• Title/Summary/Keyword: 내황산염시멘트

Search Result 9, Processing Time 0.022 seconds

An Experimental Study on the Hydration and Mechanical Properties of High Strength Concrete with High Calcium Sulfate Cement (고황산염시멘트를 이용한 고강도콘크리트의 수화 및 역학적 특성에 관한 실험적 연구)

  • 박승범;임창덕
    • Magazine of the Korea Concrete Institute
    • /
    • v.5 no.1
    • /
    • pp.129-138
    • /
    • 1993
  • 프리텐션 방식 원심력 고강도 콘크리트 말뚝[KS F 4306]제조에 관한 실험적 연구로써 고황산염시멘트를 이용한 800kg/$ extrm{cm}^2$이상의 고강도콘크리트 제조시 수화 특성검토와 콘크르트 조직내의 기공율과 압축강도간의 상관식을 도출하여 고강도 발현기구를 규명하였으며 콘크리트 압축 및 휨강도간의 상관식 유도와 내구성 측면에서의 내동해성, 건조수축, 화학저항성등을 보통 포틀랜드 시멘트와 비교 고찰한 결과, 고황상염시멘트의 내구성이 우수함을 확인하였다.

Evaluation of Durability of Cement Matrix Replaced with Ground Calcium Carbonate (중질탄산(重質炭酸)칼슘을 혼합(混合)한 시멘트 경화체(硬化體)의 내구특성(耐久特性) 평가(評價))

  • Jung, Ho-Seop;Lee, Seung-Tae;Kim, Jong-Pil;Pak, Kwang-Pil;Kim, Seong-Soo
    • Resources Recycling
    • /
    • v.15 no.3 s.71
    • /
    • pp.74-80
    • /
    • 2006
  • In this article, we would like to investigate a durability characterization of cement mortar with inert filler, which is ground calcium carbonate(GCC). The kinds of techniques to evaluate cement mortar are chloride ion ingress, carbonation and sulfate attack. For the experimental result of the resistance of chloride ion ingress, carbonation and sulfate attack, as the addition of GCC makes decreasing the permeability by micro-filler effect, the specimens of $5{\sim}15%$ ratio of replacement are superior to the GCC0 mortar specimen with respect to durability of cement matrix in this scope.

A Study on the Basic Properties of Concrete and Characteristics of Blended Low Heat Cement (혼합형 저발열 시멘트의 특성과 콘크리트 기초 물성에 관한 연구)

  • 송용순;한정호;강석화;김상철
    • Magazine of the Korea Concrete Institute
    • /
    • v.10 no.5
    • /
    • pp.177-187
    • /
    • 1998
  • 최근 국내에서 해양 구조물, 장대 교량의 하부구조물, LNG저장탱크 등 매스콘크리트의 증가추세에 따라 구조물의 고내구성과 관련하여 시멘트의수화열에 의한 온도균열의 발생을 최소화 시킬 수 있는 3성분계 혼합형 저발열시멘트가 개발되어 실 구조물의 적용단계에 있으나, 저발열시멘트가 개발되어 실 구조물의 적용단계에 있으나 저발열시멘트의 특성에 대한 전반적인 연구보고가 국내에서는 미진한 실정이다. 따라서 본 연구에서는 3성분계 혼합형 저발열시멘트의 특성 및 코\ulcorner리트의기초물성을 1종 보통포틀랜트 시멘트, 5종 내황산염시멘트, 슬래그시멘트와 비교하였다. 글 결과 저발열 콘크리트의 찹축강도는 초기재령에서 강도발현률이 적은 반면 장기강도발현률은 상당히 큰 경향을 보였다. 또한 수화열은 1종시멘트를 사용한 콘크리트에 비하여 1/3~1/2정도로 매스콘크리트의 수화열을 대폭적으로 저감시킬 수 있을 뿐만 아니라 염소이온에 대한 저항성이 상대적으로 높게 나타나 거대 해양 구조물의 적용에 매우 유리한 시멘트로 판단되었다.

A Study on Corrosion Resistance of the Reinforement in Concrete Using Blast-Furnace Slag Powder (고로슬래그미분말을 사용한 콘크리트의 염화물이온에 의한 철근부식 저항성 연구)

  • Kim Eun-Kyun;Kim Jin-Keun;Lee Dong-Hyuk;Kim Young-Ung;Kim Yong-Chul
    • Journal of the Korea Concrete Institute
    • /
    • v.16 no.1 s.79
    • /
    • pp.1-9
    • /
    • 2004
  • This paper represents the permeability of chloride ions and the corrosion performance in the concrete blended with granulate blast furnace slag exposed to chloride environment. An ordinary cement (type I ) and sulfate resisting cement(type V) were used for the experiment. The two cements were combined with $0\%$, $25 \%$, $40\%$, and $55\%$ of the granulated blast furnace slag. The accelerated permeability tests of chloride ions were performed in accordance with ASTM C1202, and the accelerated corrosion tests of steel were carried out by using the method of immersion/drying cycles. After water curing 28 days, 56 days and 91 days, these tests were conducted until 30 cycles. In every cycle, test specimens were wetted in $3\%$ NaCl solution for three days and dried again in $60^{\circ}C$ air for four days. As an experimental results, the diffusion coefficient of chloride ions of the ordinary cement Concrete Combined granulated blast furnace slag was much lower than that of non granulated blast furnace slag concrete. Moreover, the diffusion coefficient of chloride ions of sulfate resisting cement concrete was higher than that of ordinary cement concrete. On the basis of the results of accelerated corrosion tests, corrosion resistance of the concrete mixed with granulated blast furnace slag shows good to corrosion resistance, however, the concrete with sulfate resisting cement shows bad to corrosion resistance.

Ettringite/Thaumasite Formation, Stability and Their Effect on Deterioration of Concrete (에트린자이트/사우마사이트의 형성 및 안정도와 콘크리트 성능저하에 미치는 영향)

  • 이효민;황진연
    • Journal of the Mineralogical Society of Korea
    • /
    • v.16 no.1
    • /
    • pp.75-90
    • /
    • 2003
  • Ettringite and thaumasite were observed in some concrete. The morphology and occurrence of these minerals were closely examined by performing SEM/EDAX analyses. We also experimentally induced the concrete deterioration using $Na_2SO_4$ solution with application of various environmental conditions. The stability of these minerals and deterioration characteristics under applied experimental conditions were determined. Abundant ettringite formed by“through solution reaction”occurred in many open spaces, and some microscopic ettringite formed by "tophochemical replacement" of calcium aluminate also occurred in cement paste. Severe cracking of cement paste causing premature deterioration was often associated with ettringite location. Under specific condition, ettringite was transformed to thaumasite, tricthloroaluminate, or decomposed. Thaumasite occurred with association of ettrinsite in concrete containing carbonate aggregate being subject to dedolomitization or in some concrete being subject to carbonation. Thaumasite appears to be formed under the similar condition to the general ettringite forming condition, but it formed solid solution with ettringite by substituting pre-existing ettringite. Ettringite can also be transformed to trichloroaluminate in the presence of abundant chlorides, but trichloroaluminate changed back to ettringite in late sulfate attack. It is considered that the substitution reaction direction solely depend on the concentration of chloride and sulfate ion.

Mechanical Properties of Granulated Ground Blast Furnace Slag on Blended Activator of Sulfate and Alkali (황산염 및 알칼리계의 혼합 활성화제에 대한 고로슬래그미분말의 역학적 특성)

  • Kim, Tae-Wan;Jun, Yu-Bin;Eom, Jang-Sub
    • Journal of the Korea institute for structural maintenance and inspection
    • /
    • v.19 no.5
    • /
    • pp.104-111
    • /
    • 2015
  • This study shows the mechanical properties of alkali-activated slag cement (AASC) synthesized using sulfate with NaOH solution. The used sulfates were calcium sulfate ($CaSO_4$, denoted CS) and sodium sulfate ($Na_2SO_4$, denoted SS). The replacement ratio of sulfates was 2.5, 5.0, 7.5 and 10.0% by weight of slag. NaOH solution of 2M and 4M concentration was used. A sample was activated with sulfate and activated with blended activator (blending NaOH solution with sulfate) respectively. 24 mix ratios were used and the water-binder weight ratio for the test was set 0.5. This research carried out the compressive strength, flexural strength, ultrasonic pulse velocity (UPV), absorption and X-ray diffraction (XRD). In the case of samples with CS, sample with 7.5% CS, sample with 2M NaOH+5.0% CS and sample with 4M NaOH+5.0% CS showed the good performance in the strength development. In the case of samples with SS, sample with 10.0% SS, sample with 2M NaOH+7.5% SS and sample with 4M NaOH+2.5% SS obtained good performance in strength. The results of UPV and water absorption showed a similar tendency to the strength properties. The XRD analysis of samples indicated that the hydration products formed in samples were ettringite, CSH and silicate phases. In this study, it is indicated that when compared to the use of sulfate only, the use of both sulfate and NaOH solution makes mechanical properties of AASC better.

A Experimental Study on the Seawater Attack Resistance of Grouting Mixtures (내해수성 주입재 배합에 관한 실험적 연구)

  • Chun, Byungsik;Choi, Dongchan;Kim, Younghun;Kim, Jinchun
    • Journal of the Korean GEO-environmental Society
    • /
    • v.11 no.1
    • /
    • pp.53-59
    • /
    • 2010
  • In seawater deposition condition, the corrosion and chemical attack of grouts are similar to those of concrete structure. Used in domestic MSG (Micro Silica Grouting) mixtured large amounts of silicate materials containing as cement powder is $8,000cm^2/g$ of the specific surface area or more due to the high hydration activity and high-strength, high durability, and features, $C_3A$ content of less than 5% to meet the standards chemical attack of seawater was evaluated as a cement material. Therefore, in this paper, with excellent seawater attack resistant MSG in combination with rapid hardening mineral was used, those of seawater characteristics were evaluated experimentally. Typically, sodium-silicate minerals or rapid hardening cements are used in domestic. About the homogel specimens with combination of MSG and rapid hardening agents for compressive strength, weight and length change characteristics were evaluated experimentally, and so we could present the excellent seawater resistant grouts combination.

Secondary Mineral Formation and Expansion Mechanisms Involved in Concrete Pavement Deterioration (콘크리트 포장 도로의 성능저하에 관련된 이차광물형성과 팽창메카니즘)

  • ;Rober D. Cody
    • The Journal of Engineering Geology
    • /
    • v.12 no.1
    • /
    • pp.95-109
    • /
    • 2002
  • A significant question is what role does newly-formed expansive mineral growth play in the premature deterioration of concrete. These minerals formed in cement paste as a result of chemical reactions involving cement paste and coarse/fine aggregate. Petrographic observations and SEM/EDAX analysis were conducted in order to determine chemical and mineralogical changes in the aggregate and cement paste of samples taken from lowa concrete highways that showed premature deterioration. Formation and expansive mechanisms involved in deterioration were Investigated. Brucite, Mg(OH)$_2$, is potentially expansive mineral that farms in cement paste of concretes containing reactive dolomite aggregate as a result of partial dedolomitization of the aggregate. No cracking was observed to be spatially associated with brucite, but most brucite was microscopic in size and widely disseminated in the cement paste of less durable concretes. Expansion stresses associated with its growth at innumerable microlocations may be retrieved by cracking at weaker locations in the concrete. Ettringite, 3CaO.Al$_2$O$_3$.3CaSO$_4$.32$H_2O$, completely fills many small voids and occurs as rims lining the margin of larger voids. Microscopic ettringite is common disseminated throughout the paste in many samples. Severe cracking of cement paste causing premature deterioration is often closely associated with ettringite locations, and strongly suggests that ettringite contributed to deterioration. Pyrite, FeS2, is commonly present in coarse/fine aggregates, and its oxidation products is observed in many concrete samples. Pyrite oxidation provides sulfate ions for ettringite formation.

Properties on the Freeze-Thaw of Concrete Subjected to Seawater Attack (해수의 영향을 받은 콘크리트의 동결융해 특성)

  • Park, Kwang-Pil;Kim, Seong-Soo;Lee, Seung-Tae;Kim, Jong-Pil;Jung, Ho-Seop
    • Journal of the Korea Concrete Institute
    • /
    • v.23 no.1
    • /
    • pp.23-30
    • /
    • 2011
  • In this study, deterioration degrees of concrete were investigated at laboratory under seawater attack and cycling freeze-thaw, which are major durability performance deterioration factors of concrete. Deteriorations of mixed concrete using Portland & blended cement were examined by instrumental analysis of changes in relative dynamic modulus of elasticity and compressive strength. After 520 cycles of freeze-thaw, relative dynamic modulus of elasticity and compressive strength of concrete mixed with normal Portland and LHC over 75% showed relatively low resistance of approximately 44% of those values of SRC. Concrete replaced with 50% fine powder of blast furnace slag showed the most excellent freeze-thaw resistance among the tested blended cement concrete.