The Engineering Properties of Concrete Exposed at High Temperature (고온을 받은 콘크리트의 공학적 특성)

  • 권영진;김용로;장재봉;김무한
    • Fire Science and Engineering
    • /
    • v.18 no.1
    • /
    • pp.31-36
    • /
    • 2004
  • The purpose of this study is to present data for the reusing, rehabilitation and estimation of safety of RC structure damaged by fire, and for the prevention of explosive spatting by investigation the properties of explosive spalling, compressive strength and ultrasonic pulse velocity according to kinds of fine aggregate, admixture and water-cement ratios. In explosive spalling properties with kinds of aggregate, explosive spalling does not appear or little at surface in the case of used sea sand, but the case of using recycled sand or crushed sand is worse and worse. Property with the kind of admixture does not appear specially. And high strength concrete with W/C 30.5% was taken spalling, but 55% does not appear. It is found that residual compressive strength after exposed at high temperature showed 45% in W/C 55%, and 64% in W/C 30.5% of its original strength averagely. Ultrasonic pulse velocity is different with kinds of aggregate. W/C. and heating time. When 3 month age after heating ultrasonic pulse velocity is recovered abut 1.3%~8.4% of its 1 month age after heating.

An Experimental Study on the Mechanical Properties of High Density Concrete Using Magnetite Aggregate (자철광 골재를 이용하는 철근콘크리트의 역학적 특성에 관한 관험적 연구)

  • 반호용;한천구;김을용
    • Magazine of the Korea Concrete Institute
    • /
    • v.2 no.3
    • /
    • pp.81-88
    • /
    • 1990
  • For the protectioon of radioactive leakage, the quality control of main concrete structure in nuclear power plants is very important. So, this studey is designed to analyze the influence of kind of cement and aggregate on the mechanical properties of high density concrete. Test results of this study are as follows; 1)The slump of magnetite aggregate concrete(MAC) is found half value of nat.ural aggregate concrete (NAC). 2)As the effect of cement, the compressive strength of concrete using moderate heat cement is found higher 5-19 % than that of ordinary portland cement. 3)As the effect of fine aggregate, t.he compressive strength of MAC is found higher than that. of NAC below 340kg/$cm^2$ and lower t.han NAC above 340kg/$cm^2$. 4)As the effect of coarse aggregate, the compressive strength of MAC is found higher 17-22% than that of NAC.

Physical Properties of Polymer Composite Recycling Recycled Aggregate (순환골재를 재활용한 폴리머 복합재료의 물성)

  • Hwang, Eui-Hwan;Jeon, Jong-Ki
    • Applied Chemistry for Engineering
    • /
    • v.20 no.1
    • /
    • pp.67-74
    • /
    • 2009
  • Nowadays, recycling of recycled aggregates from the waste concrete is seriously demanded for the protection of environment and the shortage of aggregates owing to the large scale construction project. In this study, for the development of polymer composite recycling recycled aggregates from the waste concrete, twenty five specimens of the polymer composite were prepared with the five levels of replacement ratios of recycled aggregates (0, 25, 50, 75, 100%) and polymer-cement ratios (0,5, 10, 15, 20%), respectively. For the evaluation of the performance of polymer composite specimens, various physical properties such as compressive and flexural strengths, water absorption, hot water resistance, total pore volume and porosity were investigated. As a result, physical properties of polymer composite were remarkably improved with an increase of polymer cement ratios, but greatly decreased with the replacement ratios of recycled aggregates.

A Study on the Influence of Aggregate on the Estimation of Compressive Strength by Small Size Core (소구경 코어에 의한 콘크리트 압축강도 추정에 미치는 골재의 영향에 관한 연구)

  • 김경민;백병훈;한민철;윤기원;한천구;송성진
    • Proceedings of the Korean Institute of Building Construction Conference
    • /
    • 2002.11a
    • /
    • pp.51-54
    • /
    • 2002
  • This study is intended to investigate an influence of the kinds and the maximum size of aggregate on the compressive strength of small size core specimen. According to the results, the compressive strength of standard specimen is large in order of basalt, granite and limestone aggregate, and shows increasing tendency as the maximum size of aggregate grows large. The compressive strength of concrete using basalt aggregate shows similar tendency to granite aggregate, and that of concrete using limestone aggregate decreases slightly, compared with granite aggregate. The reducing ratio of the compressive strength of 25mm core specimen is least when the maximum size of aggregate is 10mm. But the compressive strength of 50 and 100mm core specimen is almost not influenced by the maximum size of aggregate.

  • PDF

ITZ Analysis of Cement Matrix According to Surface Coated Lightweight Aggregate Type using EIS (EIS를 이용한 표면코팅 경량골재 종류별 시멘트 경화체의 계면 분석)

  • Kim, Chang-Hyun;Jeong, Su-Mi;Kim, Ju-Sung;Park, Sun-Gyu
    • Proceedings of the Korean Institute of Building Construction Conference
    • /
    • 2023.11a
    • /
    • pp.151-152
    • /
    • 2023
  • Lightweight aggregates has a dry specific gravity of 2.0 or less, which is lower than natural aggregates. Lightweght aggregate is efficient for weight reduction but has low compressive strength. In this study, EIS(electrochemical Impedance Spectroscopy) was used to confirm the ITZ(Interfacial Transition Zone) between the lightweight aggregate and cement paste according to the coated of blast furnace slag powder. As a result of EIS measurement, the correlation between ITZ characteristics and compressive strength was determined. The phase angle of EIS was different depending on the blast furnace slag powder coated of the lightweight aggregate. The surface-cotead lightweight aggregate was improved and the ITZ was strengthened.

  • PDF

Compressive Strength and Water Contact Angle Properties of Cement Mortar by Type of Water Repellent (발수제종류별 잔골재 입도에 따른 시멘트 모르타르의 강도 및 발수특성)

  • Kang, Suk-Pyo;Kang, Hye-Ju;Kim, Sang-Jin;Suh, Jeong-In
    • Journal of the Korea Institute of Building Construction
    • /
    • v.21 no.6
    • /
    • pp.529-538
    • /
    • 2021
  • In this study, the compressive strength and water contact angle were measured before and after surface abrasion of mortar specimens prepared by mixing two types of water repellents and two types of sands. In addition, the hydration products and chemical bonding of cement mortar by repellent were examined using X-ray diffraction(XRD), thermogravimetry-differential thermal analysis(TG-DTA), and Fourier-transform infrared spectroscopy(FT-IR) to evaluate the performance of these cement mortar mixtures as repair materials. We found that the compressive strength of the cement mortar with water repellent added was decreased compared to that of the plain cement mortar, and that of the oligomeric system was higher than that of the monomeric system. We further found that the contact angle of mortar with water repellent added was increased compared to that of the plain cement mortar, and that of the oligomeric system was increased compared to that of the monomer.

Mechanical Properties Evaluation of 3D Printing Recycled Concrete utilizing Wasted Shell Aggregate (패각 잔골재를 활용한 3D 프린팅 자원순환 콘크리트의 역학적 성능 평가)

  • Jeewoo Suh;Ju-Hyeon Park;Tong-Seok Han
    • Journal of the Computational Structural Engineering Institute of Korea
    • /
    • v.37 no.1
    • /
    • pp.33-40
    • /
    • 2024
  • The volume of shells, a prominent form of marine waste, is steadily increasing each year. However, a significant portion of these shells is either discarded or left near coastlines, posing environmental and social concerns. Utilizing shells as a substitute for traditional aggregates presents a potential solution, especially considering the diminishing availability of natural aggregates. This approach could effectively reduce transportation logistics costs, thereby promoting resource recycling. In this study, we explore the feasibility of employing wasted shell aggregates in 3D concrete printing technology for marine structures. Despite the advantages, it is observed that 3D printing concrete with wasted shells as aggregates results in lower strength compared to ordinary concrete, attributed to pores at the interface of shells and cement paste. Microstructure characterization becomes essential for evaluating mechanical properties. We conduct an analysis of the mechanical properties and microstructure of 3D printing concrete specimens incorporating wasted shells. Additionally, a mix design is proposed, taking into account flowability, extrudability, and buildability. To assess mechanical properties, compression and bonding strength specimens are fabricated using a 3D printer, and subsequent strength tests are conducted. Microstructure characteristics are analyzed through scanning electron microscope tests, providing high-resolution images. A histogram-based segmentation method is applied to segment pores, and porosity is compared based on the type of wasted shell. Pore characteristics are quantified using a probability function, establishing a correlation between the mechanical properties and microstructure characteristics of the specimens according to the type of wasted shell.

A Study on the Residual Expansibility of Electric Arc Furnace Slag Aggregate (전기로슬래그 골재의 잔류팽창성에 대한 고찰)

  • Yoo, Jung-Hoon;Choi, Jae-Jin
    • Journal of the Korean Recycled Construction Resources Institute
    • /
    • v.2 no.1
    • /
    • pp.128-135
    • /
    • 2006
  • Steel slag (divided into electric arc furnace slag and convener slag) is being produced by millions of tons per every year in many industrial countries. About 6.5 million tonnes of steel slag is produced yearly as an industrial by-product in Korea. Generally natural aggregate is relatively stable and does not enter into complex chemical reactions with water. Unfortunately, however. steel slag aggregate contains a small amount of free lime. The hydration of free lime makes steel slag aggregate unstable and liable to expand. In this paper, firstly, several aging methods are used in order to decrease the volume expansion of electric arc furnace slag, that is stabilization. The volume expansion of electric arc furnace slag is formulated from the experiment. From the formula, the residual expansibility is predicted with immersion expansion. Compressive strength of concrete with electric arc furnace slag has relation with the residual expansibility in slag aggregate.