Fracture Mechanism and Characterization of Falling Weight Impact in CF/Epoxy Composite Plates Under Law-Velocity Impact (저속충격 하에서 CFRP 복합적층판의 낙추 충격특성과 파괴기구)

  • 임광희;박노식;김영남;김선규;심재기;양인영
    • Composites Research
    • /
    • v.17 no.4
    • /
    • pp.53-60
    • /
    • 2004
  • This paper describes a method for a falling weight impact test to estimate the impact energy absorbing characteristics and impact strength of CFRP laminate plates based on considerations of stress wave propagation theory. The absorbed energy of T300 orthotropic composites is higher than that of quasi-isotropic specimen over impact energy 6.8J, but in case of using T700 fiber, much difference does not show. Also, absorbed energy of T300 orthotropic composites, which are composed of the same stacking number and orientation became more than that of T700 fiber specimen; however there was no big difference in case of quasi-isotropic specimens. The delamination areas of the impacted specimen were measured with the ultrasonic C-scanner to find correlation between impact energy and delamination area. The fracture surfaces were observed by using the SEM (scanning electron microscope) through a low-velocity impact test in order to confirm the fracture mechanism.

Preparation of Cellulose Nanoparticles Loaded with Vitamin E Acetate (비타민 E 아세테이트가 봉입된 셀룰로오스 나노입자의 제조)

  • 남다은;정택규;김승수;신채호;신병철
    • Polymer(Korea)
    • /
    • v.28 no.2
    • /
    • pp.128-134
    • /
    • 2004
  • Cellulose nanoparticles loaded with vitamin I acetate were prepared by modified spantaneous emulsification solvent diffusion method. After cellulose derivatives were dissolved in mixed acetone/ethanol organic solvent with vitamin E acetate, cellulose nanoparticle suspensions were dispersed in poly(oxyethylene sorbitane monooleate) solution using ultrasonicator. Particle size and loading amount of vitamin I acetate were measured by particle size analyser and UV-spectrometer, respectively. The stability of nanoparticle was determined by measuring the change of the particle size at room temperature for 30 days and the morphology was observed by SEM. Morphology of cellulose nanoparticles was spherical and particle size was not changed at room temperature for 30 days. The optimum condition for the preparation of cellulose nanoparticles was 1% w/v cellulose nitrate with 8% w/v poly(oxyethylene sorbitane monooleate) solution. It showed that particle size and loading amount of vitamin E acetate was 65nm and 71%, respectively.

Properties of TiN Thin Films Synthesized with HiPIMS and DC Sputtering (HiPIMS와 DC 스퍼터링으로 제조한 TiN 박막 특성)

  • Yang, Ji-Hun;Byeon, In-Seop;Kim, Seong-Hwan;Jeong, Jae-In
    • Proceedings of the Korean Institute of Surface Engineering Conference
    • /
    • 2017.05a
    • /
    • pp.93-93
    • /
    • 2017
  • 고전력 펄스 전원공급장치를 이용한 마그네트론 스퍼터링(high-power impulse magnetron sputtering; HiPIMS)과 직류(direct current; DC) 전원공급장치를 이용한 마그네트론 스퍼터링(DC 스퍼터링)을 이용하여 제조한 티타늄 질화물(titanium nitride; TiN) 박막의 특성을 비교하였다. HiPIMS와 DC 스퍼터링 공정 중에 빗각증착을 적용하여 TiN 박막의 미세구조와 기계적 특성의 변화를 확인하였다. TiN 박막을 코팅하기 위한 기판으로 스테인리스 강판(SUS304)과 초경(cemented carbide; WC-10wt.%Co)을 사용하였다. 기판은 알코올과 아세톤으로 초음파 처리를 실시하여 기판 표면의 불순물을 제거하였다. 기판 청정 후 진공용기 내부의 기판홀더에 기판을 장착하고 $2.0{\times}10^{-5}torr$의 기본 압력까지 진공배기를 실시하였다. 진공 용기의 압력이 기본 압력에 도달하면 아르곤(Ar) 가스를 진공용기 내부로 ${\sim}10^{-2}torr$의 압력으로 주입하고 기판홀더에 라디오 주파수(radio frequency; rf) 전원공급장치를 이용하여 - 800 V의 전압을 인가하여 글로우 방전을 발생시켜 30 분간 기판 표면의 산화막을 제거하는 기판청정을 실시하였다. 기판청정이 완료되면 기본 압력까지 진공배기를 실시하고 Ar과 질소($N_2$)의 혼합 가스를 진공용기 내부로 ${\sim}10^{-3}torr$의 압력으로 주입하여 HiPIMS와 DC 스퍼터링으로 TiN 박막 제조를 실시하였다. 빗각의 크기는 $45^{\circ}$$-45^{\circ}$이었다. 제조된 TiN 박막은 주사전자 현미경, 비커스 경도 측정기 그리고 X-선 회절 분석기를 이용하여 특성을 분석하였다. HiPIMS로 제조한 TiN 박막은 기판 전압을 인가하지 않아도 색상이 노란색을 보이지만, DC 스퍼터링으로 제조한 TiN 박막은 기판 전압을 인가하지 않으면 노란색을 보이지 않고 어두운 갈색에 가까운 색을 보였다. TiN 박막의 경도는 HiPIMS로 제조한 TiN 박막이 DC 스퍼터링으로 제조한 TiN 박막보다 높았다. 이러한 TiN 박막의 특성 차이는 DC 스퍼터링과 비교하여 높은 HiPIMS의 이온화율에 의한 결과로 판단된다. 빗각을 적용한 TiN 박막은 미세구조 변화를 보였으며 이러한 미세구조 변화는 TiN 박막의 특성에 영향을 미치는 것을 확인하였다.

  • PDF

Preparation and Characterization of Zaltoprofen-Loaded Polyoxalate Microspheres for Control Release (방출제어를 위한 잘토프로펜이 함유된 폴리옥살레이트 미립구의 제조와 특성)

  • Kim, Kyoung Hee;Lee, Cheon Jung;Jo, Sun A;Lee, Jung Hwan;Jang, Ji Eun;Lee, Dongwon;Kwon, Soon Yong;Chung, Jin Wha;Khang, Gilson
    • Polymer(Korea)
    • /
    • v.37 no.6
    • /
    • pp.702-710
    • /
    • 2013
  • Zaltoprofen loaded polyoxalate (POX) microspheres were prepared by an emulsion solvent-evaporation/extraction method like oil-in-water (O/W) for sustained release of zaltoprofen. The influence of several preparation parameters such as fabrication temperature, stirring speed, intensity of the sonication, initial drug ratio, molecular weight ($M_w$) of POX, concentration of POX and concentration of emulsifier has been investigated on the zaltoprofen release profiles. Physicochemical properties and morphology of zaltoprofen loaded POX microspheres were investigated by scanning electron microscopy (SEM), X-ray diffraction (XRD), differential scanning calorimeter (DSC) and Fourier transform infrared (FTIR). Through the analyzed results, it was demonstrated that the characteristics of the microspheres greatly affected by the prepared condition. The releases behavior of zaltoprofen was investigated for 10 days in vitro. It was confirmed that the release behavior of zaltoprofen can be controlled by the manufacturing factor of solvent-evaporation/extraction method.

Friction Welding of Ni-Base ODS Alloy Prepared by Mechanical Alloying (기계적 합금법으로 제조된 Ni기 산화물 분산강화 합금의 마찰압접에 관한 연구)

  • 강지훈;박성계;김지순;권영순
    • Proceedings of the Korean Powder Metallurgy Institute Conference
    • /
    • 1994.10b
    • /
    • pp.15-15
    • /
    • 1994
  • M MA ODS 합금의 보다 폭넓용 실용확훌 위해 크게 요구되고 있는 적정 접합기술 개발의 한 방안£로, 마찰압접(Friction Welding) 방법의 가능성옳 조사하기 위하여 마찰압력과 시간, 마 찰 후 접촉압력(Upset Pressure) 풍을 다양하게 변화시켜 접합체톨 제조한 후, 접합체 강도에 대한 인장시험과 접합계연의 결합 및 미세구조에 대한 현미경 관찰, EDS에 의한 원소분석, 접 합이옴부의 경도분포와 파단면 분석 풍율 행하였다. 실험에 사용된 모재는 기계적 합금법으로 제조된 Inca사의 Ni기 MA 754 합금이었으며, 직경 l 10 mm, 길이 50 mm로 가공한 후, 아세통£로 초음파 세척하여 접합에 사용하였다. 접합온 브 레이크식 마찰압접기틀 사용하여 행하였으며, 회전시험편의 회전수는 2400 rpm이었A며, 다른 한쪽의 고정시험편과의 마찰압력 및 마찰시간온 각각 50 - 500 MPa과 1-5초로, 또한 업셋압 력도 50 - 600 MPa로 변화시켰다. 이때 업셋압력은 모든 시편에 대해 일정하게 6초동안 가하 였다. 얻어진 접합체는 각 압접조건 당 2개 이상의 접합시험편에 대해 상온 인장강도톨 측정하 였으며, 파단이 일어난 위치를 확인한 후 파면에 대한 분석율 주사전자현미경(SEM)과 에너지 분산형 분광분석기mDS)릎 사용하여 행하였다. 컵합이옴부의 첩합성올 확인하기 위하여, 접합 체를 접합변에 수직으로 절단, 연마한 후 광학현미경과 SEM, EDS 퉁으로 관찰, 분석하여 접 합부의 형상과 결합형성 여부, 접합계면의 미세조직 퉁옳 조사하였다. 또한 마찰압접에 따론 모재와 접합계연부의 경도분포훌 접합이옴부로부터 모재쪽으로 일정 간격율 두어 마이크로 비 커스 경도기로 측정, 조사하였다. 이상의 설험 결과, 다옴과 같온 결론옳 얻었다. ( (1) 접합체 강도가 모채 강도의 95% 이상이 되는 양호한 렵합체흩 얻기 위한 마찰압력 조건 온, 2400 rpm의 회전속도와 6초의 업셋압력 유지시간에서 마찰압력과 업셋압력, 그리고 마찰시 간이 각각 400 MPa 이상과 500 MPa 이상,2초입율 확인하였다. ( (2) 컵합이옴부의 관찰 결과, 모든 마찰압접 조건에서 컵합이옴부는, 기폰 모재의 texture 조직 을 유지하고 있는 모재부 영역(영역 ill)과 첩합계면부에 인접하여 업셋압력이 주어질 때 단조 효과에 의해 계연 외부로 metal flow가 일어나면서 형성된 영역 II, 매우 미세한 결정립으로 구성된 중앙부의 영역 1 로 이투어져 있옴융 확인하였다. ( (3) 최적접합조건이 충족되지 않온 경우, 접합부의 영역 I 에서 관찰된 void와 균열, 불균일한 접합계면 통의 접합결함에 Al과 Y. Ti 퉁£로 구성된 산화물률이 용집되어 있옴을 확인하였 다-( (4) 접합체의 파단 양상온 크게 접합부 파단과 모재부 파단, 이률의 혼합형 파단i로 나눌수 있었다. 모재부 파단의 경우, 파단면이 매끄럽고 파변상의 결정립도 매우 미세하였으며, 산확물 의 용집도 찾아보기 어려웠 나, 접합부 파단의 경우에는 파변의 굴곡이 비교척 심하고 연성 입계파괴의 형태를 보였£며, 결정립도 모채부 파단의 경우에 비해 조대하였다. 조대하였다.

  • PDF

Evaluation of titanium surface properties by $Nd:YVO_4$ laser irradiation: pilot study ($Nd:YVO_4$ 레이저 조사에 따른 티타늄의 표면특성 평가: 예비 연구)

  • Kim, Ae-Ra;Park, Ji-Yoon;Kim, Yeon;Jun, Sei-Won;Seo, Yoon-Jeong;Park, Sang-Won
    • The Journal of Korean Academy of Prosthodontics
    • /
    • v.51 no.3
    • /
    • pp.167-174
    • /
    • 2013
  • Purpose: This study was conducted to evaluate the roughness and surface alternations of three differently blasted titanium discs treated by $Nd:YVO_4$ Laser irradiation in different conditions. Materials and methods: Thirty commercially pure titanium discs were prepared and divided into three groups. Each group was consisted of 10 samples and blasted by $ZrO_2$ (zirconium dioxide), $Al_2O_3$ (aluminum oxide), and RBM (resorbable blasted media). All the samples were degreased by ultrasonic cleaner afterward. Nine different conditions were established by changing scanning speed (100, 300, 500 mm/s) and repetition rate (5, 15, 35 kHz) of $Nd:YVO_4$ Laser (Laser Pro D-20, Laserval $Korea^{(R)}$, Seoul, South Korea). After laser irradiation, a scanning electron microscope, X-ray diffraction analysis, energy dispersive X-ray spectroscopic analysis, and surface roughness analysis were used to assess the roughness and surface alternations of the samples. Results: According to a scanning electron microscope (SEM), titanium discs treated with laser irradiation showed characteristic patterns in contrast to the control which showed irregular patterns. According to the X-ray diffraction analysis, only $Al_2O_3$ group showed its own peak. The oxidation tendency and surface roughness of titanium were similar to the control in the energy dispersive X-ray spectroscopic analysis. The surface roughness was inversely proportional to the scanning speed, whereas proportional to the repetition rate of $Nd:YVO_4$. Conclusion: The surface microstructures and roughness of the test discs were modified by the radiation of $Nd:YVO_4$ laser. Therefore, laser irradiation could be considered one of the methods to modify implant surfaces for the enhancement of osseointegration.

Effect of Unilateral Renal Perfusion of Cyclosporine and Mitomycin on Rat's Kidney (Cyclosporine과 Mitomycin의 일측성 신관류로 초래되는 백서 신병변에 관한 연구)

  • Baek Seung In;Lim Hyun Suk;Shin Weon Hye;Ko Cheol Woo;Koo Ja Hoon;Kwak Jung Sik
    • Childhood Kidney Diseases
    • /
    • v.2 no.2
    • /
    • pp.138-144
    • /
    • 1998
  • Purpose : The use of cyclosporine and mitomycin in various immunologic or neoplastic disorders has been known to cause wide-ranged nephrotoxic effects including thrombotic microangiopathy. However, the mechanism of nephrotoxicity of these drugs has not been studied adequately, so that present experimental study has been undertaken to find out whether these drugs can cause direct damage to the kidney and to clarify the pathogenetic mechanism of nephrotoxic effect of these drugs. Materials and methods : Sprague-Dawley rats weighing 250-300 gm were used for experimental animals and unilateral renal perfusion technique, modified from the method described by Hoyer et al was used. Isolation of left kidney from systemic circulation was made by clamping aorta and left renal vein and a hole was punctured in the anterior wall of the left renal vein. Cyclosporine (2.5 mg in 4 ml solution) and mitomycin (1.6 mg in 4ml solution) were infused through left renal artery and normal saline was used in control rats. Forty-eight hours after infusion of the drugs, animals were sacrificed and left kidney removed and processed for histologic examination. Total ischemic time of left kidney was less than 15 minutes: Results : Cyclosporine-perfused group showed severe swelling of glomerular endothelial ceil along with swelling of glomerular epithelial cell and interstitial vascular endothelial cell. Mitomycin-perfused group also showed severe swelling of glomerular endothelial and epithelial cells. And in addition to these findings, they demonstrated platelets aggregation, swelling and degranulation of platelets and fibrin accumulation in some of the capillaries, indicating occurrance of thrombotic microangiopathy. Conclusion : present experiment indicates that cyclosporine and mitomycin can cause direct toxic injury to renal endothelial cell. And this direct toxic damage to endothelial cell seems to be an important initiating event for the development of thrombotic microangiopathy.

  • PDF

Investigation on the optical, structural and electrical properties of the RF sputtered layers obtained from CuInSe2 single precursors (CuInSe2 단일전구체에서 스퍼터링된 박막의 광학적, 구조적 및 전기적 특성평가)

  • Jeong, Chaehwan;Kim, Saerok;Kim, Jinhyeok;Kim, Kwangbok
    • 한국신재생에너지학회:학술대회논문집
    • /
    • 2010.06a
    • /
    • pp.78.2-78.2
    • /
    • 2010
  • Cu(In,Ga)Se2 (CIGS)박막태양전지는 간단한구조와 가격경쟁력 및 고효율화 가능성에 대한 기대감에 의해 많은 연구가 수행되어오고 있다. 특히 높은 흡수계수와 적절한 밴드갭, 큰 결정크기와 같은 물질의 특성들이 장점으로 작용하고 있기 때문이다. 또한 CIGS박막태양전지는 다른 태양전지에 비해 광열화가 적다는 장점도 가지고 있다. CIGS 박막은 CuInSe2내의 In 사이트에 Ga을 도핑함으로서 형성이 되는데 그때의 밴드갭은 약 1.4eV이며 이를 형성하기 위해 많은 방법들이 제안되고 있는데, CIGS박막 형성 시 가장 중요시 여겨야 될 인자는 구성원소로부터 최적화된 조성비를 찾는 것이다. 이러한 관점에서 볼때 evaporation법이나 sputtering법같은 진공방식의 공정법이 비진공방식에 비해 최적의 조성비를 찾는 것이 수월할 것으로 생각된다. selenization을 하기전에, 동시증착이나 다층박막형성을 통해 Cu-In-Se의 조합이 일반적으로 이루어진다. 어떤방법이든 Se의 부가적인 공급이 이루어지는데 시작 전구체의 조합에서 그 해법을 제시하는 것에 대한 논의가 많이 부족한 현실로서, CuInSe2의 단일전구체에 의한 박막형성과 특성평가에 대해 구체적인 논의가 필요하다. 본 실험에서는 Cu-In-Se 전구체를 CuInSe2 단일 타겟에서부터 RF 마그네트론 스퍼터링법을 이용하여 박막증착을 하여 Se의 Rapid Thermal Process(RTA)법을 통해 Se이 순차적으로 공급되었다. 이때 형성되는 박막의 태양전지 흡수층 적용을 위한 광학적, 전기적 및 구조적에 대한 논의된다. Soda lime glass(SLG)와 Corning 1737 유리를 기판으로 하여 아세톤-에탄올을 이용, 초음파세척을 실시하였다. 스퍼터 공정을 하기전에 흡착된 물분자를 제거하기 위하여 약 30분간 $120^{\circ}C$로 열을 가해주었으며, 공정을 위한 총 아르곤 가스의 양은 약 50sccm이며 이때의 공정압력은 20mtorr로 고정하였다. 우선 RF power와 기판온도에 따른 단일전구체 형성을 관찰하기 위하여 각각 30~80W, RT~$400^{\circ}C$로 변화를 주어 박막을 형성한 후 모든 sample에 대하여 $500^{\circ}C$분위기에 effusion cell을 이용하여 Se 분위기에서 결정화를 실시하였다. 샘플의 두께는 Surface profiler로 측정하였고 단면은 전자주사현미경으로 관찰되었다. 동시에 SEM이미지를 통하여 morphology와 grain size 및 EDX를 통하여 조성분석을 하였다. 밴드갭, 투과율 및 흡수계수는 UV-VIS-NIR분광분석법을 통하여 수행되었으며, 전기적 특성분석을 위해 4-point-probe와 Hall effect측정을 수행하였다. 공정변수에 따른 단일타겟으로 얻어 결정화된 CuInSe2박막의 자세한 결과와 논의에 대하여 발표한다.

  • PDF

Preparation of ZnO/SiO2 Nano-Composition and Photocatalysts and Antibacterial Activity (ZnO/SiO2 나노 입자의 화학적 합성과 광촉매 및 항균성 특성에 관한 연구)

  • Kim, Jae-Uk;Yuk, Young-Sam;Kim, Jong-Gyu
    • Journal of the Korean Chemical Society
    • /
    • v.61 no.4
    • /
    • pp.179-184
    • /
    • 2017
  • In this paper, a $ZnO/SiO_2$ nano-composite was prepared by a simple chemical method at room temperature. For the synthesis of ZnO nanoparticles (NPs), a sonochemical method was used, and $SiO_2$ NPs were prepared by precipitation method. The formation of $ZnO/SiO_2$ NCs was characterized by X-ray diffractometer (XRD) and confirmed by field-emission scanning electron microscopy (FE-SEM) and Fourier transform infra-red spectroscopy(FT-IR). The photocatalytic properties of $ZnO/SiO_2$ NCs formed at different concentrations of $SiO_2$ were evaluated by rhodamine-B dye. It was confirmed that increasing $SiO_2$ concentration resulted in an increase in the photocatalytic property. In addition, the antibacterial activity of $ZnO/SiO_2$ NCs was conducted against Escherichia coli (E. coli) and Staphylococcus aureus (S. aureus). As a result, the antibacterial activities of E.coli and S. aureus were increased in the presence of thick SiO NPs layer.

COMPARATIVE STUDY ON MORPHOLOGY OF CROSS-SECTION AND CYCLIC FATIGUE TEST WITH DIFFERENT ROTARY NITI FILES AND HANDLING METHODS (수종의 NiTi 전동 파일 단면 형태 비교 및 pecking motion의 사용방법이 피로 파절에 미치는 영향)

  • Kim, Jae-Gwan;Kum, Kee-Yeon;Kim, Eui-Seong
    • Restorative Dentistry and Endodontics
    • /
    • v.31 no.2
    • /
    • pp.96-102
    • /
    • 2006
  • There are various factors affecting the fracture of NiTi rotary files. This study was performed to evaluate the effect of cross sectional area, pecking motion and pecking distance on the cyclic fatigue fracture of different NiTi files. Five different NiTi $files-Profile^{(R)}$ (Maillefer, Ballaigue, Switzerland), $ProTaper^{TM}$(Maillefer, Ballaigue, Switzerland), $K3^{(R)}$ (SybronEndo. Orange, CA) , Hero $642^{(R)}$ (Micro-mega, Besancon, France), Hero $Shaper^{(R)}$ (Micro-mega, Besancon, France)-were used. Each file was embedded in temporary resin, sectioned horizontally and observed with scanning electron microscope. The ratio of cross-sectional area to the circumscribed circle was calculated. Special device was fabricated to simulate the cyclic fatigue fracture of NiTi file in the curved canal,. On this device, NiTi files were rotated (300rpm) with different pecking distances (3 mm or 6 mm) and with different motions (static motion or dynamic pecking motion) . Time until fracture occurs was measured. The results demonstrated that cross-sectional area didn't have any effect on the time of file fracture. Among the files, $Profile^{(R)}$ took the longest time to be fractured. Between the pecking motions, dynamic motion took the longer time to be fractured than static motion. There was no significant difference between the pecking distances with dynamic motion, however with static motion, the longer time was taken at 3mm distance. In this study, we could suggest that dynamic pecking motion would lengthen the time for NiTi file to be fractured from cyclic fatigue.