레독스-흐름 2차 전지는 레독스 쌍이 녹아있는 수용액을 탱크에 저장한 다음 펌프로 유통형 전해 셀에 공급해 충방전하는 2차 전지의 한 종류이며, 종래의 2차 전지와는 다른 재생형 연료전지 중의 하나이다[1]. 이러한 전지의 원리는 19세기말부터 알려져 있었지만, 중량과 용적이 컸기 때문에 소형화, 경량화가 중시되는 2차 전지로서는 부적당하였고, 수용액을 사용하기 때문에 기전력이 낮다는 결점이 있었다.(중략)
Membrane characterization methods for aqueous redox flow batteries aqueous RFBs were modified for non-aqueous RFBs. The modified characterization methods, such as ion exchange capacity, transport number, permeability and single cell test, were carried out to evaluate commercial membranes in non-aqueous electrolyte. It was found that columbic efficiency and energy efficiency in a single cell test were dependent on the ion selectivity of commercial anion exchange membranes. Neosepta AHA anion exchange membrane showed the anion transport number of 0.81, which is a relatively low ion selectivity in non-aqueous electrolyte, however, exhibited 92% of coulombic efficiency and 86% of energy efficiency in a single cell test. It was also found that a porous membrane without ion selectivity is suitable for a non-aqueous redox flow battery at a high current density.
The cation exchange membrane using the block co-polymer of polysulfone and polyphenylenesulfidesulfone was prepared for a separator of all-vanadium redox flow battery. The membrane property of the prepared cation exchange membrane was measured. The thermal stability of the prepared cation exchange analyzed by TG showed a more stable than that of Nafion117. The lowest measured membrane resistance, equilibrated in 1mol/L $H_2SO_4$ aqueous solution, $0.96{\cdot}cm^2$ at 3 cc of CSA (chlorosulfuricacid) which was introduction agent of ion exchange group. Electrochemical property of all-vanadium redox flow battery using the prepared cation exchange membrane was measured. Electromotive force in 100% of state of charge was 1.4 V which was that of all-vanadium redox flow battery, and cell resistance in charge and discharge at each state of charge had a low value compared with that of all-vanadium redox flow battery using Nafion117.
Proceedings of the Membrane Society of Korea Conference
/
1993.10a
/
pp.63-64
/
1993
레독스-흐름 2차전지는 발전소의 잉여전력, 태양전지 및 전기자동차 등 응용 분야가 넓은 유망한 에너지 저장 방법의 하나이다[1,2]. Fe-Cr계 2차전지와 비교하여 수소 가스의 발생이 없고 양쪽 액의 확산에의한 혼합으로 전지의 용량이 떨어지지 않고 rebalance의 필요가 없는 등 많은 장점을 가지고 있으며 조작이 간단하며 기전력 (1,4 V)과 에너지 밀도가 높기 때문에 compact화가 가능하다[1].
In this study, we synthesized vinylbenzyl chloride-co-styrene-co hydroxyethyl acrylate (VBC-co-St-co-HEA) copolymer that can be applied to redox the flow battery process. The anion exchange membrane was prepared by the amination and crosslinking of VBC-co-St-co-HEA copolymer. The chemical structure and thermal properties of VBC-co-St-co-HEA copolymer and aminated VBC-co-St-co-HEA(AVSH) membrane were characterized by FTIR, $^1H$ NMR, TGA, and GPC analysis. The membrane properties such as ion exchange capacity(IEC), electrical resistance, ion conductivity and efficiency of all-vanadium redox flow battery were measured. The IEC value, electrical resistance, and ion conductivity were 1.17 meq/g, $1.9{\Omega}{\cdot}cm^2$, 0.009 S/cm, respectively. The charge-discharge efficiency, voltage efficiency and energy efficiency from all-vanadium redox flow battery test were 99.5, 72.6 and 72.1%, respectively.
바나듐 3, 4, 5가 이온은 공기 중에서 안정하지만, 바나듐 2가 이온은 쉽게 산화된다. 그러므로 바나듐 2가 이온이 담겨져 있는 음극 탱크가 공기와 접촉하지 않게 하는 것이 중요하다. 충전 중 음극 탱크에 공기가 침투되면, 바나듐 2가 이온은 3가 이온으로 산화되기 때문에 음극과 양극의 전해질에 불균형을 초래한다. 이러한 불균형은 바나듐 레독스 흐름전지 용량저하의 원인이 된다. 본 연구에서는 공기 중 2가 이온 산화에 의한 전해질의 불균형 현상을 쉽게 보여주기 위해, 공기노출과 차단조건에서 충방전 중에 발생한 음극과 양극의 바나듐 이온 상태변화량을 UV-Visible spectrophotometer를 이용해 정량적으로 분석하였다. 분석 결과, 공기노출 조건에서 음극의 충전 시, 충방전 cycle이 진행 될수록 바나듐 2가 이온의 양이 현격히 줄어들었지만, 공기차단 조건에서는 2가 이온의 양이 공기노출 조건보다 훨씬 더 적게 줄어들었다. 즉, 공기차단 조건에서는 바나듐 2가 이온이 3가로 산화되지 않아서 음극의 충전 후 바나듐 3가에서 2가로 전환되는 양이 공기노출 조건보다 더 많은 것을 확인할 수 있었다. 이러한 영향으로 인해, 충방전 10th cycle을 진행해 본 결과, 공기차단 조건에서는 충방전 용량감소가 거의 없었지만 공기노출 조건에서는 현격한 충방전 용량 감소를 보였다.
Redox flow secondary battery have been studied actively as one of the most promising electrochemical energy storage devices for a wide range of applications, such as electric vehicles, photovoltaic arrays, and excess power generated by electric power plants. In all-vanadium redox flow battery using solution of vanadium-sulfuric acid as a active material, the difficulty in developing an efficient ion selective membrane can still be identified. The asymmetric cation exchange membrane(M-30) as a separator of all-vanadium redox flow battery which were obtained by the reaction of chlorosulfonation for 30 minutes under the irradiation of UV, showed its superiority in the transport number of 0.94 and electrical resistivity of $0.5{\Omega}{\cdot}cm^2$. The base membrane were prepared by lamination a low density polyethlene film of $10{\mu}m$ thickness on polyolefin membrane(HIPORE 120). The electrical resistivity of M-30 membrane in real solution of vanadium-sulfuric acid was $3.79{\Omega}{\cdot}cm^2$ and it was similar to that of Nafion 117 membrane. Also the cell resistivity was $6.6{\Omega}{\cdot}cm^2$and lower than that of Nafion 117. In considertion of electrochemical properties and costs of membranes, M-30 membrane was better than that of Nafion 117 and CMV of Asahi glass Co. as a separator of all-vanadium redox flow battery.
In this study, we investigated the electrocatalytic effects of the N and O co-doping of Graphite Felt (GF) electrode for the vanadium redox flow battery (VRFB) at the cathode and the anode reaction, respectively. The electrodes were prepared by chemical vapor deposition (CVD) with $NH_3-O_2$ at 773 K, and its effects were compared with an electrode prepared by an O doping treatment. The surface morphology and chemical composition of the electrodes were characterized by scanning electron microscopy (SEM) and photoelectron spectroscopy (XPS). The electrocatalytic properties of these electrodes were characterized in a VRFB single cell comparing the efficiencies and performance of the electrodes at the cathode, anode, and single cell level. The results exhibited about 2% higher voltage and energy efficiencies on the N-O-GF than the O-GF electrode. It was found that the N and O co-doping was particularly effective in the enhancement of the reduction-oxidation reaction at the anode.
Proceedings of the Korean Institute of Surface Engineering Conference
/
2015.11a
/
pp.338-338
/
2015
VRFB(Vanadium Redox Flow Battery)는 바나듐계 이온을 전해질로 사용하는 레독스 흐름 전지로, 전해질의 양이 전지의 용량을 결정하기 때문에 주로 대용량의 전력이 필요한 플랜트 등에서 주로 사용하는 전지이다. 이 VRFB내에는 Current collector의 부식 방지용으로 두꺼운 Graphite판을 BP(Bipolar plate)로 사용한다. 플랜트에서는 대용량 전지를 필요로 하여 Single stack으로는 사용되기 어렵고, Multi stack으로 주로 사용한다. Multi stack의 경우, 수 백장의 BP가 들어가 전지의 부피가 매우 커지게 되고, 이에 본 연구에서는 BP의 두꺼운 Graphite를 얇은 $TiO_2$ 기판으로 교체하여 성능을 비교하는 연구를 진행하였다. Ti 금속기판을 양극산화법으로 $TiO_2$ 나노튜브 구조를 만든 후, $TiO_2$의 전도도 향상을 목적으로 $IrO_2$를 코팅하였다. 결과적으로 기존의 Graphite에 비해 전기화학적 특성이 향상되었음을 확인하였으며, Cell test를 통해 VRFB의 성능을 평가하였다.
본 논문은 레독스 흐름 전지(Redox Flow Battery : RFB)용 양극성을 갖는 DC-DC 컨버터의 기본 동작 원리 및 최적 스위칭 기법에 관한 것이다. 양극성을 갖는 DC-DC 컨버터는 매우 낮은 배터리 전압에서도 완전 방전을 위해 고승압이 필요하고, 완전 방전 후 극성 반전이 되어 매우 낮은 전압에서도 충전이 가능하여야 한다. 본 논문에서는 이러한 동작이 요구되는 RFB용 DC-DC 컨버터의 스위칭 손실을 최소화하기 위한 스위칭 방법을 제안한다. 최종 발표 시 실험 결과를 제시하고자 한다.
본 웹사이트에 게시된 이메일 주소가 전자우편 수집 프로그램이나
그 밖의 기술적 장치를 이용하여 무단으로 수집되는 것을 거부하며,
이를 위반시 정보통신망법에 의해 형사 처벌됨을 유념하시기 바랍니다.
[게시일 2004년 10월 1일]
이용약관
제 1 장 총칙
제 1 조 (목적)
이 이용약관은 KoreaScience 홈페이지(이하 “당 사이트”)에서 제공하는 인터넷 서비스(이하 '서비스')의 가입조건 및 이용에 관한 제반 사항과 기타 필요한 사항을 구체적으로 규정함을 목적으로 합니다.
제 2 조 (용어의 정의)
① "이용자"라 함은 당 사이트에 접속하여 이 약관에 따라 당 사이트가 제공하는 서비스를 받는 회원 및 비회원을
말합니다.
② "회원"이라 함은 서비스를 이용하기 위하여 당 사이트에 개인정보를 제공하여 아이디(ID)와 비밀번호를 부여
받은 자를 말합니다.
③ "회원 아이디(ID)"라 함은 회원의 식별 및 서비스 이용을 위하여 자신이 선정한 문자 및 숫자의 조합을
말합니다.
④ "비밀번호(패스워드)"라 함은 회원이 자신의 비밀보호를 위하여 선정한 문자 및 숫자의 조합을 말합니다.
제 3 조 (이용약관의 효력 및 변경)
① 이 약관은 당 사이트에 게시하거나 기타의 방법으로 회원에게 공지함으로써 효력이 발생합니다.
② 당 사이트는 이 약관을 개정할 경우에 적용일자 및 개정사유를 명시하여 현행 약관과 함께 당 사이트의
초기화면에 그 적용일자 7일 이전부터 적용일자 전일까지 공지합니다. 다만, 회원에게 불리하게 약관내용을
변경하는 경우에는 최소한 30일 이상의 사전 유예기간을 두고 공지합니다. 이 경우 당 사이트는 개정 전
내용과 개정 후 내용을 명확하게 비교하여 이용자가 알기 쉽도록 표시합니다.
제 4 조(약관 외 준칙)
① 이 약관은 당 사이트가 제공하는 서비스에 관한 이용안내와 함께 적용됩니다.
② 이 약관에 명시되지 아니한 사항은 관계법령의 규정이 적용됩니다.
제 2 장 이용계약의 체결
제 5 조 (이용계약의 성립 등)
① 이용계약은 이용고객이 당 사이트가 정한 약관에 「동의합니다」를 선택하고, 당 사이트가 정한
온라인신청양식을 작성하여 서비스 이용을 신청한 후, 당 사이트가 이를 승낙함으로써 성립합니다.
② 제1항의 승낙은 당 사이트가 제공하는 과학기술정보검색, 맞춤정보, 서지정보 등 다른 서비스의 이용승낙을
포함합니다.
제 6 조 (회원가입)
서비스를 이용하고자 하는 고객은 당 사이트에서 정한 회원가입양식에 개인정보를 기재하여 가입을 하여야 합니다.
제 7 조 (개인정보의 보호 및 사용)
당 사이트는 관계법령이 정하는 바에 따라 회원 등록정보를 포함한 회원의 개인정보를 보호하기 위해 노력합니다. 회원 개인정보의 보호 및 사용에 대해서는 관련법령 및 당 사이트의 개인정보 보호정책이 적용됩니다.
제 8 조 (이용 신청의 승낙과 제한)
① 당 사이트는 제6조의 규정에 의한 이용신청고객에 대하여 서비스 이용을 승낙합니다.
② 당 사이트는 아래사항에 해당하는 경우에 대해서 승낙하지 아니 합니다.
- 이용계약 신청서의 내용을 허위로 기재한 경우
- 기타 규정한 제반사항을 위반하며 신청하는 경우
제 9 조 (회원 ID 부여 및 변경 등)
① 당 사이트는 이용고객에 대하여 약관에 정하는 바에 따라 자신이 선정한 회원 ID를 부여합니다.
② 회원 ID는 원칙적으로 변경이 불가하며 부득이한 사유로 인하여 변경 하고자 하는 경우에는 해당 ID를
해지하고 재가입해야 합니다.
③ 기타 회원 개인정보 관리 및 변경 등에 관한 사항은 서비스별 안내에 정하는 바에 의합니다.
제 3 장 계약 당사자의 의무
제 10 조 (KISTI의 의무)
① 당 사이트는 이용고객이 희망한 서비스 제공 개시일에 특별한 사정이 없는 한 서비스를 이용할 수 있도록
하여야 합니다.
② 당 사이트는 개인정보 보호를 위해 보안시스템을 구축하며 개인정보 보호정책을 공시하고 준수합니다.
③ 당 사이트는 회원으로부터 제기되는 의견이나 불만이 정당하다고 객관적으로 인정될 경우에는 적절한 절차를
거쳐 즉시 처리하여야 합니다. 다만, 즉시 처리가 곤란한 경우는 회원에게 그 사유와 처리일정을 통보하여야
합니다.
제 11 조 (회원의 의무)
① 이용자는 회원가입 신청 또는 회원정보 변경 시 실명으로 모든 사항을 사실에 근거하여 작성하여야 하며,
허위 또는 타인의 정보를 등록할 경우 일체의 권리를 주장할 수 없습니다.
② 당 사이트가 관계법령 및 개인정보 보호정책에 의거하여 그 책임을 지는 경우를 제외하고 회원에게 부여된
ID의 비밀번호 관리소홀, 부정사용에 의하여 발생하는 모든 결과에 대한 책임은 회원에게 있습니다.
③ 회원은 당 사이트 및 제 3자의 지적 재산권을 침해해서는 안 됩니다.
제 4 장 서비스의 이용
제 12 조 (서비스 이용 시간)
① 서비스 이용은 당 사이트의 업무상 또는 기술상 특별한 지장이 없는 한 연중무휴, 1일 24시간 운영을
원칙으로 합니다. 단, 당 사이트는 시스템 정기점검, 증설 및 교체를 위해 당 사이트가 정한 날이나 시간에
서비스를 일시 중단할 수 있으며, 예정되어 있는 작업으로 인한 서비스 일시중단은 당 사이트 홈페이지를
통해 사전에 공지합니다.
② 당 사이트는 서비스를 특정범위로 분할하여 각 범위별로 이용가능시간을 별도로 지정할 수 있습니다. 다만
이 경우 그 내용을 공지합니다.
제 13 조 (홈페이지 저작권)
① NDSL에서 제공하는 모든 저작물의 저작권은 원저작자에게 있으며, KISTI는 복제/배포/전송권을 확보하고
있습니다.
② NDSL에서 제공하는 콘텐츠를 상업적 및 기타 영리목적으로 복제/배포/전송할 경우 사전에 KISTI의 허락을
받아야 합니다.
③ NDSL에서 제공하는 콘텐츠를 보도, 비평, 교육, 연구 등을 위하여 정당한 범위 안에서 공정한 관행에
합치되게 인용할 수 있습니다.
④ NDSL에서 제공하는 콘텐츠를 무단 복제, 전송, 배포 기타 저작권법에 위반되는 방법으로 이용할 경우
저작권법 제136조에 따라 5년 이하의 징역 또는 5천만 원 이하의 벌금에 처해질 수 있습니다.
제 14 조 (유료서비스)
① 당 사이트 및 협력기관이 정한 유료서비스(원문복사 등)는 별도로 정해진 바에 따르며, 변경사항은 시행 전에
당 사이트 홈페이지를 통하여 회원에게 공지합니다.
② 유료서비스를 이용하려는 회원은 정해진 요금체계에 따라 요금을 납부해야 합니다.
제 5 장 계약 해지 및 이용 제한
제 15 조 (계약 해지)
회원이 이용계약을 해지하고자 하는 때에는 [가입해지] 메뉴를 이용해 직접 해지해야 합니다.
제 16 조 (서비스 이용제한)
① 당 사이트는 회원이 서비스 이용내용에 있어서 본 약관 제 11조 내용을 위반하거나, 다음 각 호에 해당하는
경우 서비스 이용을 제한할 수 있습니다.
- 2년 이상 서비스를 이용한 적이 없는 경우
- 기타 정상적인 서비스 운영에 방해가 될 경우
② 상기 이용제한 규정에 따라 서비스를 이용하는 회원에게 서비스 이용에 대하여 별도 공지 없이 서비스 이용의
일시정지, 이용계약 해지 할 수 있습니다.
제 17 조 (전자우편주소 수집 금지)
회원은 전자우편주소 추출기 등을 이용하여 전자우편주소를 수집 또는 제3자에게 제공할 수 없습니다.
제 6 장 손해배상 및 기타사항
제 18 조 (손해배상)
당 사이트는 무료로 제공되는 서비스와 관련하여 회원에게 어떠한 손해가 발생하더라도 당 사이트가 고의 또는 과실로 인한 손해발생을 제외하고는 이에 대하여 책임을 부담하지 아니합니다.
제 19 조 (관할 법원)
서비스 이용으로 발생한 분쟁에 대해 소송이 제기되는 경우 민사 소송법상의 관할 법원에 제기합니다.
[부 칙]
1. (시행일) 이 약관은 2016년 9월 5일부터 적용되며, 종전 약관은 본 약관으로 대체되며, 개정된 약관의 적용일 이전 가입자도 개정된 약관의 적용을 받습니다.