Marginal and internal fit of all ceramic crown using the replica technique and the triple-scan protocol (Replica technique과 Triple-scan protocol을 이용한 지르코니아 전부도재관의 변연 및 내면 적합도에 관한 비교 연구)

  • Shin, Mi-Sun;Lee, Jang-Hoon
    • The Journal of Korean Academy of Prosthodontics
    • /
    • v.55 no.4
    • /
    • pp.372-380
    • /
    • 2017
  • This study was conducted to compare the marginal and internal fit of all ceramic crown using the replica technique and the triple-scan protocol. Materials and methods: Twenty zirconia ceramic crowns were fabricated using titanium abutment model. All crowns were divided into two groups of 10 each, depending on the replica technique and the triple-scan protocol. The internal and marginal fit of 10 zirconia ceramic crowns were measured at 17 points for each specimen using the replica technique. The other 10 ceramic crowns were measured using the triple-scan protocol. Statistical analysis was performed by t-test (${\alpha}=.05$). Results: The mean and standard deviation of marginal and internal fit were significantly different between the replica technique ($49.86{\pm}29.69{\mu}m$) and triple-scan protocol ($75.35{\pm}64.73{\mu}m$, P<.001). The mean and standard deviation of internal fit except marginal fit were $58.38{\pm}31.77{\mu}m$ and $64.00{\pm}46.43{\mu}m$, respectively (P>.343). Conclusion: There was a statistically significant difference in the marginal fit measured by the two methods. However, there was no statistically significant difference in the internal fit between the two methods.

Influence of High Temperature of the Porcelain Firing Process on the Marginal Fit of Zirconia Core (도재 소성 과정에서의 고온이 지르코니아 코어의 변연적합도에 미치는 영향)

  • Kim, Jae-Hong;Kim, Ki-Baek
    • Journal of dental hygiene science
    • /
    • v.13 no.2
    • /
    • pp.135-141
    • /
    • 2013
  • One factor for successful prognosis of finished dental prosthesis is good marginal fit. The purpose of this study in vitro investigation was to compare the marginal fit of all-ceramic crown before and after porcelain veneering, to evaluate the influence of high temperature of the porcelain firing on the fit. For this experiment, model of abutment tooth of maxillary right central incisor was prepared. Ten working models were produced. Ten zirconia cores were made by dental computer aided design/computer aided manufacturing system. The marginal fit of specimens were examined using silicone replica technique. Silicone replicas were sectioned four times and were measured through a digital microscope (${\times}160$). Marginal fit is a distance connected between edge end part of specimen and abutment margin. Each specimens was measured twice, the first measurement was done prior to veneering porcelain firing, while the second measurement was done after the porcelain firing to evaluate this process. Statistical analyses were performed with paired t-test. $Mean{\pm}SD$ marginal fit was $60.8{\pm}14.2{\mu}m$ for zirconia core and $86.1{\pm}13.3{\mu}m$ for all-ceramic crown. They were statistically significant differences (p<0.001). But all specimens showed a marginal fit where the gap widths ranged within the clinical recommendation ($120{\mu}m$), all-ceramic crown production using the zirconia core was adequate.

Clinical convergence angle and rounding radius on tooth preparation for zirconia all-ceramic crown (지르코니아 전부도재관 지대치 삭제시 축면 경사각과 만곡 반경에 대한 조사)

  • Kim, Hye-Eun;Woo, Yi-Hyung;Pae, Ah-Ran;Kim, Hyeong-Seob
    • The Journal of Korean Academy of Prosthodontics
    • /
    • v.49 no.1
    • /
    • pp.22-28
    • /
    • 2011
  • Purpose: This article attempted to examine how teeth for restoration is made in a clinical practice and utilize it as future educational material of teeth formation and basic data for additional research. Materials and methods: This experiment investigated the models sent to milling center for production of zirconia crowns. After scanned with Lava CAD/CAM System (3M ESPE, Seefeld, Germany), they are measured on 'ImageJ (version 1.32j, National Institutes of Health, USA)' program and compared and analyzed. Convergence angle from mesio-distal surfaces and bucco-lingual surfaces of each teeth are measured. Also, bucco-lingual diameter of the region lowered as much as 0.4 mm from incisal edge in anterior teeth except canines.(This measure is defined as the Peak 0.4) The analysis of data between each group was conducted by Windows SPSS statistic program, and was proved significant on 95% confidence level by independent t-test, one-way ANOVA and multiple analysis (Sheff${\'{e}}$ test). Results: The mean value of convergence angle was $18.67^{\circ}$ It is ranked as molar ($26.70^{\circ}$) > premolar ($16.87^{\circ}$) > anterior teeth ($14.81^{\circ}$) in the order of mesio-distal convergence angle; anterior teeth ($22.32^{\circ}$) > molar ($20.93^{\circ}$) > premolar ($15.41^{\circ}$) in the order of bucco-lingual convergence angle. The mean value of Peak 0.4 was 1.18 mm. Conclusion: Convergence angle of abutment of zirconia all ceramic crown has difference depending on the location in the arch. Due to the nature of production of zirconia all ceramic crown, convergence angle of abutment and line angle finishing degree can have an effect on internal suitability of restoration.

A comparison of the fidelity of various zirconia-based all-ceramic crowns fabricated with CAD/CAM systems (수종의 CAD/CAM 시스템으로 제작한 지르코니아 기반 완전도재관의 적합도 비교)

  • Kim, Sung-Jun;Jo, Kwang-Hun;Lee, Kyu-Bok
    • The Journal of Korean Academy of Prosthodontics
    • /
    • v.47 no.2
    • /
    • pp.148-155
    • /
    • 2009
  • Statement of problem: The interest in all-ceramic restorations has increased as more techniques have become available. With the introduction of machinable dental ceramics and CAD/CAM systems there is a need to evaluate the quality levels of these new fabrication techniques. Purpose: This study is to evaluate the crown fidelity(absolute marginal discrepancy and internal gap) of various zirconia-based all-ceramic crowns fabricated with different CAD/CAM(computer-assisted design/computer-assisted manufacturing) systems and conventional cast metal-ceramic crowns. Material and methods: A resin tooth of lower right second premolar was prepared. After an impression was taken, one metal master die was made. Then 40 impressions of metal master dies were taken for working dies. 10 crowns per each system were fabricated using 40 working dies. Metal-ceramic crowns were cast by using the conventional method, and Procera, Lava, and Cerec inLab crowns were fabricated with their own CAD/CAM manufactruing procedures. The vertical marginal discrepancies and internal gaps of each crown groups were measured on a metal master die without a luting agent. The results were statistically analyzed using the one-way ANOVA and Tukey's HSD test. Results: 1. Vertical marginal discrepancies were $50.6{\pm}13.9{\mu}m$ for metal-ceramic crowns, $62.3{\pm}15.7{\mu}m$ for Procera crowns, $45.3{\pm}7.9{\mu}m$ for Lava crowns, and $71.2{\pm}2.0{\mu}m$ for Cerec inLab crowns. 2. The Internal gaps were $52.6{\pm}10.1{\mu}m$ for metal-ceramic crowns, $161.7{\pm}18.5{\mu}m$ for Procera crowns, $63.0{\pm}10.2{\mu}m$ for Lava crowns, and $73.7{\pm}10.7{\mu}m$ for Cerec inLab crowns. Conclusion: 1. The vertical marginal discrepancies of, 4 crown groups were all within the clinically acceptable range($120{\mu}m$). 2. The internal gaps of LAVA, Cerec inlab, and metal-ceramic crowns were within clinically acceptable range except Procera crown($140{\mu}m$).

The effect of repeated firings on the color of zirconia-based all-ceramic system (반복 소성이 지르코니아 전부도재관의 색조에 미치는 영향)

  • Jang, Jung-Eun;Kim, Mu-Hyon;Yun, Mi-Jung;Jeong, Chang-Mo;Jeon, Young-Chan
    • The Journal of Korean Academy of Prosthodontics
    • /
    • v.49 no.1
    • /
    • pp.73-79
    • /
    • 2011
  • Purpose: The aim of this study was to evaluate the effect of repeated firings on the color of zirconia restoration with different shading method. Materials and methods: Three different types of zirconia frameworks (adding metallic pigments to the initial zirconia powder before sintering (Group NM), dipping the milled frameworks in dissolved coloring agents (Group KI), or application of liner material to the sintered white frameworks (Group KW) were used to support A3 shade dentin porcelain. Repeated firings (3, 5, or 7) were performed, color differences among ceramic specimens were measured using a colorimeter. Repeated measurements analysis of variance (ANOVA) was used to analyze the data for significant difference. The Tukey Honestly Significant Different (HSD) test was used to perform multiple comparisons (${\alpha}$ = .05). Results: 1. $L^*a^*b^*$ values of the ceramic systems were affected by the number of firings (1, 3, 5 or 7 firings) (P < .001) and shading methods (P < .001). 2. As the number of firings increased, the $L^*$ (for all groups) and $a^*$ value (for KW and NM groups) decreased and the $b^*$ value(for all groups) increased. 3. The mean color differences caused by repeated firings were perceptible (${\Delta}E$ > 1) for group KW and KI fired after 3 times, except for group NM fired after 7 times. 4. In order of decreasing ${\Delta}E$ value fired after 7 times, the values were group KI(${\Delta}E$ = 2.26) > group KW (${\Delta}E$ = 1.47) > group NM (${\Delta}E$ = 1.08) (P < .001). Conclusion: Repeated firings influenced the color of the zirconium-oxide all-ceramic specimens with different shading methods.

Comparative study in fracture strength of zirconia cores fabricated with three different CAD/CAM systems (3종의 CAD/CAM 시스템에서 지르코니아 코어의 파절 강도에 관한 비교 연구)

  • Shin, Eon-Sick;Lee, Young-Soo;Park, Won-Hee
    • The Journal of Korean Academy of Prosthodontics
    • /
    • v.46 no.1
    • /
    • pp.22-30
    • /
    • 2008
  • Purpose: The purpose of this study is to compare three different CAD/CAM systems through the fracture strength of zirconia core and to evaluate the clinical availability of each system. Material and methods: The following three groups of 30 maxillary mesial incisor core for all-ceramics(each group 10) were fabricated as follows: group 1. $Adens^{(R)}$ CAD/CAM system, group 2. $Cerasys^{(R)}$ CAD/CAM system, group 3. 3M $Lava^{(R)}$ CAD/CAM system. All specimens were manufactured consistently thickness 0.5mm and relief $40{\mu}m$. Specimens were subjected to compressive loading on the lingual area by Z250/$SN5S^{(R)}$. Each group's mean and standard deviation were calculated and Kruskal Waillis test, Wilcoxon Rank Sum test were utilized to find out the relationship among the groups. Results: The results were as follows: 1. The mean fracture strength of $Adens^{(R)}$ system was $615.89{\pm}156.1N$, the $Cerasys^{(R)}$ system was $863.98{\pm}151.5N$, and the 3M $Lava^{(R)}$ system was $1143.1{\pm}286.6N$. 2. The fracture strength of the systems showed the significant statistical differences in order of 3M $Lava^{(R)}$ system, $Cerasys^{(R)}$ system, $Adens^{(R)}$ system. Conclusion: In this study, in spite of the differences among the groups, every group showed clinically useful results. It is necessary to study further clinical experiments on a long term basis.

Fracture strength of zirconia ceramic crowns according to tooth position (치아 부위에 따른 지르코니아 도재관의 파절강도)

  • Lee, In-Seob;Kim, Jeong-Mi;Dong, Jin-Keun
    • The Journal of Korean Academy of Prosthodontics
    • /
    • v.48 no.2
    • /
    • pp.94-100
    • /
    • 2010
  • Purpose: The purpose of this study was to compare the fracture strength of the zirconia ceramic crowns according to tooth position. Material and methods: After 10 metal dies were made for each group, the zirconia ceramic crowns were fabricated using CAD/CAM system ($Lava^{TM}$ All-Ceramic System) and each crown was cemented on each metal die with resin cement (Rely $X^{TM}$ Unicem). The cemented zirconia ceramic crowns mounted on the testing jig were inclined with 30 degrees to the long axis of the tooth and the universal testing machine was used to measure the fracture strength. Results: 1. The fracture strength of the zirconia ceramic crown in the lower 1st molar (2963 N) had the highest and that in the lower central incisor (1035 N) had the lowest. 2. The fracture strength of zirconia ceramic crown was higher than that of the IPS Empress crowns in all tooth position. 3. The fracture mode of the crowns was similar. Most of fracture lines began at the loading area and extended through proximal surface perpendicular to the long axis of the crowns. 4. There were no significant differences on the fracture strength of the zirconia ceramic crowns according to tooth position except in premolar group. Conclusion: Within the limitations of this study, the results suggested that strength of zirconia ceramic crown is satisfactory for clinical use.

The Effect of Veneering Techniques on the Color Parameters of Y-TZP Based All Ceramic Restoration of Varying Ceramic Core Thickness (지르코니아 코어 두께에 따른 전부도재관의 상부도재 축성방법이 보철물 색조에 미치는 영향)

  • Huh, Sung-Yoon;Son, Ho-Jung;Kim, Hae-Young;Kim, Jae-Hong
    • Journal of dental hygiene science
    • /
    • v.12 no.2
    • /
    • pp.123-129
    • /
    • 2012
  • The aim of study was to compare the color parameters and mean color difference of porcelain specimens by different veneering technique in order to examine the effect of veneering technique on esthetics of yttria-stabilized tetragonal zirconia polycrystalline(Y-TZP) all ceramic restoration. Three groups of square-shaped core ceramic specimens(14mm in diameter and 0.3, 0.5, 0.7 mm) and two groups of veneering ceramic specimen were prepared for analysis. Color parameter($L^*,a^*,b^*$) and color difference of zirconia core squares and core-veneer specimens were measured with ShadeEye $NCC^{(R)}$ spectrophotometer, respectively. Mean color difference(${\Delta}E^*$)were calculated using color difference formula. Two-way analysis of variance(ANOVA) combined with a Tukey multiple-range test were used to analysis the data(${\alpha}=0.05$). ${\Delta}E^*$ values were not significantly affected by core thickness and veneering porcelain(p=0.083). The color differences(${\Delta}E^*$) of core-veneer specimens with 0.5, 0.7 mm-A1,A2,A3.5 shade were mostly below 3.7 which was within the clinically acceptable range, while color differences between 0.3 mm-A1,A2 showed more than 3.7. All-ceramic system has color characteristics that clinicians have to consider when selecting materials. Also, manufacturers of different porcelain systems must make every effort to achieve color reproducibility.