Recycling of Chilled Converter Slag as Aggregate in Cement Mortar (급랭 진로슬래그 모르타르 골재 재활용 특성)

  • Kim, Tae Heui;Park, Kyung Bong
    • Clean Technology
    • /
    • v.12 no.4
    • /
    • pp.238-243
    • /
    • 2006
  • The aggregate properties of chilled converter slag reformed by atomizing liquid converter slag were investigated. The properties of mortars with various replacement of standard sand by chilled converter slag as recycled fine aggregates were investigated. The particle shape of chilled converter slag by atomizing was a sphere with an open cavity which is enclosed with two layers like a bored coconut. Specific gravity, unit weight and fineness modulus increased with increasing the replacement, and solid content had the maximum at the replacement of 75% and water absorption rate had the minimum at the replacement. The hardened mortars with higher replacements have the higher specific gravity and the denser texture.

  • PDF

Fatigue Strength Improvement of Carbon Steel by Rapid Cooling from $700^{\circ}C$ (가열급냉에 의한 저탄소강의 피로 강도 향상)

  • 정호신
    • Journal of Welding and Joining
    • /
    • v.12 no.2
    • /
    • pp.119-127
    • /
    • 1994
  • 용접 이음부는 토우부의 응력집중에 의해 피로강도가 저하된다는 것은 잘 알려져 있는 사실이다. 이 때문에 용접 이음부의 피로강도 개선을 위하여 여러 방법이 제안되어 있으나 본 연구에서는 강을 가열후 급랭하여 극저탄소강의 피로강도 개선에 미치는 시효의 영향을 조사하였다. 탄소 함유량 0.019-0.080% 범위의 8종의 탄소강을 용해 제조하여 압연한 후 피로시험편을 가공하였다. 이 시험편을 $A_1$점 이하 $700^{\circ}C$로 가열하여 급랭 시효에 의한 저탄소강의 피로강도에 미치는 탄소함유량의 영향을 조사하였다. $700^{\circ}C$로부터의 급랭 및 시효에 의하여 인장강도 및 피로강도는 노랭, 공랭재의 경우에 비하여 훨씬 높아짐을 알 수 있었다. 또한 급랭후의 시효에 의한 피로강도 향상 효과가 가장 크게 나타나는 것을 페라이트의 탄소고용한도 0.02%에 가까운 합금 조성을 갖는 경우이었다.

  • PDF

Utilization of Blast Furnace Slag Quenched with Water as a Source of Silicate Fertilizer -I. Physico-chemical and Mineralogical Characteristics (급랭광재(急冷鑛滓)의 비료화(肥料化)에 관(關)한 연구(硏究) -I. 급랭광재(急冷鑛滓)의 특성(特性))

  • Shin, Jae-Sung;Lim, Dong-Kyu;Kim, Maun-Soo
    • Korean Journal of Soil Science and Fertilizer
    • /
    • v.16 no.4
    • /
    • pp.343-346
    • /
    • 1983
  • This paper was prepared to characterize a physico-chemical and mineralogical examination on blast furnace slag as a source of silicate fertilizer, which was quenched with high pressure water stream in process of iron refinery at Pohang Iron and Steel Manufacturing Inc. Quenched slag was more coarse in particle size compared to present commercial silicate fertilizer milled from air-cooled slag and mostly generated in size of 1 to 2 mm. The total chemical composition of quenched and air-cooled slags was same but mineralogical composition was quite different. The former was composed of amorphous materials resulting in more soluble silica content, however, the latter contained dominantly crystalline minerals such as akermanite, gehlenite and wollastonite which meant less soluble ones. Latent cementing property and angular surface of gain of the slag made it difficult to apply the slag directly, however, it could be used as a source of silicate fertilizer and soil ammendment.

  • PDF

Utilization of Blast Furnace Slag Quenched with Water as a Source of Silicate Fertilizer -II. Effect of Particle Size Distribution of Quenched Slag on Rice Yields (급랭광재(急冷鑛滓)의 비료화(肥料化)에 관(關)한 연구(硏究) -II. 수도(水稻)에 대한 급랭광재(急冷鑛滓)의 입도별(粒度別) 비효(肥效))

  • Lim, Dong-Kyu;Shin, Jae-Sung;Kim, Heung-Bae
    • Korean Journal of Soil Science and Fertilizer
    • /
    • v.18 no.1
    • /
    • pp.67-71
    • /
    • 1985
  • The objective of this study was to attest the feasibility of the utilization of the blast furnace slag, quenched with water as a source of silicate fertilizer. A pot experiment was conducted to evaluate the effect of quenched slag and its particle size distribution on rice plant growth over the corresponding air-cooled slag of milled commercial silicate fertilizer. The yields of rice were slightly higher in quenched slag than in the commericial air-cooled slag, however, no significant statistical difference was observed. The silica content of rice plants through the growing period was high in quenched slag in any tested particle sizes. This indicated that the quenched slag might release silica fastly in soil. On the other hand, the available silica content retained in soil was high in air cooled slag, which implied that the silica of air-cooled slag was low acting. The results suggested that the quenched slag may be potentially utilized as a source of silicate fertilizer.

  • PDF

A Study on Fundamental Properties of Rapid Cooling Slag to Utilize as Fine Aggregate for Concrete (콘크리트용 잔골재로 활용하기 위한 습식 급랭 전로슬래그의 기초 물성에 관한 연구)

  • Choi, Yun-Wang;Choi, Byung-Keol;Oh, Se-Wang;Cho, Bong-Suk
    • Journal of the Korean Recycled Construction Resources Institute
    • /
    • v.3 no.2
    • /
    • pp.171-179
    • /
    • 2015
  • Recently, development of substitution aggregate is urgently needed because aggregate shortage is continuing due to the exhaustion of natural aggregate and strict restrictions of environment in construction industry. Therefore, In this study, new processing method to solve the problems of processing method of existing converter slag, namely, rapid cooling slag produced by the rapid cooling and crushing process of the high temperature melten slag into the rotary drum and then using the cooling water, compressed air and steel ball was examined fundamental properties for utilize as fine aggregate for concrete. In addition, through this study, we propose the utilization method of rapid cooling slag as fine aggregate for concrete.

The hardening effect by ice-quenching after oxidation of a Pd-Ag-Sn-Au metal-ceramic alloy during porcelain firing simulation (금속-세라믹용 Pd-Ag-Sn-Au계 합금의 모의소성 시 산화처리 후 급랭에 의한 경화 효과)

  • Shin, Hye-Jeong;Kim, Min-Jung;Kwon, Yong-Hoon;Kim, Hyung-Il;Seol, Hyo-Joung
    • Korean Journal of Dental Materials
    • /
    • v.44 no.3
    • /
    • pp.197-206
    • /
    • 2017
  • The hardening effect by ice-quenching after oxidation of a Pd-Ag-Sn-Au metal-ceramic alloy during porcelain firing simulation was investigated by means of hardness test, field emission scanning electron microscopic observations, and X-ray diffraction analysis. The hardness decreased by ice-quenching after oxidation, which was induced by the homogenization of the ice-quenched specimen. The decreased hardness by ice-quenching after oxidation was recovered from the wash stage which was the first stage of the remaining firing process for bonding porcelain. After wash stage, the hardness of the ice-quenched specimens decreased during the subsequent porcelain firing process. But the final hardness of the ice-quenched specimens after oxidation was higher than that of the specimens cooled at stage 0 after oxidation. The increase in hardness of the specimens during the first firing process was caused by the lattice strains generated at the interface between the face-centered cubic Pd-Ag-rich matrix and the face-centered tetragonal Pd3(Sn, Ga, In) precipitate. The decrease in hardness of the specimens during the remaining firing process was caused by the microstructural coarsening.

Competitive Adsorption Characteristics of Rapid Cooling Slag in Single- and Multi-Metal Solutions (단일 및 복합중금속용액에서 제강급랭슬래그의 경쟁흡착특성)

  • Park, Jong-Hwan;Kim, Hong-Chul;Kim, Seong-Heon;Lee, Seong-Tae;Kang, Byung-Hwa;Kang, Se-Won;Seo, Dong-Cheol
    • Korean Journal of Environmental Agriculture
    • /
    • v.35 no.1
    • /
    • pp.24-31
    • /
    • 2016
  • BACKGROUND: Heavy metal adsorption not only depends on rapid cooling slag(RCS) characteristics but also on the nature of the metals involved and on their competitive behavior for RCS adsorption sites. The goal of this study was to investigate the competitive absorption characteristics of Cu, Cd and Zn in single- and multi-metal forms by RCS.METHODS AND RESULTS: Both single- and multi-metal adsorption experiments were conducted to determine the adsorption characteristics of RCS for the heavy metals. Adsorption behaviors of the heavy metals by RCS were evaluated using both the Freundlich and Langmuir adsorption isotherm equations. The maximum adsorption capacities of metals by RCS were in the order of Cu(16.6 mg/g) > Cd(8.1 mg/g) > Zn(6.2 mg/g) in the single-metal adsorption isotherm and Cu(14.5 mg/g) >> Zn(1.3 mg/g) > Cd(0.6 mg/g) in the multi-metal adsorption isotherm. Based on data obtained from Freundlich and Langmuir adsorption models and three-dimensional simulation, multi-metal adsorption behaviors differed from single- metal adsorption due to competition. Cadmium and Zn were easily exchanged and substituted by Cu during multi-metal adsorption.CONCLUSION: Results from adsorption experiments indicate that competitive adsorption among metals increases the mobility of these metals.

Phosphorus Adsorption Characteristic of Ferronickel and Rapid Cooling Slags (페로니켈슬래그와 제강급랭슬래그의 인 흡착특성)

  • Park, Jong-Hwan;Seo, Dong-Cheol;Kim, Seong-Heon;Park, Min-Gyu;Kang, Byung-Hwa;Lee, Sang-Won;Lee, Seong-Tae;Choi, Ik-Won;Cho, Ju-Sik;Heo, Jong-Soo
    • Korean Journal of Environmental Agriculture
    • /
    • v.33 no.3
    • /
    • pp.169-177
    • /
    • 2014
  • BACKGROUND: The ferronickel and rapid cooling slags used in present study are industrial wastes derived from a steel factory in Korea. These slags are used as almost road construction materials after magnetic separation. However, the use of slag to remove phosphorus from wastewater is still a relatively less explored. The objective of this work was to evaluate the feasibility of ferronickel slag (FNS) and rapid cooling slag (RCS) as sorbents for phosphorus removal in wastewater. METHODS AND RESULTS: Adsorption experiments were conducted to determine the adsorption characteristics of the FNS and RCS for the phosphorus. Adsorption behaviour of the phosphorus by the FNS and RCS was evaluated using both the Freundlich and Langmuir adsorption isotherm equations. FNS and RCS were divided into two sizes as effective sizes. Effective sizes of FNS and RCS were 0.5 and 2.5 mm, respectively. The adsorption capacities (K) of the phosphorus by the FNS and RCS were in the order of RCS 0.5 (0.5105) > RCS 2.5 (0.3572) ${\gg}$ FNS 2.5 (0.0545) ${\fallingdotseq}$ FNS 0.5 (0.0400) based on Freundlich adsorption isotherm. The maximum adsorption capacities (a; mg/kg) of the phosphorus determined by the Langmuir isotherms were in the order of RCS 0.5 (3,582 mg/kg) > RCS 2.5 (2,983 mg/kg) > FNS 0.5 (320 mg/kg) ${\fallingdotseq}$ FNS 2.5 (187 mg/kg). RCS 0.5 represented the best sorbent for the adsorption of phosphorus. In the experiment, the Langmuir model showed better fit with our data than the Freundlich model. CONCLUSION: This study indicate that the use of RCS in constructed wetlands or filter beds is a promising solution for phosphorus removal via adsorption and precipitation mechanisms.