• Title/Summary/Keyword: 접착제 파손

Search Result 43, Processing Time 0.025 seconds

Failure Mode and Strength of Unidirectional Composite Single Lap Bonded Joints I. Experiments (일방향 복합재료 Single Lap접합 조인트의 파손 모드 및 강도 I. 실험)

  • Kim Kwang-Soo;Yoo Jae-Seok;An Jae-Mo;Jang Young-Soon
    • Composites Research
    • /
    • v.17 no.6
    • /
    • pp.14-21
    • /
    • 2004
  • Failure process, mode and strength of unidirectional composite single lap bonded joints were investigated experimentally with respect to bonding methods, those are, co-curing with and without adhesive and secondary bonding. The co-cured joint specimens without adhesive had the largest failure strength. Progressive failures along the adhesive layer occurred in the secondary bonded specimens. In the co-cured specimens with adhesive film which had better material strength and adhesion performance, delamination failure occurred and the joint strengths were less than those of secondary bonded specimens. Delamination failure did not occur in the secondary bonded specimens because of earlier crack growth and progressive failure in the adhesive layer. Therefore, failure strength of composite bonded Joints were not always proportionate to material strength and adhesion performance of the adhesive due to the weakness of delamination in composite materials. The effects of surface roughness, bondline thickness and fillets were also studied on secondary bonded specimens.

Failure Mode and Strength of Unidirectional Composite Single Lap Bonded Joints II. Failure Prediction (일방향 복합재료 Single Lap 접합 조인트의 파손 모드 및 파손 강도 II. 파손 예측)

  • Yi Young-Moo;Kim Chun-Gon;Kim Kwang-Soo
    • Composites Research
    • /
    • v.18 no.1
    • /
    • pp.1-9
    • /
    • 2005
  • A methodology is presented for the failure prediction of composite single-lap bonded joints considering both of composite adherend failure and bondline failure. An elastic-perfectly plastic model of adhesive and a delamination failure criterion are used in the methodology. The failure predictions have been performed using finite element method and the proposed methodology. The failure prediction results such as failure mode and strength have very good agreements with the test results of joint specimens with various bonding methods and parameters. The influence of variations in the effective strength (that is, adhesion performance) and plastic behavior of adhesive on the failure characteristics of composite bonded Joints are investigated numerically. The numerical results show that optimal joint strength is archived when adhesive and delamination failure occur in the same time.

Experimental Debonding Failure Behaviors of Composite Skin-Stiffener Bonded Specimens (복합재료 스킨-보강재 접합 시편의 파손 특성에 대한 시험 연구)

  • Kim, Kwang-Soo;An, Jae-Mo;Jang, Young-Soon;Yi, Yeong-Moo
    • Composites Research
    • /
    • v.20 no.6
    • /
    • pp.8-14
    • /
    • 2007
  • Debonding failure characteristics of the composite skin-stiffener specimens were experimentally investigated. The influences of bonding methods, types of stiffener shape and various secondary bonding parameters were evaluated. Present test results combined with the previous test results[1] showed that the failure displacement of the skin-stiffener specimens well evaluates the skin-stiffener debonding failure strength of the composite stiffened panels. The specimens with an open type stiffener had lower bending stiffness and larger failure displacement than those with a closed type stiffener. Secondary bonding and co-curing with adhesive had better failure strength than co-curing without adhesive film. Secondary bonded specimens failed by adhesive failure and co-cured specimens failed by delamination failure. As the bondline thickness was thinner, the skin-stiffener specimens had higher failure strength. The fillets had no influence on failure strength of the specimens. The influence of the surface roughness was shown according to types of stiffener shape.

Testing and Numerical Analysis on the Fracture Characteristics of Composite Adhesive Bonded Single-Lap Joints (복합재료 Single-Lap 본딩 조인트의 파괴 특성에 대한 실험 및 수치해석 연구)

  • 김광수;박재성;장영순;이영무
    • Composites Research
    • /
    • v.16 no.5
    • /
    • pp.45-53
    • /
    • 2003
  • The experimental and numerical investigations on the failure characteristics of the secondary bonded composite single-lap joints were performed. The initiations and growths of cracks were observed using CCD camera and acoustic emission sensor during the tension tests of the joint specimens. The structural behaviors of the specimens were predicted by the geometric nonlinear two-dimensional finite element analysis. The three types of observed initial cracks were included in each finite element models and the strain energy release rates of each specimen models were calculated by VCCT(Virtual Crack Closure Technique) technique. The tension tests showed that the initial cracks occurred in the 60∼90% of final failure loads and the major failure modes of the specimens were adhesive failure and the delamination between the 1st and 2nd ply of laminate. The specimens with the thicker bondline had earlier crack initiation loads but higher crack propagation resistance and eventually better loading capability. The delaminations were mostly observed in the thicker bondline specimens. The mode I values of calculated strain energy release rates were higher than the mode II values in the all specimen models considering the three types of initial cracks. The mode I and total strain energy release rates were calculated as higher values in the order of initial crack in the edge interface, comer interface and delamination between the plies of laminate.

Strength of sandwich-to-laminate single-lap bonded joints in elevated temperature and wet condition (샌드위치와 적층판을 접착한 단일겹침 체결부의 고온습도 강도특성 연구)

  • Choi, Bae-Hyun;Kweon, Jin-Hwe;Choi, Jin-Ho;Shin, Sang-Jun;Song, Min-Hwan
    • Journal of the Korean Society for Aeronautical & Space Sciences
    • /
    • v.38 no.11
    • /
    • pp.1115-1122
    • /
    • 2010
  • The main objective of this study is to experimentally investigate the effect of adhesive thickness and environmental conditions on the failure and strength of sandwich-to-laminate bonded joints. Three different adhesive thicknesses (t=0.2, 2 and 4 mm) and two different environmental conditions were considered. Environmental conditions include the RTD(room temperature and dry condition) and ETW(elevated temperature and wet condition). Test results show as the adhesive thickness increases from 0.2 mm to 2 and 4 mm, the joint strength decreases 16 and 30%, respectively. Regarding the effect of environmental conditions, except for one case, the joint strength in the ETW conditions turned out to be 12% higher than those in the RTD conditions. In the joints with adhesive thickness of 0.2 mm, remarkable difference from RTD condition was not found.

Effect of Micro-bolt Reinforcement for Composite Scarf Joint (복합재 스카프 조인트에서의 마이크로 볼트 보강에 대한 타당성 연구)

  • Lee, Gwang-Eun;Sung, Jung-Won;Kweon, Jin-Hwe
    • Composites Research
    • /
    • v.32 no.1
    • /
    • pp.37-44
    • /
    • 2019
  • The reinforcement effect of micro-bolt for a bonded scarf joint was investigated. Three scarf ratios of 1/10, 1/20, and 1/30 were considered to examine the effect of scarf patch configuration on joint strength. To maintain the same density of micro-bolt, 16, 32, and 48 bolts were installed in the scarf joint specimens with scarf ratios of 1/10, 1/20, and 1/30, respectively. Tests were also carried out on the joints that are bonded with only adhesive and that are fastened with only micro-bolts to obtain reference values. The average failure loads of the adhesive joints with scarf ratios of 1/10, 1/20, and 1/30 were 29.7, 39.6, and 44.8 kN, respectively. In case of micro-bolt reinforcement, the failure loads at the same scarf ratios were 28.4, 37.2, and 40.1 kN, respectively, which corresponds to 96, 94, and 90% of the pure adhesive joint failure loads. In the case of using only micro-bolts, the failure loads were only 13-25% of the average failure loads of pure adhesive joints. Fatigue test was also conducted for the joints with scarf ratio of 1/10. The results show that the fatigue strength of hybrid joints using both adhesive and microbolts together slightly increased compared to the fatigue strength of adhesive joint, but the rate of increase was small to 2-3%. Through this study, it was confirmed that the reinforcement effect of micro-bolt is negligible in the scarf joints where shear stress is dominating the failure, unlike in the structure where peel stress is dominant.

Convergence Study on Fracture at Joint Using Adhesive at Inhomogeneous Materials Bonded with CFRP (CFRP와 결합된 이종재료들에서의 접착제를 이용한 접합부의 파손에 관한 융합 연구)

  • Kim, Jae-Won;Cho, Jae-Ung
    • Journal of the Korea Convergence Society
    • /
    • v.9 no.5
    • /
    • pp.151-156
    • /
    • 2018
  • In this study, CFRP and metal or nonmetal were bonded with adhesive and the fracture study on this material was carried out. CFRP at the upper side of specimen and metal or nonmetal were assigned at the lower side of specimen by using DCB specimen as the analysis condition. And it was desribed that the structural adhesive were bonded between both upper and lower sides. As this analysis result, the least equivalent stress was shown at the specimen bonded with aluminium. The maximum shear stress was shown to become lowest at the de-bonded CFRP specimen when titanium was used. In conclusion, it was shown that the deformation of specimen became lowest when titanium was used. On the basis of this study result, the esthetic sense can be shown as the fracture data of bonded interface using adhesive are grafted onto the real life.

A Study on Failure Strength of Single Lap Adhesive Joint with Thick Adherend (후판 단일 겹침 접착 조인트의 파손강도에 관한 연구)

  • Park, Jae-Hyun;Choi, Jin-Ho;Kweon, Jin-Hwe
    • Journal of the Korean Society for Aeronautical & Space Sciences
    • /
    • v.38 no.2
    • /
    • pp.111-118
    • /
    • 2010
  • The joints are often the weakest areas in composite structures. In this paper, the thick aluminum-aluminum joint specimens and thick composite-aluminum single lap adhesive joint specimens were manufactured and the tensile tests were performed. The fracture mode of each specimen was investigated and the modified damage zone theory based on the yield strain was proposed and compared with experimental failure load of each mode. The failure loads of the thick aluminum-aluminum joint and composite-aluminum joint were predicted by the same failure criterion and they could be predicted to within 19.3% using the damage zone ratio method for all 14 cases investigated.

A Parametric Study on the Strength of Single-Lap Bonded Joints of Carbon Composite and Aluminum (탄소 복합재-알루미늄 단일겹침 접착 체결부의 강도에 관한 인자연구)

  • Kim, Tae-Hwan;Seong, Myeong-Su;Choi, Jin-Ho;Kweon, Jin-Hwe
    • Composites Research
    • /
    • v.20 no.5
    • /
    • pp.34-42
    • /
    • 2007
  • Strength and failure of adhesively bonded carbon composite-to-aluminum single-lap joints were studied by experiment. The main objective of this study is to investigate the effect of various parameters such as curing pressure for bonding, overlap lengths, and adherend thickness on the failure loads and modes of the bonded Joints with dissimilar materials. Experimental results show that the bonding pressure for composite-to-aluminum dissimilar materials should be 4 atm at the lowest. Failure load of the joints increases as the overlap length increases, but the strength (failure load divided by bonded area) decreases rapidly after the overlap width-to-length ratio is greater than 1. When the adherend thickness increase to double, bonding strength increase $12{\sim}55%$. Major failure mode of the joints is the delamination in the composite laminate and the location of delamination goes deeper into the laminates as the bonding pressure and overlap length increase.

An Experimental Study on the Strength of Single-Lap Bonded Joints of Carbon Composite and Aluminum (탄소 복합재와 알루미늄 이종재료 단일겹침 접착 체결부의 강도에 관한 실험 연구)

  • Kim, Tae-Hwan;Lee, Chang-Jae;Choi, Jin-Ho;Kweon, Jin-Hwe
    • Journal of the Korean Society for Aeronautical & Space Sciences
    • /
    • v.35 no.3
    • /
    • pp.204-211
    • /
    • 2007
  • Experiments were conducted to investigate the failure and strengths of carbon composite-to-aluminum single-lap bonded joints with 5 different bonding lengths. Joint specimens were fabricated to have secondary bonding of laminate and aluminum with a film type adhesive, FM73m. Tested joints have the bonding strengths between the values of aluminum-to-aluminum joints and composite-to-composite joints. In the joints with bonding length-to-width ratio smaller than 1, the strength decreases as the bonding length increases. In the joints with the ratio larger than 1, however, the strength converges to a constant value. Final failure mode of all the specimens was delamination. To use the maximum strength of the adhesive, it is important to design the joint to have strong resistance to delamination.