Durability of MEA Using sPEEK Membrane Reinforced with Poly Imide in PEMFC (고분자전해질연료전지에서 폴리이미드 강화 sPEEK막 MEA의 내구성)

  • Lee, Hye-Ri;Na, Il-Chai;Oh, Sung-Jun;Park, Kwon-Pil
    • Korean Chemical Engineering Research
    • /
    • v.55 no.3
    • /
    • pp.296-301
    • /
    • 2017
  • Recently, there are many efforts focused on development of more economical non-fluorinated membranes for PEMFCs (Proton Exchange Membrane Fuel Cells). In this study, sulfonated poly (ether ether ketone) (sPEEK) membrane reinforced with poly imide was made to enhance of membrane durability. In order to test durability of single (un-reinforced) membrane and reinforced membrane MEA (Membrane and Electrode Assembly), degradation accelerated stress test was used. Before and after degradation, I-V polarization curve, hydrogen crossover current, electrochemical surface area, membrane resistance and charge transfer resistance were measured. As a result of experiments, hydrogen crossover current of reinforced MEA was lower than that of single MEA, therefor durability of reinforced MEA was higher than that of single MEA. There was not especially short phenomena in reinforced MEA after degradation accelerated stress test.

Effect of Pt-Co/C Cathode Catalyst on Electrochemical Durability of Membrane in PEMFC (PEMFC에서 Pt-Co/C Cathode 촉매가 고분자막의 전기화학적 내구성에 미치는 영향)

  • Sohyeong Oh;Dong Geun Yoo;Myoung Hwan Kim;Ji Young Park;Kwonpil Park
    • Korean Chemical Engineering Research
    • /
    • v.61 no.2
    • /
    • pp.189-195
    • /
    • 2023
  • As a PEMFC (Polymer Exchange Membrane Fuel Cell) cathode catalyst, Pt-Co/C has recently been widely used because of its improved durability. In a fuel cell, electrodes and electrolytes have a close influence on each other in terms of performance and durability. The effect on the electrochemical durability of the electrolyte membrane when Pt-Co/C was replaced in the Pt/C electrode catalyst was studied. The durability of Pt-Co/C MEA (Membrane Electrode Assembly) was higher than that of Pt/C MEA in the electrochemical accelerated degradation process of PEMFC membrane. As a result of analyzing the FER (Fluorine Emission Rate) and hydrogen permeability, it was shown that the degradation rate of the membrane of Pt-Co/C MEA was lower than that of Pt/C MEA. In the OCV (Open Circuit Voltage) holding process, the rate of decrease of the active area of the Pt-Co/C electrode was lower than that of the Pt/C electrode, and the amount of Pt deposited on the membrane was smaller in Pt-Co/C MEA than in Pt/C MEA. Pt inside the polymer membrane deteriorates the membrane by generating radicals, so the degradation rate of the membrane of Pt/C MEA with a high Pt deposition rate was higher than Pt-Co/C MEA. When the Pt-Co/C catalyst was used, the electrode durability was improved, and the amount of Pt deposited on the membrane was also reduced, thereby improving the electrochemical durability of the membrane.

Humidification model and heat/water balancing method of PEMFC system for automotive applications (자동차용 연료전지 시스템의 가습모델과 열/물균형 유지방법)

  • Jung, Seung-Hun;Yoon, Seok-Ho;Kim, Min-Soo
    • 한국신재생에너지학회:학술대회논문집
    • /
    • 2005.06a
    • /
    • pp.339-344
    • /
    • 2005
  • A PEMFC system model for FCEV was constructed and simulated numerically to examine the heat/water flow of the system and air/fuel humidification process for various operation conditions (ambient pressure /temperature/humidity, operating temperature, power load). We modeled PEMFC stack which can generate maximum electricity of about 80 kW. This stack consists of 400 unit cells and each unit cell has $250cm^2$ reacting area. Uniform current density and uniform operating voltage per each cell was assumed. The results show the flow characteristics of heat and water at each component of PEMFC system in macro-scale. The capacity shortage of the radiator occurred when the ambient was hot $(over\;40^{\circ}C)$ and power level was high (over 50 kW). In spite of some heat release by evaporation of water in stack, heat unbalance reached to 20kW approximately in such a severe operating condition. This heat unbalance could be recovered by auxiliary radiators or high speed cooling fan with additional cost. In cold environment, the capacity of radiator exceeded the net heat generation to be released, which may cause a problem to drop the operating temperature of stack. We dealt with this problem by regulating mass flow rate of coolant and radiator fan speed. Finally, water balance was not easily broken when we retrieved condensed and/or unused water.

  • PDF

Platinum Nanoparticles Synthesis using Recovered Platinum from Waste Fuel cell (폐연료전지(廢燃料電池)스택으로부터 회수(回收)된 백금(白金)의 나노 입자(粒子) 제조(製造))

  • Kim, Young-Ae;Kwon, Hyun-Ji;Koo, Jeong-Boon;Kwak, In-Seob;Sin, Jang-Sik
    • Resources Recycling
    • /
    • v.20 no.2
    • /
    • pp.67-73
    • /
    • 2011
  • In this study, for recovery of renewable noble metal from used stack of fuel cell, synthesis of platinum nano particle is established through effect of platinum solution concentration, pH value, reducing agent and dispersing agent at a volume ratio of 1 mM $H_2PtCl_6$:10 mM $NaBH_4$:8 mM Cl4TABr = 1:0.4:0.4(vol.%), pH4, $50^{\circ}C$, 160 rpm and 10min. Less than 5 nm platinum particles were synthesized using Pt leaching solution from used MEA of stack under same condition of method using simulated Pt solution. The characteristics of synthesized nano particles was illustrated by XPS analysis as the reduction of platinum ions into platinum metals(zero-valent).

Enhancement of Membrane Durability in PEMFC by Fucoidan and Tannic Acid (후코이단과 탄닌산에 의한 PEMFC 고분자막의 내구성 향상)

  • Mihwa Lee;Sohyeong Oh;Cheun-Ho Chu;Young-Sook Kim;Il-Chai Na;Kwonpil Park
    • Korean Chemical Engineering Research
    • /
    • v.61 no.1
    • /
    • pp.45-51
    • /
    • 2023
  • In order to improve the durability of the PEMFC(Proton Exchange Membrane Fuel Cells) polymer membrane, a radical scavenger and a support are used. In this study, the durability of membranes containing fucoidan extracted from seaweeds and tannic acid serving as a crosslinking agent is evaluated to improve chemical and physical durability. Physical durability is evaluated by measuring tensile strength, and chemical durability is measured by Fenton experiment. Membrane and electrode assembly (MEA) is prepared and mechanical and chemical durability are measured through accelerated durability evaluation in the cell. The tensile strength measurement showed that fucoidan and tannic acid can improve the mechanical durability of the membrane by improving the strain rate and yield strength. It is shown in Fenton experiment that fucoidan acts as a radical scavenger. As a result of the accelerated durability test in the unit cell, fucoidan improved both chemical and mechanical durability, increasing the accelerated durability evaluation time by 38.1% compared to the additive-free membrane. When tannic acid is added, the durability of the polymer membrane is improved by 13.9% by improving the mechanical durability.