Permeability and strength characteristics of Self-Sealing and Self-Beating materials as landfill liners (매립지 차수재로서 자가치유재의 투수 및 강도특성)

  • 장연수;문준석
    • Journal of Soil and Groundwater Environment
    • /
    • v.7 no.1
    • /
    • pp.41-51
    • /
    • 2002
  • Recently, domestic waste landfills are constructed sometimes on seashore area to provide large landfill area. In order to strengthen the foundation of landfills and to prevent the infiltration of leachate through the bottom, many cases of constructing cement hardened liners on seashore clays are found. In these cases, it is possible to have cracks in the hardened liners due to settlement with waste load since the stiffness of the hardened liner Is greater than that of clay liners. In this study, the capability of Self-Sealing and Self-Healing (SSSH) liner made with a seashore clay in the metropolitan landfill to prevent the percolation of water and leachate is examined using flexible-wall permeameter test and using uniaxial compression test. Applicability of SSSH to weathered granitic soil is also examined for self-sealing capabilities. The result of Flexible permeameter test for SSSH with the seashore clay showed that permeability obtained was lower than permeability criteria of Korean waste management law. The permeability and strength characteristics of SSSH with granitic soil and bentonite showed better results than with the seashore clay.

Dynamic measurements during Dynamic Compaction (동다짐시 동적 거동 계측)

  • 나영묵
    • Proceedings of the Korean Geotechical Society Conference
    • /
    • 1997.10a
    • /
    • pp.81-88
    • /
    • 1997
  • 현재 국내외에서 해안가에 수심이 낮은 지역을 중심으로 대규모 매립공사를 수행하여 주택단지, 항만시설, 공업단지 및 공항부지 등으로 사용하고 있다. 매립재를 양질의 모래로 사용하는 경우 매립방법에 따라 매립토의 조밀정도는 다르나 어떠한 경우든 상당히 느슨하거나 중간정도 느슨한 상태로 존재한다. 이런한 느슨한 사질토는 지진 시 액상화 현상에 민감하고, 낮은 지지력 및 큰 즉시침하를 야기시킨다. 따라서 매립된 느슨한 사질토는 향후 시설될 구조물의 중요도에 따라 개량할 필요가 있다. 본 현장의 준설 매립된 사질토의 지반 개량에 적용된 동다짐의 시험시공중 pounder에 accelerometer를 설치하고 적외선 beam을 이용, 충격시의 pounder의 deccleration과 impact velocity를 측정하였다. 여기에서는 이들 실측치를 근거로 중량물체(pounder)의 동적 거동 및 충격시 과잉간극수압 변화를 살펴보았다.

  • PDF

A Study on Landfill Reduction Possibility by Characteristics of Industrial Thermal Treatment Residues (사업장 열적처리 잔재물의 특성에 따른 매립저감 가능성 연구)

  • Lee, Suyoung;Kim, Kyuyeon;Jeon, Taewan;Shin, Sunkyoung
    • Journal of the Korea Organic Resources Recycling Association
    • /
    • v.27 no.1
    • /
    • pp.65-75
    • /
    • 2019
  • The government is promoting recycling of waste resources through the enactment of Fundamental Law on Resource Circulation, the revision of the Wastes Control Act and zero-landfilling of untreated waste through improved processes such as recycling and diversification. As of 2015, the total amount of landfilled waste is 38,308 ton/day in Korea. The amount of landfilled waste from industrial sectors is 23,577 ton/day, accounting for 62 % of total landfilled waste. In the study, we investigated the characteristics of the thermal treatment residue among inorganic wastes and estimated the landfill reduction potential according to the relevant recycling criteria, which can go through recycling paths. As a result, it is estimated that about 5~42 % of the landfilled waste can be reduced in case mandatory recycling and landfill suppression policies such as recycling criteria for thermal processing residues and expansion of recycling obligation targets should be implemented. In order to minimize landfill disposal, it is necessary to expand the diversity of waste recycling type and the usage of recycled products.

Embedded EM Sensor for Tensile Force Estimation of PS tendon of PSC Girder (PS 긴장재 긴장력 계측을 위한 PSC 거더 내부 매립용 EM 센서)

  • Park, Jooyoung;Kim, Junkyeong;Zhang, Aoqi;Lee, Hwanwoo;Park, Seunghee
    • Journal of the Computational Structural Engineering Institute of Korea
    • /
    • v.28 no.6
    • /
    • pp.691-697
    • /
    • 2015
  • In this paper, an embedded EM sensor was researched to estimate prestressing force of PS tendon in PSC girder. Recent methodologies for managing prestressing force loss were staying on verifying a applying prestressing force under construction, namely the loss management can not be controlled after construction. To estimate the tensile force of PS tendon during lifetime of PSC girder, this research proposed a bobbin-type embedded EM sensor that can be embedded in PSC girder is designed and fabricated considering the shape properties of anchorage zone and sheath. To verify the proposed sensor, a small PSC girder test was performed. The embedded EM sensor was connected to a sheath and anchor block, and the concrete was poured. After curing, the change of the permeability of PS tendon under tensile forces of 200, 710, 1070, 1300kN was measured using embedded EM sensor. The permeability of PS tendon had decreased according to the increment of applied tensile force. Also it is confirmed that the change of permeability due to applied tensile force could resolve the applied tensile force values. As a result, proposed embedded EM sensor could be embed into the PSC girder and it could be used to estimate the tensile force variation during lifetime of PSC girder.

A Study on the Earlier Stabilization for the Landfill of Municipal Refuse (매립지의 도시폐기물 조기안정화 방안에 관한 연구)

  • Choung, Youn Kyoo
    • KSCE Journal of Civil and Environmental Engineering Research
    • /
    • v.13 no.1
    • /
    • pp.221-232
    • /
    • 1993
  • In this study, the period for stabilization in the case of recycling leachate was compared and analyzed with the case of non-cycle type, using lysimeters filled with municipal organic refuse. The lysimeters were operated with various detention time. In addition, the degree of stabilization was estimated by the way of measuring the quantity of gas from landfills. As the results, the recycle of leachate, which was modified as the neutral level of pH, accelerated the biological decomposition of organics with the raped growth of anaerobic bacteria in the system, and reduced the period for the stabilization. In the case of BOD and COD in leachate, COD. which had been originality similar to BOD, had increased more rapidly than BOD as time lapsed. Moreover, the quantity of gas from the recycle reactor was larger than from the non-cycle reactor. The shorter the detention time of leachate gas, the larger the quantity of gas produced in the lysimeters.

  • PDF

Grinding Effects of Coal-Fired Pond Ash on Compressive Strength of Geopolymers (화력발전소 매립 석탄재의 분쇄가 지오폴리머의 강도에 미치는 영향)

  • Lee, Sujeong;Kang, Nam-Hee;Chon, Chul-Min;Jou, Hyeong-Tae
    • Resources Recycling
    • /
    • v.23 no.6
    • /
    • pp.3-11
    • /
    • 2014
  • Bottom ash from coal fired power plants is not widely used due to a broad range of particle sizes and a high carbon content for producing geopolymers. The effect of mechanical activation on compressive strength of bottom ash- based geopolymers was examined by rod and planetary-ball milling to encourage full-fledged recycling of bottom ash, the main component of pond ash. The amount of amorphous component in the milled ash samples did not change significantly after the mechanical activation. It is presumably because needle-shaped mullite crystals, which is a major crystalline phase and grown in a glassy matrix, possess high strength and toughness, and therefore, they could endure external shocks and remain almost intact. Milling operation, however, decreased the particle size and improved the homogeneity of ash, thereby leading to increase reactivity of milled ash with alkali activators. Rod milling produced a relatively narrow particle size distribution of the milled ash particles; however, it was less effective in reducing the particle size. Nevertheless, it was interesting to observe that rod milling had equal effect on improving the compressive strength of geopolymers up to about 37%, as that of planetary ball milling. Rod milling is believed to be suitable process for enhancing the reactivity of bottom ash for large-scale recycling of bottom ash and producing geopolymers.

Experimental Study on Engineering Characteristic of the Waste Landfill Soil Admixed Linear (폐기물매립지 토사계 혼합 차수재의 공학적 특성에 대한 실험적 연구)

  • Chang, Yongchai;Kim, Jinchun;Jeong, Ogki
    • Journal of the Korean GEO-environmental Society
    • /
    • v.8 no.1
    • /
    • pp.13-20
    • /
    • 2007
  • Leachates resulting from the waste landfill of waste can possibly cause the second pollution, such as the underground water and environmental pollution. Accordingly, Liner layer has been installed in the reclaimed land of waste to block and purify permeation water to and prevent this second pollution. The material used as Liner layer should have water resistance and be less than permeability coefficient of $1{\times}10^{-7}$ cm/sec. As it is very difficult to get this kind of natural clay with low permeability around the field, the suitable way to get the low permeable material is to use blend with good watertighness by mixing it with natural soil which is spread in the site. While this mixed soil, which can resist water, is commonly used in the site, namely, bentonite and MCG cementious mateiral mixed soil, which is widely used as Liner layer in the reclaimed land of waste, is recognized in Liner and durability. The study was performed to find the effect of additive of the bottom liner in the waste landfill. The aim of this paper is to explain of the field application examples as well as the data of experimental research with the engineering properties of Liner layer of the reclaimed land.

  • PDF

Analysis of the Relationship between the Seasonal Temperature Change and the Electrical Resistivity Value of Landfill Site (매립지의 계절별 온도변화와 전기비저항값의 상관성 분석)

  • Sim, Nak Jong;Ryu, Don Sik;Kim, Chang Gyun;Lee, Chul Hee
    • Journal of Korean Society of Environmental Engineers
    • /
    • v.39 no.9
    • /
    • pp.534-541
    • /
    • 2017
  • The bioreactor type of landfill is to operate to enhance waste decomposition by continuously supplying water such as leachate and wastewater within the landfill, which helps increase the landfill gas production, which in turn prematurely stabilize the landfill. Recently, the environmental law for the operation of the bioreactor type of landfill has been enacted and thereafter the bioreactor type of landfill has been introduced for the first time in Korea to the SUDOKWON landfill site. In order to properly apply for bioreactor to the landfill, it is necessary to investigate the water distribution inside the landfill so that water recirculation should be optimally allocated with the zone of concern. In this regard, electrical resistivity survey has been suitably performed to delineate the water distribution in the landfill. That is, it has surveyed for long-term of period that the recirculation of leachate has been properly reflected from electrical resistivity within the second landfill of SUDOKWON landfill site. As a result, the electrical resistivity immediately corresponded to the variation of the extent of the seasonal temperature dynamics. From this, a calibratrion could be accomplished by correlating between temperature and electrical resistivity obtained from this study that can be applicable for optimally monitoring to keep the ideal operating condition for the bioreactor type of landfill.

Variation of Critical Chloride Content of Rebar Embedded in Concrete with Admixture (혼화재 혼입에 따른 콘크리트에 매립된 철근의 부식 임계 염화물량의 변화)

  • Park, Jang-Hyun;Lee, Yun-Su;Lee, Han-Seung
    • Journal of the Korea Institute of Building Construction
    • /
    • v.19 no.6
    • /
    • pp.511-520
    • /
    • 2019
  • The critical chloride content of rebar embedded in concrete was experimentally evaluated according to the admixture replacement ratio and admixture type. Four types of reinforced concrete were mixed OPC 100%, OPC 70% + GGBFS 30%, OPC 40% + GGBFS 60%, and OPC 40% + GGBFS 40% + FA 20%. NaCl solution was supplied to the specimens, and the open circuit potential of the embedded rebar was monitored. The specimens determined to initiate corrosion were cut at intervals of 5mm from the NaCl solution supply surface and conducted to chlorine ion profile. Corrosion initiation time of rebar embedded in concrete was delayed as the admixture replacement ratio increased. Looking at the critical chloride content of the types of reinforced concrete, it was highest in OPC 1.46kg/㎥, followed in order by S30 0.98kg/㎥, TBC 0.74kg/㎥, and S60 0.71kg/㎥.