• 제목/요약/키워드: 육성용접

검색결과 103건 처리시간 0.027초

CH-90 용접봉을 이용한 육성 용접부의 마모 특성에 관한 연구 (Wear characteristics of build-up weld metal using CH-90 Electrode)

  • 이보영;안대환;김재성;진형국
    • 대한용접접합학회:학술대회논문집
    • /
    • 대한용접접합학회 2006년 추계학술발표대회 개요집
    • /
    • pp.225-227
    • /
    • 2006
  • As rail steel at a crossing area must undergo much higher loading than those at regular railway, Mn-alloyed steel is normally used for its high load-carrying capability and reduced wear rate. However, as these Mn-alloyed steel is tend to have casting defects, manufacturing cost to produce defect-free Mn-alloyed steel becomes quite expensive. Therefore, in order to replace Mn-alloyed steel, we performed build-up welding using CH-90 and investigated regarding to wear characteristics of build-up weld metal.

  • PDF

주철과 Fe-Mn-Al강 이종금속 용접부의 조직변화에 관한 연구 (A study on the microstructure change during the welding of a cast iron with a Fe-Mn-Al steel powder)

  • 김경중;서정현
    • Journal of Welding and Joining
    • /
    • 제8권4호
    • /
    • pp.35-45
    • /
    • 1990
  • Casting are widely used nodays as complicated and diversified forming materials due to its superior castability. However the welding of cast iron has not been accompaniced satisfactory resulting in an microstructure change happened in the heat affected zone (HAZ), especially the graphite are formed and shaped consecutively in the area and it has great impact on the crack occuring and growth together with martensite forming in this area. It case of gray cast iron welding, it is required for pre-heat treatment or specific welding consumables to restrain forming the martensite in the HAZ. In this study, by applying the plasma surface overlaid welding. Fe-Mn-Al steel powder has been used for improvement of anti-crackability in the HAZ and much attention has been paid to establish the overlaid welding method for gray cast iron so that optimum welding conditions may prevent the cracking. With our experiments, we have found that to prevent defects which may occur in the HAZ, the overlaid welding technique for gray cast iron has been developed.

  • PDF

이상 스테인리스 Clad강 육성 용접부의 기계적 성질에 미치는 후열처리의 영향에 관한 연구 (A Study on Effect of PWHT on Mechanical Properties of Overlaid Weld Metal in Duplex Stainless Clad Vessel)

  • 서창교;김영일;성회준;김대순
    • 대한용접접합학회:학술대회논문집
    • /
    • 대한용접접합학회 2004년도 추계학술발표대회 개요집
    • /
    • pp.174-176
    • /
    • 2004
  • The duplex stainless clad vessel with 38m & over thickness shall be performed to PWHT based on the ASME code. In this case, it is well-known that precipitators such as carbides and sigma($\sigma$) phase are formed at gram boundary between ferrite and austenite phase. Therefore, a weld test for simulating this situation has been planned and performed by 3309LMo71-1 for barrier layer and E2209Tl-1 for 2nd & over layer and then carried out to investigate the overlaid weld metal. Based on the test results, it could be concluded that PWHT should be carried out after the completion of 1st(barrier) layer and then 2 & over layer should be applied.

  • PDF

페라이트계 스테인리강의 FCA 육성용접부 연성 평가 (Evaluation of ferritic stainless steel FCA overlay weld metal ductility)

  • 김영일;최준태;김대순
    • 대한용접접합학회:학술대회논문집
    • /
    • 대한용접접합학회 2006년도 춘계 학술대회 개요집
    • /
    • pp.140-142
    • /
    • 2006
  • The bend ductility of Type 410S ferritic stainless steel overlay weld on carbon steel was investigated. Overlay weld that was stabilized with Nb had large columnar ferrite grain and Nb precipitate on grain boundary. And that caused fracture when bend test without concern of PWHT condition. Proper bend ductility at as-welded condition was achieved by refining ferrite grain with addition of $0.04{\sim}0.09%$ Al and $0.2{\sim}0.5%$ Ti that make oxide, carbide and nitride at high temperature.

  • PDF

1.25Cr-0.5Mo 강에서의 Electro Slag Strip 육성 용접부 특성 (Characteristics of Electro Slag Strip overlaied weldments on the 1.25Cr-0.5Mo Steel)

  • 성희준;주명수;주정권;김영일
    • 대한용접접합학회:학술대회논문집
    • /
    • 대한용접접합학회 2005년도 추계학술발표대회 개요집
    • /
    • pp.65-66
    • /
    • 2005
  • In order to evaluate disbonding properties caused by hydrogen on the Electro Slag Strip Welding for 1.25Cr-0.5Mo steel, two kinds of welding consumables were selected and tested under the disbonding condition of $97.2kgf/cm^{2}$ at $425^{\circ}C$. Chemical composition of the welds showed that they have similar chemical compositions. The microsturucture investigation, however, indicated that 'A' weld has high ratio of coarse grain area, while B weld has low. Disbonding results showed that high ratio coarse grain welds showed unacceptable, while low ratio coarse grain welds showed acceptable.

  • PDF

인코넬 육성용접에 의한 원형 문풀구조 선체블록의 열변형해석 (Thermal Distortion Analysis by Inconel Over-lay at Circular Moonpool Structures)

  • 하윤석
    • 대한조선학회논문집
    • /
    • 제49권4호
    • /
    • pp.304-311
    • /
    • 2012
  • One of the main features of Drillship or FPSO is a moonpool structure. The moonpool structures have various accuracy tolerances according to their functions and targets. This study is mainly interested in roundness of a circular moonpool structure in FPSO. Because this structure needs abrasion-resistance at which bearing of machine touches on inner wall of moonpool, we should do over-lay welding widely and deeply by using Inconel weld material. But a general over-lay can cause a severe distortion at ship block structure. If we can analyze the roundness by thermal distortion under Inconel over-lay, we can establish a special erection policy by the results. In this study, we designed stress-strain curve for strain-boundary condition analysis by an elasto-plastic material property. The results made us to decide an appropriate ship-block size and policy of crane manipulation will follow for its capacity. If a structure that needs over-lay is not large, solid elements also are not a bad choice for FEM modeling. Therefore we also developed a standard of using strain-boundary method that shell elements are used as over-lay on solid element modeling.

ABAQUS 서브루틴을 이용한 레일 보수용접 잔류응력 해석 (Residual Stress Analysis of Repair Welded Rail Using the ABAQUS User Subroutine)

  • 김동욱;전현규;이상환;장윤석
    • 한국정밀공학회지
    • /
    • 제33권7호
    • /
    • pp.551-558
    • /
    • 2016
  • Reduction of welding residual stress is very important in the railway industry, but calculating its distribution in structures is difficult because welding residual stress formation is influenced by various parameters. In this study, we developed a finite element model for simulating the repair welding process to recover a surface damaged rail, and conducted a series of parametric studies while varying the cooling rate and the duration of post weld heat treatment (PWHT) to find the best conditions for reducing welding residual stress level. This paper presents a three-dimensional model of the repair welding process considering the phase transformation effect implemented by the ABAQUS user subroutine, and the results of parametric studies with various cooling rates and PWHT durations. We found that heat treatment significantly reduced the residual stress on the upper rail by about 170 MPa.

연주롤용 육성용접 재료의 고온마모 및 부식특성에 미치는 Nb, V의 영향 (The Effects of Nb, V on the High Temperature Wear and Corrosion of the Overlaying Materials for Continuous Casting Rolls)

  • 김창규;황동수;윤재홍;강창룡;곽희환
    • 동력기계공학회지
    • /
    • 제8권3호
    • /
    • pp.30-35
    • /
    • 2004
  • In the steel making industries, the continuous casting process has been applied to the number of company because of its economical benefit. Casting rolls are utilized for frictional drive and transport of solidifying slap. Dimensional tolerances, mechanical stability and surface condition of the cast roll can affect both the surface and internal quality of the product being cast. To overcome these problems, the industry is accelerating on the rate of technology improvements. Samples were overlaid on the S45C steel by submerged arc welding process. And the hardness, wear, electrochemical corrosion and oxidation tests were carried out. Test results were that all these materials were satisfying basic requirements of caster rolls. By these results, the addition of 0.1%Nb and 0.15%V increase mechanical properties and tempering resistance by its superior carbide forming characteristics in low carbon $12{\sim}13%Cr$ martensitic stainless steels.

  • PDF