• 제목/요약/키워드: 초경공구

검색결과 96건 처리시간 0.024초

Ti-6Al-4V 타이타늄 합금의 절삭특성에 관한 연구 (A Study on the Machining Characteristics of Ti-6Al-4V Alloy)

  • 김남용;고준빈;이동주
    • 한국정밀공학회지
    • /
    • 제20권4호
    • /
    • pp.20-28
    • /
    • 2003
  • The machinability of Ti-6Al-4V titanium alloy and tool wear behavior in machining of Ti-6Al-4V titanium alloy was studied to understand the machining characteristics. This material is one of the strong candidate materials in present and future aerospace or medical applications. Recently, their usage has already been broaden to everyday's commercial applications such as golf club heads, finger rings and many decorative items. To anticipate the general use of this material and development of the titanium alloys in domestic facilities, the review and the study of the machining parameters for those alloys are necessary. This study is concentrated to the machining parameters of the Ti-6Al-4V alloy due to their dominant position in the production of titanium alloys.

U$_3$Si 분말제조에서 chip 가공조건이 분말의 입도분포에 미치는 영향

  • 이돈배;박희대;장세정;조해동;이종탁;김창규;국일현
    • 한국원자력학회:학술대회논문집
    • /
    • 한국원자력학회 1995년도 춘계학술발표회논문집(2)
    • /
    • pp.609-615
    • /
    • 1995
  • Chip machining에 의한 U$_3$Si 분말제조시 절삭가공조건이 분말 입도 분포에 미치는 영향을 조사하기 위하여 U$_3$Si ingot를 선반에서 초경공구를 사용하여 절삭속도 및 이송속도를 변화시키면서 chip을 가공하였고, 가공된 chip의 형상을 광학현미경으로 관찰하고 칩의 크기를 측정하였다. 모든 절삭조건에서 톱니모양의 칩(saw toothed chip)이 형성되었으며, 일정한 절삭속도에서 공구의 이송속도를 변화시켰을 때 이송속도가 증가함에 따라 칩 두께의 증가와 함께 chip segment의 폭도 증가하여 chip segment 의 크기가 뚜렷이 증가함을 보였다. 또한 chip segment의 크기는 절삭속도 보다는 공구의 이송속도에 크게 영향을 받는 것을 알 수 있었고 분말의 입도 분포에도 크게 영향을 미치는 것으로 나타났다.

  • PDF

Ti-6Al-4V 합금의 절삭특성과 FEM 해석 비교에 관한 연구 (A Study on the Cutting Characteristics and Analysis by a FEM in the Machining of Ti-6Al-4V alloy)

  • 김남용;홍우표;이동주
    • 한국공작기계학회논문집
    • /
    • 제10권6호
    • /
    • pp.29-35
    • /
    • 2001
  • The cutting characteristics of Ti-6Al-4V alloy and total wear when machining Ti-6Al-4V alloy was studied to understand the machining characteristics. This material is one of the strong candidate materials present and future aerospace or met ical applications. Nowadays their usage has already been broaden to commercial applications such as golf club head, finger rings and many decorative items. Anticipating the general use of this material and development of the titanium alloy in domestic facilities, the review and the study of the machining parameters far those alloys are deemed necessary. This study is concentrated to the machining parameters of the Ti-6Al-4V alloy due to their dominant position in the production of tita mum alloys.

  • PDF

TiCN PACVD코팅 초경호브의 Skiving절삭특성 평가 (An Evaluation of Skiving Cutting Characteristics of TiCN PACVD Coating Caribide Hob)

  • 천종필
    • 한국산학기술학회논문지
    • /
    • 제13권2호
    • /
    • pp.471-477
    • /
    • 2012
  • SCM420재질의 기어를 담금질을 실시한 후 초경호브(Hob)에 PACVD 코팅처리 후 표면경도가 높은 표면(HRC 60)을 절삭하였다. 코팅처리 없이 난삭재(難削材)로 분류되는 경도가 큰것, 경한 물질을 포함한 것, 강도가 높은 것에 공구수명과 생산성을 향상에는 한계성을 가지고 있다. 이를 개선하기 위해 초경호브에 TiCN코팅처리 전후에 대하여 Skiving 절삭으로 코팅처리 한 호브가 가공성이 좋고, 공구마멸이 적어, 공구수명이 2.5배 증가하는 결과를 얻었다. 실험은 CNC 스카이빙 호빙머신을 이용하여 습식절삭으로 절삭속도와 이송량으로 다양한 조건을 적용하여 공구마멸과 표면거칠기 데이터를 얻었다. 실험결과 조건 2에서(V=200m/min F=0.7mm/rev) Cutting speed가 절삭표면에 Feed Mark가 미세하고, 표면거칠기는 Rmax $4.7{\mu}m$(Ra $1.19{\mu}m$)의 데이터를 얻었다.

절삭공구의 피복층이 공구마멸에 미치는 영향에 대한 연구 (Study on Effects of Coatings on Cutting Tool Wear)

  • 손태영;양민양
    • Tribology and Lubricants
    • /
    • 제6권1호
    • /
    • pp.82-88
    • /
    • 1990
  • 마찰학적인 관점에서 피복초경공구의 피복층이 공구마멸에 미치는 영향을 조사하기 위하여 공구표면의 피복층을 선택적으로 제거한 후 마멸시험, 급속정지 실험 및 절삭력 측정 실험을 수행하였다. 실험 결과 피복층은 공구와 피삭재 사이의 점착성을 낮추어 점착마멸을 억제시키는 것으로 나타났으며, 마찰저항을 감소시켜 절삭력을 낮추는 것으로 관찰되었다. 또한 경사면상의 피복층이 플랭크 마멸의 성장을 저지하는 효과가 있는 것으로 나타났으며, 피삭재가 탄소강인 경우 경계마멸까지 고려할 때 다중피복공구가 가장 바람직한 것으로 관찰되었다.

플라즈마 이온주입에 의해 표면 개질한 초경공구의 가공특성 (Cutting Characteristics of Plasma Source Son Implanted Tungsten Carbide Tool)

  • 강성기;왕덕현;김원일
    • 한국정밀공학회지
    • /
    • 제27권1호
    • /
    • pp.33-40
    • /
    • 2010
  • In this research, the effects for surface Improvement of plasma ion implanted carbide endmill tools were observed by measuring cutting forces and tools wear affecting surface roughness in high speed cutting. From the 2nd ion mass analysis, the oxidation layer was found to be built up by sputtering. The residual gas contamination of oxygen was found to be contained impurities in nitrogen gas. The plasma implanted ion was found to be spreaded, especially the nitrogen was implanted up to 150nm depth as impressed voltage and ion implanting time. It is analyzed as bring surface improvement by spreading deeply forming oxidation on surface. The factors in Analysis of Variance(ANOVA) about mutuality cause reference of cutting force. The cutting force Fx is affected by the interaction of spindle rpm and federate, the cutting force Fy is influenced by spindle rpm and time injected ion, and cutting force Fz is affected by the interaction of impressed voltage and feedrate. Also, it was found that the cutting forces of implanted tools become lower and the surface roughness is improved by the effect of nitrogen according to the implantation.

$Si_3N_4$-TiC ceamic 공구에 화학증착된 TiC, TiN 및 Ti(C, N)에 관한 연구 (A study on the chemically vapor deposited TiC, TiN, and Ti(C, N) on $Si_3N_4$-TiC ceramic tools)

  • 김동원;김시범;이준근;천성순
    • 한국윤활학회:학술대회논문집
    • /
    • 한국윤활학회 1988년도 제7회 학술강연회초록집
    • /
    • pp.39-42
    • /
    • 1988
  • 요업체 절삭공구(ceramic tool)는 공구강이나 초경제품에 비해 고속 절삭 작업이 가능하며 생산성을 높일 수 있기 때문에 최근 주목을 받고 있다. 본 실험에서 모재(substrate)로 사용된 $Si_3N_4$-TiC ceramic은 요업체 공구중에서 파괴인성이 우수하며, 주철이나 초합금을 절삭할 때 우수한 성능을 나타낸다. 그러나 요업체 절삭공구중에서 경도가 낮은 편에 속하며, Fe,Mn,O와 $Si_3N_4$가 화학적 반응을 일으켜서, steel을 절삭할 때 상면 마모(crater wear)가 심하게 발생하기 때문에 우수한 성능을 나타내지 못하고 있는 실정이다. 따라서 이러한 단점을 보완하기 위해 공구의 표면에 보호피막(protective coating)을 입히는 것은 필수적이다. 본 연구에서는 반응변수들이 TiC 및 TiN 증착층의 증착속도, 미세구조, 화학적 조성 및 증착층과 substrate 사이의 interface를 조사하여 각 증착층의 최적증착조건을 규명하고자 한다.

  • PDF

절삭공구용 초경합금의 성형체 및 소결체의 강도에 미치는 성형조건의 영향 (Effect of the Forming Condition on Flexural Strength of Green and Sintered Bodies of Tungsten Carbide for Cutting Tool)

  • 이재우
    • 한국정밀공학회:학술대회논문집
    • /
    • 한국정밀공학회 2004년도 추계학술대회 논문집
    • /
    • pp.796-799
    • /
    • 2004
  • The effects of forming presure, organic binder content and moisture on flexural strength were investigated. As moisture content increased in the granules during compaction, the density and strength of the green body were increased. Green strengths were found to improve more strongly with increasing forming pressure in the case of using the granules of higher organic content. The sintered strength was the highest with the organic content of 0.2wt% under all forming pressures.

  • PDF

상압 기상반응법에 의한 나노 WC 분말 제조 연구 (Synthesis of Nanostructured WC Powders by Chemical Vapor Condensation process)

  • 하국현;김진천;김병기
    • 한국재료학회:학술대회논문집
    • /
    • 한국재료학회 2003년도 추계학술발표강연 및 논문개요집
    • /
    • pp.43-43
    • /
    • 2003
  • WC/Co계 초경 합금은 각종 공구 및 내마모 부품으로서 널리 사용되고 있다. 초경 합금의 특성은 WC 분말 크기에 크게 좌우되며 일반적으로 입자의 크기가 미세해 질수록 기계적 특성이 향상되는 것으로 알려지고 있다. 이를 위하여 지금까지 많은 연구가 진행되고 있으나, 현재 액상 공정을 이용하여 약 100nm급의 초경 분말이 개발되어지고 있으며, 그보다 미세한 분말의 제조는 아직 이루어지고 있지 않은 실정이다. 그러나 최근 기상 반응을 이용하여 수nm급의 분말 제조가 가능하게 되었으나, 주로 산화물계에 분말 제조에 국한되고 있다. 본 연구에서는 이러한 기상 반응법을 이용하여 초경 합금의 핵심 소재인 WC분말을 합성하고자 하였으며, 이를 위하여 장치의 설계 및 제작, 그리고 공정별 특성에 대하여 연구하였다.

  • PDF