• Title/Summary/Keyword: 루트 간격

Search Result 18, Processing Time 0.023 seconds

A Study on the Effects of Root Gap on Mechanical Properties and Microstructure of Weldment (루트간격이 용접부의 기계적 성질과 미세조직에 미치는 영향에 관한 연구)

  • Lee, Won-Kun;Jang, Gyoung-Boc;Kang, Sung-Soo
    • Journal of the Korean Society for Precision Engineering
    • /
    • v.16 no.10
    • /
    • pp.187-193
    • /
    • 1999
  • Dimensional difference by welding deformation is usually occurred at steel bridge manufacturting or multi-pass welding used at joining of thick plates. Be this, root gap out of standard is frequently developed at butt weld joints. For example, although standard root gap below 6mm at butt weld joints of plates under 15mm thickness, maximum 30mm root opening is developed at the weld field. At this case, 24mm parts out of standard is generally built up. But, there are no accumulated data and restriction about this built up welding pars. In this study, therefore, the accumulation of data for built up parts and the verification of the mechanical properties of weld part as root gap is performed. It is included that tensile, bending, impact, hardness test and microstructural review for each welding specimen of 0mm, 6mm, 30mm root opening.

  • PDF

An Algebraic Function Control on the Optimal Spaced Grounding Conductor (최적 접지도체간격에 관한 대수함수제어)

  • Song, Young-Joo;Choi, Hong-Kyoo
    • Journal of the Korean Institute of Illuminating and Electrical Installation Engineers
    • /
    • v.20 no.5
    • /
    • pp.116-124
    • /
    • 2006
  • No matter how the equally spaced grounding grid is designed there are many problem. The best-fitted design for unequally spaced grounding grid is a part that must be considered. This paper Suggest a new way of calculation for grounding grid space of ground conductor by an algebraic function control(The first-order function, Root function, Polynomial function etc.) and on the optimal spaced grounding conductor that make the under 2[%] between maximum potential and minimum potential.

Distribution of Welding Residual Stresses in T-joint Weld with Root Gap (루트부 갭이 있는 양면 필릿용접 이음부의 용접잔류응력 분포)

  • H.S. Bang;S.H. Kim;Y.P. Kim;C.W. Lee
    • Journal of the Society of Naval Architects of Korea
    • /
    • v.39 no.3
    • /
    • pp.81-88
    • /
    • 2002
  • The root joint in the welding structures are apt to failure by the stress concentration which is occurred by the external force. Therefore, in the safety and reliability of structure, the complete penetration joint welding which are obtained by the groove welding with edge preparation is generally required. Nevertheless, fillet T-joint welding without edge preparation is often carried out in the fields to reduce working time and consumption of welding electrode, however, this process is likely to produce inadequate joint penetration such as root gap. In this paper, the focus of research is to investigate distribution of welding residual stresses in the plate(or flange) and web of T-joint weld, and especially in the near of root gap notch that is due to incomplete joint penetration. For the analysis, we have chosen model of T-joint weld in the cases of single and multi-pass welding with submerged arc welding and analyzed model by using finite element programs considering the heat conduction and thermal elasto-plastic theory.

Effects of Root Gap on Residual Stresses and Deformation in the Multi-Pass Weld of Thick Plates for Steel Bridge (교량용 후판 다층용접시 잔류응력과 변형에 미치는 루트간격의 영향)

  • 장경복;김하근;강성수
    • Journal of Welding and Joining
    • /
    • v.17 no.1
    • /
    • pp.88-96
    • /
    • 1999
  • The effects of root gap on welding residual stress and deformation are dealt with the multi-pass weldment with three kinds(0, 6, 30mm) of root gap by F.E.M common code, and then compared with experiment data. In this analysis, an 100% ramp heat input model was used to avoid numerical convergence problem due to an instantaneous increase in temperature near the fusion zone, and the effect of a moving arc in a two dimensional plane was also included. During the analysis, a small time increment was applied in a period with instantaneous temperature fluctuation while a large time increment was used in the rest period. The residual stress is distributed as symmetric types and maximum value is also equivalent when the weldment with 0mm and 6mm root gap is welded. In the case of 30mm root gap welding, the distribution of the residual stress extends over a wide range as asymmetric types due to the built-up weld, and most of the residual stress is biased in the side of a built-up weld part. In case of 0mm gap welding and 6mm gap welding, a little angular distortion occurs, but the level of deformation is small. When the weldment with 30mm root gap is welded, the angular deformation of the asymmetric types, however, occurs larger than the other specimens. The experimental and the analytic results show good coincidence and indicate that the welding residual stress and deformation distribution of 30 mm root gap specimen may be asymmetric and the amplitude is larger than those of root gap specimen under standard.

  • PDF

Fatigue Assessment of High Strength Steel with Butt Welded Joints for the Root Gap Difference (고강도강 맞대기 용접 시험편의 루트갭 변경에 따른 피로강도 평가)

  • Kim, Ho-Jung;Kang, Sung-Won;Kim, Myung-Hyun
    • Journal of the Society of Naval Architects of Korea
    • /
    • v.48 no.1
    • /
    • pp.56-61
    • /
    • 2011
  • In this study, a series of fatigue tests was conducted to evaluate fatigue strength for the root gap difference with high strength steel with butt welded joints. A finite element analysis using effective notch stress method was also performed to compare effective notch factors each other with butt welded specimens made by copper backing. The results of fatigue tests were classified according to the root gap difference. Fatigue life of butt welded specimens is presented for determining the root gap of high strength steel with butt welded joints in terms of fatigue strength. Then effective notch stress was applied to interpret fatigue strength of butt welded specimen model which is reflected actual measured dimensions. As a result, fatigue strength of high strength steel with butt welded specimens is increased by root gap gets longer in length.

The Evaluation of Mixed Welded SM 490A Steel by Acoustic Emission (3) (음향방출법에 의한 SM 490A 강의 복합용접성 평가 (3))

  • 이장규;인승현;우창기;박성완;김봉각
    • Proceedings of the Korean Society of Machine Tool Engineers Conference
    • /
    • 2003.10a
    • /
    • pp.289-294
    • /
    • 2003
  • The object of this study is to investigate the effect of compounded welding by using acoustic emission (AE) signals fur weld heat affected zone (HAZ) in tensile testing. This study was carried out a SM 490A high tension steel for electronic shielded metal are welding (SMAW), $\textrm{CO}_2$ gas arc welding and TIG welding. And correspondingly, the root openings are 3, 4 and 2.8mm. Data displays are based on the measured parameters of the AE signals, along with environmental variables such as time and load. These history plots give us useful and powerful information to analyze the results of material evaluation testing.

  • PDF

The Effects of Root Gap on Mechanical Properties and Fatigue Strength of Weldment (용접부의 기계적 성질 및 피로강도에 미치는 루트 간격의 영향)

  • 이원근;장경복;강성수
    • Journal of Welding and Joining
    • /
    • v.19 no.2
    • /
    • pp.98-103
    • /
    • 2001
  • Root gap out of standard by welding deformation is frequently produced at butt weld joints of steel bridge. For example although standard root gap is below 6mm at butt weld joints of plates under 15mm thickness. maximum 35mm root opening is produced at the weld field. At this case, the part out of standard is generally built up and the rest part is welded by WPS. Direct welding without built-up welding is preferred in weld field because built-up welding process bring about the cost-up at manufacturing. To apply this direct weld to root gap out of standard, the investigation about mechanical properties and fatigue at weldment is required. Inthisstudy, therefore the verification for direct weld without built up is performed at weldment as root gap. It includes tension, bending. hardness, impact and fatigue test for each welding specimen of 6mm, 25mm, 35mm root gap.

  • PDF

Tensile Testing of Groove Welded Joints Joining Thick-HSA800 Plates (HSA800 후판재의 맞댐용접부 인장강도 실험)

  • Lee, Cheol Ho;Kim, Dae Kyung;Han, Kyu Hong;Park, Chang Hee;Kim, Jin Ho;Lee, Seung Eun;Kim, Do Hwan
    • Journal of Korean Society of Steel Construction
    • /
    • v.25 no.4
    • /
    • pp.431-440
    • /
    • 2013
  • In this study, a standard tensile welded-joint test was conducted to select a welding electrode suitable for recently developed HSA800 steel. Two welding electrodes were available at the time of this study; one was GMAW-based and the other FCAW-based. The tensile test specimens were fabricated by joining 60mm-thick HSA800 plates according to the AWS-prequalified groove welded joint details. Specimens which violate the standard root opening distance (ROD) were also included to see if poor construction tolerance could be accommodated. During fabrication, serious concerns about the welding efficiency of the GMAW-based product were raised by a certified welder. Both welding electrodes showed satisfactory and similar performance from welded joint strength perspective. But groove welded joints made by using the FCAW-based rod consistently showed more ductile and stable behavior. The AISC provisions for PJP joint strength were shown to be very conservative under direct tensile loading. Violating the AWS prequalified ROD by 100% apparently passed the strength criteria, but unusual crater-like fracture surface was observed.

Experimental Studies on Joinability of SWS 490A High Tension Steel using Acoustic Emission Signals (음향방출 신호를 이용한 SWS 490A 고장력강의 접합성 평가에 대한 실험적 연구)

  • Rhee Zhang-Kyu;Woo Chang-Ki
    • Transactions of the Korean Society of Machine Tool Engineers
    • /
    • v.14 no.3
    • /
    • pp.87-95
    • /
    • 2005
  • The object of this study is to investigate the effect of joinability by using acoustic emission(AE) signals and doing a pattern recognition for weld heat affected zone(HAZ) in tensile testing. This study was carried out an SWS 490A high tension steel for electric shielded metal arc welding(SMAW), $CO_2$ gas arc welding and TIG welding. And correspondingly, the root openings are 3, 4 and 2.8mm. The results of the tensile test of weld HAZ come out electric shield arc welding $>\;CO_2$ gas arc welding > TIG welding in case of single welding. It is believed that this is a phenomenon where difference of its root opening or base metal thickness. Also, the technique of AE is ideally suited to study variables which control time and stress dependent fracture or damage process in metallic materials.

A Study on the Back Bead control by Using Short Circuit Frequency in GMA Welding of Sheet Metal (박판 GMA 용접에서 단락 주파수를 이용한 이면비드의 제어에 관한 연구)

  • 안재현;김재웅
    • Journal of Welding and Joining
    • /
    • v.13 no.4
    • /
    • pp.75-84
    • /
    • 1995
  • In GMA welding of sheet metal, the short circuit metal transfer mdoe is preferred because of its low heat input and capability of bridging the root gap. The molten electrode is transferred to the workpiece during repectitive short circuit in the model. The waveform of welding current or voltage and the frequency of short circuiting are affected by a number of factors including: magnitude of welding current and voltage, root gap, electrode extension, power supply characteristics, and so on. In this study experimental models were proposed, which are able to determine the relationship between the root gap and short circuit frequency and the relationship between the root gap and appropriate welding speed that produces the good quality of back bead without burn through. Using the experimental models, the root gap can be obtained from measuring the short circuit frequency, and then the appropriate weldig speed to the root gap can be determined. Thus a back bead control system was constructed by controlling the welding speed for maintaining the quality of back bead. The developed system has shown the successful capability of back bead control.

  • PDF