• Title/Summary/Keyword: $Pb(Mg_{1/3}Nb_{2/3})O_3 PbZrO_3$

Search Result 60, Processing Time 0.026 seconds

Electric aging phenomena of $0.2(PbMg_{1/3}Nb_{2/3}O_3)-0.8(PbZr_{0.475}Ti_{0.525}O_3)$ Multilayer Ceramic Actuators ($0.2(PbMg_{1/3}Nb_{2/3}O_3)-0.8(PbZr_{0.475}Ti_{0.525}O_3)$ 적층형 세라믹 액츄에이터의 전기적 열화 특성)

  • Koh, Jung-Hyuk;Jeong, Soon-Jong;Ha, Moon-Su;Lee, Dong-Man;Song, Jae-Sung
    • Proceedings of the Korean Institute of Electrical and Electronic Material Engineers Conference
    • /
    • 2003.05c
    • /
    • pp.219-222
    • /
    • 2003
  • $0.2(PbMg_{1/3}Nb_{2/3}O_3)-0.8(PbZr_{0.475}Ti_{0.525}O_3)$ 조성을 이용하여 $5{\times}5{\times}5mm^3$의 적층형 세라믹 액츄에이터 소자를 tape casting 방법으로 제작하였다. 전극재로서는 Ag-Pd를 이용하여 총 50층의 layer를 적층하였으며, 적층된 액츄에이터를 $1100^{\circ}C$의 온도에서 소결하였다. X-ray diffractometer를 이용하여 제작된 소자와 열화된 소자의 구조적인 특성을 분석하였다. 제작된 소자의 열화 특성을 알아보기 위하여 60 Hz 의 triangular wave를 인가하여 열화전과 후의 p-E hystcresis loop의 변화를 살펴보았으며, 인가된 전압의 변화에 따라서 소자에서 발생되는 양의 열을 측정하였다. 파괴된 소자의 파단면에 대한 SEM 분석을 통하여 소자의 파괴 메카니즘을 알아보도록 하였다. 이로부터 전기적 기계적 열화가 소자의 동작에 미치는 영향에 대해서 알아 보았다.

  • PDF

Microstructure and Electrical Properties of Pb[(Mg,Mn)Nb]O3-Pb(Zr,Ti)O3 Piezoelectric Ceramics

  • Kim, Jin-Ho;Kim, Jong-Hwa;Baik, Seung-Woo
    • Transactions on Electrical and Electronic Materials
    • /
    • v.6 no.5
    • /
    • pp.202-209
    • /
    • 2005
  • Phase evolution, microstructure and the electrical properties such as $k_p$ and $Q_m$ of $Pb(Mg_{1/3}Nb_{2/3})O_3[PMN]-Pb(Mn_{1/3}Nb_{2/3})O3[PM'N]-PbZrO_3[PZ]-PbTiO_3[PT]$ quaternary system were investigated within the compositional ranges $0{\leq}y{\leq}0.125$, y+z=0.125, and $0.39{\leq}x{\leq}0.54$ of the formula $Pb_{0.97}Sr_{0.03}[Mg_{1/3}Nb_{2/3})_y\;(Mn_{1/3}Nb_{2/3})_z\;(Zr_{x}Ti_{1-x})_{1-(y+z)}]O_3$. In the case of increasing Mn/(Mg+Mn) ratio for a fixed Zr/Ti ratio of 47.5/52.5, phase relation remained unchanged but the grain size drastically decreased, and the electrical properties changed as following: both $k_P$ and $Q_m$ reached the peak values at $Mn/(Mg+Mn)\cong0.3l7$ and gradually decreased; $\varepsilon33^T$ showed a monotonic decrease; P-E hysteresis loop gradually changed to asymmetrical one, and $E_i$ increased in correspondence. With increasing Zr/Ti ratio for a fixed Mn/(Mg+Mn) ratio of 0.317, on the contrary, the cell parameter $(\alpha^2c)^{1/3}$ gradually increased, and tetragonal-rhombohedral morphotropic phase boundary appeared in the range of $51/49{\leq}Zr/Ti{\leq}54/46$. the meantime, the grain size substantially increased, and the electrical properties changed as following: $k_P$ and $\varepsilon33^T$ reached peak values at Zr/Ti=51/49 and 48/52, respectively, and then gradually decreased; change of $Q_m$ was adverse to $k_P$; both $E_C\;and\;E_i$ considerably decreased while $P_S$ moderately increased. For the system 0.125(PMN+PM'N)-0.875PZT studied, the composition Mn/(Mg+Mn)=0.3l7 and Zr/Ti=51/49 revealed some promising electrical properties for piezoelectric transformer application such as $k_P=0.58,\;Q_m\cong1000$, and $\varepsilon^T_{33}=970$, as well as dense and fine-grained microstructure.

Piezoelectric and Dielectric Characteristics of Low Temperature Sintering Pb(Mg1/2W1/2)O3-Pb(Mn1/3Nb2/3)O3-Pb(Zr1/2Ti1/2)O3 Ceramics With the Substitution of Pb(Mg1/2W1/2)O3 (Pb(Mg1/2W1/2)O3 치환에 따른 저온소결 Pb(Mg1/2W1/2)O3-Pb(Mn1/3Nb2/3)O3-Pb(Zr1/2Ti1/2)O3 세라믹스의 압전 및 유전특성)

  • Yoo Ju-Hyun;Lee Hyun-Seok;Chung Kwang-Hyun;Jeong Yeong-Ho
    • Journal of the Korean Institute of Electrical and Electronic Material Engineers
    • /
    • v.19 no.5
    • /
    • pp.417-421
    • /
    • 2006
  • In this study, in order to develop low temperature sintering piezoelectric ceramics for LTCC (Low-Temperature Cofired Ceramic) multilayer piezoelectric actuator, PMW-PMN-PZT ceramics using $0.2wt%\; Li_2CO_3$ and $0.25wt%\;CaCO_3$ as sintering aids were investigated according to the varation of PMW substution. Composition ceramics could be sintered at $900^{\circ}C$ by adding sintering aids. As the amount of PMW substitution increased, the crystal structure of PMW-PMN-PZT ceramics moved from tetragonal phase to rhombohedral phase gradually, and MPB(Morphotrophic Phase Boundary) region appeared at 2 mol% PMW substitution. At the sintering temperature of $900^{\circ}C$, the density, electromechanical coupling factor(kp), mechanical quality factor(Qm), dielectric constant(${\epsilon}r$), piezoelectric constant(d33) and Curie temperature(Tc) of 2 mol% PMW substituted PMW-PMN-PZT ceramics showed the optimal values of $7.88g/cm^3$, 0.58, 1002, 1264, 352 pC/N and $336^{\circ}C$, respectively, for LTCC multilayer piezoelectric actuator application.

Dielectric and Piezoelectric Properties of Low Temperature Sintering PZN-PZT Ceramics with a variation of $Li_2CO_3$ Addition ($Li_2CO_3$ 첨가에 따른 저온소결 PZN-PZT 세라믹스의 유전 및 압전특성)

  • Lee, Yu-Hyong;Lee, Sang-Ho;Yoo, Ju-Hyun
    • Proceedings of the Korean Institute of Electrical and Electronic Material Engineers Conference
    • /
    • 2007.06a
    • /
    • pp.307-307
    • /
    • 2007
  • 압전액츄에이터 및 초음파진동자는 전자제품의 소형화 및 경량화, 의료기기, 모바일기기 및 소형로붓의 발전에 힘입어 그 활용범위가 넓게 확장되고 있다. 1960년 Smolenski등에 의해 $A(B_1,B_2)O_3$형 복합 페로브스카이트 구조를 갖는 강유전성 세라믹스에 대한 연구가 시작된 이래 $Pb(Co,Nb)O_3-Pb(Zr,Ti)O_3$, $Pb(Zn,Nb)O_3-Pb(Zr,Ti)O_3$, $Pb(Mg,Nb)O_3-Pb(Zr,Ti)O_3$ 등 3성분계 세라믹스의 유전, 압전 및 강유전 특성에 대한 많은 연구가 진행되어 왔다. 그러나 압전성이 우수한 세라믹스들은 Pb가 포함되어 있기 때문에 $1000^{\circ}C$ 이상에서 PbO가 급격하게 휘발되는 성질에 따라서 조성의 변동이 생겨 재현성이 어려우며 이를 방지하기 위하여 과잉 PbO를 첨가시키기 때문에 환경오염뿐만 아니라, 경제적인 측면에서도 많은 문제점을 가지고 있다. 소결조제를 이용한 산화물 첨가법은 PbO의 휘발을 억제하는 저온소결 방법중 가장 효과적인 방법으로 알려져 있다. 따라서, 본 연구에서는 적층형 압전액츄에이터로 사용하기위한 저온소결 압전세라믹스를 개발하기 위하여 PZN-PZT세라믹스에 $Li_2CO_3$, $Bi_2O_3$, CuO 를 소결조제로 사용하여 $Li_2CO_3$의 첨가량 변화에 따른 압전 및 유전 특성을 관찰하였다.

  • PDF

Piezoelectric Characteristics of Pb($Mg_{1/3}Nb_{2/3}$)$O_3$+ PZT Ceramics for Substrates of High-Frequency Devices (고주파소자의 기판용 Pb($Mg_{1/3}Nb_{2/3}$)$O_3$+ PZT 세라믹스의 압전특성)

  • 이개명;장낙원;김준한;이두희;박창엽
    • Proceedings of the Korean Institute of Electrical and Electronic Material Engineers Conference
    • /
    • 1990.10a
    • /
    • pp.60-64
    • /
    • 1990
  • In this studies, structural, dielectrical piezoelectrical properties and temperature stability of 0.05Pb(Pb($Mg_{1/3}Nb_{2/3}$)$O_3$+ 0.95Pb($Zr_{0.53}Tio_{0.47}$)$O_3$+$\alpha$[wt%] $Cr_2O_3$ piezoelectric ceramics fabricated by the Hot-Press method were investigated. And Poisson ratios of the specimens were measured in order to see that they can be used as the substrates for energy-trapped devices. The specimens of which Poisson ratio was more than 3/1 had the $\alpha$ range 0.3~0.75, and piezoelectric properties were degraded in the range $\alpha$$\geq$0.75, and temperature stability was good in the $\alpha$ range 0.5~0.75. Accordingly, the optimal point of $Cr_2O_3$ additive weight is sure to be in the vicinity of 0.5[wt%].

Mn-Modified PMN-PZT [Pb(Mg1/3Nb2/3)O3-Pb(Zr,Ti)O3] Single Crystals for High Power Piezoelectric Transducers

  • Oh, Hyun-Taek;Lee, Jong-Yeb;Lee, Ho-Yong
    • Journal of the Korean Ceramic Society
    • /
    • v.54 no.2
    • /
    • pp.150-157
    • /
    • 2017
  • Three types of piezoelectric single crystals [PMN-PT (Generation I $[Pb(Mg_{1/3}Nb_{2/3})O_3-PbTiO_3]$), PMN-PZT (Generation II $[Pb(Mg_{1/3}Nb_{2/3})O_3-Pb(Zr,Ti)O_3]$), PMN-PZT-Mn (Generation III)] were grown by the solid-state single crystal growth (SSCG) method, and their dielectric and piezoelectric properties were measured and compared. Compared to (001) PMN-PT and PMN-PZT single crystals, the (001) PMN-PZT-Mn single crystals exhibited a higher transition temperature between the rhombohedral and tetragonal phases ($T_{RT}=144^{\circ}C$), as well as a higher coercive electric field ($E_C=6.3kV/cm$) and internal bias field ($E_I=1.6kV/cm$). The (011) PMN-PZT-Mn single crystals showed the highest coercive electric field ($E_C=7.0kV/cm$), and the highest stability of $E_C$ and $E_I$ during 60 cycles of polarization measurement. These results demonstrate that both Mn doping (for higher electromechanical quality factor ($Q_m$)) and a (011) crystallographic orientation (for higher coercive electric field and stability) are necessary for high power transducer applications of these piezoelectric single crystals. Specifically, the (011) PMN-PZT-Mn single crystal (Gen. III) had the highest potential for application in the fields of SONAR transducers, high intensity focused ultrasound (HIFU), ultrasonic motors, and others.

$(Na,Li)NbO_3-BaTiO_3$세라믹스의 유전 및 압전 특성

  • Seong, Geum-Hyeon;Lee, Yu-Hyeong;Ryu, Ju-Hyeon;Jeong, Yeong-Ho
    • Proceedings of the Korean Institute of Electrical and Electronic Material Engineers Conference
    • /
    • 2009.11a
    • /
    • pp.77-77
    • /
    • 2009
  • $Pb(Zr,Ti_O_3$계 세라믹스는 우수한 압전 특성으로 인하여 압전변압기 및 액츄에이터, 센서 등 많은 분야에 응용이 되어져 왔다. 그러나, 최근 들어 $1000^{\circ}C$에서 급속도로 많은 휘발을 하는 PbO는 환경 및 인체에 나쁜 영향을 미칠 뿐 아니라 사용 후의 처리도 어려워 선진국에서는 사용을 제한하거나 줄이고 있는 추세에 있다. 따라서, PbO를 포함하지 않은 무연 (Lead-free)계 압전 세라믹스에 대한 연구가 많은 관심을 끌고 있으며 앞으로는E 장래성 있는 하나의 이슈 분야가 될 것이다. 이러한 Pb-based System 세라믹스를 대체 할 재료로서 $(Bi_{1/2}Na_{1/2})TiO_3$나 Tungsten-Bronze type, $(K_{1/2}Na_{1/2})NbO_3$ 등이 주로 연구가 되고 있다. 특히, alkali niobate를 기초로 한 $(K_{1/2}Na_{1/2})NbO_3(NKN)$은 무연 압전 물질로서 많은 주목을 받고 있다. 그러나, NKN의 주요 성분인 K 의 높은 조해성 때문에 일반적인 고상방법으로는 고 밀도의 세라믹을 얻기 힘들뿐더러 낮은 상전이 온도 때문에 많은 응용에는 제약이 되고 있다. 이러한 세라믹의 단점을 보완하고자 Hot forging, RTGG, SPS 등 과 같이 특수한 소결방법을 사용하여 고밀도의 세라믹을 제작하지만 이 방법들은 제품 대량 생산에 있어 경제적으로나 복잡한 제조과정을 고려할 때 매우 비효율적이라고 판단된다. 그러므로 $BaTiO_3$, $LiTaO_3$, Mg, Ca등을 첨가 시켜 소결을 향상시키고 고밀도를 얻기 위해 많은 연구가 진행 중이다. 따라서 본 연구에서는 Pb-based계의 세라믹스를 대체할 우수한 특성의 세라믹스를 제작하고자 기존의 $(K_{1/2}Na_{1/2})NbO_3(NKN)$세라믹스에서 낮은 용융온도 때문에 소결하기 어려운 $KNbO_3$를 제거한 $NaNbO_3$$LiNbO_3$$BaTiO_3$를 추가한 $NaLiNbO_3-BaTiO_3$세라믹스에 $K_4CuNb_8O_{23}$(KCN)을 첨가함으로서 이에 따른 압전 및 유전 특성을 조사하였다.

  • PDF

Effect of CuO Additions on Microstructures and Piezoelectric Properties of the 0.4Pb$(Mg_{1/3}Nb_{2/3})O_3-0.25PbZrO_3-0.35PbTiO_3$ Ceramics (CuO 첨가에 따른 0.4Pb$(Mg_{1/3}Nb_{2/3})O_3-0.25PbZrO_3-0.35PbTiO_3$ 세라믹스의 압전특성과 미세조직의 변화)

  • Jeon, So-Hyun;Kim, Min-Soo;Jeong, Soon-Jong;Kim, In-Sung;Song, Jae-Sung
    • Proceedings of the Korean Institute of Electrical and Electronic Material Engineers Conference
    • /
    • 2008.11a
    • /
    • pp.194-194
    • /
    • 2008
  • Lead oxide based ceramics, represented by PZT, are the most widely used materials for piezoelectric actuators, sensors, and transducers due to their excellent piezoelectric properties. In particular, high-performance multilayered piezoelectric ceramics for advanced electronic components have drawn great attention. In order to develop piezoelectric ceramics capable of being sintered at low temperature for multilayer piezoelectric device applications, the effect of CuO additions on the microstructures and electromechanical properties of the 0.4Pb$(Mg_{1/3}Nb_{2/3})O_3-0.25PbZrO_3-0.35PbTiO_3$ ceramics was investigated. The samples with CuO addition were synthesized by ordinary sintering technique. X-ray diffractions indicated that all samples formed a single phase perovskite structure. The addition of CuO improved the sinterability of the samples and caused an increase in the density and grain size at low temperature. The optimum sintering temperature was lowered by CuO additions. Excellent piezoelectric and electromechanical responses, $d_{33}$ ~ 663 pC/N, $k_p$ ~ 0.72, were obtained for the samples of high density with 0.1 wt% CuO addition sintered at $1050^{\circ}C$ for 4 h in air. These results show that the piezoelectric properties of PMNZT ceramics can be improved by controlling the microstructure and this system is potentially a good candidate as multilayer piezoelectric device for a wide range of electro-mechanical transducer applications.

  • PDF

Piezoelectric and strain characteristics of PMN-PT-PZ ceramics with Ba addition (Ba치환된 $Pb(Mg_{1/3}Nb_{2/3})O_3$-$PbTiO_3$-$PbZrO_3$계 세라믹스의 압전 및 변위특성에 관한 연구)

  • 지승한;이덕출;이능헌
    • Electrical & Electronic Materials
    • /
    • v.10 no.1
    • /
    • pp.20-25
    • /
    • 1997
  • In this study, piezoelectric actuator samples were fabricated using 0.375PMN-0.37OPT-0.255PZ system ceramics with Barium substitution and the strain properties of them were investigated. Dielectric constant of the specimens increased with the increase of Ba content up to 5mol% and decreased with futher addition of Ba. The largest piezoelectric coefficient and electromechanical coupling coefficient were observed at the sintering temperature of 1250'C and Barium content of 5mol%. The characteristics of strain hysteresis was found largely with varing the sintering temperature on the single round type, and the strain is proportional to piezoelectric coefficient.