  • This experimental study presents the strength properties of mortar using the blast-furnace slag sand. The mix disign of this study is based on the each three classes of unit water; (250, 275, 300)kg/㎥ and four classes of W/C; (45, 50, 55, 60)% and substitution rate(0, 25, 50, 75, 100)%. It gives following result. As W/C ratio increase, the strength is decrease. In case of mortar using air-cooled blast-furnace slag sand, the 3-days and 7-days compression strength is increase as substitution rate is higher. But in case of the mortar using the quenched blast-furnace slag sand, the compression strength is decrease as substitution rate is higher.

  • PDF

An Experimental Study on the Stregth characteristics of Mortar using the Blast-Furnace Slag Sand (서냉슬래그 모르터의 강도특성에 관한 연구)

  • 임남기;김종락;김성식;김영회;정상진
    • Proceedings of the Korea Concrete Institute Conference
    • /
    • 1998.10c
    • /
    • pp.60-65
    • /
    • 1998
  • This experimental Study presents the strength properties of mortar Using the Blast-furnace Slag Sand. It gives following result. The 3-days and 7-days compression strength is increase as substitution rate is higher. As W/C ratio increase, the strength is decrease. The flexural strength is increase as substitution rate is higher specially. As flexural strength ratio for compression strength is each 16.7%, 21.1%, 25.4% on 3-days, 7-days, 28-days, long age flexural strength is higher than short age.