• Title/Summary/Keyword: 강-콘크리트 합성구조물

Search Result 35, Processing Time 0.025 seconds

Evaluation of Optimum Mix Proportion and Filling Performance of High-fluidity Concrete for SCP Module charging (SCP 모듈 충전용 고유동 콘크리트의 최적배합 도출 및 채움성능 평가)

  • Park, Gi-Joon;Kim, Sung-Wook;Park, Jung-Jun;Lee, Dong-Gyu
    • Journal of the Korea Academia-Industrial cooperation Society
    • /
    • v.18 no.3
    • /
    • pp.452-459
    • /
    • 2017
  • In recent years, to reduce self-weight of structural elements, the use of SCP (Steel Concrete Plate) instead of prestressed concrete is increasing. Because SCP has a complicated sectional shape and includes a large number of studs, the use of high-fluidity concrete is required. Therefore, in this study, to prevent the restrained shrinkage behavior by the stud, the effects of using an expansive agent (EA) and shrinkage reducing agent (SRA) were investigated, and the optimal mixture proportions to maximize the filling capacity were determined based on the fine aggregate ratio. The test results indicated that the combined use of EA and SRA exhibited the smallest shrinkage. The ratio of the crushed sand and washed sea sand was determined to be 5:5, and the proper fine aggregate ratio was found to be 55.6%, because when the ratio was too high, a decrease in strength and an increase in shrinkage strain were expected. The high-fluidity concrete effectively filled the large-sized SCP module.

Experimental Study on Flexural Capacity of Precast Steel Mesh Reinforced Mortar Panel (프리캐스트 스틸메쉬 보강 모르타르 패널의 휨 성능에 대한 실험적 연구)

  • Yi, Na Hyun;Kim, Jang Ho Jay;Lee, Sang Won;Kim, Tae Gyun
    • Journal of the Korea institute for structural maintenance and inspection
    • /
    • v.17 no.3
    • /
    • pp.10-19
    • /
    • 2013
  • Recently, researches related to precast modular construction have been actively conducted for nuclear power plant, LNG gas tank, and small-medium PCCV as well as bridges and buildings. In this study, the precast panel cast with steel mesh reinforced mortar (SRM) which is similar reinforced ferrocement was developed for efficient precast construction, construction time reduction, and easy transportation. Mortar mixture with high strength and flowability was obtained from various case studies using silica fume and GGBS. Also, $1,200{\times}600{\times}150mm$ SRM and reinforced concrete (RC) panels were manufactured with reinforcing ratio of 2% and 4%. To verify structural performance of the SRM specimen, the basic material tests, free shrinkage test, and 3-point flexural test with a line loading were carried out. From the test results, it was determined that SRM specimens showed outstanding flexural capacity and ductility. However, the 4% reinforced SRM specimens must consider shear reinforcing to be used as a precast modular member.

Analysis on Shear Force of Specimens Using Perfobond Rib Shear Connector (Perfobond Rib 전단연결재를 사용한 실험체의 전단강도 분석)

  • Choi, Jin Woong;Park, Byung Gun;Kim, Hyeong Jun;Jeong, Ho Seong;Park, Sun Kyu
    • Journal of the Korea institute for structural maintenance and inspection
    • /
    • v.15 no.1
    • /
    • pp.138-147
    • /
    • 2011
  • The objective of this study which it sees direct shear stress and comparative analysis of flexural shear stress leads and it is a shear stress analysis which it follows in load direction of the structure which uses Perfobond Rib shear connectors. To analyze direct shear stress, five Perfobond Rib shear connect experiments were fabricated with five variables and conducted Push-out Tests. After experiments, mechanism of Perfobond Rib shear connector was examined and direct shear formula was proposed based on primary factors which influence direct shear stress. Also, for the analysis of flexural shear steel-concrete composite slab specimens were fabricated and static flexural test. Based on the static flexural test it analyzed the flexural behavior and the flexural shear stress it calculated. Direct shear stress and EN 1994-1-1 to lead and be calculated, it compared the flexural shear stress and it analyzed in about the shear resistance stress which it follows in load direction.

Strength Characteristics of Hollow Prestressed Concrete Filled Steel Tube Piles for Hybrid Composite Piles (복합말뚝용 중공형 콘크리트 충전 강관말뚝의 강도 특성)

  • Paik, Kyu-Ho
    • Journal of the Korean Geotechnical Society
    • /
    • v.34 no.1
    • /
    • pp.37-46
    • /
    • 2018
  • Hollow prestressed concrete filled steel tube (HCFT) piles, which compose hollow PHC piles inside thin wall steel tubes, are developed. In order to investigate the strength characteristics of HCFT piles, flexural and shear tests were conducted on HCFT piles as well as PHC and steel pipe piles with the same diameter. Results of the test program showed that the flexural strength of HCFT piles was 2.88 and 1.19 times those of ICP and steel pipe piles with thickness of 12 mm, respectively, and its shear strength was 2.40 times that of steel pipe piles. The shear key attached to the inside of thin wall steel tube did not affect the flexural behavior of HCFT piles. It was also observed that the flexural strengths of HCFT piles with diameters of 450 and 500 mm were 35 to 63% higher than the sum of the flexural strengths of its components, respectively, because the strength of concrete in compressive zone increased by confining effect of thin wall steel tube on concrete. HCFT piles used as upper piles in hybrid composite piles might decrease the lateral displacement and increase the structural safety of structures subjected to lateral loads.

Chloride Binding Properties of Portland Cement Binder Incorporating CaAl2O4-CaAl4O7 (CaAl2O4-CaAl4O7 혼입 포틀랜드 시멘트 결합재의 염소이온 고정 특성)

  • Han, Jae-Doh;Lee, Yun-Su;Lee, Han-Seung
    • Journal of the Korea institute for structural maintenance and inspection
    • /
    • v.24 no.4
    • /
    • pp.1-9
    • /
    • 2020
  • This study conducted to understand effects of CA (CaAl2O4) and CA2 (CaAl4O7) ratio on chloride binding ability and compressive strength and pore structure of cement mortar incorporating mixture of CA and CA2. The Portland cement based specimens were mixed with the clinkers CA and CA2, and these calcium aluminate clinker mixture were replaced 0, 5, 10% by weight of cement. After all the test specimens were cured for 28 days under water curing, they were immersed in the distilled water and NaCl solution. As a result, 28 days compressive strength of all specimens was similar, and As the replacement ratio of calcium aluminate clinker in the specimen increased, Friedel's salt production tended to increase. However, it was dependent on the amount of Al2O3 in the level of 5% replacement and CA ratio in the level of 10% replacement. Through equilibrium isotherm result, it was also indicated that as replacement ratio of calcium aluminate clinker in cement matrix increased, chloride binding capacity was improved, and chloride penetration was suppressed. In this study, the specimen replaced with 10% of the calcium aluminate clinker mixture (CA 39%, CA2 60%) was remarkable to control chloride attack. We figured out necessity to understand optimal CA/CA2 ratio to effectively apply CA2 as a sustainable building material by improving the chloride binding ability in Portland cement based system.