Structure and Dielectric properties of BST Thin Films prepared by Sol-gel method for Tunable element application (Tunable 소자 응용을 위한 Sol-gel 법으로 제작된 BST 박막의 Bi 첨가에 따른 구조적, 유전적 특성)

  • Kim, Tae-Hyung;Kim, Kyoung-Tae;Kim, Chang-Il
    • Proceedings of the Korean Institute of Electrical and Electronic Material Engineers Conference
    • /
    • 2004.07b
    • /
    • pp.565-568
    • /
    • 2004
  • An alkoxide-based sol-gel method was used to fabricate $Ba_{0.6}Sr_{0.4}TiO_3$ thin films doped by Bi from 5 to 20 mol% on a Pt/Ti/SiO2/Si substrate. The structural and dielectric properties of BST thin films were investigated as a function of Bi dopant concentration. The dielectric properties of the Bi doped BST films were strongly dependent on the Bi contents. The dielectric constant and dielectric loss of the films decreased with increasing Bi content. However, the leakage current density of the 10 mol% Bi doped $Ba_{0.6}Sr_{0.4}TiO_3$ thin film showed the lowest value of 5.13 10-7 at 5 V. The figure of merit (FOM) reached a maximum value of 32.42 at a 10 mol% Bi doped $Ba_{0.6}Sr_{0.4}TiO_3$ thin films. The dielectric constant, loss factor, and tunability of the 10 mol% Bi doped $BBa_{0.6}Sr_{0.4}TiO_3$ thin films were 333,0.0095, and 31.1%, respectively.

  • PDF

Fabrication of BST thin films with Bi addition by Sol-gel method and their Structure and Dielectric properties (Sol-gel 법으로 제작된 BST 박막의 Bi 첨가에 따른 구조적, 유전적 특성)

  • Kim, Kyoung-Tae;Kim, Chang-Il
    • Proceedings of the Korean Institute of Electrical and Electronic Material Engineers Conference
    • /
    • 2004.04b
    • /
    • pp.18-21
    • /
    • 2004
  • An alkoxide-based sol-gel method was used to fabricate $Ba_{0.6}Sr_{0.4}TiO_3$ thin films doped by Bi from 5 to 20 mol% on a $Pt/Ti/SiO_2/Si$ substrate. The structural and dielectric properties of BST thin films were investigated as a function of Bi dopant concentration. The dielectric properties of the Bi doped BST films were strongly dependent on the Bi contents. The dielectric constant and dielectric loss of the films decreased with increasing Bi content. However, the leakage current density of the 10 mol% Bi doped $Ba_{0.6}Sr_{0.4}TiO_3$ thin film showed the lowest value of $5.13{\times}10^{-7}\;A/cm^2$ at 5 V. The figure of merit (FOM) reached a maximum value of 32.42 at a 10 mol% Bi doped $Ba_{0.6}Sr_{0.4}TiO_3$ thin films. The dielectric constant, loss factor, and tunability of the 10 mol% Bi doped $Ba_{0.6}Sr_{0.4}TiO_3$ thin films were 333, 0.0095, and 31.1%, respectively.

  • PDF

Screen printed $BaSrTiO_3$ composite for embedded capacitor apprication (Embedded capacitor 적용을 위한 screen printed $BaSrTiO_3$ 복합체)

  • Park, Yong-Jun;Koh, JUng-Hyuk
    • Proceedings of the Korean Institute of Electrical and Electronic Material Engineers Conference
    • /
    • 2007.06a
    • /
    • pp.311-312
    • /
    • 2007
  • In this study, composite $BaSrTiO_3$ has been studied for high frequency device applications. Composite $Ba_{0.5}Sr_{0.5}TiO_3$ has high dielectric permittivity and low loss tangent at the relative frequency range from MHz to GHz. 10,30 and 50 wt% of epoxy doped $Ba_{0.5}Sr_{0.5}TiO_3$ powders were prepared with bisphenol A and F polymer employing ball milling process. Epoxy/($BaSrTiO_3$) composites thick films were screen printed on the Cu plated PCB substrates through screen printing methods. The specimens were designed for the embedded capacitor applications. Temperature dependent dielectric permittivity of Epoxy doped $BaSrTiO_3$ ceramics was measured.

  • PDF

Structural and C-V characteristics of SrTiO$_3$ /PbTiO$_3$ thin film deposited on Si (Si 기판위에 증착한 SrTiO$_3$ /PbTiG$_3$ 고용체 박막의 구조적 특성 및 C-V 특성)

  • 이현숙;이광배;김윤정;박장우
    • Proceedings of the Korean Institute of Electrical and Electronic Material Engineers Conference
    • /
    • 2000.07a
    • /
    • pp.71-74
    • /
    • 2000
  • Pt/Pb$TiO_3$/$SrTiO_3$/p-Si films were prepared by metallo-organic solution deposition(M0SD) method and investigated its structure and ferroelectric properties. Crystallinity of specimen as a funtions of post annealing temperature and the thickness of $SrTiO_3$(STO) buffer layer was studied using XRD and AFM. Based on C-V and P-E curve, $PbTiO_3$(PTO) capacitors showed good ferroelectric hysteresis arising from the polarization switching properties. When the thickness of ST0 buffer layer between PTO and Si substrate was 260 nrn and the post annealing temperature was $650^{\circ}C$, it was showed that production of the pyrochlore phase due to interdiffusion of Si into FTO was prevented. The dielectric constant of FTO thin films calculated from a maximum Cma in the accumulation region was 180 and the dielectric loss was 0.30 at 100 kHz frequency. The memory window in the C-V curve is 1.6V at a gate voltage of 5V.

  • PDF

Dielectric Properties of (Ba,Sr)$TiO_3$ Thin Films with Substrate Temperature (기판온도에 따른 (Ba,Sr)$TiO_3$ 박막의 유전특성)

  • Lee, Sang-Chul;Chung, Jang-Ho;Bae, Seon-Gi;Lee, Young-Hie
    • Proceedings of the KIEE Conference
    • /
    • 1999.07d
    • /
    • pp.1879-1881
    • /
    • 1999
  • (Ba,Sr)$TiO_3$[BST] thin films were fabricated on Pt/Ti/$SiO_2$/Si substrate by RF sputtering. We investigated the effects of substrate temperature on the structural and dielectric properties of BST thin films. Increasing the substrate temperature, barium multi titanate phases were decreased, and BST (100), (200) peaks were increased. The relative dielectric constant and dielectric loss of the BST thin films at the substrate temperature of $500^{\circ}C$ were 300 and 0.018, respectively at l[kHz]. In all films, the dielectric constants decreased. Dielectric losses increased as increasing the frequency. The switching voltage was 5V of the BST thin films at the substrate temperature of $500^{\circ}C$.

  • PDF

Structure and electrical properties of $BaTiO_3$ System Array Thick Films for Infrared Detector Device (적외선 감지 소자를 위한 $BaTiO_3$계 어레이 후막의 구조 및 전기적 특성)

  • Noh, Hyun-Ji;Nam, Sung-Pill;Lee, Sung-Gap;Kim, Dae-Yeong;Bae, Seon-Gi;Lee, Young-Hie
    • Proceedings of the Korean Institute of Electrical and Electronic Material Engineers Conference
    • /
    • 2009.06a
    • /
    • pp.180-181
    • /
    • 2009
  • $(Ba_{0.6},Sr_{0.3}Ca_{0.1})TiO_3$ powders, which were prepared by sol-gel method using a solution of Ba-acetate, Sr-acetate and Ca-acetate and Ti iso-propoxide, $(Ba_{0.6},Sr_{0.3}Ca_{0.1})TiO_3$ array thick films doped with 0.1 mol% $MnCO_3$ and $Yb_2O_3$ (0.1~0.7 mol%) were fabricated by the screen printing method on the alumina substrate. And the structural and electrical properties as a function of $Yb_2O_3$ amount were investigated. The thickness of all (Ba,Sr,Ca)$TiO_3$ thick films was approximately 60mm. The Curie temperature of doped with 0.1 mol% $Yb_2O_3$ specimen was $45^{\circ}C$, and the dielectric constant and at this temperature was 1062.

  • PDF

Effect of RTA on the interfacial Properties of Top Electrodes on $(Ba_{0.5}Sr_{0.5})TiO_3$ ($(Ba_{0.5}Sr_{0.5})TiO_3$ 박막의 상부전극 RTA에 따른 계면 특성 변화)

  • Jeon, Jang-Bae;Kim, Dyeok-Kyu;So, Soon-Jin;Park, Choon-Bae
    • Proceedings of the KIEE Conference
    • /
    • 1998.11c
    • /
    • pp.740-742
    • /
    • 1998
  • In this paper, we described the effect of rapid thermal annealing on the electrical properties of interfacial layer between various top electrodes and $(Ba_{0.5}Sr_{0.5})TiO_3$ thin films. BST thin films were fabricated on Pt/TiN/$SiO_2$/Si substrate by RF magnetron sputtering technique. AI, Ag, and Cu films for the formation of top electrode were deposited on BST thin films by thermal evaporator. Top electrodes/BST/Pt capacitor annealed with rapid thermal annealing at various temperature. In $(Ba_{0.5}Sr_{0.5})TiO_3$ thin films with Cu top electrode annealed at $500^{\circ}C$, the dielectric constant was measured to the value of 366 at 1.2 [kHz] and the leakage current was obtained to the value of $5.85{\times}10^{-7}\;[A/cm^2}$ at the forward bias of 2 [V].

  • PDF

Structureal and dielectric properties of $(Pb_{x},Sr_{x-1})TiO_{3}$ thin film for tunable device application (Tunable 소자 응용을 위한 $(Pb_{x},Sr_{x-1})TiO_{3}$ 박막의 구조 및 유전특성)

  • Kim, Kyoung-Tae;Kim, Chang-Il;Lee, Sung-Gap
    • Proceedings of the Korean Institute of Electrical and Electronic Material Engineers Conference
    • /
    • 2002.05b
    • /
    • pp.78-81
    • /
    • 2002
  • Ferroelectric thin film is a very attractive material for the tunable microwave device applications such as electronically tunable mixers, delay lines, filters and phase shifters. Thin films of $Pb_{x}Sr_{1-x}TiO3(PST)$ were fabricated onto Pt/Ti/SiO2/Si substrate by the sol-gel method. We have investigated the structural and dielectric properties of PST(50/50) thin films for tunable microwave device applications. The PST thin films show typical polycrystalline structure with a dense microstructure without secondary phase formation. Dielectric properties of PST films are strongly dependent on annealing temperature. The dielectric constants, loss and tunability of the PST (50/50) thin films were 404, 0.023 and 51.73 %, respectively.

  • PDF