The Thinning Phenomena of the Wall Thickness during $360^{\circ}$ Cold Bending of Ti-6Al-4V Large-Diameter Seamless Tube (대 직경 이음매 없는 Ti-6Al-4V 합금 튜브의 $360^{\circ}$ 냉간 굽힘 시 벽두께 감소현상)

  • 허선무;박종승
    • Journal of the Korea Institute of Military Science and Technology
    • /
    • v.3 no.1
    • /
    • pp.231-236
    • /
    • 2000
  • The wall thickness of the Ti-6Al-4V Large-Diameter Seamless Tube, which is supposed to be a very important parameter in a system design, was measured during $360^{\circ}$ cold bending processes. The factors or processes affecting the wall thickness include 1) primary bending, 2)secondary or finishing step of the $360^{\circ}$ bending, 3)cleaning processes in CERO TRUTM(CT)process. But thinning effects of the wall thickness during the cleaning processes are negligible compared to those during the formers. The variations in the percentages of the change in wall thickness were found to be from -14% to +16%.

  • PDF

$360^{\circ}$ Cold Bending of Ti-6Al-4V Large-Diameter Seamless Tube (대 직경 이음매 없는 Ti-6Al-4V 튜브의 $360^{\circ}$ 냉간 굽힘)

  • 허선무;박종승
    • Journal of the Korea Institute of Military Science and Technology
    • /
    • v.3 no.1
    • /
    • pp.176-182
    • /
    • 2000
  • $360^{\circ}$ bending of Ti-6Al-4V large-diameter seamless tube(62.37 mm $OD {\times} 4.40mm$ wall thickness) has been achieved at room temperature without heating. The bending process comprised two steps : the first step is $360^{\circ}$ bending by an uniquely designed rotary bender allowing spring back, which is subsequently eliminated by the second or finishing step which comprised repeated bending processes by powered three roll bender, In odor to prevent collapse of tube during bending, Cerro $Tru^{TM}$(Trade name of a non-ferrous low melting point alloy)has been employed as a filler metal. The resultant ovality(out of roundness) obtained was 1.28%, as compared with 6~8% without applying Cerro $Tru^{TM}$.

  • PDF