• Title/Summary/Keyword: 용출수

Search Result 1,262, Processing Time 0.027 seconds

Elution Properties of Naringin from Soft Contact Lens Containing Naringin (나린진(naringin)이 함유된 소프트 콘택트렌즈에서 나린진의 용출 특성)

  • Ryu, Geun-Chang;Jun, Jin;Jin, Moon-Seok;Chae, Soo-Chul;Kim, In-Suk
    • Journal of Korean Ophthalmic Optics Society
    • /
    • v.13 no.3
    • /
    • pp.45-50
    • /
    • 2008
  • Purpose: A soft contact lens was manufactured by adding naringin known as natural anti-bacterial material to resin solution. With solution eluted from manufactured contact lens, we examined its optical properties, physical and chemical states of naringin in the polymer, and elution properties. Methods: The soft contact lens with naringin was synthesized by bulk polymerization method. IR spectrum and HPLC were used to define the bonding type of naringin itself in the soft contact lens contained naringin, elution process of naringin to the saline solution, and the amount of naringin solution eluted from the lens with elapsed time. Results: Naringin was continuously eluted with constant concentration from the soft contact lens for about a month and the structure ofnaringin which is eluted was as same as before it was added to resin solution. Any change in optical properties such as transmittance couldn't be found. Bonding state and the structure of naringin in contact lens were explained with IR spectrum and HPLC results. Conclusions: In the contact lens with naringin, naringin remained in the contact lens bonding with weak hydrogen bonding and/or van der Waals force between naringin and polymer. Naringin was continuously eluted from the contact lens contained naringin during about 1 month. Even after 1 month, it showed that the concentration of the naringin eluted was approximately 10 ppm in a day. From the results, adding naringin to the soft contact lens resin is very effective method for manufacturing the soft contact lens which has anti-bacterial function for a period of time.

  • PDF

Immediate Drug Release Enhancement of Nateglinide Using Fumaric Acid (푸마르산을 이용한 나테글리니드 함유 속방출형 제형의 약물방출 개선에 관한 연구)

  • Lee, Sung-Hoon
    • Journal of the Korea Academia-Industrial cooperation Society
    • /
    • v.18 no.1
    • /
    • pp.506-512
    • /
    • 2017
  • The purpose of this study was to improve release rate and bioavailability of nateglinide formulation. Polymorphism selection and particle size control were performed to enhance formulation dissolution rate, and a pH modifier was included in the formulation to overcome pH-dependent solubility of nateglinide. The enhanced dissolution rate was characterized by using a dissolution test. The results showed that H-type raw material had a higher dissolution rate than that of B-type raw material. There was 6.2% difference in dissolution between the two materials at 60 min. With regard to particle size, raw material with a $1.13{\mu}m$ particle size showed a 20% faster release rate than that of raw material with a $2.28{\mu}m$ particle size. Furthermore, fumaric acid was included in formulation as a pH modifier. That addition produced a greater than 50% improvement in dissolution rate. In conclusion, dissolution rate of nateglinide can be enhanced by optimizing its polymorphism and particle size; moreover, a synergistic effect on the enhancement of dissolution rate is obtained by including fumaric acid, a pH modifier, in the formulation.

용융아연도금 공정에서 초기 Fe 함량이 강판의 용출속도에 미치는 영향 및 강판의 용출 메커니즘 고찰

  • Lee, Sang-Myeong;Park, Ju-Hyeon
    • Proceedings of the Korean Institute of Surface Engineering Conference
    • /
    • 2016.11a
    • /
    • pp.106-106
    • /
    • 2016
  • 강의 산화 및 부식을 방지할 수 있는 표면처리 강판의 수요가 늘어나고 있다. 그 중 용융아연도금 강판은 뛰어난 경제성 및 도금성, 그리고 희생적 방식 특성으로 각광받고 있다. 자동차용 강판의 경우 도금 공정 이후의 표면 상태가 매우 중요하다. 도금 공정의 주된 표면 결함은 강판이 도금욕 내에서 이동 하면서 수반된 도금욕 내의 Zn-Fe-Al dross 입자에 기인한다. 도금공정 중 강판으로부터 용출된 Fe는 도금욕 내의 Zn 와 Al 과 반응하여 밀도가 높은 Bottom dross 나 밀도가 낮은 Top dross를 형성한다. 이에 본 연구에서는 강판으로부터 Fe의 용출속도에 미치는 도금욕 내 초기Fe 농도의 영향을 속도론적으로 평가하였다. 본 연구에서는 'Finger rotating method (FRM)' 방법론을 적용하였으며. 실험을 위해 수직 관상로 내부에 Zn-Al-Fe 시료를 장입한 알루미나 도가니를 위치시킨 후 온도를 $455^{\circ}C$로 설정하고, 지름 20mm의 Iron rod를 회전모터에 연결하여 Zn-Al-Fe 용탕에 침적한 후 회전시켰다. 실험 결과, 초기 Fe 함량과 용탕의 Fe포화 농도의 차이가 적을수록 Fe의 용출 속도는 감소하였으며 Dross 생성량 또한 적었다. 용탕 및 Iron rod 샘플 관찰 결과를 바탕으로 회전하는 Fe 시편으로부터 도금욕으로의 Fe 용출 메커니즘을 고찰하였다. 용출 모델을 토대로 모델링 한 결과, 용탕 내 Fe 농도 변화양상이 모델링 data와 실험 data가 동일한 양상을 보임을 확인 하였다.

  • PDF

The Neutralization Treatment of Waste Mortar and Recycled Aggregate by Using the scCO2-Water-Aggregate Reaction (초임계이산화탄소-물-골재 반응을 이용한 폐모르타르와 순환골재의 중성화 처리)

  • Kim, Taehyoung;Lee, Jinkyun;Chung, Chul-woo;Kim, Jihyun;Lee, Minhee;Kim, Seon-ok
    • Economic and Environmental Geology
    • /
    • v.51 no.4
    • /
    • pp.359-370
    • /
    • 2018
  • The batch and column experiments were performed to overcome the limitation of the neutralization process using the $scCO_2$-water-recycled aggregate, reducing its treatment time to 3 hour. The waste cement mortar and two kinds of recycled aggregate were used for the experiment. In the extraction batch experiment, three different types of waste mortar were reacted with water and $scCO_2$ for 1 ~ 24 hour and the pH of extracted solution from the treated waste mortar was measured to determine the minimum reaction time maintaining below 9.8 of pH. The continuous column experiment was also performed to identify the pH reduction effect of the neutralization process for the massive recycled aggregate, considering the non-equilibrium reaction in the field. Thirty five gram of waste mortar was mixed with 70 mL of distilled water in a high pressurized stainless steel cell at 100 bar and $50^{\circ}C$ for 1 ~ 24 hour as the neutralization process. The dried waste mortar was mixed with water at 150 rpm for 10 min. and the pH of water was measured for 15 days. The XRD and TG/DTA analyses for the waste mortar before and after the reaction were performed to identify the mineralogical change during the neutralization process. The acryl column (16 cm in diameter, 1 m in length) was packed with 3 hour treated (or untreated) recycled aggregate and 220 liter of distilled water was flushed down into the column. The pH and $Ca^{2+}$ concentration of the effluent from the column were measured at the certain time interval. The pH of extracted water from 3 hour treated waste mortar (10 ~ 13 mm in diameter) maintained below 9.8 (the legal limit). From XRD and TG/DTA analyses, the amount of portlandite in the waste mortar decreased after the neutralization process but the calcite was created as the secondary mineral. From the column experiment, the pH of the effluent from the column packed with 3 hour treated recycled aggregate kept below 9.8 regardless of their sizes, identifying that the recycled aggregate with 3 hour $scCO_2$ treatment can be reused in real construction sites.

Environmental Leachability of Electric Arc Furnace Dust for Applying as Hazardous Material Treatment (제강분진을 이용한 유해물질 처리기술 적용을 위한 안전성 평가)

  • Lee, Sang-Hoon;Kang, Sung-Ho;Kim, Jee-Hoon;Chang, Yoon-Seok
    • Journal of Korean Society of Environmental Engineers
    • /
    • v.28 no.3
    • /
    • pp.329-336
    • /
    • 2006
  • Iron manufacturing process involves production of various by-product including slag, sludge, sintering and EAF(Electric Arc furnace dust). Some of the by-products such as EAF and sintering dust are disposed of as waste due to their high heavy metal contents. It has been notice for many years that the EAF dust also contain about 65% of Fe(0) and Fe(II) and then the possible utilization of the iron. One possibility is to apply the EAF as a lining material in conjunction with clay or HDPE liners, in waste landfill. The probable reaction between the leachate containing toxic elements such as TCE, PCE dioxine and $Cr^{6+}$ is reduction of the toxic materials in corresponding to the oxidation of the reduced iron and therefore diminishing the toxicity of the leachate. It is, however, prerequisite to evaluate the leaching characteristics of the EAF dust before application. Amelioration of the leachate would be archived only when the level of toxic elements in the treated leachate is less than that of in the untreated leachate. Several leaching techniques were selected to cover different conditions and variable environments including time, pH and contact method. The testing methods include availability test, pH-stat test and continuous column test. Cr and Zn are potentially leachable elements among the trace metals. The pH of the EAF dust is highly alkaline, recording around 12 and Zn is unlikely to be leached under the condition. On the contrary Cr is more leachable under alkaline environment. However, the released Cr should be reduced to $Cr^{3+}$ and then removed as $Cr(OH)_3$. Removal of the Cr is observed in the column test and further study on the specific reaction of Cr and EAF dust is underway.

A Study on the Hydration Property of Mortar with Balst Furnace Slag using Water Eluted from Recycled Coarse Aggregates (순환골재 용출수를 활용한 고로슬래그 미분말 혼입 모르터의 강도특성)

  • Shin, Sang-Yeop;Jeong, Euy-Chang;Kim, Young-Soo
    • Proceedings of the Korean Institute of Building Construction Conference
    • /
    • 2012.11a
    • /
    • pp.81-82
    • /
    • 2012
  • The purpose of this study is the hydration properties of motar using Blast-Furnace Slag(BFS) with water elured from recycled coarse aggregate. The results of the experiment show that the water eluted from recycled coarse aggregate mixed with blast furnace slag has comparatively higher hydration activity than the mortar not mixed with one in early-age mortar causing the calcium hydroxide in the recycled coarse aggregate to work on as a stimulus to the hydration of ground granulated blast furnace slag. BFS mixed with the eluting water the hydration reaction was a promotion.

  • PDF

Bench Scale급 건식 가스화기에서 생성된 Slag의 분석

  • 이계봉;조성수;유희종;윤용승
    • Proceedings of the Korea Society for Energy Engineering kosee Conference
    • /
    • 1996.10b
    • /
    • pp.123-128
    • /
    • 1996
  • Bench Scale급 건식 가스화기에서 중국 Datong탄과 미국 Alaska Usibelli탄으로부터 생성된 Slag의 구조적인 특성과 화학적인 특성을 조사하였다. Datong slag은 표면이 매끄럽고 검으며 속이 약간 비어 있는 구형을 띄고 있고 Alaska Usibelli탄으로부터의 slag은 속이 조밀하게 차여있는데, 이들 slag의 내부는 Datong, Alaska Usibelli탄 두 경우 다 회분이 결정화된 형상의 특징을 보여주고 있다. 그리고 Cu, Zn외 11가지 중금속이 slag에 다량으로 농축되어 제거되었음을 알 수 있었으며, slag들의 침출여부를 조사하기 위하여 용출시험을 수행한 후 용출액에 대하여 중금속 분석을 한 결과 대부분 중금속들은 검출되지 않았다. 내화재의 주성분인 Cr이 slag에 포함되어 나오는 것으로 측정되었으나 용출시험 결과 검출이 안되어 2차오염에는 전혀 문제가 없음이 입증되었다. 따라서 건식 가스화기로부터 생성된 slag을 재사용할 때, 용출되는 중금속에 관한 2차 환경오염이 유발되지 않을 것으로 확인되었다.

  • PDF

새로운 오메프라졸염의 개발 및 제제화 연구

  • 이계주;이기명;이창현;우종수
    • Proceedings of the Korean Society of Applied Pharmacology
    • /
    • 1994.04a
    • /
    • pp.329-329
    • /
    • 1994
  • OMZ과 HP-$\beta$-CD 포접화합물의 유형은 $A_{L}$ type의 가용성 복합체이며, CD, UV, IR, DSC, XRD pattern 및 $^1$H-NMR 방법으로 측정한 포접화합물의 결함형태는 OMZ의 benzimidazole부분이 HP-$\beta$-CD 공동에 포접된 형태이었고, OMZ과 HP-$\beta$-CD의 결합조성몰비는 1:1, 안정도 상수는 약 34 M$^{-1}$이었다. 또한 cholestyramine 수지와 OMZ 복합체는 방출양상이 신속하였다. OMZ-cholestyramine 수지염은 안정성이 양호하고 용출율이 우수한복합체로 경구용 재제를 개발할 수 있었으며, 용출시험 및 산 저항성이 양호하고 pellet의 제조에 있어서 core의 제조는 정제수 : 에탄올(7: 3) 결합액을 이용하여 lactose를 주로 사용하고 기타 PEG 6000, sorbitol, Avicel PH101, sodium lauryl sulfate 및 무수 PVP K-30을 적절히 배합하여 제조하고, 장용코팅의 내산성은 90.5% 이었으며, 소장에서의 용출경향이 85%이상이 10분 이내에 용출되어 규정에 적합하였다.

  • PDF

Modeling Leaching Concentrations of Gasoline Components from Residual Gasoline in Contaminated Soil (오염토양 중 잔류가솔린의 용출농도에 대한 모델링 연구)

  • 염익태;이상현;허상철;안규홍
    • Proceedings of the Korean Society of Soil and Groundwater Environment Conference
    • /
    • 1998.06a
    • /
    • pp.38-42
    • /
    • 1998
  • Soil venting이 오염토양중 가솔린의 용출거동에 미치는 영향을 정량적으로 예측하기 위하여 가솔린의 휘발과 용해거동이 Raoult의 법칙에 의해 설명되어 질 수 있는지를 평가해보았다. 먼저 순수 가솔린의 용해거동과 휘발거동에 대해 검토해 보고 이후 토양중 가솔린의 거동에 적용하여 보았다. 가솔린성분들의 용해거동은 휘발에 의한 성분조성의 변화와 상관없이 Raoult의 법칙에 의해 비교적 정확하게 예측될 수 있었으며 오차범위는 naphthalene을 제외하고는 최고 $\pm$ 100% 이내였다. 오염토양의 형태로 가솔린이 존재하는 경우에도 Raoult의 법칙에 의해 정확히 예측될수 있었으나 토양중 농도가 초기 20,000 mg/kg에서 1,360 mg/kg로 감소한 경우에는 용출농도가 예측치의 50-70% 수준으로 낮은 경향을 보였다. 한편 soil venting시 휘발에 따른 조성변화를 Raoult의 법칙을 이용하여 산정하고 각 성분조성에 대한 개별물질들의 용출잠재성을 결정하는 모델을 이용하여 실험결과와 비교하여 보았다.

  • PDF

Solidification/Stabilization of Heavy Metals in Sewage Sludge Prior to Use as a Landfill Cover Material (매립지 복토재로의 활용을 위한 하수슬러지 내 중금속의 고형화/안정화)

  • Park, Youn-Jin;Shin, Won-Sik;Choi, Sang-June;Lee, Hoon-Ha
    • Journal of Korean Society of Environmental Engineers
    • /
    • v.32 no.7
    • /
    • pp.665-675
    • /
    • 2010
  • The effects of chemical binders (ladle slag, ordinary portland cement (OPC), hydroxyapatite and calcium hydroxide) on the solidification/stabilization of heavy metals (Cd, Cu, Ni, Pb, Zn) in sewage sludge were evaluated by chemical leaching tests such as EDTA extraction, TCLP and sequential extraction. The results of EDTA extraction showed that heavy metal concentrations in sewage sludge were highly reduced after solidification/stabilization with slag, cement or calcium hydroxide. However, EDTA interrupted solidification/stabilization of heavy metals by hydroxyapatite. The TCLP-extracted heavy metal concentrations in sewage sludge after solidification/stabilization with chemical amendments were highly reduced. However, Cu concentration in the sewage sludge solidified/stabilized with slag, cement or calcium hydroxide increased because the pH of TCLP solution was higher than 7. Mixtures of sludge 1 : slag 0.2 : calcium hydroxide 0.1 (wt ratio) showed the least leachability in batch TCLP and EDTA extraction. The results of sequential extraction (SM&T, formaly BCR) indicated that the distribution of heavy metals changed from exchangable and carbonate fractions to strongly bound organic fraction. It was found that maximum leachate concentrations of Ba, Cd, Cr and Pb from sewage sludge amended with slag and calcium hydroxide were far below US EPA TCLP regulations.