고내산성 무기바인더의 내황산성에 관한 기초적 특성 연구 (A Fundamental Study on Sulfate Resistance of Inorganic Binder with High Acid Resistance)

  • 최중구;이건철;이건영;고동근;高山
    • 한국건축시공학회:학술대회논문집
    • /
    • 한국건축시공학회 2015년도 추계 학술논문 발표대회
    • /
    • pp.11-12
    • /
    • 2015
  • This study analyzed sulfate resistance of strongly acid-resistant inorganic binder based on industrial byproducts. According to the study experiment, compared to OPC mixture, the mixture of high acid-resistant inorganic binder had excellent chemical resistance against 10% H2SO4 solution. In the case of ordinary portland cement, its sample with 28 days of immersion had severe corrosion on its mortar erosion part, and thus external appearance was damaged greatly, and compression strength decreased by around 57% and more.

  • PDF

내황산성 자기치유 콘크리트 및 단면복구재 개발에 관한 연구 (A study on the development of self-healing concrete and repair materials with the resistance to sulfuric acid attack)

  • 방신영;김정미;안태호
    • 한국건축시공학회:학술대회논문집
    • /
    • 한국건축시공학회 2015년도 춘계 학술논문 발표대회
    • /
    • pp.84-85
    • /
    • 2015
  • The aim of this study is to develop crack self-healing concrete and repair materials with the sulfate resistance using geo-materials and by-products for practical industrial application. Research has been done on the healing of cracks in aged concrete, but it seems that very little is known about the actual healing mechanism and its conditions. In this research, the essential properties of geo-materials with pozzolanic reaction for self-healing were analyzed and discussed.

  • PDF

발전소 부산물 활용 결합재를 이용한 콘크리트의 내구성 평가 (The Durability Evaluation of Concrete using CFBC-ash Binder)

  • 임귀환;강용학
    • 한국건축시공학회:학술대회논문집
    • /
    • 한국건축시공학회 2018년도 춘계 학술논문 발표대회
    • /
    • pp.259-260
    • /
    • 2018
  • This study evaluated the compressive strength, freeze-thaw and sulfate resistance characteristics of concrete using CFBC-Ash. The CFBC-Ash was adjusted to a particle size of 75 ㎛ or less and using by increasing the fineness of powder through milling. As a result, it was confirmed that the concrete using CFBC-Ash shows a high compressive strength, durability. Also, it is confirmed that CFBC-ash can be used as a concrete binder.

  • PDF

알칼리자극제 및 고로슬래그미분말을 병용한 에폭시수지 혼입 폴리머 시멘트 모르타르의 성질 (Properties of Epoxy-Modified Mortars with Alkali Activators and Ground Granulated Blast Furnace Slag)

  • 김완기
    • 한국구조물진단유지관리공학회 논문집
    • /
    • 제25권1호
    • /
    • pp.85-92
    • /
    • 2021
  • 본 연구는 액상폴리머인 에폭시수지를 이용한 고내구성 폴리머 시멘트계 재료를 개발할 목적으로 고로슬래그미분말 치환율을 20%로 고정하고, 4종류의 알칼리 활성화제를 이용한 경화제 무첨가 에폭시수지 혼입 폴리머 시멘트 모르타르를 제작하여, 강도 특성, 에폭시수지 경화도, 흡수율, 내황산성, 중성화 및 염화물이온 침투저항성을 검토한 것이다. 그 결과, 알칼리 자극제의 종류에 관계없이, 고로슬래그 미분말 20%를 사용한 경화제 무첨가 EMM의 압축강도는 폴리머 결합재비 10%에서 최댓값을 나타냈으며, 폴리머 결합재비 20%에서는 에폭시수지의 경화도 감소와 함께 압축강도 또한 감소하는 것으로 나타냈다. 휨강도는 압축강도와 마찬가지로 수산화칼슘을 첨가한 것이 가장 우수하게 나타났으며, 폴리머 결합재비의 증가와 함께 증가하였으며, 모두 9.0 MPa 이상의 휨강도를 발현하였다. 알칼리 자극제의 종류에 관계없이, 경화제 무첨가 EMM의 방수성, 중성화 및 염화물이온 침투저항성은 폴리머 결합재비의 증가와 함께 현저히 개선되었으며, 4종류의 알칼리 자극제 가운데 수산화칼슘을 첨가한 모르타르가 가장 우수한 것으로 나타났다. 한편, 알칼리 자극제의 종류에 관계없이, 경화제 무첨가 EMM의 내황산성은 폴리머 결합재비의 증가와 함께 떨어졌는데, 이것은 폴리머 결합재비의 증가에 따른 에폭시수지의 미경화 에폭시수지의 증가에 기인한 것으로 판단된다. 4가지 알칼리 자극제의 종류에 대하여 물성 및 내구성을 비교 검토한 결과, 수산화칼슘을 첨가한 것이 가장 우수한 것으로 확인되었다.

경량 및 내황산 특성을 가진 고성능 단면복구 모르타르의 개발 (Development of high performance patching repair mortars with light weight and sulfuric acid resistance properties)

  • 김경민;박준희;안태호
    • 한국결정성장학회지
    • /
    • 제27권4호
    • /
    • pp.167-172
    • /
    • 2017
  • 본 연구는 경량 및 내황산 특성을 가진 단면복구 모르타르 개발의 관한 연구로 Type I의 경량 및 폴리머 모르타르와 Type II의 내황산 단면복구 모르타르의 성능평가를 진행하였다. 성능평가는 KS F 4042의 품질기준으로 이루어졌으며, 그 결과 경량 및 내황산성이 우수하며 KS F 4042의 품질 기준을 모두 만족하는 결과를 도출하였다.

알칼리 활성화 슬래그 시멘트 모르타르의 내황산성 (Resistance of Alkali Activated Slag Cement Mortar to Sulfuric Acid Attack)

  • 민경산;이승헌
    • 한국세라믹학회지
    • /
    • 제44권11호
    • /
    • pp.633-638
    • /
    • 2007
  • The setting time of alkali activated slag cement tends to be much faster than ordinary Portland cement, and its compressive strength had been higher from the 1 day but became lower than that of the cement on the 28 days. According to the results of the surface observation, weight loss, compressed strength, and erosion depth tests on the sulphuric acid solution. It has been drawn that alkali activated slag cement has a higher sulphate resistance than ordinary Portland cement, and in particular, the alkali activated slag cement added 5 wt% alumina cement has little deterioration on the sulphuric acid solution. The reason why the alkali activated slag cement has higher sulphate resistance than other hardened cement pastes is that it has no $Ca(OH)_2$ reactive to sulphate ion, and there is little $CaSO_4{\cdot}2H_2O$ production causing volume expansion, unlike other pastes. And it is supposed that $Al(OH)_3$ hydrates with high sulphate resistance, which is produced by adding the alumina cement increases the sulfate resistance.

유사 하수환경에서 글라이코 캘릭스 코팅 콘크리트의 효율성 평가 (Evaluation of Effectiveness of Concrete Coated with Bacterial Glycocalix under Simulated Sewage Environments)

  • 윤현섭;양근혁
    • 한국건설순환자원학회논문집
    • /
    • 제8권1호
    • /
    • pp.97-104
    • /
    • 2020
  • 이 연구에서는 글라이코 캘릭스 형성 박테리아를 이용한 콘크리트 구조체의 표면 코팅기술의 실제 적용의 중요성과 문제점을파악하기 위하여 유사 하수환경에서 Mock-up 실험을 수행하였다. 황산염 열화의 조건에서 원주형 콘크리트시험체의 압축강도와 질량의 변화를 평가하였다. 박테리아의 생장성 및 글라이코 캘릭스 생성량은 하수관에서 채취한 시료로부터 평가되었다. 이와 함께 유사 하수환경에서 Rhodobacter capsualtus의 적용이 주변 생태환경에 미치는 유해성을 평가하기 위해 차세대 염기서열 분석이 수행되었다. Mock-up 실험결과 개발된 코팅재가 적용된 콘크리트 시험체는 황산염 열화에 의한 콘크리트의 압축강도 저하 및 질량감소는 발생하지 않았으며, 하수 환경에서 우수한 열화저항성능을 갖는 것으로 평가되었다. 재령 91일에서 경화된 코팅재에서 분리된 박테리아의 생균수 및 글라이코 캘릭스 생성량은 각각 1.4×104cell/mL 및 67.5mg/㎤이었다. 더불어 글라이코 캘릭스 코팅 콘크리트 하수관이 설치된 하수에서는 유해균주가 발견되지 않았다. 이는 코팅 재료로서 활용된 Rhodobacter capsulatus가 하수 환경에서 주변 생태환경에 미치는 영향이 없음을 의미한다.

함침계 표면보호제에 의한 콘크리트 표면의 세공구조 변화 및 내구성 향상 (Improvement of Durability and Change of Pore Structure for Concrete Surface by the Penetrative Surface Protection Agent)

  • 강석표;김정환
    • 콘크리트학회논문집
    • /
    • 제18권1호
    • /
    • pp.125-132
    • /
    • 2006
  • 최근 들어 툭별한 물리적 방법을 사용하지 않고 내구성능이 저하된 콘크리트의 성능을 회복시키는 방법의 일환으로서 콘크리트 표면보호재에 대한 관심이 높아지고 있다. 표면보호는 직접적인 의미로서는 콘크리트 구조물의 표면을 보호하는 것뿐만아니라 다양한 열화요인의 침투를 억제함으로서 내부의 콘크리트 및 철근의 열화를 억제하여 콘크리트 구조물을 보호하게 된다. 이와 같은 표면보호재 중 함침계 표면보호재는 콘크리트 표면층의 공극에 충전 혹은 생성물을 석출시켜 치밀한 층으로 하느 충전계와 콘크리트 표면층의 외부 및 내부표면의 성질을 개선하는 표면계로 분류하는 것이 가능하다. 따라서 본 연구는 규플르오르화염을 주성분으로 하는 표면형 함침계 표면보호제 도포에 의한 콘크리트 표면의 세공구조의 변화 및 중성화, 염해, 화학적 침식 등의 내구성 향상을 실험실증적으로 검토함으로서 콘크리트 구조물의 내구성향상 방안을 제시하고자 한다. 그 결과, 표면보호제를 도포함으로서 모든 물시멘트비에서 도포전과 비교하여 전세공용적이 감소하고 있으며, 특히 50nm이상의 비교적 큰 세공경인 모세관공극의 용적이 감소함으로서 물흡수성, 중성화 저항성, 내황산성, 염소이온침투 저항성 등의 내구성 향상에 기여하는 것으로 나타났으며, 그 효과는 물시멘트비가 클수록 높게 나타났다.

콘크리트용 골재로서의 Bottom Ash 활용성 평가 (Evaluation of Bottom Ash on the Application for the Aggregate of Concrete)

  • 김상철
    • 한국건설순환자원학회논문집
    • /
    • 제5권2호
    • /
    • pp.105-115
    • /
    • 2010
  • 산업의 발전과 함께 산업폐기물의 증가와 그에 따른 처리할 회사장 부족, 유해한 성분 함유로 인한 환경상의 문제 등에 대한 해결 방안의 일환으로, 본 연구에서는 석탄 화력발전소에서 발생되는 석탄회 중에서 bottom ash를 대상으로 콘크리트용 골재로서의 유용성 여부를 평가하고자 하였다. 먼저 잔골재와 굵은 골재의 대체재로서의 적절성 평가를 위해 경도시험, 입도분포시험, 흡수량시험, S.E.M 분석시험 등의 물리적 시험을 수행하였고, 화학적 시험으로는 강열감량시험, X-ray를 통한 분석시험을 수행하였다. 콘크리트에 적용하였을 때 미치는 영향은 대체재로서의 비율을 달리하여 작업성 확보차원에서 슬럼프의 변화를 측정하였고, 굳은 콘크리트에서는 강도확보, 내투수성, 동결융해 저항성, 내황산성, 탄산화 저항성에 대해 평가하였다. 실험결과, 미립분의 부족과 일부 bottom ash에서 결속력 상의 문제가 존재하였으나 천연골재와 혼합하여 사용하고 배출시 공정 개선을 한다면 골재로써 충분히 사용성이 있는 것으로 평가되었다. 또한, 다공성을 갖고 있어 작업성 확보를 위해서는 단위수량이나 감수제의 증가가 요구되지만 일반강도 한도 내에서는 일정 비율로 천연골재와 혼합하여 사용하면 강도 확보에 문제가 없고 오히려 내구성 확보에 있어서는 유리한 것으로 나타났다.