANCE OF LIGHT INTENSITY OF VISIBLE-LIGHT CURING MACHINES FOR THE POLYMERIZATION OF COMPOSITE RESINS (복합레진 중합용 가시광선 광중합기의 적정 광강도 유지를 위한 임상적 고찰)

  • Lee, Dong-Soo;Jeong, Tae-Sung;Kim, Shin
    • Journal of the korean academy of Pediatric Dentistry
    • /
    • v.28 no.3
    • /
    • pp.363-368
    • /
    • 2001
  • It is well known that numerous factors influence the light output of curing units, but many dentists are un aware that the output of their curing lights are inadequate. This study was conducted to evaluate the light in tensity of visible-light curing units in some private dental clinics and hospital dental clinics. In order to determine the maximum light intensity of the curing units, lamps, filters and fiber optic bundles, they were replaced with new ones and light intensity was remeasured. Light intensity was measured by employing a digital radiometer (EFOS model #8000, USA). Light intensity ranged in $29\sim866mW/cm^2$ (below $150mW/cm^2$ ; 17.8%, $150\sim300mW/cm^2$ : 46.6%, above $300mW/cm^2$ ; 35.6%). The replacement of the components increased the light intensity, with maximum increases of 94.8% for lamps, 82.3% for filters, 200.8% for fiber optics and 361.5% for all three parts. According to the manufacturer of radiometer, curing light is considered as unsuitable for use with a reading of above $300mW/cm^2$ by the radiometer. Applying these criteria to the present study, 64.4% of the curing units required repair or replacement. The results of this study indicated that the light intensities of the curing units used in dental practice were lower than optimum level.

  • PDF

A study on marginal fit of the ceramic-based hybrid resin restoration for dental CAD/CAM systems (치과용 CAD/CAM 전용 세라믹기반 하이브리드 레진 수복물의 변연 적합 연구)

  • Jeong, Chang-Seop;Park, Jong-Kyoung
    • Journal of Technologic Dentistry
    • /
    • v.42 no.3
    • /
    • pp.228-233
    • /
    • 2020
  • Purpose: This study aimed to assess and compare the marginal fit of ceramic-based hybrid resin restoration (HYB) and zirconia restoration (ZIR) for dental computer-aided design/computer-aided manufacturing systems. Methods: A stainless steel master model was produced. The impression was first made with silicone, and then stone working models were produced. A total of twenty restorations were fabricated with two different materials: ZIR and HYB. The silicone film thickness of the marginal gap was measured using a digital microscope; digital photos were taken at a magnification of ×160, and then analyzed using a measurement software. The values of the result were evaluated with the independent-sample t-test (α=0.05). All statistical analyses were performed with a statistical software. Results: The mean values for the marginal gap was 37.14±2.96 ㎛ for HYB, compared with 40.37±5.26 ㎛ for ZIR. No significant difference was found between ZIR and HYB (p=0.107). Conclusion: As a result, the marginal fit of the restoration fabricated using the hybrid resin was better than that of the restoration fabricated using zirconia. Also, the marginal fit of all groups was below the clinical acceptable range of 120 ㎛. Thus, HYB for dental CAD/CAM system in this study is expected to be suitable for clinical use in dentistry.

Physical Properties of Light Cured Dental Composite Resin with Novel Photosensitizers (새로운 광증감제를 사용한 치과용 광중합형 복합레진의 기계적 특성)

  • Sun, Gum-Ju;Lee, Hee-Kyung
    • Journal of Technologic Dentistry
    • /
    • v.35 no.4
    • /
    • pp.313-320
    • /
    • 2013
  • Purpose: The purpose of this study was to know the physical properties of UDMA dental composite resins containing two photosensitizers, PD, DA, as a photosensitizer instead of CQ. We want to know Remaining Double Bond(RDB) of UDMA unfilled resin and diametral tensile strength and flexural strength of composite resin containing PD and DA were compared with those of CQ, most widely used photosensitizer for dental composite resins. Methods: The RDB of UDMA studied by FT-IR spectroscopy increased with irradiation time. The composite resins were tested for their physical properties. The dental composite resins were made with UDMA as a monomer, silanized silica as filler, N,N-dimethylaminoethyl methacrylate (DAEM) as amine initiator, and one of the two kinds of new photosensitizers. Results: The relative RDB of UDMA was in the order: DA > CQ > PD but the physical properties of the composite resins show PD and DA with higher results compared with that containing CQ. The reason for the results is that PD and DA serve not only as a photosensitizer but also as a photo-crosslinking agent. Conclusion: PD and DA show as effective photosensizers, suitable for UDMA dental composite resin compare with a higher efficiency than CQ.