• Title/Summary/Keyword: 초전계수

Search Result 48, Processing Time 0.024 seconds

A Study on Vibration Characteristics of Flywheel Energy Storage System Using Superconducting Magnetic Bearings (초전도자기베어링을 이용한 플라이휠 에너지 저장장치의 진동특성에 관한 연구)

  • 김종수;이수훈
    • Journal of the Korean Society for Precision Engineering
    • /
    • v.15 no.2
    • /
    • pp.170-177
    • /
    • 1998
  • The purpose of superconducting magnetic bearing flywheel energy storage system(SMB-FESS) is to store unused nighttime electricity as kinetic energy and convert it to electricity during daytime. The SMB-FESS is proposed as an efficient energy storage system because there is no mechanical problems, such as friction and wear The flywheel over SMB is rotated at a high speed, 50,000rpm. The major source of energy loss in the SMB-FESS is vibration of flywheel. Therefore, the vibration characteristics of SMB-FESS should be identified. In this study, the axial/radial stiffness and damping coefficient of SMB are measured by a vibration test. Natural frequencies and natural modes of flywheel and magnet are analyzed by a finite element method. The modal analysis of system is performed using the modal parameters of each component and the measured stiffness/damping coefficient. So, natural at frequencies and mode shapes of the joined system can be obtained. According to critical speed analysis, the system has two rigid conical modes in the low speed range. Nevertheless, the system has not been affected by the critical speed in the main operating range.

  • PDF

Diffus ion-Weighted MR Imaging of Spinal Cord Infarction (척수경색의 확산강조자기공명영상)

  • 김윤정;서정진;임남열;정태웅;김윤현;박진균;정광우;강형근
    • Investigative Magnetic Resonance Imaging
    • /
    • v.6 no.2
    • /
    • pp.166-172
    • /
    • 2002
  • Purpose : To evaluate the usefulness of diffusion-weighted imaging(DWI) and quantitative apparent diffusion coefficient (ADC) maps in the patients with spinal cord infarction. Materials and methods : We studied 6 patients presented symptoms with spinal cord infarction, retrospectively (3 men and 3 women). We obtained multi-shot echo planar-based, DWI using 1.5T MR scanner at 5.4 mean days after the onset of ischemic symptoms. In six patients, signal intensity was acquired at conventional b value $1000s/\textrm{mm}^2$). The ADC value for the normal spinal cord and for infarcted lesions was measured from the trace ADC maps by using regions of interest positioned over the spinal cord. We analyzed signal intensity of lesion on MRI and DWI, and compared with ADC values in infarcted lesions and normal site. Results : T1-weighted MR image showed isosignal intensity in four of six patients and low signal intensity in two of six. T2-weighted MR image demonstrated high signal intensity in all of six. All DWI were considered to be diagnostic. All of six depicted a bright signal intensity on DWI. ADC values of infarcted lesion were measured lower than that of normal spinal cord on ADC map. The differences in ADC values between infarcted and normal spinal cord were significantly different (p<0.05). Conclusion : It is possible to obtain DWI and ADC map of the spinal cord and DWI may be useful in the early diagnosis and localization of lesion site in patients with spinal cord infarction.

  • PDF

Equivalent Mechanical and Thermal Properties of Multiphase Superconducting Coil Using Finite Element Analysis (유한요소해석을 이용한 다상의 초전도 코일에 대한 기계적 열적 등가 물성)

  • Sa, J.W.;Her, N.I.;Choi, C.H.;Oh, Y.K.;Cho, S.;Do, C.J.;Kwon, M.;Lee, G.S.
    • Proceedings of the KSME Conference
    • /
    • 2001.06a
    • /
    • pp.975-980
    • /
    • 2001
  • Like composite material. the coil winding pack of the KSTAR (Korea Superconducting Tokamak Advanced Research) consist of multiphase element such as metallic jacket material for protecting superconducting cable, vacuum pressurized imprepregnated (VPI) insulation, and corner roving filler. For jacket material, four CS (Central Solenoid) Coils, $5^{th}$ PF (Poloidal Field) Coil, and TF (Toroidal Field Coil) use Incoloy 908 and $6-7^{th}$ PF coil, Cold worked 316LN. In order to analyze the global behavior of large coil support structure with coil winding pack, it is required to replace the winding pack to monolithic matter with the equivalent mechanical properties, i.e. Young's moduli, shear moduli due to constraint of total nodes number and element numbers. In this study, Equivalent Young's moduli, shear moduli, Poisson's ratio, and thermal expansion coefficient were calculated for all coil winding pack using Finite Element Method.

  • PDF

Electrical properties of 0.05pb($Sn_{0.5}Sb_{0.5}O_3-xPbTiO_3-yPbZrO_3$ PZT System With variation Of PT/PZ (0.05pb($Sn_{0.5}Sb_{0.5}O_3-xPbTiO_3-yPbZrO_3$계에서 PT/PZ비 변화에 따른 전기적 특성)

  • 황학인;박준식;오근호
    • Journal of the Korean Crystal Growth and Crystal Technology
    • /
    • v.7 no.4
    • /
    • pp.589-598
    • /
    • 1997
  • The effects of PT/PZ ratio variations in a modified PZT system on crystal structure and electrical properties were studied. $0.05Pb(Sn_{0.5}Sb_{0.5})O_3+xPbTiO_3+yPbZrO_3$+0.4Wt% $MnO_2$(=0.55PSS+0.11PT+0.84PZ+0.4wt%$MnO_2$ ; x+y=0.95) systems with variations of PT/PZ from 0.50/0.45 to 0.l1/0.84 were sintered at $1250^{\circ}C$ for 2 hr, and then sintering density, crystal structure, dielctric, piezoelectric, pyroelectic and voltage responsity to infrared were investigated. Sintering density was increased from 7.52g/$\textrm {cm}^3$ to 7.82g/$\textrm {cm}^3$ with increasing PZ content. Dielectric constants at 1 KHz were decreased from 1147 to 193 with variation of PT/PZ from 0.50/0.45 to 0.l1/0.84 after poling of $4 KV_{DC}$/mm at $140^{\circ}C$ for 20 minutes. All Dielectric losses at 1 KHz were less than 1 % in all specimens. $K_{p}$ was increased near to 1 of PT/PZ, and maximun value of 48.2 % was .at 0.45/0.50. Pyroelectric coefficient of PT/PZ with 0.l1/0.84 was maximun value, 0.0541 C/$\m^2$K, and voltage responsity to infrared was 1.5 V.

  • PDF

Effect of $\delta$'Phase on the Aging Behavior and the Tensile Property of AI-2.5wt%Li Alloy (Al-2.5wt%Li합금의 시효거동과 인장성질에 미치는 $\delta$'상의 영향)

  • Yu, Chang-Yeong;Lee, Min-Sang
    • Korean Journal of Materials Research
    • /
    • v.7 no.8
    • /
    • pp.701-706
    • /
    • 1997
  • AI-2.5wt%Li 합금을 시효처리하여 시효거동과 인장성질에 미치는 $\delta$' 상의 영향을 조사하였다. $\delta$' 상의 입자 반경은 시효 시간의 1/3승에 비례하여 조대화하였다. $\delta$' 상과 기지상과의 계면에너지는 0.0073 J/$m^2$, 확산계수는 1.42$\textrm{cm}^2$/sec, 초대화 거동은 MLSW이론에 부합됨을 알 수 있었다. 미세하고 균일하게 분포한 $\delta$'상은 전반적으로 인장강도의 상승을 가져왔으며, 평형상인 $\delta$상의 석출과 이로 인한 무석출물대의 존재로 과시효시 강도가 감소하였다. 인장변형시 전위는 초전위로 아시효와 피크시효시에는 $\delta$'상을 전단하지만 과시효시에는 $\delta$'상을 전단하지 못하고 우회하여 전위루우프를 형성한다.

  • PDF

Analysis of Sticking Coefficient in Bi-Superconducting Thin film (Bi 초전도 박막의 부착계수 해석)

  • 천민우;박용필;이성일
    • Journal of the Korean Institute of Electrical and Electronic Material Engineers
    • /
    • v.15 no.11
    • /
    • pp.997-1002
    • /
    • 2002
  • BSCCO thin films are fabricated by an ion beam sputtering method, and sticking coefficients of the respective elements are evaluated. The sticking coefficient of Bi element in BSCCO film formation was observed to show a unique temperature dependence; it was almost a constant value of 0.49 below about 730$^{\circ}C$ and decreased linearly over about 730$^{\circ}C$ In contrast, Sr and Ca, displayed no such remarkable temperature dependence. This behavior of the sticking coefficient was explained consistently on the basis of the evaporation and sublimation processes of Bi$\sub$2/O$\sub$3/. It was concluded that Bi(2212) thin film constructs from the partial melted Bi(2201) phase with the aid of the liquid phase of Bi$\sub$2/O$\sub$3/.

Crystalline and Electrical Properties of (Pb, La)TiO3 Ferroelectric Films ((Pb,La) TiO3 강유전체막의 결정성과 전기적특성)

  • 장호정
    • Journal of the Microelectronics and Packaging Society
    • /
    • v.5 no.2
    • /
    • pp.59-64
    • /
    • 1998
  • Pt/SiO2/Si 기판구조위에 스크린인쇄법과 졸-겔법에 의해 (Pb, La)TiO3(PLT) 후막 과 박막을 도포시켜 $650^{\circ}C$후속열처리 온도에서 결정화한후 결정특성과 전기적 특성을 조사 하였다. $650^{\circ}C$ 온도에서 후속열처리된 PLT 시료의 경우 전형적인 perovskite 결정구조를 보 여주었다. SEM 단면형상으로부터 Pt 전극과 PLT막 사이에는 비교적 평활한 계면형상을 보여주었다. PLT 후막과 박막시료의 잔류분극(2Pr) 값은 약 1$\mu$C/cm2 으로각각 나타났으며 이와같이 후막 PLT시료에 비해 박막시료의 잔류분극값이 큰이유는 박막시료가 보다 양호 한 결정성을 지니기 때문이었다. 상온부근에서 후막과 박막시료의 초전계수값은 약 1.5nC/cm2.$^{\circ}C$와 4.0nC/cm2.$^{\circ}C$의 값을 각각 나타내었으며 누설전류의 크기는 약 0.3~0.8$\mu$ A/cm2의 비교적 양호한 누설전류 특성을 얻었다.

Analysis of Sticking Coefficient in BSCCO Superconductor Thin Film Fabricated by Co-deposition (공증착법으로 제작한 BSCCO 초전도 박막의 부착계수 해석)

  • An, In-Soon;Chun, Min-Woo;Park, Yong-Pil
    • Proceedings of the Korean Institute of Electrical and Electronic Material Engineers Conference
    • /
    • 2001.11b
    • /
    • pp.300-303
    • /
    • 2001
  • BSCCO thin films are fabricated via a co-deposition process by an ion beam sputtering with an ultra-low growth rate, and sticking coefficients of the respective elements are evaluated. The sticking coefficient of Bi element exhibits a characteristic temperature dependence : almost a constant value of 0.49 below $730^{\circ}C$ and decreases linearly with temperature over $730^{\circ}C$. This temperature dependence can be elucidated from the evaporation and sublimation rates of bismuth oxide, $Bi_{2}O_{3}$, from the film surface. It is considered that the liquid phase of the bismuth oxide plays an important role in the Bi 2212 phase formation in the co-deposition process.

  • PDF

Analysis of Sticking Coefficient in BSCCO Superconductor Thin Film Fabricated by Co-deposition (공증착법으로 제작한 BSCCO 초전도 박막의 부착계수 해석)

  • 안인순;천민우;박용필
    • Proceedings of the Korean Institute of Electrical and Electronic Material Engineers Conference
    • /
    • 2001.11a
    • /
    • pp.300-303
    • /
    • 2001
  • BSCCO thin films are fabricated via a co-deposition process by an ion beam sputtering with an ultra-low growth rate, and sticking coefficients of the respective elements are evaluated. The sticking coefficient of Bi element exhibits a characteristic temperature dependence : almost a constant value of 0.49 below 730$^{\circ}C$ and decreases linearly with temperature over 730$^{\circ}C$. This temperature dependence can be elucidated from the evaporation and sublimation rates of bismuth oxide, Bi$_2$O$_3$, from the film surface. It is considered that the liquid phase of the bismuth oxide plays an important role in the Bi 2212 phase formation in the co-deposition process.

  • PDF

Development of HTS-FCL Location Selection Program using Sensitivity Factor (감도계수를 고려한 초전도한류기의 계통적용점 선정 연구)

  • Choi, Heung-Kwan;Yoon, Jae-Young;Kim, Jong-Yeul;Lee, Seung-Ryul;Lee, Byong-Jun
    • Proceedings of the KIEE Conference
    • /
    • 2004.11b
    • /
    • pp.240-242
    • /
    • 2004
  • Maximum short circuit current of modern power system is becoming so large that the current should transmission capability. Although there are various kinds of method to solve this, approached from super conductivity Fault Current Limiter application viewpoint among them. High Temperature Superconductor-Fault Current Limiter (HTS-FCL) development is progressing according to HTS technology development, and system application is tried. For actual system application of such super conductivity FCL, an more efficient method was developed to find suitable FCL application locations using sensitivity factor comparing previous paper.

  • PDF