• Title/Summary/Keyword: 절연 파괴

Search Result 707, Processing Time 0.021 seconds

Electrical Breakdown and Flashover Characteristics of Gaseous Helium at Cryogenic Temperature (극저온 헬륨가스의 절연파괴 및 연면방전 특성)

  • Kwag, Dong-Soon
    • Progress in Superconductivity and Cryogenics
    • /
    • v.14 no.3
    • /
    • pp.38-42
    • /
    • 2012
  • Fixtures such as bushings in terminations of high temperature superconducting(HTS) power cable systems are subjected to high voltages, which have to transition from ambient to cryogenic temperatures. As such it is imperative to ensure the integrity of the dielectrics under all operating conditions, including thermal aspects brought about by the passage of current. Gaseous helium(GHe) at high pressure is regarded as a potential coolant for superconducting cables. The dielectric aspects of cryogenic helium gas are both complex and demanding. In this experimental study we looked at the interface between a smooth epoxy surface and high pressure helium gas in a homogeneous electric field. The alternating current(AC) flashover voltages of epoxy samples are presented. The results have been analyzed by using Weibull statistics. In addition to the behavior of the epoxy in gaseous helium as a function of pressure and temperature we also present data of the characteristics of the epoxy in mineral oil and in liquid nitrogen($LN_2$). The breakdown characteristics of a uniform field gap in gaseous helium as a function of pressure and temperature under AC, direct current(DC) and lightning impulse voltages are also given. Electric field calculations have been made for one of the experimental geometries in an attempt to explain some of the anomalies in the experimental results.

Study on the AC Interfacial Breakdown Properties in the Interface between toughened Epoxy and Silicone Rubber (Toughened 에폭시와 실리콘고무 계면의 교류 절연파괴 현상에 관한 연구)

  • 박우현;이기식
    • Journal of the Korean Institute of Electrical and Electronic Material Engineers
    • /
    • v.15 no.12
    • /
    • pp.1079-1084
    • /
    • 2002
  • Because complex insulation method is used in EHV(extra high voltage) insulation systems, macro Interfaces between two different bulk materials which affect the stability of insulation system exist inevitably. Interface between toughened epoxy and silicone rubber was selected as a interface in EHV insulation systems and tested AC interfacial breakdown properties with variation of many conditions to influence on electrical Properties, such as interfacial pressure, roughness and oil. Specimen was designed to reduce the effect of charge transport from electrode in the process of breakdown and to have the tangential electrical potential with the direction of the interface between epoxy and silicone rubber by using FEM(finite elements method). It could control the interfacial pressure, roughness and viscosity of oil. From the result of this study, it was shown that the interfacial breakdown voltage is improved by increasing interfacial Pressure and oil. In particular, the dielectric strength saturates at certain interracial Pressure level. The decreasing ratio of the interfacial breakdown voltage in non-oiled specimen was increased by the temperature rising, while oiled specimen was not affected by temperature.

Shperulites Formation of Low Density Polyethylene Thin Film and Characteristics of Dielectric Breakdown (저밀도 폴리에틸렌 박막의 결정 형성과 절연파괴 특성)

  • Kang, J.H.;Yu, Y.B.;Kim, J.S.;Park, K.S.;Kim, S.K.;Han, S.O.;Shin, D.K.
    • Proceedings of the KIEE Conference
    • /
    • 1997.07d
    • /
    • pp.1420-1423
    • /
    • 1997
  • To make clearly breakdown rl1cchanism and path at interface of crystal and amorphous region, we fabricated HDPE and LDPE thin film by dropping solution onto glass substrate. then annealed the film at $140^{\circ}C$. Shperulites formation and its interface prepared from of two different materials differ from each other. Comparing breakdown site and breakdown field of HDPE with those of LDPE, we can demonstrate the reason that breakdown holes in HDPE are concentrated on the region of interface. From the result, It is appeared that interface of crystallites lead not to weakness as electrical insulating materials.

  • PDF

A study on the recognition system design of one-time use of a standard plastic garbage bag at automaticat garbage facility (자동 쓰레기 집하 시설에 사용되는 1회사용 종량제 봉투 인식 장치 설계에 관한 연구)

  • Kim, Kea-Kook;Seo, Chang-Ok
    • Proceedings of the Korean Society of Computer Information Conference
    • /
    • 2012.01a
    • /
    • pp.41-43
    • /
    • 2012
  • Today many people are greatly interested in the environment. Especially increasing affluent of food causes a great amount of food waste. To handle this effectively, we now have a lot of problems of disposing garbage all over the world. In Korea, in order to reduce this garbage, we should use a standard plastic garbage bag in which we have to throw away our garbage. So it has an effect on significantly reducing the waste amount every year. Now, there are a lot of cases that residents again use a standard plastic garbage bag. The purpose of this study is to propose algorithm preventing the re-cycling of a standard plastic garbage bag.

  • PDF

The Effect of Conducting Particles on Breakdown Phenomena in GIS (GIS내에서 금속이물이 절연파괴에 미치는 영향)

  • Kim, Min-Kyu;Moon, In-Wook;Kim, Youn-Taeg;Kim, Ik-Soo;Lee, Hyeong-Ho
    • Proceedings of the KIEE Conference
    • /
    • 1994.07b
    • /
    • pp.1574-1576
    • /
    • 1994
  • $SF_6$ gas has become an important insulation medium in modern electric power apparatus, because of its high insulation withstand levels and good arc quenching capability. For the application of $SF_6$ gas in GIS the estimation of insulation properties is a fundamental point. Moreover the reduction of withstand levels in case of inhomogeneous fields caused by particles or fixed protrusions is of special interest. It is known that the presence of free conducting particles in GIS can significantly lower the insulating level of $SF_6$ gas at elevated pressure and also it has been recently shown that dielectric strength is greatly reduced by fast transients such as disconnector surges where metallic particles are involved. In this paper, we have disigned the particle test chamber rated 362kV for the purpose of investigating the discharge characteristics in SF6 gas where inhomogenius fields are caused by metallic particles.

  • PDF

A Stud on the Self Healing Characteristics of MPPF by Voids (보이드에 의한 MPPF의 셀프힐링 특성 연구)

  • 박하용;곽희로
    • Journal of the Korean Institute of Illuminating and Electrical Installation Engineers
    • /
    • v.14 no.4
    • /
    • pp.77-82
    • /
    • 2000
  • This paper describes the self healing characteristics of a metalized polypropylene film(MPPF) by voids under a.c condition. PDIVs were increased with the number of pre-self healing due to void defects, and several pre-self healing events took place at lower voltage than the critical breakdown voltage of a PPF. Self healing mainly occurred at pin tips, wrinkle sides, and cross points of wrinkles, and the main self healing voltage was increased with PPF thickness. The burn out area at self healing was increased with the applied voltage, and the peak currents in a grounding conductor at self healing was also increased with the applied voltage.

  • PDF

A Characteristic of Tracking Progress Happened at the End of the VCTFK (VCTFK 끝단에서 발생되는 트래킹의 진전특성)

  • Jee, Seung-Wook;Kim, Shi-Kuk;Ok, Kyung-Gea;Lee, Chun-Ha;Lee, Kwang-Sik
    • Journal of the Korean Institute of Illuminating and Electrical Installation Engineers
    • /
    • v.24 no.8
    • /
    • pp.78-83
    • /
    • 2010
  • This paper describes the characteristic of tracking progress happened at the end of the polyvinyl chloride insulated cabtyre oval cord(VCTFK) that is widely used for distribution cord. Tracking is occurred owing to the drop of electrolyte at the end of the VCTFK. The tracking progress and its characteristic happened at the end of the VCTFK are as follow; Carbonization and electrical erosion are happened at the end of the VCTFK. Electrical erosion is begun at the insulation layer near conductors. After that, it is also happened at the sheath layer. Accumulation of carbonized insulation and sheath materials at the end of the VCTFK is begun after progress of electrical erosion. When the accumulation is progressed arc discharge is appeared and finally it goes to tracking breakdown.

Electric Fire Prediction by Detection of Spark Signals (스파크 신호검출에 의한 전기화재 예측)

  • 김일권;송재용;길경석;권장우
    • Proceedings of the Korean Institute of Information and Commucation Sciences Conference
    • /
    • 2001.10a
    • /
    • pp.371-374
    • /
    • 2001
  • This paper describes a technique that can predict electric fires by detecting a spark signal generated from operation of electric facilities. An electric fire lead a loss of life as well as huge property, therefore it is very Important to predict an electric fire and eliminate the causes of it. Electrical spark which is ranked as majority causes of electric fires has a characterized frequency bandwidthdistinguishedfrompowerfrequenry. In the experiment, various spark signals are simulated in a condition such as short circuit, flashover and surface discharge. The results showed that the monitoring of spark signals can predict electric fires.

  • PDF

An Insulation Life Time of the Epoxy Composites according to Breakdown Time (파괴시간을 이용한 에폭시 복합체의 절연수명)

  • Shin, C.G.;Kim, J.S.;Cho, C.N.;Lee, D.K.;Lee, S.I.;Park, G.H.;Kim, C.H.
    • Proceedings of the Korean Institute of Electrical and Electronic Material Engineers Conference
    • /
    • 2008.04b
    • /
    • pp.8-9
    • /
    • 2008
  • In the procedure of the estimation, the short time breakdown characteristics for the epoxy composite specimens, which were made with the variation of hardener and/or filler, were tested firstly. Then the long time voltage-to-time test was implemented. Finally, the long time breakdown voltage of each specimen was estimated with the parameters obtained from the statistical treatment with Weibull distribution. Base on the results, it has been found that the optimal weight ratio of epoxy resin/hardener/filler that has the excellent long time breakdown characteristic was 100/100/65. It was due to the silane treatment which relieves the electric field at the interface between filler and epoxy.

  • PDF

The Positive Bubble Effect and the Breakdown Characteristics in $SF_6$ and $LN_2$ ($SF_6$와 액체 질소의 절연파괴특성과 정기포현상)

  • Lee Kwang-Sik;Choi Eun-Hyuck;Park Kwang-Seo;Kim Jong-Whan;Lim Chang-Ho
    • The Transactions of the Korean Institute of Electrical Engineers C
    • /
    • v.54 no.8
    • /
    • pp.355-360
    • /
    • 2005
  • In this paper the experiments of breakdown characteristics by temperature change of $SF_6$ gas, $SF_6$ liquid ($LSF_6$) and $N_2$ liquid ($LN_2$) in model GIS(Gas Insulated Switchgear) were described. From the experiments results, the breakdown voltage of $SF_6$ increases with the drop of temperature and the increase of the inner pressure in model GIS. The ability of $LSF_6$ insulation is higher than high-pressurized $SF_6$ gas and $LN_2$. The breakdown characteristics of $LSF_6$ were produced by bubble formed evaporation of $LSF_6$ and bubble caused by high electric emission. It is considered in this paper that the results are fundamental data for electric insulation design of superconductor and cryogenic equipments machine교 which will be studied and developed in the future.