Pore Structures and Mechanical Properties of Early Frost Damaged Concrete using Electric Arc Furnace Slag as Aggregate (초기동결 피해를 받은 전기로 산화 슬래그 혼입 콘크리트의 공극 구조 및 역학적 특성)

  • Lee, Won-Jun;Choi, So-Yeong;Kim, Il-Sun;Yang, Eun-Ik
    • Journal of the Korea institute for structural maintenance and inspection
    • /
    • v.24 no.2
    • /
    • pp.68-77
    • /
    • 2020
  • The purpose of the paper is to evaluate the pore structure and mechanical properties of early frost damaged concrete using electric arc furnace slag as aggregate. From the results, when the concrete is exposed to frost damage at an early age, the peak point of pores 100 to 150 ㎛ in diameter were transferred into larger one. When the freezing duration is not exceeded 24 hours, it is possible that the pore distribution of under the 200 ㎛ is maintained and pore size of over 500 ㎛ is not formed, and, the freezing resistance of concrete using EFG could be improved. When BFS was mixed in concrete using EFG as coarse aggregate, the relative strength is higher than that of natural coarse aggregate. Meanwhile, the elastic modulus and resonance frequency did not change significantly due to the early frost damage as compared with the compressive strength. So, it is necessary to analyze the correlation between the experimental results in order to evaluate the performance degradation due to early frost damage.

Seismic Fragility Evaluation of Chimney Structure in Power Plant by Finite Element Analysis (유한요소 해석을 통한 발전소 연돌 구조물의 지진취약도 분석)

  • Kwon, Gyu-Bin;Kim, Jin-Sup;Kwon, Min-Ho;Park, Kwan-Soo
    • Journal of the Korea Academia-Industrial cooperation Society
    • /
    • v.20 no.3
    • /
    • pp.276-284
    • /
    • 2019
  • Seismic research on bridges, dams and nuclear power plants, which are infrastructure in Korea, has been carried out since early on, but in the case of structures in thermal power plants, research is insufficient. In this study, a total of 192 dynamic analyzes were performed for 16 actual seismic waves and 12 PGAs. As a result, the probability of failure increased as the PGA value increased for each applied seismic wave, but it was different for each seismic wave. As a result, at 0.22G, the ratio of the compressive limit reached to the limit state was 25% and the ratio of the relative displacement reached the limit state was 13%. So, the probability of collapse due to compressive failure Is higher. Therefore, the fragility curve of the chimney which is the subject of this study can be used as a quantitative basis to determine the limit state of the target structure when an earthquake occurs and to be used for the safety design of the thermal power plants.

Settlement Characteristics of a Large-Scale Foundation over a Sabkha Layer Consisting of Carbonate Sand (Sabkha층 탄산질 모래의 침하특성 및 상부기초의 거동)

  • Kim, Seok-Ju;Han, Heui-Soo
    • The Journal of Engineering Geology
    • /
    • v.23 no.3
    • /
    • pp.247-256
    • /
    • 2013
  • The carbonate sands of the Sabkha layer in the Middle East have very low shear strength. Therefore, instant settlement and time-dependent secondary settlement occur when inner voids are exposed, as in the case of particle crushing. We analyzed settlement of the Sabkha layer under a large-scale foundation by hydrotesting, and compared the field test results with the results of laboratory tests. With ongoing particle crushing, we observed the following stress-strain behaviors: strain-hardening (Sabkha GL-1.5 m), strain-perfect (Sabkha GL-7.0 m), and strain-softening (Sabkha GL-7.5 m). General shear failure occurred most frequently in dense sand and firm ground. Although the stress-strain behavior of Sabkha layer carbonate sand that of strain-softening, the particle crushing strength was low compared with the strain-hardening and strain-perfect behaviors. The stress-strain behaviors differ between carbonate sand and quartz sand. If the relative density of quartz sand is increased, the shear strength is also increased. Continuous secondary compression settlement occurred during the hydrotests, after the dissipation of porewater pressure. Particle crushing strength is relatively low in the Sabkha layer and its stress-strain behavior is strain-softening or strain-perfect. The particle crushing effect is dominant factor affecting foundation settlement in the Sabkha layer.

Shear Strength Estimation of Clean Sands via Shear Wave Velocity (전단파 속도를 통한 모래의 전단강도 예측)

  • Yoo, Jin-Kwon;Park, Duhee
    • Journal of the Korean Geotechnical Society
    • /
    • v.31 no.9
    • /
    • pp.17-27
    • /
    • 2015
  • We perform a series of experimental tests to evaluate whether the shear strength of clean sands can be reliably predicted from shear wave velocity. Isotropic drained triaxial tests on clean sands reconstituted at different relative densities are performed to measure the shear strength and bender elements are used to measure the shear wave velocity. Laboratory tests reveal that a correlation between shear wave velocity, void ratio, and confining pressure can be made. The correlation can be used to determine the void ratio from measured shear wave velocity, from which the shear strength is predicted. We also show that a unique relationship exists between maximum shear modulus and effective axial stress at failure. The accuracy of the equation can be enhanced by including the normalized confining pressure in the equation. Comparisons between measured and predicted effective friction angle demonstrate that the proposed equation can accurately predict the internal friction angle of granular soils, accounting for the effect of the relative density, from shear wave velocity.

Mechanical Properties and Resistance to Freezing and Thawing of the Recycled Aggregate Concrete with Metakaolin (메타카올린을 혼합한 재생골재 콘크리트의 역학적 특성 및 동결융해 저항성)

  • Moon, Han-Young;Kim, Yang-Bae;Moon, Dae-Joong
    • Journal of the Korea institute for structural maintenance and inspection
    • /
    • v.9 no.4
    • /
    • pp.270-278
    • /
    • 2005
  • Recycled aggregate concrete has lower strength and durability compared to concrete with natural aggregate. Therefore, metakaolin is used to improve the properties of recycled aggregate concrete. Main components of metakaolin are $SiO_2$ and $Al_2O_3$. and specific surface area is 9 times larger than that of ordinary portland cement. Quality of demolished-recycled aggregate(DRA) satisfies the type 1 of KS F 2573, but quality of source-recycled aggregate(SRA) does not satisfy with the type 2 of KS F 2573. When metakaolin was replaced with 20% of cement, compressive strength of concrete with SRA and DRA develops about 40~64% of control concrete. Water absorption ratio was reduced about 2% by replacing 20% metakaolin and it represents low compared to the natural aggregate concrete without metakaolin. In addition, the resistance to freezing and thawing, of concrete with DRA is indicated to remarkably enhanced due to the contribution of metakaolin. However, when metakaolin is replaced with 20% of cement, relative dynamic modulus of elasticity of concrete with SRA was below 60% at 210 freezing and thawing cycles.

Active Video Watermarking Technique for Infectious Information Hiding System (전염성 정보은닉 시스템을 위한 능동형 비디오 워터마킹 기법)

  • Jang, Bong-Joo;Lee, Suk-Hwan;Kwon, Ki-Ryong
    • Journal of Korea Multimedia Society
    • /
    • v.15 no.8
    • /
    • pp.1017-1030
    • /
    • 2012
  • Most watermarking schemes for video contents protection have been studied to increase watermark's robustness and invisibility against such compressions and many kinds of signal processing after embedding copyright information to the original contents. This paper proposes an active watermarking that infect watermark to contents in the video decoding process using embedded infectious watermark and control signals from a video encoder side. To achieve this algorithm, we design a kernel based watermarking in video encoder side that is possible to recover the original contents and watermark in watermark detection procedure perfectly. And then, by reversible de-watermarking in video decoder side, we design the active watermark infection method using detected watermark and control signal. This means that our system can provide secure re-distributions of video contents without any quality degration and watermark bit error against transcoding or re-encoding processing. By experimental results, we confirmed that the embedded watermark was infected by video contents and codec perfectly without any declines of compression ratio and video quality.

Effect of Hardening of Granulated Blast Furnace Slag on the Liquefaction Strength (고로 수쇄슬래그의 경화가 액상화 강도에 미치는 영향)

  • Baek, Won-Jin
    • Journal of the Korean Geotechnical Society
    • /
    • v.22 no.8
    • /
    • pp.99-106
    • /
    • 2006
  • In the present study, in order to clarify the effects of latent hydraulic property of granulated blast furnace slag (GBF slag) on the liquefaction, GBF slag was cured in the high temperature alkali water (adding the calcium hydroxide, pH=12, water temperature is about $30^{\circ}C$), and then the cyclic and the static tri-axial compression tests were carried out. Then the results were compared with those for Japanese standard sand of Toyoura sand and natural sand of Genkai sand. From the test results, it is clarified that the liquefaction strength of the GBF slag increases with the increase of the curing period by the hardening due to the latent hydraulic property. It is also shown that GBF slag with Dr=50% and 80% which was cured for 189 days in the fresh-water shows cohesion due to developing of latent hydraulic property. In addition, as for the liquefaction strength of GBFS during the hardening process, a linear relation between the cyclic stress ratio $R_{20}$ at the number of stress cycles Nc=20 and cohesion $C_{d}$ was observed. It is also clarified that the liquefaction strength for cured GBF slag in the high temperature alkali water is predicted by the cohesive strength or the unconfined compressive strength.

Dry Sliding Wear Behavior of Carbide-Particle-Reinforced 7075 Al Alloy Matrix Composites (탄화물(SiC, TiC, $B_4C$ ) 입자 강화 7075 Al 합금 기지 복합재료의 건식 미끄럼 마멸 거동)

  • 강석하;박형철;강신철;김용석
    • Proceedings of the Materials Research Society of Korea Conference
    • /
    • 2003.03a
    • /
    • pp.27-27
    • /
    • 2003
  • 무가압침투법으로 제조된 부피분율 10~24% SiC, TiC, B$_4$C 탄화물 입자강화 7075 Al 합금 기지 복합재료의 건식 미끄럼 마멸거동을 강화입자의 종류, 크기 및 부피 분율을 변수로 연구하였다. 미끄럼 마멸 시험은 pin-on-disk 형태의 마멸 시험기를 사용하여, AISI 52100 베어링강을 상대재로 상온 대기 중에서 실시되었다. 마멸특성의 분석과 마멸기구의 규명을 위하여 마멸면과 마멸단면을 SEM, EDS를 이용하여 분석하였다. 제조된 복합재료의 압축 시험을 통하여 측정된 항복강도와 가공경화지수는 서로 반비례하였고, 각 시편간의 경도 차는 크지 않았다. 마멸 시험결과, 크기 및 부피 분율이 7$\mu\textrm{m}$ !0%인 SiC 입자로 강화된 복합재료를 제외하고, 전체 복합재료 시편은 7075 Al 기지 합금에 비해 낮은 마멸 속도를 보였다. 10N 이하의 저하 중에서는 강화상의 종류와 상관없이 복합재료는 낮은 마멸 속도를 보였고, 25N 이상의 고하중에서는 TiC 입자강화 복합재료가 가장 낮은 마멸 속도를, SiC 입자강화 복합재료가 가장 높은 마멸 속도를 나타내었다. 강화 입자의 크기 및 부피 분율이 동일한 경우 SiC 입자로 강화된 복합재료가 가장 낮은 내마멸성을 나타내었다. 강화상의 크기 및 부피 분율이 증가함에 따라 미소 마멸에서 격렬 마멸로의 천이 하중이 증가하였다.

  • PDF

Permeability and Freeze-Thaw Resistance of Latex Modified Concrete (라텍스 개질 콘크리트의 투수성 및 동결융해 저항 특성)

  • 김기헌;이종명;홍창우;윤경구
    • Journal of the Korea Concrete Institute
    • /
    • v.13 no.5
    • /
    • pp.484-490
    • /
    • 2001
  • This study focused on the investigation of durability of latex modified concrete in the points of chloride ion permeability and freeze-thaw resistance as latex content variated such as 5%, 10%, 15% and 20%. When latex was mixed in concrete and cured, the concrete consisted of hydrated cement and aggregate interconnected by a film of latex particles. An increasing the amount of latex produced concrete with increased flexural strength, but with slightly lower compressive strength. The increase in flexural strength might be attributed to the latex films between the hydrated cement and aggregates, and the decrease in compressive strength to the flexibility of the latex component named by Butadiene. The rapid chloride permeability test was used to evaluate the relative permeability of latex-modified concretes and conventional concretes. The results showed that the permeability of latex-modified concretes was considerably lower than conventional concretes tested, which might be due to the latex filled in voids and interconnections of hydrated cement and aggregates by a film of latex particles. The freeze-thaw resistance of LMC was quite good comparing to conventional concrete. Air entraining agent has been used in conventional concrete to improve the freeze/thaw resistance, but latex modified concrete does not need additional air entraining agent for freeze-thaw resistance provided adequate cure occurs.

Evaluation of Freeze-Thaw Damage on Concrete Using Nonlinear Ultrasound (초음파의 비선형 특성을 이용한 콘크리트 동결융해 손상 평가)

  • Choi, Ha-Jin;Kim, Ryul-Ri;Lee, Jong-Suk;Min, Ji-Young
    • Journal of the Korea institute for structural maintenance and inspection
    • /
    • v.25 no.4
    • /
    • pp.56-64
    • /
    • 2021
  • Leakage due to deterioration and damage is one of the major causes of volume change by freezing and thawing, and it leads micro-cracking and surface scaling in concrete structures. The deterioration of damaged concrete accelerates with the chloride attack. Thus, in the detailed guidelines for facility performance evaluation (2020), the quality of cover concrete and the freeze-thaw (FT) repetition cycle were newly suggested for concrete durability assessment. The quality of cover concrete should be evaluated by the rebound hammer test and the FT repetition cycle should be also considered in the deterioration environmental assessment. This study suggested the application of fast dynamic based nonlinear ultrasound method to monitor initial micro-scale damage under freezing and thawing environment. Concrete specimens were fabricated with different water-cement ratios (40%, 60%) and air contents (1.5% and 3.0%). The compressive strength, rebound number, relative dynamic modulus, and nonlinear ultrasound were measured with different FT cycles. The scanning electron microscopy was also performed to investigate the micro-scale FT damage. As a result, both the rebound number and the relative dynamic modulus had difficulty to detect early damage but the proposed method showed a potential to detect initial micro-scale damage and predict the FT resistance performance of concrete.