Atmospheric corrosion rate and corrosivity categories of industrial metals in Asan area (아산지역에서 산업재료의 대기부식속도 측정)

  • Kim, Jin-Hyung;Lee, Jong-Kwon
    • Journal of the Korea Academia-Industrial cooperation Society
    • /
    • v.14 no.10
    • /
    • pp.4653-4657
    • /
    • 2013
  • The atmospheric corrosion rate were measured in Asan area for four years according to ISO 9224. The tested metals chosen as the most frequently used in industry, aluminum were copper, carbon steel, weathgering steel, and galvanized steel. The assessed corrosivity categories was 3 in average. The corrosivity categories of asan area was higher than typical rural area and even urban area, whereas it slightly lower than marine area. The results were discussed, specially as the regional climatic characteristics.

Characterization on the Behavior of Heavy Metals and Arsenic in the Weathered Tailings of Songcheon Mine (송천광산의 풍화광미 내 중금속 및 비소 거동 특성)

  • Lee, Woo-Chun;Kim, Young-Ho;Cho, Hyen-Goo;Kim, Soon-Oh
    • Journal of the Mineralogical Society of Korea
    • /
    • v.23 no.2
    • /
    • pp.125-139
    • /
    • 2010
  • Behavior of heavy metals and arsenic in the tailings of Songcheon Au-Ag mine was characterized via both mineralogical and geochemical methods. Mineral composition of the tailings was investigated by X-ray diffractometry, energy-dispersive spectroscopy, and electron probe micro-analyzer (EPMA) and total concentrations of heavy metals and arsenic and their chemical forms were analyzed by total digestion of aqua regia and sequential extraction method, respectively. The results of mineralogical study indicate that the tailings included mineral particles of resinous shape mainly consisting of galena, sphalerite, pyrite, quartz, and scorodite, and specifically socordite was identified in the form of matrix. EPMA quantitative analyses were performed to evaluate the weatherability of each mineral, and the results suggest that it decreased in the sequence of arsenopyrite > galena > sphalerite > pyrite. The weathering pattern of galena was observed to show distinctive zonal structure consisting of secondary minerals such as anglesite and beudantite. In addition, almost all of arsenopyrite has been altered to scorodite existing asmatrix and galena, sphalerite, and pyrite which have lower weatherability than arsenopyrite were identified within the matrix of scorodite. During the process of alteration of arsenopyrite into scorodite, it is likely that a portion of arsenic was lixiviated and caused a great deal of detrimental effects to surrounding environment. The results of EPMA quantitative analyses verify that the stability of scorodite was relatively high and this stable scorodite has restrained the weathering of other primary minerals within tailings as a result of its coating of mineral surfaces. For this reason, Songcheon tailings show the characteristics of the first weathering stage, although they have been exposed to the surface environment for a long time. Based on the overall results of mineralogical and geochemical studies undertaken in this research, if the tailings are kept to be exposed to the surface environment and the weathering process is continuous, not only hazardous heavy metals, such as lead and arsenic seem to be significantly leached out because their larger portions are being partitioned in weakly-bound (highly-mobile) fractions, but the potential of arsenic leaching is likely to be high as the stability of scorodite is gradually decreased. Consequently, it is speculated that the environmental hazard of Songcheon mine is significantly high.

Mechanical Deterioration Characteristics of ACSR due to a Flame (화염으로 인한 ACSR의 기계적 열화 특성)

  • 박창기;이광식;강지원;김영달
    • Journal of the Korean Institute of Illuminating and Electrical Installation Engineers
    • /
    • v.17 no.6
    • /
    • pp.160-168
    • /
    • 2003
  • In Korea, a large portion of aerial power-transmission cables is installed in the mountains. In the case of a fire in the mountains, steel wires coated with zinc and aluminum wires of those power cables exposed to the fire or near around will be deteriorated by the blaze and the high temperature. Deterioration proceeds by interactions of a variety of factors like quality, manufacturing process, the condition of installation and exposure environment of a wire, and so on. Generally, the characteristic of a conductor affect by a forest fire can not be analyzed without the effect through simulating a forest fire. However, there are little research accomplishments of that kind of simulation about it, and there's been no analysis of a sample exposed to an actual forest fire. This thesis shows the experimental results that apply to a new wire by an artificial flame-maker because it's difficult to directly analyze the characteristic of deterioration by a forest fire. Those results include the intensity of extension and wrench for a conductor. In addition, there's been an experiment and analysis about the mechanical characteristics of the wire of ACSR 480[$\textrm{mm}^2$] which was removed from Pohang area by a forest fire. Then, the database will be made to predict the state of deteriorated wires by a forest fire using those two data, and data necessary to diagnose the life state of an ACSR wire affected by a forest fire will be given.

Characteristics of Elements Extraction in Waste Rocks on the Abandoned Jangpoong Cn Mine (장풍 동광산 폐광석 내 원소의 용출 특성)

  • Lee, In-Gyeong;Choi, Sang-Hoon
    • Economic and Environmental Geology
    • /
    • v.41 no.6
    • /
    • pp.695-708
    • /
    • 2008
  • In order to evaluate the geochemical behaviors of elements with waste rocks in the abandoned Jangpoong Cu mine area, total concentration analysis and leaching experiments were performed. The content of elements within waste rocks compared with background values decreased in order of As>>Cu>Pb>Cd>Co. Leaching experiments were carried out at various extraction environments, considering the acid rain ($0.00001{\sim}0.001N\;HNO_3$) and the acid mine drainage ($0.001{\sim}0.1N$ HNO3). After 24 hours of reaction with different acidic solution, the leaching characteristics of waste rocks were classified into three types according to final pH of leaching solution. Type I refers to the case that the final pH of leaching solution was lower than that of the reaction solution due to the dissolution of acidic minerals from rocks, while type 2 and 3 refer to the case that the final pH maintained higher than that of the reaction solution. Theses types include in acid buffering minerals such as clay minerals and carbonate minerals. The leaching characteristics of the elements after the reaction could be categorized into As-Co-Fe, Cu-Mn-Cd-Zn, and Pb. As-Co-Fe started to get leached under 2.5 of pH regardless of changes in the final pH, and Cu-Mn-Cd-Zn showed different initial leaching pH according to the types of final pH changes. Based on the pH value where leaching started regardless of leaching concentration, the relative mobility of each element was in the order of Mn Zn>Cd>Cu>>Fe Co>As>Pb. Thus, more higher mobility elements(Zn, Mn and Cu) were leached by reacting with acid rain water. Acid mine drainage may result in distributions of elements having relatively less mobility(As, Fe, Co and Pb).

Hydrothermal Alteration and Its Cenetic Implication in the Casado Volcanic-hosted Epithermal Cold-Silver Deposit: Use in Exploration (가사도 화산성 천열수 금은광상의 열수변질대 분포 및 성인: 탐사에의 적용)

  • 김창성;최선규;최상훈;이인우
    • Journal of the Mineralogical Society of Korea
    • /
    • v.15 no.3
    • /
    • pp.205-220
    • /
    • 2002
  • The gold-silver deposits in the Casado district were formed in the sheeted and stockwork quartz veins which fill the fault fractures in volcanic rocks. K-Ar dating of alteration sericite (about 70 Ma) indicates a Late Cretaceous age for ore mineralization. These veins are composed of quartz, adularia, carbonate, and minor of pyrite, sphalerite, chalcopyrite, galena, Ag-sulfosalts (argentite, pearceite, Ag-As-Sb-S system), and electrum. These veins are characterized by chalcedonic, comb, crustiform and feathery textures. Based on the hydrothermally altered mineral assemblages, regional alteration zoning associated with mineralization in the Gasado district is defined as four zones; advanced argillic (kaolin mineral-alunite-quartz), argillic (kaolin mineral-quartz), phyllic (quartz-sericite-pyrite) and propylitic (chlorite-carbonate-quartz-feldspar-pyroxene) zone. Phyllic and propylitic zones is distributed over the study area. However, advanced argillic zone is restricted to the shallow surface of the Lighthouse vein. Compositions of electrum ranges from 14.6 to 53.7 atomic % Au, and the depositional condition for mineralization are estimated in terms of both temperature and sulfur fugacity: T=245。$~285^{\circ}C$, logf $s_2$=$10^{-10}$ ~ $10^{-12}$ Fluid inclusion and stable isotope data show that the auriferous fluids were mixed with cool and dilute (158。~253$^{\circ}C$ and 0.9~3.4 equiv. wt. % NaCl) meteoric water ($\delta^{18}$ $O_{water}$=-10.1~8.0$\textperthousand$, $\delta$D=-68~64$\textperthousand$). These results harmonize with the hot-spring type of the low-sulfidation epithermal deposit model, and strongly suggest that Au-Ag mineralization in the Gasado district was formed in low-sulfidation alteration type environment at near paleo-surface.

Measurement of Adhesion Strength of Polyurethane Foam to Surface-Treated Carbon Steel and Effect of Water Vapor Absorption (발포 폴리우레탄과 탄소강과의 접착 강도 측정 및 수증기 흡착의 영향)

  • 김장순;조재동;임연수
    • Polymer(Korea)
    • /
    • v.27 no.4
    • /
    • pp.340-348
    • /
    • 2003
  • A previous stud-pull test was modified to measure the bond strength of polyurethane foam to carbon steel substrate. This test was appropriate in that the specimen foamed on Zn phosphated steel (0.95 kN) was broken at higher load than that of smooth galvanizing treated steel (0.38 kN). Among the samples foamed on the substrate atvarious preheating temperatures, the polyurethane foam to the steel held over 60$^{\circ}C$ exhibited very high bond strength. The samples were exposed at water vapor absorption, and, then, their bond strengths were measured. The adhesion was significantly reduced in the samples foamed on the steel at temperatures below 40$^{\circ}C$ and above 70$^{\circ}C$. For the polyurethane foams formulated with two blowing gases, the adhesion was higher by 0.03 kN in the samples with HCFC-l4lb than that with HFC-245fa. When the these samples were exposed at water vapor soaking, the reduction of the bond strength for the HFC-245fa blown sample was negligible due to smaller area fraction of void area filled with gas at interfacial area. Consequently, it was found that adhesion of polyurethane foam to metal substrate was determined by variation of microstructural features with substrate preheating, surface treatment type of blowing agent.

식품중의 발암성 물질 -니트로소 화합물-

  • 성낙주
    • Proceedings of the Korean Journal of Food and Nutrition Conference
    • /
    • 1997.06b
    • /
    • pp.11-12
    • /
    • 1997
  • 니트로소디메틸아민이 발암성 물질이라는 것이 1954년 Barnes와 Magee에 의해 발견된 이래 이것이 지금까지 학자들에게 관심의 대상이 되고 있는 이유는 발암력이 강하여 극미량으로도 생체내에 암을 유발시킬 수 있을 뿐만 아니라, 대부분의 발암성 물질이 신체의 특정기관에 발암작용을 나타내는데 비해 이 물질은 신체의 여러 부위에 암을 유발시킬 수 있다는 점 그리고 이 물질이 햄, 소시지, 베이컨, 알코올음료, 김치 및 어류 가공품 등 어려 가지 식품에 널리 분포되어 있다는 사실 등을 들 수 있다. 니트로소 화합물은 구조로 보아 티트로소아민과 니트로소아미드로 구분되는데 전자는 제 2급 아연이 산화질소 유도체와 반응하여 생성된 니트로소 유도체이과 후자는 오소, 아미드 등이 치환된 니트로소 유도체로서 화학적인 성질이나 생물학적인 작용이 상이하다. 즉 니트로소아민은 식품에서 안정한 화합물인 반면에 대부분의 니트로소아미드는 불안정하다. 지금까지 연구된 바에 의하면 3백 여종의 니트로소 화합물에 대하여 동물실험을 행한 결과 발암성이 90% 이상 인정되었다. 식품 중 니트로소 화합물의 전구물질 중 질산염과 아질산염은 식품의 가공 저장 및 조리과정 중 니트로화의 된 전구물질인데 이는 육가공품의 색소고정, Cl. Botulinum에 의한 식중독 방지 및 풍미의 향상을 위하여 수 세기 동안 식품첨가제를 사용되어 왔으며, 유럽이나 미국 등지에서는 아직도 육가공품에 아질산염의 첨가가 논란의 대상이 되고 있다. 식품 중 니트로소 화합물에 대한 북유럽 식품 3천여 점을 분석한 결과 검출된 니트로소 화함물은 니트로소디메틸아민이 대부분이며 맥주에서 66%로 검출률이 가장 높았고 다음으로 염지육 및 치즈의 순 이었다. 조리한 일본산 해산 식품 중에 니트로소디메틸아민이 최고 313$\mu$g/kg, 캐나다산 해산 건조 식품에서는 67$\mu$g/kg, 홍콩산 염건어에는 1,400 $\mu$g/kg , 훈연어류에는 N-nitrosothiazolidine이 13,700 $\mu$g/kg , 우리 나라 해산 식품 중 니트로소디메틸아민은 건조가오리, 동결건조명태, 건조오징어, 굴비 및 소건새우 등에서 2.8~86.0 $\mu$g/kg 으로서 비교적 높은 양이 검출되었을 뿐 아니라 이들 식품을 조리할 경우 3.6~13배 증가하였다. 또한 김치와 젓갈류 중에서도 니트로소디메틸아민이 검출된다는 연구가 있다. 식품 중 니트로소 화합물의 생성율 억제시키기 위하여 최근 20여년간 연구된 바를 요약하면 아스코르브산과 같은 억제제의 첨가, 가공방법 및 조리방법의 개선이 비교적 바람직한 방법으로 인정되고 있다. 위의 방법을 적용하여 베이컨을 조리한 결과 낮은 온도에서 오랜 시간 가열하는 것이 높은 온도에서 짧은 시간 가열한 것보다 니트로화 반응이 훨씬 낮았고 또 마이크로웨이브로 조리하는 것이 니트로소아민을 최소화 시키는 방법이었다. 염지육은 아스코르브산이나 토코페롤 등의 니트로화 억제제를 첨가할 경우 니트로소 화합물이 현저히 감소 하였는데 이는 산화질소의 소거 능력이 우수하기 때문인 것으로 밝혀졌다. 가공방법의 개선으로서는 가공시 식품을 공기에 노출시킬 경우 특히 직화로 가열된 공기에 노출되면 니트로소아민의 생성이 매우 높은 것으로 보고되어 있는데 그 대표적인 예로 맥아를 직화로 건조할 경우 맥주 중에 니트로소 화합물이 훨씬 높은 양이 검출된다고 보고되어 있다. 대체로 식품의 가공 조리 및 저장 중 니트로소화합물에 대한 메커니즘은 상세히 밝혀져 있으나 생체내에서의 생성이나 억제 등에 대한 연구는 아직도 미흡한 실정이라이 분야에 대한 연구가 절실히 요구된다.

  • PDF

Effects of Indomethacin on the Production of Cytokines in Mice Exposed to Excessive Zinc (과량의 아연에 노출된 생쥐의 사이토카인 생산에 미치는 인도메타신의 영향)

  • 채병숙;신태용
    • YAKHAK HOEJI
    • /
    • v.46 no.4
    • /
    • pp.258-264
    • /
    • 2002
  • Zinc plays an important role in immunobiological responses, while excessive zinc attenuates immune functions in a dose-dependent manner. Zinc excess has been reported to increase levels of plasma prostaglandin E$_2$ (PGE$_2$), which is known to inhibit production of Th (helper T) 1-associated cytokines and to induce inflammatory responses. Thus, this study was investigated the effects of indomethacin, a potent inhibitor of PGE$_2$ synthesis, on the proinflammatory cytokine and lymphokine production in ICR mice exposed to excessive zinc. Indomethacin at doses of 5 mg/kg was administered i.p. 30 minutes before zinc chloride (Zn) 30 mg/kg orally daily for 10 days. Excessive Zn remarkedly increased tumor necrosis factor (TNF)-$\alpha$ and interleukin (IL)-1$\beta$ levels in both serum and splenic supernatants compared with those in controls, while indomethacin significantly reduced the excessive Zn-induced levels of IL-1$\beta$. In serum, excessive Zn significantly decreased the levels of IL-2 and interferon (IFN)-${\gamma}$ compared with those in controls, whereas indomethacin significantly enhanced the excessive Zn-decreased levels of IFN-${\gamma}$ but did not affect the Zn-decreased levels of serum IL-2. In splenic supernatants, All of excessive Zn, indomethacin, and combination of Zn and indomethacin significantly enhanced IL-2 levels compared with those in controls, but indomethacin didn't affect the Zn-induced production of IL-2. These data, therefore, suggest that indomethacin significantly attenuated the in vivo and ex vivo IL-1$\beta$ production increased by excessive zinc and remarkedly enhanced the in vivo excessive zinc-suppressed production of IFN-${\gamma}$ but not IL-2.

Experimental Study on the Torque Coefficient and Clamping Force of High Strength Bolts Subjected to Environmental Parameters (고력볼트 시공환경에 따른 토크계수와 체결축력에 관한 실험적 연구)

  • Lee, Hyeon Ju;Nah, Hwan Seon;Kim, Kang Seok;Kim, Jin Ho;Kim, Jin Man
    • Journal of Korean Society of Steel Construction
    • /
    • v.20 no.1
    • /
    • pp.43-53
    • /
    • 2008
  • Because the torque control method, which is also caled the clamping method in domestic construction sites, is affected by a variation of the torque coefficient, quality control of the torque coefficient is essential. This study was focused to evaluate the effects of several environmental factors and errors when installing bolts while tightening high-strength bolts. Conditioning environmental parameters include wet, rusty and exposure-to-air-only conditions. In addition, because of errors in workability such as instalation of two washers, upset washers are selected. During the tests, torque, torque coefficient, tension and angle of nut rotation were obtained using a bolt testing machine. Test specimens of four types of bolts (High-Strength Hexagon bolt on KS B 1010, Torque Shear Bolt on KS B 2819, High-Strength Hexagon bolt coated with zinc, and ASTM 490 bolt) were recomended. Based on test results, the tightening characteristics subjected to environmental parameters were investigated and compared with the results in normal condition.

Assessment of Zeolite Soil Mixture as Adsorptive Fill Material at Industrial Zones (산업단지에서의 흡착 성토재로써 제올라이트 토양혼합물의 특성평가)

  • Kwon, Patrick Sun;Rahim, Shahrokhishahraki;Park, Jun Boum
    • KSCE Journal of Civil and Environmental Engineering Research
    • /
    • v.39 no.1
    • /
    • pp.203-209
    • /
    • 2019
  • A number of industrial zones in South Korea were reported contaminated by heavy metals. Such contamination could cause severe damage to the subsurface environment including soil and groundwater. The treatment of zeolite mixing with soil at the bottom of such industrial zones might prevent, or at least reduce the damage of contamination by adsorption of the heavy metals from the leakage. However, such mixtures should maintain the proper bearing capacity as a foundation fill material from the geotechnical point of view at the same time. To investigate the effect of mixtures of zeolite with local soils for the adsorption of heavy metals (Zn, Pb) and sustainability of bearing capacity, adsorption isotherm tests and direct shear test with compaction tests were performed. Results showed that the mixing zeolite with local soils effectively reduces the spreading of the heavy metal contamination when maintaining its proper geotechnical properties as a fill material of industrial zones.