• Title/Summary/Keyword: 진성파괴전압

Search Result 4, Processing Time 0.018 seconds

A Study on Electric Field Dependence of Tree Shape in Low Density Polyethylene (저밀도폴리에틸렌에서 트리 형상의 전계의존성에 관한 연구)

  • 김재환;박창옥;윤헌주
    • Fire Science and Engineering
    • /
    • v.14 no.1
    • /
    • pp.1-7
    • /
    • 2000
  • Internal insulators give rise to partial discharge(PD), which cause local breakdown and even entire insulation breakdown. Treeing due to PD is one of the main causes of breakdown of the insulating materials and reduction of the insulation life. Therefore the necessity for establishing a method to diagnose the aging of insulation materials and to predict the breakdown of insulation has become important. From this viewpoint, we have studied on Electric Field dependence of tree shape in Low Density Polyethylene about treeing phenomena occurring on the high electrical field. As the result, under the reasoning that the growing of tree supposing when the inner part of tree is either dielectrec or conductor has the intermediate characteristics between dielectrec and conductor, theoretically investicated results well according with the experimental results.

  • PDF

The Characteristics of $PbTiO_{3}-PbZrO_{3}-Pb(Ni_{1/3}Nb_{2/3})O_{3}$ Piezoelectric Thin Film Made by Sol-Gel Method (Sol-Gel 법으로 제작한 $PbTiO_{3}-PbZrO_{3}-Pb(Ni_{1/3}Nb_{2/3})O_{3}$ 압전박막의 특성)

  • Yoon, Wha-Joong;Lim, Moo-Yeol;Koo, Kyung-Wan
    • Journal of Sensor Science and Technology
    • /
    • v.4 no.4
    • /
    • pp.75-80
    • /
    • 1995
  • In order to fabricate the piezoelectric thin film of the PZT-PNN ternary compound, the metal alkoxides were used as starting materials. The electrical and crystalline properties of the thin film were evaluated. The X- RD study shows that the crystallization of the film is optimized at $550^{\circ}C$ of sintering temperature. According to the D-E hysterisis curve, the coercive field is 28.8 kV /cm, and the remanent polariztion is $18.3\;{\mu}C/cm^{2}$. The break down voltages of the thin films are $76.0\;{\sim}\;27.0\;MV/m$. When the sintering temperature is raised, the break down voltage is lowered. As a result of measuring the C-V characteristic curve of the ternary compound piezoelectric thin film, the relative dielectric constants are 406 for the composition (50:40:10), 1084 for the composition (50:30:20), 723 for the composition (45:35:20) and 316 for the composition (40:40:20).

  • PDF

Electrical properties of sol-gel derived $ PbZrO_3$-$PbTiO_3$-$Pb(Ni_{1/3}Nb_{2/3})O_3$ thin film (Sol-Gel 법에 의한$ PbZrO_3$-$PbTiO_3$-$Pb(Ni_{1/3}Nb_{2/3})O_3$)

  • 임무열;구경완;한상옥
    • Electrical & Electronic Materials
    • /
    • v.10 no.2
    • /
    • pp.134-140
    • /
    • 1997
  • PbTiO$_{3}$-PbZrO$_{3}$-Pb(Ni$_{1}$3/Nb $_{2}$3/O$_{3}$)(PZT-PNN) thin films were prepared from corresponding metal organics partially stabilized with diethanolamine by the sol-gel spin coating method. Each mol rates of PT:PZ:PNN solutions were #1(50:40:10), #2(50:30:20), #3(45:35:20) and #4(40:40:20), respectively. The spin-coated PZT-PNN films were sintered at the temperature from 500.deg. C to 600.deg. C for crystallization. The P-E hysteresis curve was drawn by Sawyer-Tower circuit with PZT-PNN film. The coercive field and the remanent polarization of #4(40:40:20 mol%) PZT-PNN film were 28.8 kV/cm and 18.3 .mu.C/cm$^{2}$, respectively. Their dielectric constants were shown between 128 and 1120, and became maximum value in MPB(40:40:20 mol%). The leakage currents of PZT-PNN films were about 9.4x 10$^{-8}$ A/cm$^{2}$, and the breakdown voltages were about 0.14 and 1.1 MV/cm. The Curie point of #3(45:35:20 mol%, sintered at 600.deg. C) film was 330.deg. C.

  • PDF

A Study on the Design Parameters of the Static Ring in the Ultra-high Voltage Non-uniform Electric Field (초고압 불평등 전계에서 정전링 설계변수에 대한 연구)

  • Kim, Jin-Sung;Seo, Min-Seong
    • Journal of the Korea Academia-Industrial cooperation Society
    • /
    • v.21 no.7
    • /
    • pp.577-582
    • /
    • 2020
  • Electricity produced at power plants is distributed to consumers through several stages of substations. At this time, an ultra-high voltage transformer is needed in the initial transmission stage to transmit a voltage suitable for each consumer. A high voltage, non-uniform electric field is formed at the end of the winding of the ultra-high voltage transformer, which carries a risk of dielectric breakdown. The winding of the ultra-high voltage transformer is an electrode, which is the key to converting the magnitude of the voltage. A non-uniform electric field is formed along the shape of the winding end, resulting in high electrical stress. The static ring installed at the upper and lower ends of the winding is used to disperse the stress at the winding end. Several variables should be considered when designing a static ring. Among them, this study examined how the curvature of the static ring, the thickness of the insulating paper, the number of barriers, and barrier thickness affect the electrical stress of the static ring using the Finite Element Method. Suggestions to be considered when designing the static ring are proposed through the FEM results.