• Title/Summary/Keyword: $Y_2Ti_2O_7$

Search Result 1,307, Processing Time 0.035 seconds

Microwave Dielectric Properties in Bi-Substituted BaO.$Nd_{2}O_{3}$.$4TiO_{2}$ (Bi 가 치환된 BaO.$Nd_{2}O_{3}$.$4TiO_{2}$ 세라믹스의 마이트로파 유전특성)

  • Cheon, Jae-Il;Kim, Jeong-SeoG
    • Korean Journal of Materials Research
    • /
    • v.8 no.7
    • /
    • pp.659-663
    • /
    • 1998
  • The effect of Bi-substitution in $BaO.(Nd_{1-x}Bi_x)_2O_3.4TiO_2$ ceramic was studied on the formation of crystal phases, microstructure, and microwave dielectric properties. $BaO.(Nd_{1-x}Bi_x)_2O_3.4TiO_2$, solid solution (0$\leq$x$\leq$0.2) were formed by Bi-substitution into the Nd site of $BaO.(Nd_{1-x}Bi_x)_2O_3.4TiO_2$ ceramics. Average grain size increased with Bi-substitution. Dielectric constant(${\varepsilon}_r$) increased from 84 to U8, and the temperature coefficient of resonant frequency(${\tau}_f$) decreased from 44 ppm/$^{\circ}C$ to -30 ppm/$^{\circ}C$ when Bi contents increased up to x=0.2 in $BaO.(Nd_{1-x}Bi_x)_2O_3.4TiO_2$ solid solutions. $BaO.(Nd_{1-x}Bi_x)_2O_3.4TiO_2$ solid solutions with x=0.04~0.08 showed the most superior microwave dielectric properties, those are ${\varepsilon}_r$= 89-92, Q . f = 5855~6091 GHz, and (${\tau}_f$)= -7.5-7.5 ppm/$^{\circ}C$.

  • PDF

Microwave Dielectric Properties of the 0.7Mg4Ta2O9-0.3SrTiO3 Ceramics with Sintering Temperature (소결온도에 따른 0.7Mg4Ta2O9-0.3SrTiO3 세라믹스의 마이크로파 유전특성)

  • Kim, Jae-Sik;Choi, Eui-Sun;Lee, Moon-Kee;Lee, Young-Hie;Bae, Seon-Gi
    • Journal of the Korean Institute of Electrical and Electronic Material Engineers
    • /
    • v.18 no.6
    • /
    • pp.538-542
    • /
    • 2005
  • The structural and microwave dielectric properties of $0.7Mg_4Ta_2O_9-0.3SrTiO_3$ ceramics with sintering temperature were investigated. All the sample of the $0.7Mg_4Ta_2O_9-0.3SrTiO_3$ ceramics were prepared by conventional miked oxide method and the sintering temperature was $1425\~1500^{\circ}C$. The hexagonal phase of $Mg_4Ta_2O_9$ and the cubic phase of $SrTiO_3$ were coexisted. The porosity of $0.7Mg_4Ta_2O_9-0.3SrTiO_3$ ceramics were reduced with increasing sintering temperature. In the case of $0.7Mg_4Ta_2O_9-0.3SrTiO_3$ ceramics sintered at $1475^{\circ}C$, dielectric constant, quality factor and temperature coefficient of resonant frequency were 14.51, 82,596 GHz and $-3.14\;ppm/^{\circ}C$, respectively.

Dielectric Properties of Non-reducible X7R Dielectric Materials in $BaTiO_3$-$Er_2$$O_3$--MgO ($BaTiO_3$-$Er_2$$O_3$-MgO 첨가계를 이용한 내환원성 X7R 재질의 유전특성에 관한 연구)

  • 한영호;최상근;황진현
    • Journal of the Korean Ceramic Society
    • /
    • v.38 no.7
    • /
    • pp.615-620
    • /
    • 2001
  • E $r_2$ $O_3$-MgO 복합 첨가가 BaTi $O_3$계 내환원성 X7R 재질의 유전특성에 미치는 영향에 대하여 환원성 분위기에서 연구하였다. (B $a_{1-x}$ E $r_{x}$)( $Ti_{1-y}$M $g_{y}$ ) $O_3$첨가계에서 1.0 mol% 이상 MgO의 복합첨가로 E $r_{Ba}$ 도너 불순물과 $Mg_{Ti}$ 억셉터 불순물이 전기적으로 보상되어, 환원성분위기 소결 후에도 $10^{10}$Ωcm 이상의 높은 절연저항을 나타내었다. E $r_2$ $O_3$가 첨가된 시편에서 MgO가 2.0 mol% 이상 첨가될 경우, 유전율의 온도안정성이 향상되어 X7R 규격을 만족시켰으며 1.0$mu extrm{m}$ 이하의 작고 균일한 입자가 관찰되었다. 한편, E $r_2$ $O_3$의 첨가량이 3.0 mol%로 증가함에 따라 유전율의 온도안정성이 향상되었으나 상대적으로 상온 유전상수값이 현저히 감소하였다.였다.다.

  • PDF

The Electric Properties of SrTiO$_3$Varistor Prepared by Co-precipitation Process (공침법으로 제초한 SrTiO$_3$바리스터의 전기적 특성)

  • 이종필;신현창;최정철;최승철
    • Journal of the Microelectronics and Packaging Society
    • /
    • v.7 no.3
    • /
    • pp.7-11
    • /
    • 2000
  • The low-voltage driven $SrTiO_3$ceramic varistor device was fabricated from $SrTiO_3$ powders prepared by co-precipitation method with $CuO-SiO_2$additives. Compare with conventional process, this process has advantages such as the reduction of the sintering temperature of $SrTiO_3$ ceramics by 100-$150^{\circ}C$ and the simplification of processing procedure. The non-linear coefficient value ($\alpha$) of the varistor showed 8.47 when it was sintered at $1350^{\circ}C$ for 2 h with 5 wt% additives in reducing atmosphere of 5% $H_2/N_2$ mixed gas. The low-voltage driven $SrTiO_3$ceramic varistor was obtained which has a breakdown voltage as low as 7 V.

  • PDF

Surface Modification of Mica Using TiO$_2$ prepared by Alkoxide Hydrolysis Method (알콕사이드 가수분해법에 의핸 제조된 TiO$_2$ 분말을 이용한 Micad의 표면 개질)

  • 한상필;윤영훈;이상훈;최성철
    • Journal of the Korean Ceramic Society
    • /
    • v.36 no.7
    • /
    • pp.691-697
    • /
    • 1999
  • TiO2 powder was adsorbed on the surface of mica using the heterocoagulation method in water TiO2 powder was prepared from hydrolysis of titanium-iso propoxide in a mixed solvent of anhydrous ethanol and water. When the molar ratio of water to titanium iso-propoxide was 0.25 monodispersed spherical TiO2 particles were obtained. The prepared TiO2 powder showed anatase phase after heat treatment at 50$0^{\circ}C$ for 2 h and then transformed to rutile phase after heat treatment at 100$0^{\circ}C$ for 2h. The iso-electric points of TiO2 and Mica were pH 3.9 and pH 3.25 respectively which were measured by the Z-potential analysis in water base. The maximum Z-potential difference between two powders was observed in the range of pH 3.6~3.7 TiO2 powder was adsorbed on the surface of mica by heterocoagulation method in pH 3.6~3,7 The properties of prepared TiO2 powder was haracterized by TG-DTA, XRD and SEM The morphology and thermal properties of TiO2-adsorbed mica were examined.

  • PDF

Photodegradation of Pyrene, Chrysene and Benzo[a]pyrene in Water (II) (수중의 Pyrene, Chrysene 및 Benzo[a]pyrene의 광분해(II))

  • 감상규;김지용;주창식;이민규
    • Journal of Environmental Science International
    • /
    • v.12 no.7
    • /
    • pp.775-782
    • /
    • 2003
  • The photodegradations of pyrene, chrysene and benzo[a]pyrene that were similar in structure among polycyclic aromatic hydrocarbons (PAHs) were investigated with a low-pressure mercury lamp(the wavelength of 253.7 nm and UV output of 1.35${\times}$10$\^$-3/J/s). The optimum concentrations of TiO$_2$ and H$_2$O$_2$ on the photodegradation of pyrene, chrysene and benzo[a]pyrene were 1 g/L and 1.5${\times}$10$\^$-3/ M, respectively. By these optimum concentrations, their rates increased with increasing the concentration of TiO$_2$ and H$_2$O$_2$ because the amounts of OH radical formed increased, but for the higher concentrations than the optimum, their rates decreased with increasing those concentrations because the white turbidity phenomena occurs in case of TiO$_2$ and H$_2$O$_2$ acts as an OH radical inhibitor. The photodegradation rates among the photodegradation processes such as UV, UV/TiO$_2$, UV/H$_2$O$_2$, and UV/H$_2$O$_2$/TiO$_2$ decreased in the following sequences.: UV/H$_2$O$_2$/TiO$_2$> UV/H$_2$O$_2$> UV/TiO$_2$> UV.

A Study OH the Character and Activity of $TiO_2$ Photocatalysts Prepared With Various Condition (다양한 조건에서 제조된 $TiO_2$ 광촉매 특성 및 활성에 관한 연구)

  • Kim, Seung-Min;Youn, Tae-Kawun;Hong, Dae-Il;Kim, Sung-Kuk;Park, Sang-Won
    • Journal of Korean Society of Environmental Engineers
    • /
    • v.27 no.9
    • /
    • pp.932-938
    • /
    • 2005
  • [ $TiO_2$ ] nanoparticles were prepared from the precipitation in $TiCl_4$ and the sol-gel profess in $Ti(OC_3H_7)_4$ as starting materials with various synthetic conditions. The samples were characterized by XRD, SEM, and TEM testing techniques. The photocatalytic degradation of congo red has been investigated in $TiO_2/UV$ process to evaluate photocatalytic activities for the samples. $TiO_2$ nanoparticles calcined at $400^{\circ}C$ had the best photocatalytic activity with the rate constant of the degradation of congo red as $0.0319\;min^{-1}$. The rate constant of $TiO_2$ photocatalysts was increased with the calcination temperature under $400^{\circ}C$ and decreased with the calcination temperature upper $400^{\circ}C$. In the case of $TiO_2$ photocatalysts, the photocatalytic activity wasn't greatly affected by the frequencies of usage. In the similar synthesis condition, the degradation efficiency of the $TiO_2$ particle prepared by $TiCl_4$ was increased to 8.8%, when the rate was compared with the sample prepared by $Ti(OC_3H_7)_4$. The photocatalytic activities of $TiO_2$ photocatalysts synthesized by $Ti(OC_3H_7)_4$ with various conditions were also discussed.

A Study on the Glass-Ceramics of the Cordierite System -the effects of -$TiO_2$ Addition (코디어라이트계 결정화 유리에 관한 연구 -$TiO_2$ 첨가 효과)

  • 박용완;현부성;정준상
    • Journal of the Korean Ceramic Society
    • /
    • v.30 no.12
    • /
    • pp.1054-1058
    • /
    • 1993
  • The effects of TiO2 addition as a nucleating agent on the cordierite glass-ceramics were investigated. The glass compositiion was stoichiometric cordierite composition of 13.7MgO-34.9Al2O3-51.4SiO2(wt%), and TiO2 as a nucleating agent was added by 5, 10 and 15wt% in addition. The optimum amount of TiO2 addition and appropriate heat treatment schedule were determined by using dilatometer, DTA, XRDA and SEM. The composition containing 10wt% TiO2 was proved to be the best among the investigated compositions. And the optimum heat treatment schedule was 840℃-2h for the nucleation and 1140℃-2h for the crystallization. The properties were as follows. The crystallinity was ∼75%, thermal expansion coefficient 33×10-7/℃(25∼700℃), dielectric constant 7.6(1KHz) and Vicker's hardness 5.1GPa.

  • PDF

Preparation of $N-TiO_2$ Photocatalysts and Activity Test ($N-TiO_2$ 광촉매의 제조와 광촉매 활성 검토)

  • Kang, Young-Gu;Shin, Ki-Seok;Ahn, Sung-Hwan;Hahm, Hyun-Sik
    • Journal of the Korean Applied Science and Technology
    • /
    • v.29 no.3
    • /
    • pp.466-472
    • /
    • 2012
  • Visible-light-responding photocatalysts, $N-TiO_2$, were prepared by nitrogen doping onto $TiO_2$. The crystalline structure and morphology, doping state of the prepared photocatalysts were characterized by XRD, FE-SEM, and XPS. The activity of the prepared photocatalysts was examined by the decomposition of methyleneblue. The prepared catalysts were anatase type and the crystallinity was increased with pH. The particle sizes of the prepared catalysts were 5.42, 5.99, 7.58 nm at pH 2.2, 4.7, 9.0, respectively. The particle sizes of the prepared catalysts were slightly increased with pH. The activity of the photocatalysts was directly proportional to the crystallinity of the catalysts. $N-TiO_2$ prepared by nitrogen doping onto $TiO_2$ showed activity under visible light. The doped nitrogen was located not in the lattice but on the surface.