Mechanical Properties of the Pressureless Sintered $Al_2O_3-SiC$ Composite(1) : Dispersion Effects of SiC Powder (상압소결 $Al_2O_3-SiC$계 소결체의 기계적 성질 (I) : SiC분말의 분산효과)

  • 이홍림;김경수;이형복
    • Journal of the Korean Ceramic Society
    • /
    • v.25 no.3
    • /
    • pp.231-236
    • /
    • 1988
  • In order to investigate the effect of second phase on $Al_2O_3$ matrix, SiC particles were dispersed in $Al_2O_3$ matrix as a second phase over the content range of 5 vol.% to 20 vol.%. To this mixture, $Y_2O_3$ or $TiO_2$ powders were added as a sintering additive before isostatically pressing and pressurelessly sintering at 180$0^{\circ}C$ for 90 min in $N_2$ atmosphere. With increasing SiC content, relative densities of composites were decreased but mechanical properties of composites were improvjed. In the case of adding $Y_2O_3$ as a sintering additive, maximum values of flexural strength, hardness and fracture toughness were 525 MPa, 17.1 GPa, 4.1 MPa.m1/2 respectively. In the case of adding X$TiO_2$ as a sintering additive, maximum values of flexural strength, hardness were 285 MPa, 12.1 GPa respectively. Improved mechanical properties were found to be the results of grain growth control of $Al_2O_3$ matrix and crack deflection by the second phase SiC particles.

  • PDF

The Dielectrical Properties of $(1-x)(Sr_a.Pb_b.Ca_c)TiO_3-xB_i2O_3.TiO_2$ system affected by $Bi_2O_3.3TiO_2$ amounts and $MnO_2$ ($(1-x)(Sr_a.Pb_b.Ca_c)TiO_3-xB_i2O_3.TiO_2$계에서의 $Bi_2O_3.3TiO_2$$MnO_2$첨가에 따른 유전특성에 관한 연구)

  • 박상도;이응상
    • Journal of the Korean Ceramic Society
    • /
    • v.34 no.2
    • /
    • pp.123-130
    • /
    • 1997
  • In this study, (Sr.Pb.Ca)TiO3-Bi2O3.3TiO2(SPCT) systems were investigated to develop a new material which has a high dielectric constant, a low dielectric loss and a small TCC(Temperature Coefficient of Capa-citance), and are suitable for high voltage applications as a function of the additions of Bi2O3.3TiO2 from 5 mol.% to 9 mol.%. The result obtained from our investigation showed that up to 6 mol.% Bi2O3.3TiO ad-dition the dielectric constant increased and it deteriorated at higher concentrations with increasing amount of the acicular grains. As a result of some dopants (SiO2, Nb2O3, MnO2) addition to SPCT, the specimens with MnO2 showed good dielectric properties. The dielectric constant decreased, but the TCC was improved with the addition of MnO2 from 0.15 wt.% to 0.45 wt. %.

  • PDF

Charaterization of (Bi,La)Ti3O12 Ferroelectric Thin Films on Pt/Ti/SiO2/Si Substrates by sol-gel Method (졸-겔법으로 Pt/Ti/SiO2/Si 기판위에 제작된 (Bi,La)Ti3O12 강유전체 박막의 특성 연구)

  • Hwang, Sun-Hwan;Chang, Ho-Jung
    • Korean Journal of Materials Research
    • /
    • v.12 no.11
    • /
    • pp.835-839
    • /
    • 2002
  • Metal-Ferroelectric-Metal(MFM) capacitors were prepared using $Bi_{3.3}$ $La_{0.7}$ $Ti_3$$O_{12}$ (BLT) ferroelectric thin films which were spin coated on $Pt/Ti/SiO_2$/Si substrates by the Sol-Gel method. BLT thin films annealed at above $650^{\circ}C$ showed polycrystalline structures with typical c-axis preferred orientation. The grain size and surface roughness were increased as the annealing temperature increased from $650^{\circ}C$ to $700^{\circ}C$. In addition, the full width at half maximum (FWHM) values were decreased with increasing annealing temperatures, indicating the improvement of crystallinity. The remanent polarization (2Pr= $Pr^{+}$ $+Pr^{-) }$ and leakage current of the BLT film annealed at $650^{\circ}C$ were about 29.3 $\mu$C/cm$^2$ and $2.3$\times$10^{-8}$$ A/cm^2$ at 3V. There were no distinct changes in the retention charges after $10^{10}$ polarization switching cycles, showing good fatigue property of the annealed BLT films.

A Study on Oxidative Decomposition of CFC-113 over TiO2-SiO2 Catalysts Prepared by the Sol-Gel Method (솔-젤법으로 제조된 TiO2-SiO2 촉매상에서 CFC-113의 산화분해반응에 관한 연구)

  • Chang, Won-Chul;Lee, Doo-Hyoung;Lee, Tae-Jin
    • Applied Chemistry for Engineering
    • /
    • v.10 no.7
    • /
    • pp.963-968
    • /
    • 1999
  • The global environmental problems have been caused by the release of CFCs. Therefore, methods for safe destruction of recoverd CFCs will be eventually needed. The objective of this study was to develop and test a catalyst operating at a mild condition for the decomposition of CFC-113. In this work, catalytic oxidative decomposition of CFC-113 was carried out over aerosol $TiO_2/SiO_2(ATS)$ catalysts prepared by the sol-gel method. All ATS catalysts(Ti/Si mol ratio=1, 2, 2.33, 4) showed high initial activity. However, the deactivation of ATS catalysts was found that more remarkable due to an attack of fluorine and the destruction of ATS structure(Si-F reaction) from analyses of SEM-EDX, XRD than $TiO_2/SiO_2(ATS)$ catalyst prepared by the precipitation method. ATS catalysts prepared by more acidic prehydrolysis condition were found to have still more activity and longer life-time by increasing of acidity. The activity of ATS catalyst also depend on the content of $TiO_2$. There was reason that the acidity of the ATS catalyst was increased with the increased content of $TiO_2$ from 50 to 80 mol %. Solid superacid catalyst ($ATX/SO_4{^{2-}}$) modified with $H_2SO_4$ solution was prepared for high activity and lower deactivation. The reaction of $ATS/SO_4{^{2-}}$ catalyst also exhibited even higher activity and lower deactivation than the original ATS catalyst. It is suggested that the addition of the sulphate species clearly inhibit the deactivation.

  • PDF

Preparation Of Composite particles with planarized $SiO_2$ Particles (평탄면을 갖는 $SiO_2$미립자의 제조와 이를 이용한 $SiO_2/TiO_2$복합입자의 제조)

  • 신달식;김광수;이옥섭;이성호
    • Journal of the Society of Cosmetic Scientists of Korea
    • /
    • v.25 no.1
    • /
    • pp.37-54
    • /
    • 1999
  • Planarized SiO$_2$ particles were prepared by two-step reduction method of making much smaller particles, micron-sized ones, to improve spreadability, adherence, and smoothness. Various pigments known as flaky extender usually have terrace layers on their surfaces, but SiO$_2$ Particles in this study exhibit a smooth surface structure. These single SiO$_2$ particles were used for core particles to prepare the composite particles coated with ultra fine TiO$_2$ particles by a homogeneous precipitation method. The thickness and the morphology of the deposited TiO$_2$ layer could be altered by adjusting the reactant concentrations, reaction time and temperature. The characteristics of SiO$_2$/TiO$_2$composite in the field of color cosmetics is to give a UV-cut effect and to enhance the chroma of human skin color, one of optical properties.

  • PDF

Transparent Hydrophobic Anti-Reflection Coating with SiO2\TiO2 Thin Layers (SiO2\TiO2 박막에 의한 투명 발수 반사방지 코팅)

  • Noh, Yeoung-Ah;Kim, Ki-Chul
    • Journal of the Korea Academia-Industrial cooperation Society
    • /
    • v.18 no.3
    • /
    • pp.1-6
    • /
    • 2017
  • Functional coatings, such as anti-reflection and self-cleaning, are frequently applied to cover glass for photovoltaic applications. Anti-reflection coatings made of mesoporous silica film have been shown to enhance the light transmittance. $TiO_2$ photocatalyst films are often applied as a self-cleaning coating. In this study, transparent hydrophobic anti-reflective and self-cleaning coatings made of $SiO_2/TiO_2$ thin layers were fabricated on a slide glass substrate by the sol-gel and dip-coating processes. The morphology of the functional coatings was characterized by field emission scanning electron microscopy (FE-SEM) and atomic force microscopy (AFM). The optical properties of the functional coatings were investigated using an UV-visible spectrophotometer. Contact angle measurements were performed to confirm the hydrophobicity of the surface. The results showed that the $TiO_2$ films exhibit a high transmittance comparable to that of the bare slide glass substrate. The $TiO_2$ nanoparticles make the film more reflective and lead to a lower transmittance. However, the transmittance of the $SiO_2/TiO_2$ thin layers is 93.5% at 550 nm with a contact angle of $110^{\circ}$, which is higher than that of the bare slide glass (2.0%).

Anti-reflection coating on the facet of a spot size converter integrated laser diode using a pair of TiO2 and SiO2 thin films (TiO2와 SiO2 박막 쌍을 이용한 광모드 변환기가 집적된 반도체 레이저 단면의 무반사 코팅)

  • 송현우;김성복;심재식;김제하;오대곤;남은수
    • Korean Journal of Optics and Photonics
    • /
    • v.13 no.5
    • /
    • pp.396-399
    • /
    • 2002
  • Using a bi-layer anti-reflection coating of $TiO_2$and $SiO_2,$ we have achieved a minimum facet reflectivity of $~10^{-5}$ and a band width of 27 nm for a reflectivity of $~10^{-4}$ or less for 1.3 $\mu\textrm{m}$ spot size converter integrated semiconductor lasers. This coating is applicable to external-cavity-tuned laser sources and semiconductor optical amplifiers.

Formation of $PbTiO_3$ Thin Films by Thermal Diffusion from Multilayrs (다층 구조로부터 열 확산에 의한 $PbTiO_3$ 박막의 제조)

  • 서도원;최덕균
    • Journal of the Korean Ceramic Society
    • /
    • v.30 no.6
    • /
    • pp.510-516
    • /
    • 1993
  • $PbTiO_3$ thin films have been formed by rapid thermal annealing(RTA) of $TiO_2$/Pb/$TiO_2$ multilayer films deposited on Si wafers by RF sputtering. Based on the optimal depositon conditions of TiO2 and Pb, $TiO_2$/Pb/$TiO_2$ three layers were deposited for 900$\AA$ each. These films were subjected to RTA process at the temperatures ranging from $400^{\circ}C$ to $900^{\circ}C$ for 30 seconds in air, and were analyzed by X-ray diffraction and transmission electron microscopy to investigate the phases and the microstructures. As a result, perovskite $PbTiO_3$ phases was obtained above $500^{\circ}C$ with the trace of unreacted $TiO_2$. RBS analysis revealed the anisotropic behavior of diffusion that the diffusivity of Pb to the bottom $TiO_2$ layer was faster than that of Pb to the top $TiO_2$ layer. The amorphous Pb-silicate was formed between film and Si substrate due to the diffusion of Pb, but Pb-silicate existed locally at the interface and the amount of that phase was very small. Therefore the effect of bottom $TiO_2$ layer as a diffusion barrier was confirmed. $PbTiO_3$ films formed by current technique showed a relative dielectric constant of 60, and the maximum breakdown field reached 170kV/cm.

  • PDF

Effects of Sintering Additives and Atmospheres on the Piezoelectric and Sintering Properties of $Pb_{0.98}Cd_{0.02}Zr_{0.36}Ti_{0.39}Ni_{0.083}Nb_{0.167}O_3$ (소결첨가제와 분위기가 $Pb_{0.98}Cd_{0.02}Zr_{0.36}Ti_{0.39}Ni_{0.083}Nb_{0.167}O_3$의 소결 및 압전 특성에 미치는 영향)

  • 문종하;박진성;박현수
    • Journal of the Korean Ceramic Society
    • /
    • v.33 no.11
    • /
    • pp.1260-1266
    • /
    • 1996
  • The effects of SiO2 MnO2 and sintering atmospheres (O2, N2) on the piezoelectric properties and densification behaviors of Pb0.98Cd0.02Zr0.36Ti0.39Ni0.083Nb0.167O3 were investigated. The addition of SiO2 to the system enhanced the rate of densification but supressed the rate of grain growth. On the other hand the addition of MnO2 to the system did not nearly affect the rate of densification but increased slightly the rate of grain growth The densification of Pb0.98Cd0.02Zr0.36Ti0.39Ni0.083Nb0.167O3 containing of SiO2 or MnO2 was promoted with increasing the partial pressure of O2. The relative dielectric constant ($\varepsilon$r) and piezoelectric constant (d33) of Pb0.98Cd0.02Zr0.36Ti0.39Ni0.083Nb0.167O3 containing of SiO2 or MnO2 sintered under O2 atmosphere were higher than under N2 atmosphere. Whereas the mechanical quality factor (Qm) of specimens sintered under O2 atmosphere were lower than under N2 atmosphere. Thus the sintering atmosphere of O2 and N2 in Pb0.98Cd0.02Zr0.36Ti0.39Ni0.083Nb0.167O3 containing of SiO2 or MnO2 acted as donor and acceptor respectively. As the amount of SiO2 increased the relative dielectric constant ($\varepsilon$r) and piezoelectric constant (d33) of Pb0.98Cd0.02Zr0.36Ti0.39Ni0.083Nb0.167O3 but the mechanical quality factor (Qm) did not nearly change, In the case of the addition of MnO2 to the system the relative dielectric constant ($\varepsilon$r) and piezoelectric constant (d33) of Pb0.98Cd0.02Zr0.36Ti0.39Ni0.083Nb0.167O3 sintered under O2 atmosphere decreased rapidly with increasing the amount of MnO2 but they were unchanged with increasing the amount of MnO2 under N2 sintering atmosphere. Therefore the differences of the relative dielect-ric constant ($\varepsilon$r) and piezoelectric constant (d33) due to sintering atmosphere were diminished as the amount of MnO2 increased.