• 제목/요약/키워드: $In_2O_3$

검색결과 30,463건 처리시간 0.061초

습식방법에 의한 $SnO_2$ 반도체 가스센사 제조 (Preparation of $SnO_2$ Semiconducting Gas Sensor by Wet Process)

  • 전병식;김홍대;최병현;최성근
    • 한국세라믹학회지
    • /
    • 제23권3호
    • /
    • pp.53-61
    • /
    • 1986
  • A gas sensor which has been made by wet process had fabricated by coating each of the mixture on alumina tube and firing at 85$0^{\circ}C$ for 3hrs. A gas concentration such $H_2$, CO, $C_3H_8$, $C_2H_2$ and $CH_4$ vs its detection voltage characteristics has been in-vestigated on $SnO_2-In_2O_3-MgO$ system doped with PdO, $La_2O_3$, $ThO_2$, NiO and $Nb_2O_5$ The optimum sensitivity composition for various gases were 90w/o $SnO_2$-9w/o $In_2O_3$-1w/o MgO for $H_2$, $C_2H_2$ CO and $C_3H_8$ and 95w/o $SnO_2$-4w/o $In_2O_3$-1w/o MgO for $CH_4$. The sample which has been made by wet process than dry process had predominated sensitivity for each gases and particle size of the sample coprecipitated with PH=9 was 0.1${\mu}{\textrm}{m}$ The $SnO_2$-In2_O_3-MgO$ system doped with 2w/o $Nb_2O_5$ and NiO was the most sensitive for $H_2$ and $C_2H_2$ gas. In $SnO_2$-In2_O_3-MgO$ system doped with $ThO_2$ the sensitivity of $H_2$ gas was decreased but CO gas was in-creased when dopant con was increased.

  • PDF

$[BaTiO_3]_{0.9}+[BaZrO_3, SnO_2, La_2O_3, ZrO_2]_{0.1}$의 Dielectric Properties 및 Temperature Characteristics에 미치는 $Bi_2O_3$의 영향 (Effect of $Bi_2O_3$ on Dielectric Properties and Temperature Characteristics of $[BaTiO_3]_{0.9}+[BaZrO_3, SnO_2, La_2O_3, ZrO_2]_{0.1}$)

  • 이병하;이경희;윤영호;손상철;유광수
    • 한국세라믹학회지
    • /
    • 제30권5호
    • /
    • pp.397-403
    • /
    • 1993
  • Widely used dielectrics, barium titanate was promising material for ceramic capacitor. It was produced by specific formulation with various dopants-La2O3, ZrO2, SnO2, CaZrO3, CaTiO3, CaSnO3, Bi2O3, and etc.-according to demanded properties of capacitor. In this study, we would examinate the study of dielectric properties and temperatuer characteristics (T.C.) with the amount of Bi2O3. The sample was prepared with [BaTiO3]10+[BaZrO3, SnO2, La2O3, ZrO2]10 and Bi2O3 varied from 1.0, 1.5, 2.0, 2.5 to 3.0wt%. After milling and mixing for 15hrs, each sample was dried and then pressed at 700kg/$\textrm{cm}^2$ into pellets. Pellets were fired at 131$0^{\circ}C$, for 3hrs in air. As the result of measurements, dielectric constant, break down voltage, and insulation resistance were increased with the amount of Bi2O3, and the resonant frequency was shifted from high frequency to low frequency range. In the case of temperature characteristics, capacitance change rate was symmetrically changed at -$25^{\circ}C$ and +85$^{\circ}C$ respectively. Therefore, it is recognized that the temperature characteristics can be moderated with doping Bi2O3 in our study.

  • PDF

Pb(Ni1/3Nb2/3)O3-PbTiO3-PbZrO3계의 삼방정, 정방정 및 상경계조성에서의 MnO2 첨가에 따른 유전 및 압전특성에 비교 (Comparisons on Dielectric and Peizoelectric Proeprties of Rhombohedral, Tetragonal and Morphotropic Phase Boundary in Pb(Ni1/3Nb2/3)O3-PbTiO3-PbZrO3 System with MnO2 Addition)

  • 전구락;손정호;김정주;조상희
    • 한국세라믹학회지
    • /
    • 제25권5호
    • /
    • pp.488-494
    • /
    • 1988
  • Effects of MnO2 addition on themicrostructure, dielectric and piezoelectric properties of Rhombohedral, Tetragonal and Morphotropic phase boundary(MPB) in Pb(Ni1/3Nb2/3)O3-PbTiO3-PbZrO3 system were investigated and respectively the amount of MnO2 addition was 0, 0.2, 0.5, 1.0, 3.0wt%. In the tetragonal region, compared with the Rhombohedral and Morpotropic phase boundary, Mechanical quality factor(Qm), Curie temperature(Tc) and Dissipation factor were promoted by addition of MnO2. According to the results of the microstructure, dielectric and piezoelectric properties, the solid solution range of MnO2 addition in this system was 0.2-0.5wt%.

  • PDF

Preparation of YBCO with additives of PbO, $BaPbO_3$ and its Superconducting Properties

  • Zhanguo, Fan;Soh, Dae-Wha
    • 동굴
    • /
    • 제78호
    • /
    • pp.17-22
    • /
    • 2007
  • The melting temperature and critical temperature (Tc) of $YBa_2Cu_3O_x$ with deferent content impurities of PbO and $BaPbO_3$ were studied. When the PbO was used as addition in $YBa_2Cu_3O_x$, although the melting point could be reduced, the superconductivity (the transition wide, ${\Delta}T_c$) became poor. From the XRD pattern of the sintered mixture of $YBa_2Cu_3O_x$ and PbO it was known that there is a reaction between $YBa_2Cu_3O_x$ and PbO, and the product is $BaPbO_3$. In the process of the reaction the superconducting phase of $YBa_2Cu_3O_x$ was decreased and in the sample $BaPbO_3$ became the main phase. Therefore the superconductivity was reduced. $BaPbO_3$ was chosen as the impurity for the comparative study. The single phase $BaPbO_3$ was synthesized by the simple way from both mixtures of $BaCO_3$ and PbO, $BaCO_3$ and $PbO_2$. Deferent contents of $BaPbO_3$ (10%, 20%, 30%) were added in the $YBa_2Cu_3O_x$. By the phase analysis in the XRD patterns it was proved that there were not reactions between $YBa_2Cu_3O_x$ and $BaPbO_3$. When $BaPbO_3$ was used as impurity in $YBa_2Cu_3O_x$ the superconductivity was much better than PbO as impurity in $YBa_2Cu_3O_x$. But the melting point of $YBa_2Cu_3O_x$ with $BaPbO_3$ could not be found when the temperature was lower than $1000^{\circ}C$ in the DTA measurement.

정극 재료용 $LiO_2-P_2O_5-Bi_2O_3-V_2O_5$ 유리의 결정화 특성 (Crystallization properties of $LiO_2-P_2O_5-Bi_2O_3-V_2O_5$ Glass for cathod material)

  • 손명모;이헌수;구할본;정인성
    • 한국전기전자재료학회:학술대회논문집
    • /
    • 한국전기전자재료학회 2000년도 영호남학술대회 논문집
    • /
    • pp.311-315
    • /
    • 2000
  • Vanadate glass in the $LiO_2-P_2O_5-Bi_2O_3-V_2O_5$ system containing 10mol% glass fonner, $P_2O_5$ and $Bi_2O_3$ was prepared by melting the batch in pt. crucible followed by Quenching on the copper plate. We found that $LiO_2-P_2O_5-Bi_2O_3-V_2O_5$ glass-ceramics obtained from nucleation of glass showed signifieantly higher capacity and longer cycle life than conventionally made crystalline $LiV_3O_{8}$. In the present paper, we describe the charge / discharge properties during crystallization process and find the best crystallization condition of $LiO_2-P_2O_5-Bi_2O_3-V_2O_5$ glass as cathod material.

  • PDF

단결정 MgO와 분말 $Fe_2O_3$간의 고상 반응 연구 (The Study on Solid-State Reaction Between MgO Single Crystal and $Fe_2O_3$ Powder)

  • 김성재;박재우
    • 한국세라믹학회지
    • /
    • 제32권2호
    • /
    • pp.234-238
    • /
    • 1995
  • MgFe2O4 formation, grain growth in Fe2O3, Fe solid-solution limit in MgO for MgO-Fe2O3 mixture were studied by means of investigating the distribution of phases and compositions in reaction area between MgO and Fe2O3. The reaction area at equlibrium was composed with MgO-FexO matrix and MgFe2O4 precipitation, MgFe2O4 was formed by precipitating from MgO-FexO matrix dependent on oxygen partial pressure. Fe contents was exponentially decreased with diffusion distance in MgO single crystal, and thus Fe solid-solution limitation in MgO was about 4mol%. The grain growth rate in Fe2O3 base was increased with Mg contents diffused from MgO single crystal.

  • PDF

${AI_2}{O_3}$/ AI 및 ${SnO_2}-{AI_2}{O_3}$/AI박막습도 센서에 관한 연구 (A Study on the ${AI_2}{O_3}$/ and ${SnO_2}-{AI_2}{O_3}$/AI Thin Film Humidity Sensors)

  • 전춘생
    • 한국재료학회지
    • /
    • 제4권2호
    • /
    • pp.159-165
    • /
    • 1994
  • 순수한 알루미늄을 양극산화한 $AI_2O_3/AI$ 소자 및 그 위에$SnO_2$를 증착, 소자를 제작하여 그들의 전기적인 특성을 여러 습도 분위기 중에서 조사하였다. 단위습도당의 표면저항 변화는 $AI_2O_3/AI$ 소자에서는 $1.40 \times 10^{-2}\Omega$ /RH이었다. 두 소자는 습도에 따른 표면저항 변화중에서 hysteresis현상을 나타내고 있지만, $SnO_2-AI_2O_3/Al$ 소자쪽이 더 작은 hysteresis현상을 나타내었다. $SnO_2-AI_2O_3/Al$ 소자에 있어서 표면저항에 대한 온도의존성은 40-$60^{\circ}C$에서 $2.50 \times 10^{-2} \Omega /^{\circ}C$인것에비해 0~$20^{\circ}C$에서는 $0.56 \times 10^{-2} \Omega /^{\circ}C$와 같이 적기 때문에 $SnO_2-AI_2O_3/Al$ 소자는 실온영역에서 습도센서로 쓸 수 있다고 결론할 수 있다.

  • PDF

NiO-ZnO-$Fe_2O_3$-$TiO_2$-$SnO_2$ 계 Spinel 고용체의 생성과 발색에 관한 연구 (Formation and Color of the Spinel Solid Solution in NiO-ZnO-$Fe_2O_3$-$TiO_2$-$SnO_2$ System)

  • 이응상;이진성
    • 한국세라믹학회지
    • /
    • 제28권4호
    • /
    • pp.305-314
    • /
    • 1991
  • This study was conducted to research the formation and the color development of NiO-ZnO-Fe2O3-TiO2-SnO2 system for the purpose of synthesizing the spinel pigments which are stable at high temperature. After preparing ZnO-Fe2O3 as a basic composition, {{{{ chi }}NiO.(l-{{{{ chi }})ZnO.Fe2O3 system, {{{{ chi }}NiO.(l-{{{{ chi }})ZnO.TiO2 system, and {{{{ chi }}NiO.(l-{{{{ chi }})ZnO.SnO2 system were prepared with {{{{ chi }}=0, 0.2, 0.5, 0.7, 1 mole ratio respectively. The manufacturing was carried out at 128$0^{\circ}C$ for 30 minutes. The reflectance measurement and the X-ray analysis of these specimens were carried out and the results were summarized as follows. 1. In the specimens which included NiO, it was difficult for the spinel structure to be formed. 2. As increasing the contents of NiO and Fe2O3, all the groups which were yellow or green colored changed to brown. 3. NiO-ZnO-Fe2O3 system and NiO-ZnO-TiO2 system formed the spinel structure and the illmenite structure appeared in NiO-TiO2 system.

  • PDF

A Novel Method for Preparing of Oxoruthenates Complexes: trans-[RuO3(OH)2]2-, [RuO4]-, (n-Pr4N)+[RuO4]- and [RuO4 and Their Use as Catalytic Oxidants

  • Shoair, Abdel-Ghany F.
    • Bulletin of the Korean Chemical Society
    • /
    • 제26권10호
    • /
    • pp.1525-1528
    • /
    • 2005
  • The synthesis and characterization of ${K_3[Ru(C_2O_4)3]{\cdot}4H_2O\;(C_2O_4}^{2-}$ = oxalato anoin) complex are described, and its redox properties (in buffer solution of pH = 12) have been investigated. This complex is used for in situ generation of oxoruthenates complexes which have been characterized by electronic spectroscopy. Reaction of ${K_3[Ru(C_2O_4)3]{\cdot}4H_2O$ with excess ${S_2O_8}^{2-}$ in molar KOH generates trans-${[RuO_3(OH)_2]^{2-}/S_2O_8}^{2-}$ reagent while with excess ${BrO_3}^-$ in molar $Na_2CO_3$ generates ${[RuO_4]^-/BrO_3}^-$ reagent. Avoiding the direct use of [$RuO_4$] the organic-soluble $(n-Pr_4N)^+[RuO_4]^-$, (TPAP) has been isolated by reaction of $K_3[Ru(C_2O_4)3]{\cdot}4H_2O$ with excess ${BrO_3}^-$ in molar carbonate and n-$Pr_4$NOH. In a mixture of $H_2O/CCl_4$ ruthenium tetraoxide can be generated by reaction of $K_3[Ru(C_2O_4)3]{\cdot}4H_2O$ with excess ${IO_4}^-$. The catalytic activities of oxoruthenates that have been made from $K_3[Ru(C_2O_4)3]{\cdot}4H_2O$ towards the oxidation of benzyl alcohol, piperonyl alcohol, benzaldehyde and benzyl amine at room temperature have been studied.

Self-cleaning Properties of TiO2-SiO2-In2O3 Nanocomposite Thin Film

  • Eshaghi, Akbar;Eshaghi, Ameneh
    • Bulletin of the Korean Chemical Society
    • /
    • 제32권11호
    • /
    • pp.3991-3995
    • /
    • 2011
  • $TiO_2-SiO_2-In_2O_3$ nanocomposite thin film was deposited on the glass substrates using a dip coating technique. The morphology, surface composition, surface hydroxyl groups, photocatalytic activity and hydrophilic properties of the thin film were investigated by AFM, XPS, methyl orange decoloring rate and water contact angle measurements. The hydroxyl content for $TiO_2$, $TiO_2-SiO_2$ and $TiO_2-SiO_2-In_2O_3$ nanocomposite films was calculated to be 11.6, 17.1 and 20.7%, respectively. $TiO_2-SiO_2-In_2O_3$ film turned superhydrophilic after 180-min irradiation with respect to pure $TiO_2$ and $TiO_2-SiO_2$ thin films. The photocatalytic decomposition of methyl orange for $TiO_2$, $TiO_2-SiO_2$ and $TiO_2-SiO_2-In_2O_3$ thin films was measured as 38.19, 58.71 and 68.02%, respectively. The results indicated that $SiO_2$ and $In_2O_3$ had a significant effect on the hydrophilic, photocatalytic and self-cleaning properties of $TiO_2$ thin film.