• Title/Summary/Keyword: 열 응력

Search Result 1,241, Processing Time 0.03 seconds

Life-time Prediction of a FKM O-ring using Intermittent Compression Stress Relaxation (CSR) and Time-temperature Superposition (TTS) Principle (간헐 압축응력 완화와 시간-온도 중첩 원리를 이용한 FKM 오링의 수명 예측 연구)

  • Lee, Jin-Hyok;Bae, Jong-Woo;Kim, Jung-Su;Hwang, Tae-Jun;Park, Sung-Doo;Park, Sung-Han;Min, Yeo-Tae;Kim, Won-Ho;Jo, Nam-Ju
    • Elastomers and Composites
    • /
    • v.45 no.4
    • /
    • pp.263-271
    • /
    • 2010
  • Intermittent CSR testing was used to investigate the degradation of an FKM O-ring, also the prediction of its life-time. An intermittent CSR jig was designed taking into consideration the O-ring's environment under use. The testing allowed observation of the effects of friction, heat loss, and stress relaxation by the Mullins effect. Degradation of O-rings by thermal aging was observed between 60 and $160^{\circ}C$. In the high temperature of range ($100-160^{\circ}C$) O-rings showed linear degradation behavior and satisfied the Arrhenius relationship. The activation energy was about 60.2 kJ/mol. From Arrhenius plots, predicted life-times were 43.3 years and 69.9 years for 50% and 40% failure conditions, respectively. Based on TTS (time-temperature superposition) principle, degradation was observed at $60^{\circ}C$, and could save testing time. Between 60 and $100^{\circ}C$ the activation energy decreased to 48.3 kJ/mol. WLF(William-Landel-Ferry) plot confirmed that O-rings show non-linear degradation behavior under $80^{\circ}C$. The life-time of O-rings predicted by TTS principle was 19.1 years and 25.2 years for each failure condition. The life-time predicted by TTS principle is more conservative than that from the Arrhenius relationship.

Studies on the Reinforced Effect of Rubber Elastomer by means of Milled Glass Fiber Treated with Silane Coupling Agents (Silane Coupling제(劑) 처리(處理) Glass Fiber에 의(依)한 탄성체(彈性體)의 보강효과(補强效果)에 관(關)한 연구(硏究))

  • Lee, Sang-Hyun;Yoo, Chong-Sun;Paik, Nam-Chul
    • Elastomers and Composites
    • /
    • v.22 no.3
    • /
    • pp.204-212
    • /
    • 1987
  • The purpose of this study is to investigate the reinforced effect between MGF treated silane coupling agents and rubber matrix under the configuration chemical bonds, also the effect of triazine thiol compounds. For this study, vulcanizates were prepared with fifteen different compounding formulas. Their vulcanization characteristics, physical properties were examined by means of the ODR(Oscillating Dist Rheometer), the tensile tester, the benzene swelling test. The results of this study obtained are as follows: 1. In the ODR test, the MA vulcanizate was the fastest one in terms of having reached to optimum cure time($t_{90}$) and, with the same formula, when MGF vulcanizates, the shortest optimum cure times has appeared. 2. The SA, SC vulcanizates were the best the other in the physical properties such as 100%modulus, 200%modulus, 300%modulus, tensile strength. The SB vulcanizate, with higher density of crosslinking than other vulcanizates. The vulcanizates, which were filled with MGF treated with silane coupling agents we were the higher density of crosslinking than vulcanizates filled with MGF only. 3. In aging properties, the silica vulcanizates appeared to be better than the other vulcanizates. The aging Properties of treated MGF vulcanizates were similar to the silica vulcanizates. The(CR+APS+silica) and(CR+APS+MCF) were easily crosslinked by exposure to the air, and the physical properties have been improved.

  • PDF

Estimation of Lateral Dynamic P-multiplier of Group Pile Using Dynamic Numerical Analysis Results (동적 수치해석 결과를 이용한 군말뚝의 횡방향 동적 P-승수 산정)

  • Park, Jeong-Sik;Jeong, Sang-Seom
    • KSCE Journal of Civil and Environmental Engineering Research
    • /
    • v.38 no.4
    • /
    • pp.567-578
    • /
    • 2018
  • In this study, to investigate the effect of the stress reduction of group piles by dynamic loading, a dynamic p-y curve was established and the dynamic p-multiplier was calculated. Dynamic numerical analysis was performed by input sinusoidal waves to the bottom of the pile - ground system for $2{\times}2$ group pile, single pile and $5{\times}5$ group pile, single pile in dry sandy soil, and the pile spacing was changed to 2.5 and 5.0 times of the pile diameter. By establishing and comparing the dynamic p-y curves of the single pile and group piles, the dynamic group pile effect of the piles according to the pile center spacing and row position of the group pile piles is analyzed. $5{\times}5$ showed symmetry of the dynamic P-multiplier value around the pile origin coordinate. The dynamic p-multiplier value at the single pile, $5{\times}5$ pile (pile spacing: 2.5D) is 0.26 ~ 0.30 at the pile number 3, pile number 23, 0.14 pile number 13, and 0.14 ~ 0.38 at the pile number 5, pile number 18. These values differed from the static p-multiplier, especially due to the different loading conditions. The dynamic p-multiplier ($P_{dm}$) estimation through various types of input dynamic loads is expected to be used for dynamic design and analysis of group pile-ground systems of civil foundation structures.

Rheological Properties of Calrose Rice and Effect of Thawing Methods on Quality Characteristics of Frozen Turmeric Rice (칼로스 쌀의 유변학적 특성과 이로 제조된 냉동 강황밥의 해동방법에 따른 품질특성 변화)

  • Kim, So Yeon;Choi, Yu Ra;Kim, Kyeong Seop;Lee, Sang Jun;Chang, Yoon Hyuk
    • Journal of the Korean Society of Food Science and Nutrition
    • /
    • v.46 no.6
    • /
    • pp.771-777
    • /
    • 2017
  • This study investigated the rheological properties of Calrose rice flour dispersions as well as the effects of different thawing methods (steamer, smart oven, and microwave oven) on quality characteristics of frozen turmeric rice. Apparent viscosity, consistency index, and yield stress significantly increased at higher rice flour concentrations. Magnitudes of storage modulus and loss modulus significantly increased with elevation of rice flour concentration. Frozen turmeric rice thawed using a steamer had the highest moisture content and largest size (length, width, and thickness) among all thawing methods. The L values of turmeric rice after thawing using a steamer was significantly higher than those of other thawing methods. The a value of turmeric rice after thawing using a steamer was significantly lower than those of other thawing methods. Textural properties (hardness, adhesiveness, springiness, cohesiveness, brittleness, and chewiness) of frozen turmeric rice after thawing using a steamer were significantly lower than those of other thawing methods. Therefore, it can be concluded that frozen turmeric rice after thawing using a steamer might be desirable for improvement of texture.

Comparative Study of Near-Wall Treatment Methods for Prediction of Heat Transfer over Gas Turbine Nozzle Guide Vane (가스터빈 노즐 베인의 열전달 예측을 위한 벽면처리법 비교연구)

  • Bak, Jeonggyu;Kim, Jinuk;Lee, Seawook;Gang, Youngseok;Cho, Leesang;Cho, Jinsoo
    • Transactions of the Korean Society of Mechanical Engineers B
    • /
    • v.38 no.7
    • /
    • pp.639-646
    • /
    • 2014
  • The comparative analysis of near-wall treatment methods that affect the prediction of heat transfer over the gas turbine nozzle guide vane were presented. To achieve this objective, wall-function and low Reynolds number methods, and the transition model were applied and simulated using NASA's C3X turbine vane. The predicted turbine vane surface pressure distribution data using the near-wall treatment methods were found to be in close agreement with experimental data. However, the predicted vane metal temperature and heat transfer coefficient displayed significant differences. Overall, the low Reynolds method and transition model did not offer specific advantages in the prediction of temperature and heat transfer than did the wall-function method. The Reynolds stress model used along with the wall-function method resulted in a relatively high accuracy of prediction of the vane metal temperature and heat transfer coefficient.

Cure and Mechanical Behaviors of Cycloaliphatic/DGEBA Epoxy Blend System using Electron-Beam Technique (전자선 조사에 의한 고리지방족/DGEBA 에폭시 블렌드 시스템의 경화 및 기계적 특성)

  • 이재락;허건영;박수진
    • Polymer(Korea)
    • /
    • v.27 no.3
    • /
    • pp.210-216
    • /
    • 2003
  • 4-Vinyl-1-cyclohexene diepoxide (VCE)/diglycidyl ether of bisphenol-A (DGEBA) epoxy blends with benzylquinoxalinium hexafluoroanti-monate were cured using an electron-beam technique. The effect of DGEBA content to VCE on cure behavior, thermal stabilities, and mechanical properties was investigated. The composition of VCE/DGEBA blend system vaned within 100:0, 80:20, 60:40, 40:60, 20:80, and 0:100 wt%. The cure behavior and thermal stability of the cured specimens was monited by near-infrared spectroscopy and thermogravimetric analysis, respectively. Also, the critical stress intensity factor ($_{4}$) test of the cured specimens was performed to study the mechanical interfacial properties. As a result, the decreases of short side-chain structure and chain scission were observed in NIR measurements as the DGEBA content increases, resulting in varying the hydroxyl and carbonyl groups. And, the initial decomposition temperature (IDT), temperature of maximum weight loss (T$\_$max/), and decomposition activation energy (E$\_$d/) as thermal stability factors were increased with increasing the DGEBA content. These results could be explained by mean of decreasing viscosity, stable aromatic ring structure, and grafted interpenetrating polymer network with increasing of DGEBA content. Also, the maximum $_{4}$ value showed at mixing ratio of 40:60 wt% in this blend system. in this blend system.

Ohmic Contact of Ti/Au Metals on n-type ZnO Thin Film (Ti/Au 금속과 n-type ZnO 박막의 Ohmic 접합 연구)

  • Lee, Kyoung-Su;Suh, Joo-Young;Song, Hoo-Young;Kim, Eun-Kyu
    • Journal of the Korean Vacuum Society
    • /
    • v.20 no.5
    • /
    • pp.339-344
    • /
    • 2011
  • The Ohmic contact of Ti/Au metals on n-type ZnO thin film deposited on c-plane sapphire substrates by pulsed laser deposition was investigated by TLM (transfer length method) patterns. The Ti/Au metal films with thickness of 35 nm and 90 nm were deposited by electron-beam evaporator and thermal evaporator, respectively. By using the photo-lithography method, the $100{\times}100{\mu}m^2$ TLM patterns with $6{\sim}61{\mu}m$ gaps were formed. To improve the electrical properties as well as to decrease an interface states and stress between metal and semiconductor, the post-annelaing process was done in oxygen ambient by rapid thermal annealing system at temperature of $100{\sim}500^{\circ}C$ for 1 min. In this study, it appeared that the minimum specific contact resistivity shows about $1.1{\times}10^{-4}{\Omega}{\cdot}cm^2$ in $300^{\circ}C$ annealed sample, which may be originated from formation of oxygen vacancies of ZnO during an oxidation of Ti metal at the interface of Ohmic contacts.

Assessment of a Pre-conceptual Design of a Spent PWR Fuel Disposal Container (가압경수로형 사용후핵연료 처분용기의 예비 개념설계 평가)

  • Choi, Jong-Won;Cho, Dong-Keun;Lee, Yang;Choi, Heui-Joo;Lee, Jong-Youl
    • Journal of Nuclear Fuel Cycle and Waste Technology(JNFCWT)
    • /
    • v.4 no.1
    • /
    • pp.41-50
    • /
    • 2006
  • In this paper, sets of engineering analyses were conducted to renew the overall dimensions and configurations of a disposal container proposed as a prototype in the previous study. Such efforts and calculation results can provide new design variables such as the inner basket array type and thickness of the outer shell and the lid & bottom of a spent nuclear fuel disposal container. These efforts include radiation shielding and nuclear criticality analyses to check to see whether the dimensions of the container proposed from the mechanical structural analyses can provide a nuclear safety or not. According to the results of the structural analysis of a PWR disposal container by varying the diameter of the container insert, the Maximum Von Mises stress from the 102 cm-container meets the safety factor of 2.0 for both extreme and normal load conditions. This container also satisfies the nuclear criticality and radiation safety limits. This decrease in the diameter results in a weight loss of a container by $\sim20$ tons.

  • PDF

Design and Prototyping of Lifting Devices for Manhole Cover using Structural Analysis and 3D Printing (3D 프린팅과 구조해석을 이용한 맨홀의 부양장치 설계 및 제작)

  • Lee, Hyoungwook
    • Journal of the Korea Academia-Industrial cooperation Society
    • /
    • v.19 no.10
    • /
    • pp.648-654
    • /
    • 2018
  • In order to maintain manholes installed on the road, the manhole should be easy to open and close. Manhole covers under harsh conditions require that they can be lifted when attempting to open the manhole because the frame and cover are stuck and difficult to open and close. In this study, the design of a lifting mechanism was carried out to improve and integrate the locking type manhole. The mechanism of the locking manhole is that when the bolt located at the center is turned, the hub connected with the bolt descends, and the hook connected to the hub is rotated. The end of the hook is hooked to the manhole frame. The auxiliary device was installed on the hook so that the manhole cover can be lifted. The structure was designed to endure about 300kg of lifting force based on 70% of the yield stress of the hook to perform lifting function. The shape design was performed through the structural analysis using the finite element method. First, the basic design was performed with the simplified 2-dimensional model and the attachment position and shape were designed through the 3-dimensional model. In order to find out the structural problems of the designed shape, the scale downed model was fabricated through 3D printing and confirmed that the lifting function worked. Finally, it was confirmed that both the locking and the average lifting of about 6.1 mm can be done by applying the lifting mechanism through the machining and applying it to the existing locking manhole.

Pre-conceptual Design of a Spent PWR Fuel Disposal Container (가압경수로형 사용후핵연료 처분용기의 예비 개념설계 평가)

  • CHO Dong-Keun;CHOI Jongwon;Lee Yang;CHOI Heui-Joo;LEE Jong-Youl
    • Proceedings of the Korean Radioactive Waste Society Conference
    • /
    • 2005.11a
    • /
    • pp.153-162
    • /
    • 2005
  • In this Paper, sets of engineering analyses were conducted to renew the overall dimensions and configurations of a disposal container proposed as a prototype in the previous study. Such efforts and calculation results can provide new design variables such as the inner basket array type and thickness of the outer shell and the lid & bottom of a spent nuclear fuel disposal container. These efforts include radiation shielding and nuclear criticality analyses to check to see whether the dimensions of the container proposed from the mechanical structural analyses can provide a nuclear safety or not. According to the results of the structural analysis of a PWR disposal container by varying the diameter of the container insert, the Maximum Von Mises stress from the 102 cm container meets the safety factor of 2.0 for both extreme and normal load conditions. This container also satisfies the nuclear criticality and radiation safety limits. This decrease in the diameter results in a weight loss of a container by ${\~}$20 tons.

  • PDF