• Title/Summary/Keyword: 순 티타늄

Search Result 68, Processing Time 0.024 seconds

Dependence of $Cl_2$ Gas Reaction Time on Tribological Properties of TiC Derived Carbon Layer (염소가스 반응시간에 따른 TiC표면 탄소막의 Tribology 특성)

  • Lim, Dae-Soon;Bae, Heung-Taek;Jeong, Ji-Hoon;Na, Byung-Chul
    • Tribology and Lubricants
    • /
    • v.25 no.1
    • /
    • pp.20-24
    • /
    • 2009
  • TiC-derived carbon coatings have been synthesized at $600^{\circ}C$ temperature treatment with $H_2/Cl_2$ mixture gases. From Raman spectroscopy measurements, the modified layer was covered with carbon and the thick-ness of the layer was increased with increasing reaction time. And $I_D/I_G$ ratio was decreased with increasing reaction time. The superior tribological property was obtained from TiC reacted with $Cl_2$ gas for 2 hrs. And the tribological property measurements indicate that TiC-derived carbon layer has $0.9{\times}10_{-6}mm^3/Nm$ in wear coefficient and 0.13 in friction coefficient.

Precise Diagnosis and Conservation Treatment of the Twin-lion Stone Lantern from the Godalsa Temple Site, Yeoju (여주 고달사지 쌍사자 석등의 정밀진단 및 보존처리)

  • National Museum of Korea Conservation Science Division;Damwon Cultural Heritage Inc.;Man Gyeong Corp.
    • Conservation Science in Museum
    • /
    • v.31
    • /
    • pp.71-103
    • /
    • 2024
  • The National Museum of Korea Conservation science division conducted a precise diagnosis and a non-destructive investigation to comprehensively assess the overall damage of the Twin-lion stone lantern from the Godalsa Temple site, Yeoju to be placed on display in the museum's outdoor stone garden, then reviewed the relevant conservation and management plan and applied conservation treatment to the artifact. The museum carried out the treatment in the following order: precise diagnosis; dismantling of the previously-restored part of the roof stone; reinforcement and restoration of the roof structure with new stone; restoration of the previously-restored part of the lantern's support stone (jungseok); surface texture treatment to the restored area; cleaning (basic, laser); and color matching. The previously-restored part of the roof stone was removed and restored with new stone material, based on the results of a safety diagnosis regarding the separation at the said part. Granite from the Sangju area was selected as the material for the restoration in consideration of the results of mineral analysis as well as the surface color and particle size. The new stone was divided into three pieces based on the descending edges of the octagonal roof structure and joined together using epoxy resin. The structure was further strengthened by inserting titanium rods. It is expected that the status diagnosis and conservation treatment of the twin-lion stone lantern from the Godalsa Temple site in Yeoju will be used as a reference for the future conservation and management of outdoor displays of stone cultural heritage.

The Microalgal Attachment and its Growth on the Artificial Surfaces Immersed in Seawater: I. Attachment and Micro-succession (해수에 잠긴 인공기질 표면에서 미세조류의 부착과 성장: I. 부착 및 천이)

  • Shim, Jae-Hyung;Kang, Jung-Hoon;Cho, Byung-Cheol;Kim, Woong-Seo
    • The Sea:JOURNAL OF THE KOREAN SOCIETY OF OCEANOGRAPHY
    • /
    • v.3 no.4
    • /
    • pp.249-260
    • /
    • 1998
  • To understand the attachment of micro algae and their subsequent growths on artificial surfaces immersed in seawater, the relationship between attachment of diatoms on the immersed artificial substrates and species pool in the surrounding water was investigated. We used acryl slides for the study of diatom attachment and examined the surrounding water samples collected in Incheon Harbour from July 1995 to February 1997. Variations of species composition and abundances by exposure time in seawater were investigated during the early phase of biofilm formation on various substrates, e.g. glass, acryl, titanium, copper and antifouling paint-treated slides. Immigration rates of diatoms to acryl slides during spring and winter were significantly correlated with the abundance of benthic diatoms in surrounding water ($r^2$=0.78, p<0.01, n=42), suggesting that immigration rates were affected by variations of benthic diatom abundances in surrounding water. Immigration coefficient of monoraphid diatoms was 5 times higher than that of biraphid diatoms, but relative abundance of monoraphid diatoms was 3 times lower than that of biraphid diatoms on acryl slides in spring. In winter, immigration coefficient and relative abundance of centric diatoms were higher compared to other raphe forms. These results suggest that the attachment of diatoms seems to be caused by the abundance and immigration coefficients of benthic diatoms in surrounding water. Pennate diatoms predominantly attached to all artificial surfaces throughout all experimental periods. Interestingly, centric diatoms predominantly attached to all artificial surfaces in winter. Hantzschia virgata, Licmophora abbreviata and Melosira nummuloides appeared dominantly on antifouling paint-treated slides, probably being tolerant of the antifouling paint. During incubations, the abundance of attached diatoms increased exponentially on glass, titanium and acryl slides with exposure time. The maximum abundance was highest on glass slide, followed by acryl, titanium, copper and antifouling paint-treated slides. The growth rates of attached diatom community on all artificial surfaces were higher at temperature of $24-25^{\circ}C$ than that of $2-3^{\circ}C$. The growth rate of attached diatoms on glass slide was generally higher compared to other slides during the study period. Dominant morphotypes of observed species with exposure time in seawater were prostrate form Amphora coffeaeformis, fan shape Synedra tabulata, stalk type Licmophora paradoxa and chain type M. nummuloides. A micro-succession in the attached microalgal community was observed. The composition of dominant species seems to be the result of species-specific response to gradually limited space with development of microalgal film.

  • PDF

DC 반응성 스퍼터링법으로 증착한 TiN/Al, TiCN/Al 박막의 전기적.기계적 특성 및 내부식성 평가

  • Lee, Hyeon-Jun;Song, Pung-Geun
    • Proceedings of the Korean Vacuum Society Conference
    • /
    • 2012.08a
    • /
    • pp.346-347
    • /
    • 2012
  • 최근 화석연료 대체 에너지원으로서 자동차용으로 연구 개발 및 응용되고 있는 고분자 전해질 연료전지(PEMFC: Proton exchange membrane fuel cells)에서 분리판(Bipolar Plate)은 스택 전체 무게의 80%, 스택 가격의 60% 정도로 가장 높은 비중을 차지한다. 분리판은 연료와 산화제를 공급해주는 통로 및 전지 운전 중에 생성된 물을 제거하는 통로 역할과 anode, cathode로서 전극 역할을 통해 스택 전력을 형성하는 핵심 기능과 전지와 전지 사이의 지지대 역할을 한다. 따라서 분리판은 전기전도성, 내부식성 및 기계적 특성이 우수해야함은 물론이고, 얇고 가벼우며 가공성이 뛰어나야 한다. 현재 가장 많이 사용되고 있는 금속 분리판 소재 중 스테인리스 스틸은 전기적, 기계적 특성 및 내부식성이 우수한 반면, 가격이 비싸고, 중량이 무거운 단점이 있다. 따라서 본 연구에서는 DC 반응성 마그네트론 스퍼터링법으로 전기적, 기계적 특성 및 내부 식성이 우수한 TiN, TiCN 박막을 스테인리스에 비해 중량이 1/3, 소재 단가가 1/4인 알루미늄 기판 위에 증착하여 박막 물성을 평가하였다. DC Power는 400 W, 기판과 타겟 사이의 거리는100 mm, 공정 압력은 0.5 Pa로 고정하였고, 3 inch의 지름과 순도 99.95%를 갖는 티타늄 타겟을 사용하였다. 공정 가스는 Ar을 주입하였으며, 질소와 탄소의 공급원으로는 질소($N_2$)와 메탄($CH_4$) 가스를 사용하여 챔버 내 주입혼합가스의 전체 유량을 50 sccm으로 고정시켰다. 증착된 박막의 전기적, 기계적 특성을 측정하였고, X-ray diffraction (XRD), Scanning electron microscope (SEM)을 이용하여 박막의 미세구조 및 표면 상태를 확인하였다. 또한, 내부식 특성을 평가하기 위해 potentiostatic, potentiodynamic 법을 이용하여 박막의 부식저항을 측정하였다. 증착된 TiN 박막의 경우 질소 함량의 증가에 따라 박막 증착속도는 감소하는 경향을 보였다. 이는 타겟 부근의 질소 라디칼 비율이 증가함에 따라 질화반응이 촉진된 것으로 생각된다. 또한, 증착된 TiN과 TiCN 박막은 반응성 질소 유량과 탄소 유량에 따라 각각 다른 미세구조를 가지는 것을 확인하였다. TiN과 TiCN은 NaCl형의 면심입방격자(FCC)로 같은 구조이며, 격자상수가 비슷하여 전율고용되어 TiCN을 형성하고, 탄소와 질소의 비에 따라 전기적 기계적 특성이 달라짐을 확인하였다.

  • PDF

Low Temperature Diffusion Brazing of Commercial Pure(CP)-Ti alloy with Zr-based Filler Metal (Zr기 필러메탈을 이용한 상용 순 티타늄(CP-Ti) 합금의 저온 브레이징 특성)

  • Sun, J.H.;Shin, S.Y.;Hong, J.W.
    • Journal of the Korean Society for Heat Treatment
    • /
    • v.29 no.1
    • /
    • pp.1-7
    • /
    • 2016
  • Titanium and its alloys can be usually joined with brazing method. And the alloys should be brazed at low temperature to keep their original microstructure. In this study, the mechanical strength and microstructure of the CP-Ti joint-brazed with $Zr_{54}Ti_{22}Ni_{16}Cu_8$ filler metal having melting temperature of $774{\sim}783^{\circ}C$ were investigated. The tensile strengths of the joint-brazed at $800^{\circ}C$ with $100^{\circ}C/min$ of cooling rate showed more than 400 MPa which was as high as base metal. The $Widmanst{\ddot{a}}tten$ structure consisting of Ti and $Ti_2Ni$ phase was observed in the joint area. However, the tensile strengths of the joint-brazed at $800^{\circ}C$ with $15^{\circ}C/min$ of cooling rate were decreased and the Ti, $(Ti,Zr)_2Ni$ and $Ti_2Ni$ phases were observed at the joint area. It is believed that the $(Ti,Zr)_2Ni$ laves phases could decrease the mechanical strength of the joint and the cooling rate should be controled to get high strength of the titanium joint.

A Study on the Treatment of soil Flushing Effluent Using Electrofloatation (전기부상법을 이용한 토양세정 유출수 처리에 관한 연구)

  • 소정현;최상일
    • Journal of Soil and Groundwater Environment
    • /
    • v.7 no.3
    • /
    • pp.79-84
    • /
    • 2002
  • The optimal operation conditions, including voltage applied, reaction time, distance between electrodes. and electrode material. were investigated for the treatment of soil flushing effluent using electrofloatation. When 3V was applied for 1 hour, 88% oil-water separation efficiency was achieved. In case of 6V and above, 90% efficiencies were achieved. As reaction time and distance between electrodes were longer, separation efficiencies were higher and lower, respectively. Separation efficiencies for different anode materials were copper > aluminum > iron > titanium. It might result from the differences of their electrical conductivities.

A Study of Weldability for Pure Titanium by Nd:YAG Laser(IV) - Lap Welding and Application for Heat Exchanger - (순티타늄판의 Nd:YAG 레이저 용접성에 관한 연구(IV) - 겹치기 용접 및 실물 열교환기로의 적용 -)

  • Kim, Jong-Do;Kwak, Myung-Sub;Lee, Chang-Je;Kil, Byung-Lea
    • Journal of Welding and Joining
    • /
    • v.28 no.1
    • /
    • pp.66-71
    • /
    • 2010
  • With large specific strength and outstanding corrosion resistance and erosion resistance in sea water, titanium and titanium alloy are widely used in heat exchanger production. In particular, pure titanium demonstrates outstanding molding performance and may be considered optimal for production of heat exchanger. Since titanium is very vulnerable to oxidation and embrittlement during welding, processes with less heat input are widely used, and laser welding is widely applied by considering production performance and shield etc in atmosphere. So far, 1st report and 2nd report compared and analyzed embrittlement degrees by bead colors of weldment through oxygen and nitrogen quantitative analysis and hardness measurement, and evaluated welding performance and mechanical properties of butt welding. This study evaluated field applicability of lap welding to heat exchange plate of LPG re-liquefaction device for ships through tensile stress test, hardness test and internal pressure test etc after deducing optimal weding condition and applying to actual heat exchange plate. In bead overlap area, the experiment produced sound welds with no porosity or defect by increasing and decreasing laser power, and tensile-shear test results indicated virtually the same tension and yield strength as base metal. As a result of measuring hardness at lateral cross section and bead overlap zone of actual heat exchanger welds, hardness difference within 20Hv was produced at base metal, HAZ and weldment, and as a result of pneumatic and hydraulic pressure test, no leakage occurred.

The Characteristics of Continuous Waveshape Control for the Suppression of Defects in the Fiber Laser Welding of Pure Titanium Sheet (I) - The Effect According to Applying Slope Up & Down - (순 티타늄 박판의 파이버 레이저 용접시 결함 억제를 위한 연속의 출력 파형제어 특성(I) - 슬롭 업 & 다운 적용에 따른 영향 -)

  • Kim, Jong-Do;Kim, Ji-Sung
    • Journal of Welding and Joining
    • /
    • v.34 no.6
    • /
    • pp.62-68
    • /
    • 2016
  • Laser welding has superior characteristic such as low distortion, high welding speed, easy automation and real time control. But it is easy to occur weld defects such as porosity, crater, humping bead in the area of welding start and end. These weld defects can be suppressed by applying the wave shape control. In this study CW fiber laser was used for welding of $0.5mm^t$ pure titanium. Penetration properties were evaluated with the time of slope up and down. After then the bead shape was observed, and the maximum depth and the area of crater were measured. The bead shape of welding start area changed to be sharp with increase of slope up time and non-weld area of welding start increased. The crater and humping bead were suppressed with slope down time. The cooling rate of crater area was understood through measure of the hardness. Also, The distribution tendency of alloying elements was observed by EPMA and EDS. When wave shape control didn't applied to weld, the hardness of end weld increased due to rapid cooling rate and the hardness of rear part in the crater was higher than that of fore part. On the other hand, when the wave shape control was used for end weld, the increase of hardness in the end weld couldn't be found due to gradual cooling rate.

A Study of Weldability for Pure Titanium by Nd:YAG Laser(II) - Welding Properties of Butt Welding - (순티타늄판의 Nd:YAG 레이저 용접성에 관한 연구(II) - 맞대기 용접 특성 -)

  • Kim, Jong-Do;Kwak, Myung-Sub;Song, Moo-Keun;Park, Seung-Ha
    • Journal of Welding and Joining
    • /
    • v.27 no.6
    • /
    • pp.68-73
    • /
    • 2009
  • Recently, as titanium and titanium alloys are being increasingly used in wide areas, there are on-going researches to obtain high quality weld zone. In particular, growing interest is being drawn to laser welding, which involves low heat input and large aspect ratio in various welding processes and can facilitate shield in atmospheric condition compared with electron beam welding. The first report covered the analysis of embrittlement by the bead color of weld zone through quantitative analysis of oxygen and nitrogen and measurement of hardness as basic experiment to apply laser welding to titanium. Results indicated that the element that affect embrittlement the most was nitrogen, and as embrittlement and oxygenation go on, bead color changed to silver, gold, brown, blue and gray. This study performed butt welding of pure titanium and STS304 by using 1kW CW Nd:YAG laser, and to find out basic physical properties, evaluated welding performance by laser output, welding speed, root gap and misalignment etc, and examined mechanical properties through tensile stress and Erichsen test. The reason particles of pure titanium welded metal and HAZ are greater than STS304 is because they are pure metal and do not include many impure elements that work as nuclei in case of resolidification, thus becoming coarse columnar crystals eventually. In addition, the reason STS304 requires more energy during welding than pure titanium is because the particle size of base metal is smaller.

A Study of Weldability for Pure Titanium by Nd:YAG Laser(III) - Weld Properties of Edge Welding - (순티타늄판의 Nd:YAG 레이저 용접성에 관한 연구(III) - 에지 용접 특성 -)

  • Kim, Jong-Do;Kil, Byung-Lea;Kwak, Myung-Sub;Song, Moo-Keun
    • Journal of Welding and Joining
    • /
    • v.27 no.6
    • /
    • pp.74-79
    • /
    • 2009
  • Titanium and titanium alloy can be reproduced immediately even if oxide films($TiO_2$) break apart in sea water. Therefore, since titanium demonstrates large specific strength and outstanding resistance to stress corrosion cracking, crevice corrosion, pitting and microbiologically influenced corrosion in sea water environment, it has been widely applied to heat exchanger for ships. In particular, with excellent elongation, pure titanium may be deemed as optimal material for production of heat exchanger plate which is used with wrinkles formed for efficient heat exchange. Conventional plate type heat exchanger prevented leakage of liquid through insertion of gasket between plates and mechanical tightening by bolts and nuts, but in high temperature and high pressure environment, gasket deterioration and leakage occur, so heat exchanger for LPG re-liquefaction device etc do not use gasket but weld heat exchanger plate for use. On the other hand, since welded plate cannot be separated, it is important to obtain high quality reliable welds. In addition, for better workability and production performance, lasers that can obtain weldment with large aspect ratio and demonstrate fast welding speed even in atmospheric condition not in vacuum condition are used in producing products. So far, 1st report and 2nd report compared and analyzed embrittlement degrees by bead colors of weldment through quantitative analysis of oxygen and nitrogen and measurement of hardness as fundamental experiment for the evaluation of titanium laser welding, and evaluated the welding performance and mechanical properties of butt welding. This study welded specimens in various conditions by using laser and GTA welding machine to apply edge welding to heat exchanger, and evaluated the mechanical strength through tensile stress test. As a result of tensile test, laser weldment demonstrated tensile strength 4 times higher than GTA welds, and porosity could be controlled by increasing and decreasing slope of laser power at overlap area.