An Experimental Study on the Qualities of Recycled Fine Aggregate and Properties of Mortar Producted by the Dry Manufactured Method (건식 제조방식에 의해 생산된 재생 잔 골재의 품질 및 모르타르 특성에 관한 실험적 연구)

  • 윤종기;장재봉;송민섭;나철성;장종호;김무한
    • Proceedings of the Korea Concrete Institute Conference
    • /
    • 2003.05a
    • /
    • pp.229-232
    • /
    • 2003
  • Recently, it is increased on the concern for the reuse of waste concrete because of the shortage of natural aggregate and the increase of waste concrete. And recycled coarse aggregate is used variously, but the existing wet method producted recycled fine aggregate has problems like the high price facilities, the long time progress of the work and recycled fine aggregate of poor. The aim of this study is to investigate the possibility of the method of dry producted high qualities recycled fine aggregate. The results of this study have shown that the possibility of the method of dry is certificated as the qualities of recycled fine aggregate satisfied the KS and the compressive strength of mortar was similar to plain.

  • PDF

The experimental regarding the affix mortar quanity measurement of the recycled fine aggregate (재생(순환)잔골재의 부착모르타르량 측정에 관한 실험적 연구)

  • Cho Hyun Dae;Jaung Jae Dong;Lee Do Heun;Jun Myoung Hoon
    • Proceedings of the Korea Concrete Institute Conference
    • /
    • 2004.11a
    • /
    • pp.189-192
    • /
    • 2004
  • This study bases on showing the pictures of how to keep a recycled fine aggregate well (quality control) and how to invent the measurement of mortar's quantities which largely effect on basic properties of matter: strength, durability and so on. As a result of the experiment by immersion, quantities of adhesive cement takes 7 to 8 days to stabilize by sulfuric. However, by hydrochloric acid, it takes a little quicker due to the first quick reaction, aggregate of the measurement of adhesive mortar by immersion used acid liquids are likely applicable following a suitable inspection and complementarity.

  • PDF

Evaluation of Reduction of CO2 Emission Achieved by Using Low-carbon Recycled Cement with Cementitious Waste Powder (폐미분말을 원료로 한 저탄소형 재생시멘트의 CO2배출량 저감평가)

  • Kwon, Eun-Hee;Ahn, Jae-Cheol;Park, Dong-Cheon
    • Proceedings of the Korean Institute of Building Construction Conference
    • /
    • 2014.05a
    • /
    • pp.250-251
    • /
    • 2014
  • With the recent movement toward sustainable development, many efforts have been made to reduce environmental loads in various domains of industry. In particular, a great deal of research and technology development has been underway on approaches to reducing industrial waste and the emission of greenhouse gases. For this reason, a quantitative analysis of the reduction in CO2 emission that could be achieved by replacing limestone material with cementitious waste powder was performed in this study. Through the analysis, it was found that CO2 emissions were reduced by up to 50 percent compared with the scenario in which OPC was used, which suggests that it is possible to reduce global CO2 emissions by approximately 5percent, or by 446.4 Tg of the 965 Tg of CO2 emissions generated by the cement industry, in the total global CO2 emissions of 19300Tg.

  • PDF

A Study on the Physical Properties of Recycled Fine Aggregate (by Dry and Wet Type Production formula) Mortar Using Blast Furnace Slag (고로슬래그를 사용한 건식 및 습식 재생 잔골재 모르타르의 물리적 특성에 관한 연구)

  • Shim, Jong-Woo;Lee, Sea-Hyun;Seo, Chi-Ho
    • Proceedings of the Korea Concrete Institute Conference
    • /
    • 2006.11a
    • /
    • pp.501-504
    • /
    • 2006
  • Recycled aggregate mortar contains plenty of calcium hydroxide to improve the strength of blast furnace slag, although the surface mortar made of recycled aggregate deteriorates adhesion to cement paste and blast furnace slag has a low initial strength. Therefore, this study assumes that the combination with both recycled aggregate and blast furnace slag will produce a better performance. The results of the experiment show that dry mortar made of recycled aggregate provides with higher strength than wet mortar does at the 3-day and 7-day age, while lower at the 28-day age. It indicates that a large amount of cement mortar made of dry recycled aggregate has deteriorated adhesion strength. The mixes with 30% and 50% of blast furnace slag and 50% and 75% of recycled aggregate provide with much better strength at the 7-day age, although they usually have latent hydraulic property at the 28-day age. It indicates that calcium hydroxide($Ca(OH){_2}$) in recycled aggregate has affected ground granulated blast furnace slag.

  • PDF

Field Application and Maintenance of sidewalk concrete block for PV Power Generation (태양광 발전을 위한 보도형 콘크리트 블록의 현장 적용과 유지관리)

  • Kim, Bong-Kyun;Kim, Yun-Yong
    • Journal of the Korea institute for structural maintenance and inspection
    • /
    • v.23 no.5
    • /
    • pp.75-83
    • /
    • 2019
  • In order to fulfill the obligation to voluntarily reduce greenhouse gas emissions under the Paris Climate Agreement, the proportion of coal and nuclear power generation is reduced worldwide and national efforts are being made to spread renewable energy including solar power generation. Korea also intends to increase the proportion of renewable energy generation to 30~35% by 2040 by introducing laws and regulations. In addition, while the country is trying to apply solar power generation to sidewalks and roads, there is no research related to it in Korea. Therefore, as a precedent study to develop solar power generation roads, solar power generation concrete blocks applicable to sidewalks and plazas were developed and the applicability was evaluated by constructing them on the site. As a result of indoor experiment, compressive strength was measured by 25.5~35.7MPa and flexural strength was measured by 5.1~10.5MPa, which showed that all domestic standards were satisfied. However, the higher the unit cement amount, the lower the strength was measured according to the mixing of the broken fine aggregate. The absorption rate was 5.7%, which satisfied the domestic standard of 7% or less. As a result of the freeze-thawing test, the reduction rate of the compressive strength after 100 cycles was up to 6.3%. As a result of measuring the settlement amount after construction, the maximum of 2.498mm was measured and irregular settlement occurred in the overall area, which is because the resolution of the sand layer was poor during construction. Maintenance techniques of sidewalk concrete block and solar panel need to be established more efficiently through long-term operation in the further.

Fundamental Properties of Low Strength Concrete Mixture with Blast Furnace Slag and Sewage Sludge (고로슬래그미분말 및 하수슬러지를 활용한 저강도 콘크리트의 기초적 물성)

  • Kwon, Chil Woo;Lim, Nam Gi
    • Journal of the Korea institute for structural maintenance and inspection
    • /
    • v.17 no.3
    • /
    • pp.136-144
    • /
    • 2013
  • In this study, in order to establish a plan that will enable safe use of renewable resources such as diverse industrial by-products and urban recycled materials, we conducted experiments that focused on flow, bleeding, compressive strength and environmental pollution evaluation to evaluate the material properties of low strength concrete using BFS and SS. In the case of low strength concrete using BFS and SS, blending of at least BFS 6000 within a 30% range regardless of the type of sand used was found to be the most effective approach for improving the workability by securing the minimum unit quantity of water, restraining the bleeding ratio and establishing compressive strength by taking account of the applicability at the work site. In particular, in view of the efficient use of SS, the optimal mixing condition was found to be the mixing of BFS 8000 with in the 30% range, not only for improving the workability restraining the bleeding ratio and establishing the compressive strength but also for application to the work site. Further, the results of tests on hazardous substance content and those of elution tests conducted on soil cement using SS indicated that all values satisfied the environmental standards without any harmful effects on the surrounding environment.

Sensitivity of NOx Removal on Recycled TiO2 in Cement Mortar (재생 이산화티탄을 혼입한 모르타르의 NOx 저감률 민감도 분석)

  • Rhee, Inkyu;Kim, Jin-Hee;Kim, Jong-Ho;Roh, Young-Sook
    • Journal of the Korean Recycled Construction Resources Institute
    • /
    • v.4 no.4
    • /
    • pp.388-395
    • /
    • 2016
  • This paper explores the photocatalytic sensitivity of cement mortar incorporated with recycled $TiO_2$ from waste water sludge. Basically, $TiO_2$ cluster sank down slowly to the bottom of cement mortar specimen before setting and hardening process. This leads the mismatch of $TiO_2$ concentration on the top and the bottom faces of a specimen. This poorly dispersed $TiO_2$-cement mortar naturally exhibits poor NOx removal efficiency especially on the top of cementitious structure. In architectural engineering application such as building or housing structures, one can simply filp over from the bottom so that more $TiO_2$ concentrated surface can be placed outward into the air. However, in highway pavement case, this could not be applicable due to in-situ installation of concrete pavement. Hence, the dispersion of $TiO_2$ cluster inside the cementitous material is getting important issue onto road construction application. To elaborate this issue, according to our results, silica fume, high-ranged water reducer, viscosity agent, blast furnace slag were not enhanced much of dispersion characteristics of $TiO_2$ cluster. The combination of foaming agent and accelerator of hardening with viscosity agent and small grain size of fine aggregate may help the dispersion of $TiO_2$ inside cementitious materials. Even though the enhanced dispersion were applied to the specimen, NOx removal efficiency doest not change much for the top surface of the specimen. This concurrently affected by the presence of tiny air voids and the dispersion of $TiO_2$ in that these voids could easily adsorbed NOx gas with the aid of large surface area.