• Title/Summary/Keyword: $NaGd(MoO_4)_2$

Search Result 3, Processing Time 0.026 seconds

Upconversion luminescence from poly-crystalline Yb3+, Er3+ co-doped NaGd(MoO4)2 by simple solid state method (Er3+, Yb3+ 이온이 동시 도핑된 NaGd(MoO4)2의 업컨버젼 분석)

  • Kang, Suk Hyun;Kang, Hyo Sang;Lee, Hee Ae;Shim, Kwang Bo
    • Journal of the Korean Crystal Growth and Crystal Technology
    • /
    • v.26 no.4
    • /
    • pp.159-163
    • /
    • 2016
  • Up-conversion (UC) luminescence properties of polycrystalline $Er^{3+}/Yb^{3+}$ doped $NaGd(MoO_4)_2$ phosphors synthesized by a simple solid-state reaction method were investigated in detail. Used to 980 nm excitation (InfraRed area), $Er^{3+}/Yb^{3+}$ co-doped $NaGd(MoO_4)_2$ exhibited very weak red emissions near 650 and 670 nm, and very strong green UC emissions at 540 and 550 nm corresponding to the infra 4f transitions of $Er^{3+}(^4F_{9/2},\;^2H_{11/2},\;^4S_{3/2}){\rightarrow}Er^{3+}(^4I_{15/2})$. The optimum doping concentration of $Er^{3+}$, $Yb^{3+}$ for highest emission intensity was determined by XRD and PL analysis. The $Er^{3+}/Yb^{3+}$ (10.0/10.0 mol%) co-doped $NaGd(MoO_4)_2$ phosphor sample exhibited very strong shiny green emission. A possible UC mechanism for $Er^{3+}/Yb^{3+}$ co-doped $NaGd(MoO_4)_2$ depending on the pump power dependence was discussed.

Microwave Sol-Gel Derived NaGd(MoO4)2:Ho3+/Yb3+ Phosphors and Their Upconversion Photoluminescence Properties

  • Lim, Chang Sung
    • Transactions on Electrical and Electronic Materials
    • /
    • v.18 no.6
    • /
    • pp.364-369
    • /
    • 2017
  • Double molybdate $NaGd_{1-x}(MoO_4)_2:Ho^{3+}/Yb^{3+}$ phosphors with proper doping concentrations of $Ho^{3+}$ and $Yb^{3+}$ ($x=Ho^{3+}+Yb^{3+}$, $Ho^{3+}=0$ and 0.05, and $Yb^{3+}=0$, 0.35, 0.40, 0.45, and 0.50) were successfully synthesized using the microwave sol-gel method. Well-crystallized particles formed after heat-treatment at $800^{\circ}C$ for 16 h showed fine and homogeneous morphologies with particle sizes of $1{\sim}3{\mu}m$. The spectroscopic properties were examined using photoluminescence emission and Raman spectroscopy. Under excitation at 980 nm, the upconversion doped samples exhibited strong yellow emissions, from the combination of strong emission bands at 545 nm and 655 nm in the green and red spectral regions, respectively. The strong 545 nm emission band in the green region corresponded to the $^5S_2/^5F_4{\rightarrow}^5I_8$ transition in the $Ho^{3+}$ ions, while the strong 655 nm band in the red region appeared because of the $^5F_5{\rightarrow}^5I_8$ transition in the $Ho^{3+}$ ions. The pump power dependence and the Commission Internationale de L'Eclairage chromaticity of the upconversion emission intensity were evaluated in detail.

Microwave Sol-Gel Derived Ho3+/Yb3+ Co-Doped NaCaGd(MoO4)3 Phosphors and their Upconversion Photoluminescence

  • Lim, Chang Sung
    • Journal of the Korean Ceramic Society
    • /
    • v.53 no.4
    • /
    • pp.456-462
    • /
    • 2016
  • $NaCaGd(MoO_4)_3:Ho^{3+}/Yb^{3+}$ ternary molybdates were successfully synthesized by microwave sol-gel method for the first time. Well-crystallized particles formed after heat-treatment at $900^{\circ}C$ for 16 h showed a fine and homogeneous morphology with particle sizes of $3-5{\mu}m$. Under excitation at 980 nm, the UC intensities of the doped samples exhibited strong yellow emissions based on the combination of strong emission bands at the 520-nm and 630-nm emission bands in the green and red spectral regions, respectively. The strong 520-nm emission band in the green region corresponds to the $^5S_2/^5F_4{\rightarrow}^5I_8$ transition of $Ho^{3+}$ ions, while the strong 630-nm emission band in the red region appears to be due to the $^5F_5{\rightarrow}^5I_8$ transition of the $Ho^{3+}$ ions. The optimal $Yb^{3+}:Ho^{3+}$ ratio was found at 9:1, as indicated by the composition-dependent quenching effect of $Ho^{3+}$ ions. The pump power dependence of the upconversion emission intensity and the Commission Internationale de L'Eclairage chromaticity coordinates of the phosphors were evaluated in detail.