• Title/Summary/Keyword: 아연도강관

Search Result 9, Processing Time 0.03 seconds

A Secular Change of Strength for Galvanized Steel Pipes for Vinyl Housing (비닐하우스용 아연도강관의 강도경년변화 시험(농업시설))

  • 남상운;김문기;권혁진
    • Proceedings of the Korean Society of Agricultural Engineers Conference
    • /
    • 2000.10a
    • /
    • pp.296-301
    • /
    • 2000
  • Bend test for metallic materials was conducted on samples of galvanized steel pipes being used in greenhouse farms. A secular change of yield strength for galvanized steel pipes was analyzed with the part of buried in the ground and exposed in the atmosphere. From those experimental results and corrosion rate of galvanized film, the standard durable years for pipe framed greenhouses are estimated that the small sized pipe houses of movable type is 7∼8 years and the large sized pipe houses of fixed type is 14∼15 years.

  • PDF

CLPP of Biofilm on Different Pipe Materials in Drinking Water Distribution System (수돗물속에서 관재질에 따른 생물막의 CLPP)

  • Lee Dong-Geun;Lee Jae-Hwa;Lee Sang-Hyeon;Ha Bae-Jin;Ha Jong-Myung
    • Journal of Life Science
    • /
    • v.14 no.6 s.67
    • /
    • pp.891-894
    • /
    • 2004
  • The effect of pipe materials on biofilm communities were investigated by CLPP (community level physiology profile) using Biolog GN plates. Heterotrophic bacterial concentrations were $10^4\;-\;10^6\;CFU/cm^2$ and there was no differences between galvanized iron and carbon steel. Average optical density of Biolog plate was similar between two pipe materials. However, CLPP was different according to the type of pipe materials and exposed times to tap water, and CLPP was independent of bacterial concentration. This represents the differences of bacterial communities with pipes and water contact times.

Resistance of Biofilm Bacteria to Chlorination (생물막 세균의 염소소독제에 대한 내성)

  • 조재창;박성주;김상종
    • Korean Journal of Microbiology
    • /
    • v.31 no.3
    • /
    • pp.255-260
    • /
    • 1993
  • The Enterobacter cloacae biofilms developed on slide glasses and galvanized-iron coupons were applied to test the attached bacterial resistance to chlorination. The chlorine resistances of biofilm bacteria grown on the slide glasses and galvanized-iron coupons were 14 and 480 times that of the suspended bacteria, respectively. The chlorine resistance of particleattached bacterial populations was 48 times that of suspended bacterial populations. The biofilm bacterial densities developed on the slide glasses and galvanized-iron coupons which were immersed in the flowing tap water for 75 days were $4.75 {\times} 10^{4}$ and $1.12 {\times} 10^5 cfu/cm^{2}$ It is concluded that main mechanisms of enteric or HPC bacterial resistance to chlorination in tap waters are bacterial attachment or . adsorption to particles or bacterial aggregations and formation of biofilms on the inner wall of distribution systems by escaped bacteria from chlorination in water treatment processes, which results in bacterial regrowth in water distribution systems.

  • PDF

Development of a Temporary Pole Supporting System to Protect the Plastic Houses from Heavy Snow Damage (비닐하우스 폭설피해 방지용 가지주 장치의 개발)

  • 남상운
    • Proceedings of the Korean Society for Bio-Environment Control Conference
    • /
    • 2001.11a
    • /
    • pp.65-70
    • /
    • 2001
  • 우리 나라의 온실 설치 면적은 1999년말 현재 51,200ha에 이르고 있으며 그 중 유리온실이 363ha로 0.7%, 철골 경질판 온실이 125ha로 0.2%이고, 아연도강관을 사용한 비닐하우스가 50,712ha로 99.1%를 차지하고 있다. 파이프 골조의 비닐하우스는 대부분 아치형의 지붕 모양을 하고 있으며, 바람에는 비교적 강하나 적설에 약한 구조이다. 전국적으로 가장 널리 분포하고 있는 직경 25.4mm, 두께 1.5mm의 파이프를 사용한 폭 6m의 단동 온실의 경우 서까래 간격 60~80cm일 때 안전 적설심은 10~14cm 정도에 불과하다(남 등, 2000). (중략)

  • PDF

Experiment on the Improvement in Corrosion Resistance of Galvanized Steel Pipes for Plastic Greenhouse (플라스틱 온실용 아연도강관의 내식성 증대방법)

  • Nam, Sang-Woon;Noh, Sang-Mok
    • Proceedings of the Korean Society of Agricultural Engineers Conference
    • /
    • 2005.10a
    • /
    • pp.175-180
    • /
    • 2005
  • Experiments on the improvement in durability of pipe framework for plastic greenhouse were carried out. Effect of protection treatment such as primer and paint coating for new pipes and old rusted ones were evaluated by change of rusty degree and yield strength. The experiments have been conducted during five years until now but it was too short to find the clear differences. However, there was a little improvement in durability of greenhouse pipes by painting after removal of rust. And also component and corrosion characteristics of pipes being used in greenhouses were analyzed, and several countermeasures for protection from corrosion were reviewed.

  • PDF

Change of Tensile Strength for Rafter Pipes of Plastic Greenhouse according to Elapsed Period (경과년에 따른 비닐하우스 서까래 파이프 인장 강도 변화)

  • Song, Hosung;Lim, Seong-Yoon;Ryu, Hee-Ryong
    • Proceedings of the Korean Society for Agricultural Machinery Conference
    • /
    • 2017.04a
    • /
    • pp.130-130
    • /
    • 2017
  • 비닐하우스의 골조를 구성하는 파이프는 부식을 방지할 목적으로 아연도강관을 사용한다. 그러나 시간이 지남에 따라 아연도금량 감소와 여러 외부 환경인자 등에 의하여 부식이나 침식이 진행되어, 외관상 녹이 생기고 강도와 연신율 등이 감소하게 된다. 이는 비닐하우스 전체의 내구성을 저하시키는 요인으로 작용하게 되는데, 이를 평가하기 위한 방법이나 기준은 미비한 실정이다. 이에 본 연구에서는 농업시설의 내구성을 평가하기 위한 방법의 하나로 각기 다른 경과년수를 갖는 비닐하우스로부터 채취한 서까래 파이프의 인장 시험을 실시하였다. 인장 시험에 사용된 서까래 파이프는 (구)시설원예시험장에 설치되어 있는 비닐하우스에서 경과년별로 채취하였으며, 지중매설부와 지상노출부로 구분하여 시편을 제작하였다. 인장 실험 결과 서까래 파이프의 경과년이 오래될수록 시편의 인장 강도는 작아지는 경향을 보이고 있으나, 파단연신율은 경과년과 연관성을 찾아보기 어려운 것으로 나타났다. 그리고 동일한 경과년을 갖는 서까래 파이프 시편에서 지중매설부의 인장 강도와 파단연신율이 지상노출부에 비해 대체로 작게 측정되었으며, 경과년이 증가할수록 인장 강도의 감소폭이 커지는 경향을 보이는 것으로 나타났다.

  • PDF

Optimum Design of Greenhouse Structures Using Genetic Algorithms (유전자알고리즘에 의한 온실구조의 최적설계)

  • Park, Choon Wook;Yuh, Baeg Youh;Lee, Hyun Woo;Lee, Suk Gun
    • Journal of Korean Society of Steel Construction
    • /
    • v.19 no.2
    • /
    • pp.171-179
    • /
    • 2007
  • The greenhouse discrete optimum design program was developed using discrete optimum algorithm based on the genetic algorithm. The basic search method for the optimum design is the genetic algorithm, which is known to be very efficient for discrete optimization. In this paper, the objective function was the weight of the greenhouse structures and the constraints were the limits state design method. The design variables were galvanized steel pipes for plastic housing KSD 3760. Objective criteria were presented for the design of economic greenhouse structure and evaluation of its stability. The standardizations of greenhouse structure were used, as well as the normalization of greenhouse-related materials. Design examples were given to show the applicability of the optimum design using the discrete optimum algorithm based on the genetic algorithm of this study.

Characteristics of Corrosion and Water Quality in Simulated Reclaimed Water Distribution Pipelines (모형 재이용관을 이용한 하수재이용수의 부식 및 수질영향 연구)

  • Kang, Sung-Won;Lee, Jai-Young;Lee, Hyun-Dong;Kim, Gi-Eun;Kwak, Pill-Jae
    • Journal of Korean Society of Environmental Engineers
    • /
    • v.34 no.7
    • /
    • pp.473-479
    • /
    • 2012
  • Water reuse has been highlighted as a representative alternative to solve the lacking water resource. This study carried out a study on the pipe corrosion and water quality change which can occur through the supply of reclaimed water, using a simulated reclaimed water distribution pipeline. Galvanized steel pipe (GSP), cast iron pipe (CIP), stainless steel pipe (STSP) and PVC pipe (PVCP) were used for the pipe materials. Reclaimed water(RW) and tap water(TW) were respectively supplied into simulated reclaimed water distribution pipelines. As a result of performing a loop test to supply reclaimed water to simulated reclaimed water distribution pipelines, the weight reduction of pipe coupons showed the sequence of CIP > GSP > STSP ${\approx}$ PVCP. In addition, reclaimed water showed a high corrosion rate comparing to that of tap water. In case of CIP, the initial corrosion rate showed 3.511 mdd(milligrams per square decimeter per day) for reclaimed water and 2.064 mdd for tap water and the corrosion rate for 90 days showed 0.833 mdd for reclaimed water and 0.294 mdd for tap water. Also in case of GSP, the initial corrosion rate showed 2.703 mdd for reclaimed water and 2.499 mdd for tap water and the corrosion rate for 90 days showed 0.349 mdd for reclaimed water and 0.248 mdd for tap water, which was a tendency similar to that appeared in CIP with a tendency to reduce the corrosion rate. As a result of water quality changes of reclaimed water at pipe materials to carry out the loop test, there was higher conversion ratio of ammonia into nitrate in CIP and GSP with higher corrosion rate than that in STSP and PVCP where no corrosion has occurred. The highest denitrification rate of nitrate could be observed from CIP with the most particles generated from corrosion. In CIP, it could be confirmed that there was MIC (Microbiologically Induced Corrosion) as a result of EDS (Energy Dispersive X-ray spectrometer System) analysis results.

Corrosion and Strength Changes of Agricultural Steel Pipes Elapsed 20 Years under the Greenhouse Environment (온실 환경 하에서 20년 경과된 농업용 강관의 부식 및 강도변화)

  • Nam, Sang-Woon;Ryu, Hee-Ryong;Choi, Man-Kwon;Shin, Hyun-Ho
    • Journal of Bio-Environment Control
    • /
    • v.29 no.2
    • /
    • pp.196-201
    • /
    • 2020
  • In order to increase the durability of the pipe framed greenhouse, galvanized steel pipes with four corrosion protection treatments were installed in the greenhouse. After 20 years, experiments on surface corrosion and strength change were conducted. Control (untreated) pipes exposed in the atmosphere showed a 1.3% reduction in strength, but little difference from other treatments. The strength of heavy protective coating pipes buried in the ground decreased by 0.6%, showing little change, but untreated pipes decreased by 15.7%. And antirust paint and asphalt coating pipes decreased by 4.2~4.4%. Pipes exposed in the atmosphere did not show severe corrosion in all samples. There was no change in heavy protective coating pipes, and no rust was found in antirust painting pipes either and there was only slight discoloration. Asphalt coating pipes discolored black and some rust was found, and untreated pipes were rusted by 20~30% of the surface. However, untreated pipes buried in the ground were completely rusted, and asphalt coating pipes were rusted by 80~90% of the surface. Antirust painting pipes were rusted by 20~30%, and heavy protective coating pipes did not change almost. The heavy protective coating treatment showed a clear corrosion protection effect even in the parts buried in the ground, and the antirust painting treatment also showed some corrosion protection effect. Therefore, it is judged to be applicable to the field of pipe framed greenhouses.