The Effects of $SrTiO_3$ Addition on the Microstructure and Magnetic Properties of YIG (YIG ($Y_3$$Fe_5$O_{12}$)의 미세구조 및 자성 특성에 대한 $SrTiO_3$첨가 영향)

  • Jang, Hak-Jin;Yun, Seok-Young;Kim, Tae-Ok
    • Korean Journal of Materials Research
    • /
    • v.11 no.3
    • /
    • pp.203-206
    • /
    • 2001
  • The effects of SrTiO$_3$ addition and sintering temperature on the microstructure and magnetic properties of yttrium iron garnet (YIG) were investigated. The lattice Parameter increasing of sintered YlG with small amount of SrTiO$_3$ addition was supposed to be substituted $Y^{+3}$, Fe$^{+3}$ ions to Sr$^{+2}$,Ti$^{+4}$ ions which are relatively large in ionic ranius. A YIG specimen sintered at 142$0^{\circ}C$ with 0.2mol% SrTiO$_3$ showed above 98% densification of theoretical density. Saturation magnetization (M$_s$) at room temperature decreased a little bit with increasing SrTiO$_3$, addition but no great chance. In addition, the coercivity (H$_c$) was almost not changed by sintering temperature.

  • PDF

$A_{2-x}La_xFeMoO_6$(A=Ca and Ba)의 자기적 특성

  • Yang, Hyeon-Mo;Han, Hyeok;Lee, U-Yeong;Lee, Bo-Hwa
    • Proceedings of the Korean Magnestics Society Conference
    • /
    • 2002.12a
    • /
    • pp.86-87
    • /
    • 2002
  • Fe과 Mo이 교대로 정렬해 있는 이중 페로브스카이트 구조를 갖는 $A_{2-x}$FeMo $O_{6}$(A=Ca, Sr, Ba) 화합물들은 망간 산화물들에 비해 높은 $T_{c}$ (310-420K)의 준강자성 상태를 갖는다.$^{1.3}$ 이 화합물들은 F $e^{3+}$ (S=5/2) 와 M $o^{5+}$(S=1/2) 스핀들 사이의 커다란 반강자성 상호작용으로 이론적으로 4$\mu$$_{B}$/f.u.의 $M_{s}$ 값을 갖는다. A-site의 평균 이온 반경( $r_{A}$)이 증가함에 따라 이 화합물들의 결정구조는 Monoclinic(A=Ca)에서 Tetragonal(Sr)과 Cubic(Ba)으로 점진적으로 변화한다.$^3$(중략)(중략)략)략)

  • PDF

Ferroelectric Properties of Substituted Aurivillius Phases SrBi2Nb2-xMxO9 (M=Cr, Mo)

  • Moon, S.-Y.;Choi, K. S.;Jung, K. W.;Lee, H.;Jung, D.
    • Bulletin of the Korean Chemical Society
    • /
    • v.23 no.10
    • /
    • pp.1463-1482
    • /
    • 2002
  • Partially doped Aurivillius phases SrBi2N$b_{2-x}M_xO_9$ (M=Cr and Mo) were successfully synthesized and characterized. The extent of the substitution was limited at ~20 mole % because of the size differences between $Nb^{5+}$ and $Cr^{6+}$, and between $Nb^{5+}$ and $Mo^{6+}$. When the amount of substitution exceeded ~20 mole%, the phases began to collapse and the second phases were made. The dielectric constants of substituted compounds were enlarged nevertheless Cr or Mo is substituted. The increment is bigger in the Mo substituted compound than in the Cr doped one although the Nb(Cr)$O_6$ octahedra could be more strongly distorted than the Nb(Mo)$O_6$ octahedra since the ionic size difference between $Nb^{5+}$ and of $Cr^{6+}$ is much bigger than that between $Nb^{5+}$ and $Mo^{6+}$. Consequently, the dielectric constant of the substituted Aurivillius phase $Bi_2$A_{n-1}B_{n-x}M_xO_{3n+1}$$ depends on the extent of distortion of the B$O_6$ octahedra and more strongly on the polarizability of the metal.

Electrolyte Preparation and Characteristics of La1-xSrxMnO3 for Solid Oxide Fuel Cell (고체전해질형 연료전지용 전해질 제작 및 La1-xSrxMnO3의 특성에 관한 고찰)

  • Rim, Hyung-Ryul;Lee, Ju-Seong
    • Applied Chemistry for Engineering
    • /
    • v.7 no.1
    • /
    • pp.9-17
    • /
    • 1996
  • Solid oxide electrolytes of 8mol% YSZ($Y_2O_3$ stabilized zirconia) were prepared at various sintering conditions and their ionic conductivities were measured. The highest ionic conductivity of $10^{-1}S.cm^{-1}$ was obtained when the sintering temperature was 1400oC and the sintering time was 10hr. Also the cathode material, $La_{1-x}Sr_xMnO_3$ was prepared by solid state reaction method and the overpotential, electrical conductivity, and charge transfer resistance between cathode material and YSZ electrolyte were studied. It was found that the optimum doping content of Sr for La was 50mo1%.

  • PDF

Structural and Dielectric Properties of $Ba_{0.5}Sr_{0.5}TiO_3$ with Addition MgO (MgO의 첨가량에 따른 $Ba_{0.5}Sr_{0.5}TiO_3$의 구조적, 유전적 특성)

  • You, Hee-Wook;Ahn, Ho-Myoung;Koo, Sang-Mo;Nam, Song-Min;Lee, Young-Hie;Koh, Jung-Hyuk
    • Proceedings of the Korean Institute of Electrical and Electronic Material Engineers Conference
    • /
    • 2006.06a
    • /
    • pp.296-297
    • /
    • 2006
  • A conventional oxide method was used to fabricate $Ba_{0.5}Sr_{0.5}TiO_3$(BST) ceramic plates doped by MgO from 10 to 60 wt%. The structural and dielectric properties of BST were investigated as a fraction of MgO dopant concentration. The dielectric properties of the MgO doped BST were strongly dependent on the MgO contents. The dielectric constant and dielectric loss of MgO doped BST decreased with increasing MgO content.

  • PDF

Synthesis and Physical Properties of MO·Fe12O18 (M/Ba and Sr) Nanoparticles Prepared by Sol-Gel Method Using Propylene Oxide (Propylene Oxide를 이용한 졸-겔법에 의한 MO·Fe12O18 (M/Ba, Sr) 나노 분말의 합성과 물리적 특성)

  • Lee, Su Jin;Choe, Seok Burm;Gwak, Hyung Sub;Paik, Seunguk
    • Applied Chemistry for Engineering
    • /
    • v.17 no.4
    • /
    • pp.420-425
    • /
    • 2006
  • Nano sized mixed metal hexagonal ferrite powders with improved magnetic properties have been prepared by sol-gel method using propylene oxide as a gelation agent. To obtain the desired ferrite, two different metal ions were used. One of the ions has only +2 formal charge. The key step in the processes is that hydrated $Ba^{2+}$ or $Sr^{2+}$ ions are hydrolyzed and condensed at the surface of the previously formed $Fe_{2}O_{3}$ gel. In this processes, all the reaction can be finished within a few minutes. The magnetic properties of the produced powder were improved by heat treatment. The highest values of the magnetic properties were achieved at temperature $150^{\circ}C$ lower than those of the previously published values. The highest observed values of coercivity and the saturation magnetization of Sr-ferrite and Ba-ferrite powder were 6198 Oe, 5155 Oe and 74.4 emu/g, 68.1 emu/g, respectively. The ferrite powder annealed at $700^{\circ}C$ showed spherical particle shapes. The resulting spheres which were formed by the aggregation of nanoparticles with size 3~5 nm have diameter around 50 nm. The powder treated at $800^{\circ}C$ showed hexagonal-shaped grains with crystallite size above 500 nm.

Crystalline and electrical properties of ${Li_2}{CO_3}$ and MgO doped ${Ba_{0.5}}{Sr_{0.5}}{TiO_3}$ composites (${Li_2}{CO_3}$와 MgO가 첨가된 ${Ba_{0.5}}{Sr_{0.5}}{TiO_3}$의 결정학적 전기적 특성)

  • You, Hee-Wook;Park, Yong-Jun;Nam, Song-Min;Koo, Sang-Mo;Park, Jae-Yeong;Lee, Young-Hie;Koh, Jung-Hyuk
    • Proceedings of the KIEE Conference
    • /
    • 2006.10a
    • /
    • pp.3-4
    • /
    • 2006
  • ${Li_2}{CO_3}$ and MgO doped paraelectric ${Ba_{0.5}}{Sr_{0.5}}{TiO_3}$, materials were prepared and compared for LTCC applications. In these days LTCC (Low Temperature Co-fired Ceramics) technology has been widely employed for electronic modules for the communication systems such as front-end modules, antenna modules, and switching modules. In this paper, 1 ${\sim}$ 5 wt % of ${Li_2}{CO_3}$, and 30 wt % of MgO were added to ${Ba_{0.5}}{Sr_{0.5}}{TiO_3}$, respectively. The crystalline properties and electrical properties will be compared and discussed.

  • PDF

Direct Methanol Synthesis by Partial Oxidation of Methane (메탄의 부분산화에 의한 메탄올 직접 합성)

  • Kim, Young-Kook;Lee, Kwang-Hyeok;Hahm, Hyun-Sik
    • Journal of the Korean Applied Science and Technology
    • /
    • v.30 no.4
    • /
    • pp.649-655
    • /
    • 2013
  • Methanol was directly produced by the partial oxidation of methane with perovskite and mixed oxide catalysts. Perovskite ($ABO_3$) catalysts were prepared by the malic acid method with changing A and B site components. Three-component mixed oxide catalysts that have Mo and Bi as a main component were prepared by the co-precipitation method. Among the perovskite catalysts, $SrCrO_3$ showed the highest methanol selectivity of 11% at $400^{\circ}C$. For the three-component mixed oxide catalysts, there were no remarkable changes in methane conversion. Among the mixed oxide catalysts, Mo-Bi-Cr mixed oxide catalyst showed the highest methanol selectivity of 15.3% at $400^{\circ}C$. The catalytic activity and methanol selectivity of the three-component mixed oxide catalysts were directly proportional to the surface area of the catalysts.

The Enhanced Magnetic Transition Temperature in Double Perovskites A2FeMoO6 (A=Ca, Sr and Ba) : Electron Doping Effects

  • Kim J.;Yang H. M.;Lee B. W.
    • Journal of Magnetics
    • /
    • v.10 no.1
    • /
    • pp.10-13
    • /
    • 2005
  • We have studied effects of the partial substitution of $La^{3+}$ for $A^{2+}$ on the magnetic properties of double perovskites $A_2FeMoO_6$ (A=Ca, Sr and Ba). Polycrystalline $A_{2-x}La_xFeMoO_6(0{\leq}x{\leq}0.2)$ samples have been prepared by the conventional solid-state reaction in a stream of 5% $H_2$/Ar gas. The x-ray data indicate that A=Ca is monoclinic with the space group P$2_1$/n, A=Sr is tetragonal with the space group I4/mmm, and A=Ba is cubic with the space group Fm3m. The substitution of $La^{3+}$ for $A^{2+}$ results in a cell volume increase for A=Ca and a cell volume reduction for A=Ba. The decrease of saturation magnetization with increasing x arises from the reduction of magnetic moment associated with the electron doping and the disorder at the Fe and Mo sites. The partial substitution of magnetic $La^{3+}$ for $A^{2+}$ considerably enhances the Curie temperature $T_c$ from 316 K for x = 0 to 334 K for x = 0.2. This enhancement of $T_c$ with $La^{3+}$ doping originates from electron doping effects in addition to ionic size ones.