• Title/Summary/Keyword: 압축 잔류응력

Search Result 242, Processing Time 0.024 seconds

The Signal Characteristics from Crack of Brittle Materials by Vickers Load (비커스 압입 하중에 의한 취성재료의 균열 신호특성)

  • Nam, Ki-Woo;Kim, Hyun-Soo
    • Journal of the Korean Society for Nondestructive Testing
    • /
    • v.22 no.2
    • /
    • pp.125-131
    • /
    • 2002
  • we analyzed acoustic emission signals obtained from three kinds of brittle materials under compression load by Vickers hardness tester. The results obtained can be summarized as follows; The signal in each material could be divided into three signal based on the properties of load. All specimens were not detected acoustic emission signals in stage II which was load constant region., and were detected in stage I and stage III. Glass was detected high amplitude signals in stage III. $Al_2O_3\;and\;Al_2O_3/Sic$ were detected high amplitude signals in stage I.

Microscopic precision evaluation of machined surface according to the variation of cooling and lubrication method (냉각.윤활방식 변화에 따른 가공면의 미시적 정밀도 평가)

  • Hwang I.O.;Kwon D.H.;Kang M.C.;Kim J.S.
    • Proceedings of the Korean Society of Precision Engineering Conference
    • /
    • 2006.05a
    • /
    • pp.225-226
    • /
    • 2006
  • As the technique of high-speed end-milling is widely adopted to machining field. The investigation for microscopic precision of workpiece is necessary for machinability evolution. The environmental pollution has become a big problem in industry and many researcher have investigated in order to preserve the environment. The environmentally conscious machining and technology have more important position in machining process. In the milling process, the cutting fluid has greatly bad influence on the environment. The damaged layer affect mold life and machine parts in machining. In this study, the cutting force, the surface roughness, micro hardness and residual stress is evaluated according to machining environment. Finally, it is obtained that the characteristics of damaged layer in environmentally conscious machining is better than that in conventional machining using cutting fluid.

  • PDF

A Study on the Grinding Characteristics according to Oil Mist Supply Method (오일 미스트 분사 방법에 따른 연삭특성)

  • 허남환;이석우;최헌종
    • Proceedings of the Korean Society of Precision Engineering Conference
    • /
    • 2002.10a
    • /
    • pp.254-257
    • /
    • 2002
  • As the large Coolant amount used of a machine holds mass serious trouble recently, an environment pollution is increased, and a machine is conquering large specific gravity in an empty cost plane. It is the stage that must reexamine the parts washing that processing is later with this current way or a problem of a liquid waste treatment back. The environmental problems by using coolant demanded the new cooling methods. As one of them, the studies on the grinding with compressed cold air and oil mist have been done. The cooling method using compressed cold air was effective through going down the temperature of compressed air supplied below -$25^{\circ}C$ and increasing the amount of compressed cold air, but had not enough cooling effect due to the low performance of lubrication. Therefore, the cooling methods using oil mist newly were suggested. This method can satisfy both cooling effect and lubrication with only small amount of coolant, also have the benefit in the point of decreasing the environmental pollution. This paper focused on analyzing the grinding characteristics of the cooling method using oil mist. The grinding test according to compressed cold air and oil mist supply direction were done.

  • PDF

Effect of Static Load Level of Ultrasonic Nanocrystal Surface Modification Technology on Fatigue Characteristics of SKD61 (초음파 나노 표면개질 기술의 정하중 레벨이 SKD61 강의 피로특성에 미치는 영향)

  • Suh, Chang-Min;Kim, Sung-Hwan
    • Journal of Ocean Engineering and Technology
    • /
    • v.22 no.2
    • /
    • pp.99-105
    • /
    • 2008
  • Ultrasonic nanocrystal surface modification (UNSM) is a method to induce severe plastic deformation to a material surface, so that the structure of the material surface becomes a nanocrystal structure from the surface to a certain depth. It improves the mechanical properties, namely hardness, compressive residual stress, and fatigue characteristics. Specimens of SKD61 were tested to verify the effects of the variation of UNSM static load level on fatigue characteristics. The results were as follows: the grain size of SKD61 treated with UNSM became very fine from the material surface to a $100{\mu}m$ depth. The surface hardness of SKD61 was increased up to 37% after UNSM. And fatigue strength at $10^7$ cycles was increased by 8.3, 11.2, and 17.9% respectively, when the static load levels of UNSM were 4, 6, 8 kgf.

The Effect of Fatigue Fracture in shot peening Marine structural steel at stress ratio (쇼트피닝 가공된 해양구조용강의 피로파괴에 미치는 응력비의 영향)

  • Park, Kyoung-Dong;Han, Kun-Mo;Jin, Young-Beom
    • Proceedings of the Korea Committee for Ocean Resources and Engineering Conference
    • /
    • 2003.10a
    • /
    • pp.138-144
    • /
    • 2003
  • Rencentely, the request for the light weight is more incresed in the area of industrial environment and machinery and consistent effort is needed to accomplish high strength of material for the direction of light weight. we got the following characteristic from crack growth test carried out in the range of stress ration of 0.1, 0.3 and 0.6 by means of opening mode displacement. At the content stress ratio, the threshold stress intensity factor crack range ${\Delta}K_{th}$in the early stage of fatigue crack growth (Region I) and dtress intensity factor range ${\Delta}K$ in the stable of fatigue crack growth (Region II) with an increase in ${\Delta}K$. Fatigue life shows more improvement in the Shot-peened material than in the Un-peening material. And compressive residual stress of surface on the Shot peening processed operate resistance force of fatigue. So we can obtain fallowings. (1) The fatigue crack growth rate on stage II is conspicuous with the size of compressive residual stress and is depend on Paris equation. (2) Although the maxium compressive residual stress is deeply and widely formed from surface, fatigue life does not improve than when maxium compressive residual stress is formed in surface. (3) The threshold stress intensity factor range is increased with increasing compressive residual stress.

  • PDF

Effect of Stress Ratio on Fatigue Fracture of a Shot Peening Marine Structural Steel (쇼트피닝 가공된 해양구조용강의 피로파괴에 미치는 응력비의 영향)

  • PARK KYOUNG-DONG;JIN YOUNG-BEOM;PARK HYOUNG-DONG
    • Journal of Ocean Engineering and Technology
    • /
    • v.18 no.5
    • /
    • pp.43-49
    • /
    • 2004
  • The lightness of components required in the automobile and machine industry necessitates the use of high strength components. In particular, the fatigue failure phenomena, which occurs when using metal, increases the danger to human life and property. Therefore, antifatigue failure technology is an integral part of current industries. Currently, the shot peening is used for removing the defect from the surface of steel, while improving the fatigue strength on surface. Therefore, in this paper, the effect of compressive residual stress of spring steel(JISG SUP-9) by shot-peening on fatigue crack growth characteristics in a stress ratio(R=0.1, R=0.3, R=0.6) was investigated, giving consideration to fracture mechanics. By using the methods mentioned above, following conclusions are drawn: (1) The fatigue crack growth rate(da/dN) of the shot-peening material was lower than that of the un-peening material and in stage I, ΔKth, the threshold stress intensity factor of the shot-peen processed material is high in critical parts, unlike the un-peening material. Also m, fatigue crack growth exponent and number of cycle of the shot-peening material, was higher than that of the un-peening material, as concluded from effect of da/dN. (2) Fatigue life shows more improvement in the shot-peening material than in the un-peening material, and the compressive residual stress of surface on the shot-peen processed operate resistance of fatigue crack propagation.

A Fundamental Study on the Fracture Mechanism of Steel Plates under Completely Alternating Load (완전교번하중하(完全交番荷重下)에서의 강판(鋼板)의 파괴기구(破壞機構)에 관한 기차적(基磋的) 연구(研究))

  • Chang, Dong Il;Chung, Yeong Wha
    • KSCE Journal of Civil and Environmental Engineering Research
    • /
    • v.2 no.3
    • /
    • pp.1-13
    • /
    • 1982
  • Transition process of plastic region. displacements, stresses and strains ahead the flaw tips were analysed by the finite element method on the steel plate with the circular hole and the one with the elliptical hole under completely alternating load (repetition of tensile loading, unloading and compressive loading). As the results, the followings were obtained. Transition process of elastic failure (yielding) region was estimated. From this the tendency was confirmed that the fracture would be initiated from ahead the flaw tip, and propagated along the $45^{\circ}$ direction. The fundamental data available in estimating the stress intensity factor that was considered as the core in analysing the fracture mechanism of steel plates were obtained. It was indicated that when unloading after tension the effect of compressive loading, and even the compressive reyield, was occured ahead the flaw tip. Similarly it was indicated that when unloading after compression the effect of tensile loading, and even the tensile reyield, was occured ahead the flaw tip. It was considered that these phenomena were occured because the unloading effect was constrained by the residual strains when unloading. It was considered that the fatigue phenomenon was occured ahead, the flaw tip by repetition of tensile yield, the above compressive reyield, compressive yeild and the above tensile reyield. In addition, the tendency was confirmed that the fracture ahead the flaw tip was occured as the flaw was changed from the circular hole to the elliptical hole and became to be the crack lastly.

  • PDF

Finite Element Post-buckling Analysis of Steel-Concrete Composite Column (철골-콘크리트 합성기둥의 후좌굴 거동에 관한 해석 연구)

  • Oh, Myoung Ho;Kim, Myeong Han;Kim, Sang Dae
    • Journal of Korean Society of Steel Construction
    • /
    • v.19 no.6
    • /
    • pp.725-735
    • /
    • 2007
  • The local buckling strength and post-local buckling strength of thin steel plates in the steel-concrete composite column were evaluated by nonlinear finite element analyses. The proposed width-to-thickness limit ratio was based on elastic buckling analyses, in which the increased local buckling capacity of the plate due to the in-filled concrete was considered by the boundary conditions of the thin plate. Considering the initial imperfections and residual stresses, we determined the initial local buckling strength and post-local buckling strength of the thin plates with various width-to-thickness ratios. The formula to evaluate the compressive capacity of the steel-concrete composite column based on the effective width of the plate was proposed. For verification, values determined by the formula were compared with the experimental results.

Contact Analysis of a Spherical Particle Between Elastomeric Seal and Steel Surface (시일과 스틸면 사이에 구형입자가 있는 접촉문제의 해석)

  • Park, Tae-Jo;Jo, Hyeon-Dong
    • Transactions of the Korean Society of Mechanical Engineers A
    • /
    • v.34 no.2
    • /
    • pp.161-166
    • /
    • 2010
  • Elastomeric seals are widely used in dynamic seal applications, and it is well known that the sealing surfaces can be gradually worn out. Abrasive wear is known to be the most dominant factor; however, little research has been carried out on this problem until now. In this study, a new contact problem related to elastomeric seals-a small spherical particle and steel surface-was modeled and analyzed using MARC. Variations of von-Mises and residual stress distributions as well as deformed seal and steel surface shapes with seal materials and interferences are presented. The stress distribution and surface deformation are highly affected by the elastic properties of seal. For PTFE, the maximum von-Mises stress exceeds the yield strength, and plastic deformation occurs on the steel surface. Therefore, the sealing surface can also be worn down by sub-surface fatigue due to intervening hard particles in the sealing surfaces together with the well-known abrasion.

A Study on the Microstructure and Fatigue Properties of TiNi/A16061 Shape Memory Composite (TiNi/A16061 형상기억복합재료의 미세조직 및 피로특성에 관한 연구)

  • Yun, Du-Pyo;Park, Yeong-Cheol;Kim, Sun-Guk;Lee, Jun-Hui;Lee, Gyu-Chang
    • Korean Journal of Materials Research
    • /
    • v.8 no.11
    • /
    • pp.993-998
    • /
    • 1998
  • In this study TiNi/A16061 shape memory composite is introduced as one of new material using a shape memory alloy. High tensile strength of composite due to compressive residual stress in matrix by the shape memory effect of TiNi fiber can be produced. This composite can remove the tensile residual stress by the difference of coefficients of thermal expansion between fiber and matrix. one of the significant weak point of metal matrix composite. In this paper, shape memory composites are made by squeeze casting. And then, microstructure and fatigue properties of the composites by shape memory effect above inverse transformation temperature A, of TiNi alloy are discussed. The results of the fatigue crack control properties of TiNi/A16061 shape memory composite by a squeeze casting are summarized as follows the effect of fatigue crack propagation control at 363K increases according to the increase of volume fraction and prestrain in composites.

  • PDF