• Title/Summary/Keyword: 미분시멘트

Search Result 328, Processing Time 0.022 seconds

Fluidity and Compressive Strength Properties of Cement-Mortar admixed with II-Anhydrite and Pozollanic Fine Powders (불산부생 II -형 무수석고와 포졸란 미분체가 혼입된 시멘트.몰탈 유동성 및 압축강도 특성)

  • 김도수;김재호;조민형;전진환;남재현;노재성
    • Proceedings of the Korea Concrete Institute Conference
    • /
    • 1996.10a
    • /
    • pp.154-165
    • /
    • 1996
  • As II-anhydrite reacts with C3A(aluminate), C4AF(ferrite) at initial hydration of cement and assists the hydrolysis of C3S(calcium silicate), the production rate of ettringite(3C3A.3CaSO4.32H2O) and C-S-H gel was acclerated. It was known that compressive strength of cement concrete improved due to the effect of II-anhydrite. For the checking these effects of II-anhydrite, the fluidity and compressive strength of cementmortar admixed with II-anhydrite and pozollanic fine powders were investigated. By means of SEM analysis, the surface structure of mortar with the condition of steam curing at curing days=28 was investigated. As a result of this experiment, it was examined that II-anhydrite had an increase on the fluidity of cementpaste and compressive strength of mortar.

  • PDF

Influence of Limestone Powder on the Hydration of Cement Contained much Chloride (석회석 미분말이 염소고함유시멘트의 수화반응에 미치는 영향)

  • Jeong, Chan-Il;Lee, Eui-Hak;Lee, Kyung-Hee
    • Journal of the Korean Ceramic Society
    • /
    • v.43 no.9 s.292
    • /
    • pp.537-543
    • /
    • 2006
  • Length change, hydration heat, setting time and compressive strength of OPC were measured by adding KCl and replacing limestone powder so as to examine the influence of limestone powder on hydration of the OPC contained much chloride. In general, the chloride modified cement was high in heat of hydration, short in its setting time, low in its fluidity and low in its strength at 28 days due to the sudden hydration in its initial stage. As a result of the experiment, it has been demonstrated that heat of hydration, became low as one replaced limestone powder to the chloride modified cement, and the fluidity and shrinkage rate of mortar decreased without change in setting time; furthermore, the compressive strength at 28 days was improved.

Effect of Curing Temperature on Mechanical Properties of Cement Mortar Using Recycled Aggregate Powder (순환골재미분말 사용 모르터의 역학적 특성에 미치는 양생온도의 영향)

  • Kim, Min-Woo;Feng, Hai-Dong;Park, Kyung-Teak;Baek, Dae-Hyun;Han, Min-Cheol
    • Proceedings of the Korean Institute of Building Construction Conference
    • /
    • 2011.05a
    • /
    • pp.93-95
    • /
    • 2011
  • This study is to investigate experimentally the engineering characteristics of cement mortar incorporating both recycled aggregate powder (RP) below 0.08 mm and cement kiln dust(CKD). RP is substituted for fine aggregate ranged from 5~15% and CKD is also substituted for RP from 10~30%. The use of RP resulted in a decrease in flow value at fresh mortar, while an increase in CKD did not affect the flow value significantly. The combination of RP and CKD provided slight increase in compressive strength at early and 28 days and in the high curing temperature at early age showed an increasing Strength value.

  • PDF

Fundamental Properties of High Strength Concrete Containing Blast Furnace Slag Using CBS-Dust as Admixture (CBS-Dust를 혼화재로 사용한 고로슬래그 미분말 함유 고강도 콘크리트의 기초적 특성)

  • Sin, Se-Jun;Han, Soo-Hwan;Lee, Dong-Joo;Kim, Jong;Han, Min-Cheol;Han, Cheon-Goo
    • Proceedings of the Korean Institute of Building Construction Conference
    • /
    • 2020.06a
    • /
    • pp.62-63
    • /
    • 2020
  • In this study, fundamental properties of high strength concrete containing blast furnace slag are investigated analyzed according to CBS-Dust replacement rate. As the CBS-Dust replacement rate increased, air content, fluidity and strength decreased, but concrete with 5~10 % of CBS-Dust showed excellent compressive strength in its early age. Therefore, 5~10 % substitution of CBS-Dust on high strength concrete containing blast furnace slag will have a positive effect on reducing waste disposal cost and improving the strength.

  • PDF

A Study on the Pozzolan Reactivity and Mechanical Characteristic of Blended Portland Cements using CFBC Fly Ash (순환유동층 플라이 애시를 사용한 혼합시멘트의 포졸란 반응성과 역학적 성질에 관한 연구)

  • Park, JongTak;Oh, Hongseob
    • Journal of the Korean Recycled Construction Resources Institute
    • /
    • v.6 no.3
    • /
    • pp.207-213
    • /
    • 2018
  • Nowadays, circulating fluidized bed combustor(CFBC) boilers system that can reduce environmental pollution particles are widely used in electric power plants. But the fly ash generated from CFBC boilers has lower $SiO_2$ and higher MgO and $SO_3$ contents and also has free CaO inducing expansion and abrupt initial setting of concrete. Therefore, revised KSL5405 for CFBC fly-ash as well as pulverized coal combustion(PCC) is introduced in the concrete field. In this study, the chemical properties and mechanical properties of blended cements with PCC and CFBC fly-ash produced in Korea are analyzed. The blended cement with only CFBC fly ash shows a lower length change than OPC but a higher flow change ratio. The compressive strength of blended cement paste with PCC and CFBC fly ash is slightly greater than that of cement paste with only PCC fly-ash. Based on the results, CFBC flyash blended cement products should be used with PCC flyash to ensure the material stability and material properties.

An Experimental Study on the Required Performances of Roof Concrete Placed in the In-ground LNG Storage Tank (지하식 LNG 저장탱크의 지붕 콘크리트의 요구성능에 관한 실험적 연구)

  • Kwon, Yeong-Ho
    • Journal of the Korea Concrete Institute
    • /
    • v.25 no.3
    • /
    • pp.339-345
    • /
    • 2013
  • This study is to derive from the required performances and the optimum mix proportion of the roof concrete placed in the in-ground LNG storage tank with a capacity of 200000 $m^3$, and propose the actual data for site concrete work. The concrete placing work without sliding and segregation in the fresh concrete condition is very important because the slope of domed roof is varied in the large range by its curvature. Also the control of hydration heat and the strength development at test ages are classified with massive section about 1.4 m thick and considered to the pre-stressing work and removal of air support after concrete placing work. Considering above condition, slump range is selected $100{\pm}25$ mm under the slope $20^{\circ}$ and $150{\pm}25$ mm over the slope $20^{\circ}$ s until 60 minutes of elapsed time. Also, the roof concrete is satisfied with compressive strength range including design strength at 91 days (30 MPa), pre-stressing work at 7 days (10 MPa), air support removal work at 21 days (14 MPa). Replacement ratio of limestone powder is determined by confined water ratio test and main design factors include water-cement ratio (W/C), sand-aggregate ratio and dosage of admixture. As test results, the optimum mix proportion of the roof concrete used low heat cement is as followings. 1) Replacement ratio of limestone powder 25% by confined water ratio test 2) Water-cement ratio 57.8% 3) Sand-aggregate ratio 42.0%. Also, test results for the adiabatic temperature rising test is satisfied with its criteria and shown the lower value compared to preceding storage tank (TK-13, 14). These required performances and the optimum mix proportion is to apply the actual construction work.

Quality Properties of Zero Cement Blast Furnace Slag Mortar Using the Recycled Fine Aggregates Depending on Mixing Factors (순환잔골재를 사용한 무 시멘트 고로슬래그 모르터의 배합요인에 따른 품질특성)

  • Han, Cheon-Goo;Son, Seok-Heon;Park, Kyung-Taek
    • Journal of the Korean Recycled Construction Resources Institute
    • /
    • v.5 no.3
    • /
    • pp.70-77
    • /
    • 2010
  • This study is to investigate experimentally the influence of mixing factors, such as a mortar mix proportion of non-cement mortar, flow, and W/B, on quality characteristics of blast furnace slag powder mortar incorporating dry type recycled fine aggregates. In the characteristics of fresh mortar, the W/B increased according to the increase in the flow due to the increase in water contents, but air contents decreased due to loss of air contrary to the increase in the W/B. In the case of hardened mortar, the compressive strength showed a decrease due to the highly determined W/B inversely according to the increase in the flow through the entire age in which the compressive strength increased proportionally according to the increase in the B/W. Also, the increasing rate of such compressive strength increased more largely due to the latent hydraulic property of the BS according to the passage of the age. The flexural strength at the age of 28 days according to the increase in the B/W represented a similar level in strength values without any increases. The flexural strength for the compressive strength was distributed as a range of 1/2 ~ 1/3 and that showed a higher range than that of conventional concretes.

  • PDF

A Study on the Electrical Conductivity and Electromagnetic Shielding of High Performance Fiber Reinforced Cementitious Composites(HPFRCC) (고성능 시멘트 복합체의 전기전도도 및 전자파 특성 시험 평가)

  • Lee, Nam-Kon;Park, Gi-Joon;Park, Jung-Jun;Kim, Sung-Wook
    • Journal of the Korea institute for structural maintenance and inspection
    • /
    • v.23 no.2
    • /
    • pp.37-43
    • /
    • 2019
  • This study investigated electrical conductivity, electromagnetic shielding effectiveness, and mechanical property to improve electromagnetic shielding performance of high performance fiber reinforced cementitious composites (HPFRCC). Steel fiber, steel slag and carbon black as a conductive material were incorporated into the HPFRCC mixes. In addition, 2% CNT solution which was produced by dispersing multi-wall carbon nanotube (MWCNT) into water was used as a conductive material. In the test results, electrical conductivity of HPFRCC specimens was very low except for the specimen incorporating 1% carbon black. Micro structure of cement matrix was changed as the curing time increased, which negatively affected the conductive network of HPFRCC. In case of HC1 specimen showing a conductive network (0.083 S/cm), the electrical conductivity of the specimen after being dried at $60^{\circ}C$ for 72 hours to exclude the effect of water on electrical conductivity was significantly reduced to 0.0003 S/cm. The most important parameter of electromagnetic shielding effect was found to be a steel fiber while the effect of carbon black and steel slag was very few. The correlation between electrical conductivity and electromagnetic shielding effect does not seem to be clear.

Engineering Properties of CB Cut-off Walls Mixed with GGBS (고로슬래그 미분말을 혼합한 CB 차수벽의 공학적 특성)

  • Kim, Taeyeon;Lee, Bongjik
    • Journal of the Korean GEO-environmental Society
    • /
    • v.23 no.5
    • /
    • pp.33-39
    • /
    • 2022
  • For a slag-cement-bentonite (slag-CB) cut-off wall, GGBS replaces a part of the cement mixed to build a CB cut-off wall, which is used to block the flow and leakage of pollutants or groundwater; prevent seawater infiltration; and repair or reinforcement an aged embankments. Slag-CB cut-off walls are used in various applications in different fields where groundwater control is required due to its excellent characteristics. Such properties include high strength, low permeability, high durability and chemical resistance. However, despite these advantages, slag-CB cut-off walls are not extensively studied in Korea and thus are not applied in many cases. Particularly, GGBS, which replaces cement in a mixture, has different properties depending on its country of production. Consequently, it is necessary to perform various studies on slag-CB cut-off walls that use GGBS produced in Korea in order to increase its usability. This study has evaluated the bleeding rate, setting time, strength, and permeability in relation to the cement replacement rate of GGBS produced in Korea for slag-CB cut-off walls, with the aim to increase its usability. The evaluation found that slag-CB cut-off walls, made of a mixture containing GGBS produced in Korea, have a lower bleeding rate and permeability, and higher strengththan CB cut-off walls. It was also analyzed that such improved performance is more effective with a higher cement replacement rate of GGBS.

Investigation on the Mechanical Properties of High-Strength Recycled Fine Aggregate Mortar Made of Nanosilica Dispersed by Sonication (나노실리카 혼입률이 실리카퓸 및 고로슬래그 미분말을 혼입한 4성분계 고강도 순환잔골재 모르타르의 역학적 성능에 미치는 영향)

  • Seong-Woo Kim;Rae-Gyo Moon;Eun-Bi Cho;Chul-Woo Chung
    • Journal of the Korean Recycled Construction Resources Institute
    • /
    • v.11 no.2
    • /
    • pp.97-104
    • /
    • 2023
  • In order to maximize the utilization of recycled fine aggregate, high strength mortar made of 100 % recycled fine aggregate was prepared, and its physical properties were evaluated to determine the possibility of using recycled fine aggregate as structural aggregate. The effect caused by the amount of nanosilica on the physical properties of w/b 0.2 recycled fine aggregate mortar consisting of cement, silica fume, and blast furnace slag. To improve the dispersion of nanosilica inside mortar, an aqueously dispersed nanosilica solution by ultrasonic tip sonication was prepared, and incorporated into the mortar to evaluate changes in mortar flow, porosity and compressive strength depending on nanosilica content. According to the experimental results, mortar flow decreased as the replacement ratio of nano-silica increased. As the replacement ratio of nanosilica increased up to 0.75 %, the porosity decreased and the compressive strength increased, but, at a replacement ratio of 1 %, the porosity increased and the compressive strength decreased. It was confirmed that the nano-silica replacement ratio of 0.75 % was optimum proportion to maximize the mechanical performance of high-strength recycled fine aggregate mortar.