A Study on Heating Element Properties of Carbon Nanotube/Silicon Carbonitride Composite Sheet using Branched Structured Polysilazane as Precursor (가지 달린 구조의 폴리실라잔을 전구체로 이용해 제조한 카본 나노튜브/실리콘 카보나이트라이드 복합체 시트의 발열특성에 관한 연구)

  • Huh, Tae-Hwan;Song, Hyeon Jun;Jeong, Yeong Jin;Kwark, Young-Je
    • Composites Research
    • /
    • v.33 no.6
    • /
    • pp.395-400
    • /
    • 2020
  • In this paper, we manufactured silsesquiaznae (SSQZ)-coated carbon nanotube (CNT) surface heating elements, which allowed stable heating at high temperatures. The prepared composite sheet was confirmed by FE-SEM that the SSQZ fully coated the surface of CNT sheet. Furthermore, it was also confirmed that the silicon carbonitride (SiCN) ceramic formed by heat treatment of 800℃ have no defects found and maintain intact structure. The CNT/SiCN composite sheet was able to achieve higher thermal stability than raw CNT sheets in both nitrogen and air atmosphere. Finally, the CNT/SiCN composite sheet was possible to heat up at a temperature of over 700℃ in the atmosphere, and the re-heating was successfully operated after cooling.

Evaluation of Thermal Durability for Thermal Barrier Coatings with Gradient Coating Thickness (경사화 두께를 갖는 열차폐 코팅의 열적 내구성 평가)

  • Lee, Seoung Soo;Kim, Jun Seong;Jung, Yeon-Gil
    • Journal of the Korea Academia-Industrial cooperation Society
    • /
    • v.21 no.8
    • /
    • pp.248-255
    • /
    • 2020
  • The effects of the coating thickness on the thermal durability and thermal stability of thermal barrier coatings (TBCs) with a gradient coating thickness were investigated using a flame thermal fatigue (FTF) test and thermal shock (TS) test. The bond and topcoats were deposited on the Ni-based super-alloy (GTD-111) using an air plasma spray (APS) method with Ni-Cr based MCrAlY feedstock powder and yttria-stabilized zirconia (YSZ), respectively. After the FTF test at 1100 ℃ for 1429 cycles, the bond coat was oxidized partially and the thermally grown oxide (TGO) layer was observed at the interface between the topcoat and bond coat. On the other hand, the interface microstructure of each part in the TBC specimen showed a good condition without cracking or delamination. As a result of the TS test at 1100 ℃, the TBC with gradient coating thickness was initially delaminated at a thin part of the coating layer after 37 cycles, and the TBC was delaminated by more than 50% after 98 cycles. The TBCs of the thin part showed more oxidation of the bond coat with the delamination of topcoat than the thick part. The thick part of the TBC thickness showed good thermal stability and oxidation resistance of the bond coat due to the increased thermal barrier effect.

A Study on Improvement of Material Characteristics by Control of Ion Implantation (이온주입 제어에 의한 재료특성 개선에 관한 연구)

  • Yang, Young-Joon;Lee, Chi-Woo;Fujita, Kazuhisa
    • Journal of Advanced Marine Engineering and Technology
    • /
    • v.32 no.8
    • /
    • pp.1178-1184
    • /
    • 2008
  • In this study, techniques of ion implantation were used in order to improve the characteristics of metal materials such as the oxidation and wear resistant. In particular it is necessary to develope their oxidation and wear resistant that could be used in severe environmental conditions. There are mainly two elementary technologies including ion implantation and/or thin film coating. Ion implantation method was performed for surface modification. As a result, it was found that some ion implantations methods such as Nb, high-temperature Nb ion implantation and Nb+C combined implantation are somewhat effective for improving the oxidation resistance of TiAl alloy. Furthermore, the fluorine PBII treatment is more effective for improving the oxidation resistance of the TiAl alloy with three-dimensional shapes. The implantation of boron ion into thin film of TiN was also effective for improving the properties of materials like high temperature wear resistance. TiCrN film was applied to the actual seal ring for steam turbines, and it was observed that its sliding property showed a successfully good performance.

The effect of Cr coated on the Ni and Inconel 601 substrate by PECVD on the oxidation behavior at high temperature (PECVD법으로 증착한 Cr코팅층이 Inconel 601과 Ni의 내산화성에 미치는 영향)

  • 강옥경;정명모;김길무
    • Journal of the Korean institute of surface engineering
    • /
    • v.28 no.3
    • /
    • pp.142-151
    • /
    • 1995
  • In this research, a thin layer of Cr was coated on the pure Ni and Inconel 601 by PECVD (Plasma Enhanced Chemical Vapor Deposition) in order to study the effect of Cr on the oxidation behavior at high temperature. Cr coated Inconel 601, which was oxidized at $1100^{\circ}C$ for 24 hours, formed a protective $Cr_2O_3$ oxide layer and the resistance to isothermai oxidation was improved. On the other hand, oxidation resistance of Cr coated Inconel 601 at 100$0^{\circ}C$ was not significantly improved, probably due to the formation or insufficient $Cr_2O_3$ layer. But, when oxidized at $1000^{\circ}C$ and $1100^{\circ}C$ for 100 hours, Cr coated Inconel 601 improved isothermal oxidation resistance by the formation of continuous $Cr_2O_3$ external scale and by the development of $Al_2O_3$ subscales. Cr coated Ni formed inner layer of $Cr_2O_3$ within almost pure NiO, which provided additional cation vacancies, thus increasing the mobility of Ni ions in this region. It is believed that this doping effect resulted in an increase in the observed oxidation rate compared with pure Ni and did not improve the oxidation resistance.

  • PDF

A strudyon the improvement of the oxidation resistance for high temperature materials by coating process (코팅에 의한 고온재료의 내산화성 향상을 위한 연구)

  • 강석철;민경안;안연상;김길무
    • Journal of the Korean institute of surface engineering
    • /
    • v.30 no.2
    • /
    • pp.93-103
    • /
    • 1997
  • High temperature materials used in the elevated temperature and corrosive atmosphere must have the good oxidation resistance and preserve their own mechanical properties simultaneously. For the oxidation resistance, it is very important to form a protective oxide scale such as $Al_2O_3$ or $Cr_2O_3$ on the substrate. However, the additions of protective oxide forming elements such as Cr and Al in the alloy to enhance its oxidation resistance are limited due to the deleterious effects on their mechanical properties. PECVD(P1asma Enhanced Chemical Vapor Deposition) coating processes were employed to improve the oxidation resistance at high temperature. Cr and/or A1 were coated on the substrates of Ni and Inconel 600 at various temperatures of 400, 500, $600^{\circ}C$ and at different conditions of specimen surfaces. Then, coated specimens were exposed to isothermal and cyclic oxidation conditions in air at 1000 and $1100^{\circ}C$. In order to enhance the adhesion between the substrate and coated layer, heat treatments of the coated specimens were conducted in a vacuum. At isothermal oxidation experiments, Al-coated Ni specimen showed better oxidation resistance than pure Ni. At cyclic oxidation experiments at $1000^{\circ}C$. Cr and Al-coated specimen showed better oxidation resistance. Cr-coated Inconel 600 had also showed better oxidation resistance due to Cr in the substrate. By PECVD coating process, oxidation resistance could be improved, but it was not improved as expected due to the weakness of the adhesion between the substrate and the coated layer.

  • PDF

A Study on the Formation of Aluminide Coating on KM 1557 Alloy by Pack Cementation Process (Pack Cementation법에 의한 KM 1557 합금의 알루미나이드 코팅층 형성에 관한 연구)

  • Yoon, Jin-Kook;Yoo, Myoung Ki;Choi, Ju;Kim, Jae-Soo
    • Analytical Science and Technology
    • /
    • v.6 no.2
    • /
    • pp.167-180
    • /
    • 1993
  • The effects of coating variables on the formation of aluminide coating layer with good oxidation resistance on the strongest hot-forged superalloy in the world, KM 1557 developed at KIST by pack cementation process were studied. Pack aluminizing were performed by high-activity process with pure aluminium powders and by low-activity process with codep powders. For high-activity process, Al deposition rate, growth rate of coating layer, and cross-sectional microstructures were influenced by the species and additive amounts of activators and the additive amounts of pure aluminium powders. For low-activity process, Al deposition rate, growth rate of coating layer, and the cross-sectional microstructures were not influenced by the species but additive amounts of activators. Surface structures of coating layer were influenced by the species of activators. Regardless of aluminium activity, Al deposition rate was proportional to the square root of time and parabolic rate constants were different with the species of activators. The activation energy for deposition of aluminium was different with the species of activators for high-activity process. Regardless of the species of activators, the activation energy for deposition of aluminium was 12~14 Kcal/mole for low-activity process.

  • PDF

Spark plasma sintering 소결법에 의해 제작 된 Ti-Al-Si 합금타겟의 물성과 합금타겟을 이용하여 제작한 박막에 관한 연구

  • Lee, Han-Chan;Jeong, Deok-Hyeong;Mun, Gyeong-Il;Lee, Bung-Ju;Sin, Baek-Gyun
    • Proceedings of the Korean Vacuum Society Conference
    • /
    • 2013.08a
    • /
    • pp.237.1-237.1
    • /
    • 2013
  • Ti 와 Al 은 금속간의 화합물이 내산화성에 우수한 성질을 가지고 있으며 낮은 밀도와 고온에도 큰 변화가 없는 성질을 가지고 있다. 그리하여 내식 및 부식 관련 연구나 고온재료를 필요로 하는 우주, 엔진 제품 등에 많은 연구가 진행되고 있다. 또한 Ti-Al-N 박막은 경도가 우수하여 고속 공구 부품에 널리 사용되고 있으며 최근 Ti-Al-N 에 Si 첨가로 인하여 40 GPa 이상의 고경도와 1,000도 이상의 산화온도를 지닌 나노 혼합물 코팅을 형성 시키는 것으로 알려져 있다. 본 연구에서는 Ti, Al, Si 원분말을 PBM (Planetary Ball Milling) 방법을 사용하여 Ti-Al-Si 혼합분말로 제조하고, 제조된 분말들은 SPS (Spark Plasma Sintering) 공정을 통하여 Ti-Al-Si 합금타겟을 제작하였다. 제작된 Ti-Al-Si 합급타겟을 사용한 Sputtering 공정을 수행하여 Ti-Al-Si 3원계 박막을 증착하였다. 그 결과 기존 Ti (82 ${\mu}m$), Al (32 ${\mu}m$), Si (16 ${\mu}m$) 크기의 원분말들이 PBM (Planetary Ball Milling) 공정 후 Ti-Al-Si (18 ${\mu}m$) 로 입도가 작아진 것을 확인 할 수 있었고, 소결 후 타겟이 99% 이상의 높은 밀도를 가졌으며 원분말의 조성과 동일한 조성을 가진 타겟이 제작되었음을 확인하였다. Ti-Al-Si 타겟의 경도는 약 1,000 Hv 이상의 값을 보였으며, Ti-Al-Si-N 박막의 경우 타겟의 조성과 동일하였고 경도는 약 35 GPa 로 높은 경도 값을 가지는 것을 확인하였다. 내산화 테스트 결과 Ti-Al-Si-N 박막은 1,000도 에서도 박막의 손상이 가지 않았다.

  • PDF

A Study on the Oxidation Behavior of Metal Materials Applicable to Oxidizer Rich Pre-Combustor (산화제 과잉 연소기에 활용 가능한 금속재료의 산화 거동에 관한 연구)

  • Shin, Donghae;Yu, Isang;Shin, Minku;Ko, Youngsung;So, Younseok;Han, Yeoungmin
    • Journal of the Korean Society of Propulsion Engineers
    • /
    • v.23 no.2
    • /
    • pp.118-125
    • /
    • 2019
  • Metals exposed to high temperature/high pressure/oxidant excess environment of an oxygen excess pre-combustor may undergo rapid oxidation. In this study, the test facility to simulate the high temperature/high pressure/oxidant excess environment was constructed and the oxidation resistance evaluation was carried out for various metal materials. As a result, the discoloration of the metallic materials, the change in the surface roughness and the peeling of the metal surface were observed, and the weight change was also observed. The resulst showed that oxidation-resistant coating of a metal material of the combustor is indispensably required, and the use of XM-19, which has the highest content of Cr and Ni, is expected to provide more structural stability.

모재/중간층/박막의 H/E ratio 구배에 따른 Cr계 경질 박막의 기계적 특성에 관한 연구

  • Kim, Hoe-Geun;Song, Myeon-Gyu;Lee, Sang-Yul
    • Proceedings of the Korean Institute of Surface Engineering Conference
    • /
    • 2018.06a
    • /
    • pp.135-135
    • /
    • 2018
  • 천이금속 질화물 코팅은 우수한 기계적 특성들로 인해 공구 코팅으로 많이 사용 되어왔다. 그 중에서도 특히 Cr계 경질 코팅은 높은 경도와 낮은 표면조도, 우수한 마찰특성 등 뛰어난 기계적 특성을 나타내므로 공구 코팅으로의 적용 가능성이 크다. 그러나 최근 공구산업의 발전으로 인해 공구가 더욱 가혹한 환경에서 사용됨에 따라, 공구의 수명을 향상시키고 보호하기 위해 코팅의 높은 밀착력이 요구되고 있으며, 모재와 코팅 사이에 중간층을 합성함으로써 공구의 밀착력을 향상시키는 연구가 활발히 진행되고 있다. 이전 연구에서 모재/중간층/코팅간의 경도와 탄성계수 비율(H/E ratio)의 구배가 코팅의 밀착력에 큰 영향을 미치는 것으로 확인되었다. 그러므로, WC 모재와 Cr계 코팅의 중간값의 H/E ratio를 갖는 중간층의 합성을 통해 코팅의 밀착력을 향상시킬 수 있을 것으로 판단된다. 본 연구에서는, 코팅의 밀착력을 향상시키기 위해 다양한 중간층을 증착한 CrZrN, CrAlN 코팅을 비대칭 마그네트론 스퍼터링 장비를 이용하여 합성하였다. 모재로는 디스크 형상의 WC-6wt.%Co 시편을 사용하였고 Cr, Zr, Si, Al single 타겟을 이용하여 Cr, CrN, CrZrN, CrZrSiN 등의 중간층이 증착된 코팅을 합성했다. 코팅의 합금상, 경도 및 탄성계수, 미세조직 및 조성, 표면 조도을 확인하기 위해 X-ray diffractometer (XRD), Fischer scope, field-emission scanning electron microscopy (FE-SEM), energy dispersive X-ray spectroscopy (EDS), atomic force microscopy를 사용하였고, 코팅의 밀착 특성을 분석하기 위해 scratch tester와 optical microscopy (OM)를 이용하였다. 코팅의 내열성을 확인하기 위해 코팅을 furnace에 넣어 공기중에서 500, 600, 700, 800, 900, $1,000^{\circ}C$로 30분 동안 annealing 한 후에 nano-indentation을 사용하여 경도를 측정하였다. CrZrN 및 CrAlN 코팅을 나노 인덴테이션으로 분석한 결과, 모든 코팅의 경도(33.4-35.8 GPa)와 탄성계수(384.1-391.4 GPa)는 중간층의 종류에 상관없이 비슷한 값을 보인 것으로 확인됐다. 그러나, 코팅의 마찰계수는 중간층의 종류에 따라 다른 값을 보였다. CrZrN 코팅의 경우 CrN 합금상 중간층을 갖을 때 가장 낮은 값을 보였으며, CrAlN 코팅의 경우 CrN/CrZrSiN 중간층을 증착하였을때 마찰계수는 0.34로 CrZrN 중간층을 증착하였을 때(0.41)에 비해 낮은 값을 보였다. 또한, 코팅의 마모율 및 마모폭도 비슷한 경향을 보인 것으로 보아, CrN/CrZrSiN 중간층을 합성한 CrAlN 코팅의 내마모성이 상대적으로 우수한 것으로 판단된다. 코팅의 밀착력의 경우도 마찰계수와 비슷한 경향을 보였다. 이것은 중간층의 H/E ratio가 코팅의 내마모성에 미치는 영향에 의한 결과로 사료된다. H/E ratio는 파단시의 최대 탄성 변형율로써, 모재/중간층/코팅의 H/E ratio 구배에 따라 코팅 내의 응력의 완화 정도가 변하게 된다. WC 모재 (H/E=0.040)와 CrAlN 코팅(H/E=0.089) 사이에서 CrN, CrZrSiN 중간층의 H/E ratio는 각각 0.076, 0.083으로 모재/중간층/코팅의 H/E ratio 구배가 점차 증가함을 확인 할 수 있었고, 일정 응력이 지속적으로 가해지면서 진행되는 마모시험중에 CrN과 CrZrSiN 중간층이 WC와 CrAlN 코팅 사이에서 코팅 내부의 응력구배를 완화시키는 역할을 함으로써 CrAlN 코팅의 내마모성이 향상된 것으로 판단된다. 모든 코팅을 열처리 후 경도 분석 결과, CrN/CrZrSiN 중간층을 증착한 CrAlN 코팅은 $1,000^{\circ}C$까지 약 28GPa의 높은 경도를 유지한 것으로 확인 되었고, 이는 CrZrSiN 중간층 내에 존재하는 SiNx 비정질상의 우수한 내산화성에 의한 결과로 판단된다.

  • PDF

Antioxidation Behavior of Submicron-sized Cu Particles with Ag Coating (서브 마이크론급 구리 입자의 은도금 공정에 따른 내산화성 강화 연구)

  • Choi, Eun Byeol;Lee, Jong-Hyun
    • Journal of the Microelectronics and Packaging Society
    • /
    • v.23 no.3
    • /
    • pp.51-56
    • /
    • 2016
  • To fabricate a copper (Cu)-based fine conductive filler having antioxidation property, submicron silver (Ag)-coated Cu particles were fabricated and their antioxidation property was evaluated. After synthesizing the Cu particles of $0.705{\mu}m$ in average diameter by a wet-reduction process, Ag-coated Cu particles were fabricated by successive Ag plating using ethylene grycol solvent. Main process parameters in the Ag plating were the concentration of reductant (ascorbic acid), the injection rate of Ag precursor solution, and the stirring rate in mixed solution. Thus, Ag plating characteristics and the formation of separate fine pure Ag phase were observed with different combinations of process parameters. As a result, formation of the separate pure Ag phase and aggregation between Ag-coated Cu particles could be suppressed by optimization of the process parameters. The Ag-coated Cu particles which were fabricated using optimal conditions showed slight aggregation, but excellent antioxidation property. For example, the particles indicated the weight gain not exceeding 0.1% until $225^{\circ}C$ when they were heated in air at the rate of $10^{\circ}C/min$ and no weight gain until 75 min when they were heated in air at $150^{\circ}C$.