• Title/Summary/Keyword: 저품위 동광

Search Result 8, Processing Time 0.023 seconds

The Survey on Froth Floatation of Low Grade Copper Ore from the Australia (호주산 저품위 동광의 부유선별에 관한 특성조사)

  • Kim, Joon Soo;Kim, Woo Jin;Hwang, Ha;Kim, Myong Jun;Kim, Wantae
    • Resources Recycling
    • /
    • v.25 no.6
    • /
    • pp.98-104
    • /
    • 2016
  • The purpose of this study is to obtain an optimum condition of the concentrate by floatation using Australian low grade copper ore of suitable particle size by crushing, grinding and sizing. The effect of the dosage of collector, activator, depressant and change of acidity on the floatation was investigated. The floatation conditions comprising of pH 9.0 acidity, 500g/t $CuSO_4{\cdot}5H_2O$ activator, 500g/t K.E.X. collector, 1500g/t $Na_2SO_3$ depressant and 25wt.% plup density were optimized. Grade and recovery of copper in the concentrate obtained by froth floatation under optimum conditions were 4wt.% and 65wt.% respectively.

Study for Seperation Process of Copper from the Low-grade Copper Ore by Hydrometallrugical Process (저품위 동광으로부터 습식제련공정에 의한 구리의 분리 공정 연구)

  • Shin, Dong Ju;Joo, Sung-Ho;Lee, Dongseok;Jeon, Ho-Seok;Shin, Shun Myung
    • Resources Recycling
    • /
    • v.30 no.5
    • /
    • pp.57-66
    • /
    • 2021
  • In this study, we attempted to separate and recover Cu from low-grade copper ore by a hydrometallurgical process. The leaching sample obtained after crushing and sieving by 0.355 mm of low-grade copper ore contained 1.5% Cu, 4.7% Fe, 1.0% Mn, and 0.3% Zn. The Cu in the oxide ore was very well leached into sulfuric acid and 97% Cu leaching efficiency was achieved at 80℃ and 3 M sulfuric acid (H2SO4). From the leaching solution, Cu was separated by solvent extraction from Fe, Mn, and Zn using LIX984N. The separation tendency between Cu and other metals was confirmed through the distribution ratio and separation factor. By plotting the McCabe-Thiele Diagram, the optimum condition for recovering Cu is 5 vol.% LIX984N, 2-stage counter-current solvent extraction, and an O/A ratio of 0.5. Using this method, 99% of the Cu was extracted and a CuSO4 solution was finally obtained that contained 1.6 g/L Cu after the stripping process using 2 M H2SO4.

A Study on the Selective Leaching of the Copper Component by Sulfation Process (황산화 배소법에 의한 구리성분의 선택적 침출연구)

  • Kim, Woo Jin;Kim, Joon Soo;Kim, Myong Jun;Tran, Tam;Lee, Jin-Young;Shin, Shun-Myung
    • Resources Recycling
    • /
    • v.25 no.5
    • /
    • pp.57-63
    • /
    • 2016
  • This study were carried out sulfation roasting and selective leaching test for the effective recovery of copper component in concentrate obtained by froth floatation of Autrallian low grade copper ore. The optimum conditions of sulfation roasting were temp. $450^{\circ}C$, $Na_2SO_4$ 2 mole ratio and time 1.5 h, and then selective leaching were room temperature and $H_2O$ or 1M $H_2SO_4$ solutions. Leaching efficiency of optimum sulfation product were 90 wt.% of copper, 20 wt.% of iron and 15wt.% of nickel elements. In this results, it was possible to selective decomposition leaching of the copper component under optimum conditions in this research.

A study on Bacterical Leaching of Low-Grade Copper Mineral(III) (저품위 동광석의 세균침출에 관한 연구 3)

  • 이강순;민봉희;장정순
    • Korean Journal of Microbiology
    • /
    • v.11 no.2
    • /
    • pp.69-78
    • /
    • 1973
  • In order to investigate the distribution of an iron-oxidizing bacterium, Ferrobacillus ferrooxidans in Korea, the authors had carried out the chemical and microbiological analysis of mine water. The results obtained were as follows : 1. Ferrobacillus ferrooxidans concerned to leaching was isolated from 10 copper mine water out of 46 sites in Korea. 2. As the results of bacterial oxidation, the contents of sulfuric acid, ferric sulphate and copper in the bacteria-bearing solutions were higher than those in bacteria-free solutions.

  • PDF

A Study on Bacterial Leaching of Low-Grade Copper Mineral(IV) (저품위 동광석의 세균침출에 관한 연구 4)

  • 박원구;이강순
    • Korean Journal of Microbiology
    • /
    • v.11 no.4
    • /
    • pp.189-195
    • /
    • 1973
  • With the gradual expansion of copper demands, the utilization of enormous tonnages of waste copper mineral containig up to 0.5% copper becomes available. In order to investigate the possibilities on the application of bacterial leaching method to waste dumps or abandoned mines, the authors had carried out microbial leaching of copper minerals by F.ferrooxidans isolated from the Dalsung copper mine water. The results obtained were as follows : 1. The copper extraction rate from the Dalsung chalcopyrite has been a little accerelated by using flasks in place of percolators. 2. The percentage of copper extracted from the Dalsung chalcopyrite sample was 100% in 30 days in the presence of iron-oxidizing bacteria F.ferrooxidans while 9.27% in the absence of bacteria. 3. F.ferroxidans was capable of producing sufficient quantities of ferric sulfate and sulfuric acid from ferrous iron to bring about the dissolution of 100% of copper from the Dalsung chalcopyrite.

  • PDF

A Study on Bacterial Leaching of Low-Grade Copper Mineral(V) (저품위 동광석의 세균침출에 관한 연구 5)

  • 민봉희;박원구;이강순
    • Korean Journal of Microbiology
    • /
    • v.12 no.1
    • /
    • pp.25-30
    • /
    • 1974
  • It was convinced that with a relatively small capital investment and with a low operating cost, appreciable amounts of cement copper could be produced from low-grade minerals by the application of a bacterial leaching method. For the recovery of cement copper from the impure pregnant solution, direct precipitation of copper with tin plates by a bacterial leaching method was feasible. The results obtained were as follows: 1)In order to remove the cement copper from the reducing metal, aeration and agitation method were more effective and economic than shaking method. 2)The rate of copper recovery from the pregnant solution was accerelated according to increasing quantities of reducing metal. However, the excess of reducing metal reduced the grade of cement copper. 3)Among the comparative experiments of copper recovery at each reaction temperature of $10^{\circ}C$, $20^{\circ}C$, and $30^{\circ}C$, the recovery rate of copper at $30^{\circ}C$from the pregnant solution was highest. 4)Direct cementation method on iron-containing metal was an excellent method for the recovery of cement copper in bacterial leaching.

  • PDF

저품위 동광석의 세균침출에 관한 연구 2

  • 이강순;민봉희;장정순
    • Korean Journal of Microbiology
    • /
    • v.10 no.1
    • /
    • pp.1-8
    • /
    • 1972
  • This experiment was carried out to investigate the physiological characteristics of isolated bacteria, Ferrobacillus ferooxidans from copper mine water in Korea. The results obtained were as follows ; 1. The optimum pH range for the growth of these bacteria was 2.0-3.0 and optimum temperature was $20^{\circ}C$-$30^{\circ}C$. 2. The oxidation curves of ferrous iron to the ferric iron ran parallel with the growth curves. 3. The optimum nitrogen concentration was 400-800 ppm and the minimal flow rate of air for the maximal growth of the bactria was 70 ml air/min./200ml medium. 4. The growth of these bacteria was inhibited by the absence of ferrous iron and by the addition of sulfur. 5. Ferrous iron at a concentration of 9000 ppm, appeared to be optimum for the most rapid growth of Ferrobacillus ferrooxidans.

  • PDF

Studies on the Bacterial Leaching of Low-grada Copper Mlnerals (저품위 동광석의 세균침출에 관한 연구 1)

  • 이강순;오재현;민봉희
    • Korean Journal of Microbiology
    • /
    • v.9 no.3
    • /
    • pp.121-129
    • /
    • 1971
  • The purpose of this study was to investigate the proprieties of practical application and possibility of bacterial leaching method to the low copper minerals in Korea. Therfore, ore samples and mine water of the Talsung, Ilkwang, Taekwang, Yongho and Siheung were analyzed chemically, mineralogically, and bacteriologically. The results obtained were as follows ; 1. The range of pH value was 2.6-3.8. 2. Copper contents in ore samples of Talsung and Ilkwang were 0.38% and 0.63%, and those in mine water of Talsung nad ilkwang were 584 .$\mu$g and 15.$\mu$g per ml, respectively. 3. Ferric sulfate contents in mine water of Tlsung and Ilkwang were 27.2.$\mu$g and 10.5.$\mu$g per ml, respectively. 4. Ferrobacillus ferroosxidans was isolated and identified from Talsung and Ilkwang mine water and specially Thiobacillus thiooxidans was isolated from Ilkwang mine water.

  • PDF