• Title/Summary/Keyword: $Fe_3O_4$ concentration

Search Result 370, Processing Time 0.026 seconds

Influence of Reduction Atmosphere and Temperature on the Separability and Distribution Behavior of Fe from FeTiO3 via Sulfurization (고온 황화반응에 의한 FeTiO3로부터 Fe의 분리성과 분배거동에 미치는 환원/황화 분위기 및 온도의 영향)

  • Shin, Seung-Hwan;Kim, Sun-Joong
    • Resources Recycling
    • /
    • v.28 no.3
    • /
    • pp.45-52
    • /
    • 2019
  • $TiO_2$ as a raw material for producing titanium can be produced by carbon reduction of natural ilmenite ores over 1823 K and acid leaching of the obtained titanium-rich slag. However, the conventional process can cause very high energy consumption and a large amount of leaching residues. In the present study, we proposed the sulfurization of $FeTiO_3$ with $Na_2SO_4$ at temperatures below 1573 K, which can separate Fe in $FeTiO_3$ as the FeS based sulfide phase and Ti as the $TiO_2-Na_2O$ based oxide phase. This study is a fundamental study for sulfurization of $FeTiO_3$ to investigate the influence of reducing atmosphere, reaction temperature and the sulfur/Fe ratio on the separability and distribution behaviors of of Fe, Ti, and Na between the oxide phase and the sulfurized phase. At 1573 K and carbon saturation condition, the Fe can be separated from $FeTiO_3$ as Fe-C-S metal and a part of FeS, and the concentration of Fe in oxide decreased to 4 mass% after sulfurization.

Effect of Fe(NO3)2 Concentration on Electrochemical Behavior of SCM430 in Zinc Phosphate Conversion Coating Solution (아연계 인산염 피막용액에서 Fe(NO3)2 농도가 SCM430 합금의 전기화학적 거동에 미치는 영향)

  • Kwon, Duyoung;Song, Pung-Keun;Moon, Sungmo
    • Journal of the Korean institute of surface engineering
    • /
    • v.52 no.4
    • /
    • pp.233-238
    • /
    • 2019
  • The formation behavior of zinc phosphate conversion coating (ZPCC) on SCM430 alloy was investigated in 25 vol.% of 1M ZnO + 170 ml/L solution containing various $Fe(NO_3)_2$ concentrations, using open-circuit potential(OCP), electrochemical impedance spectroscopy(EIS), cyclic polarization(CP) curve and tape peel test. OCP of SCM430 alloy and corrosion current density increased with increasing $Fe(NO_3)_3$ concentration. Resistance of films formed on SCM430 alloy by chemical conversion treatment decreased with increasing $Fe(NO_3)_3$ concentration. Color and adhesion of chemical conversion coatings became darker and worse, respectively, with increasing $Fe(NO_3)_3$ concentration. It is concluded that addition of $Fe(NO_3)_3$ into a zinc phosphating bath leads to faster reaction to form porous surface coatings with poor adhesion and corrosion resistance.

Degradation of toxic azo dye (AO7) using Fenton's process

  • Sharma, Ashish;Verma, Manisha;Haritash, A.K.
    • Advances in environmental research
    • /
    • v.5 no.3
    • /
    • pp.189-200
    • /
    • 2016
  • This study aimed at advanced oxidation of hetero tri-functional reactive dye Acid orange 7 using photo-Fenton conditions in a lab-scale experiment. Decolourisation of Acid Orange 7 dye by Fenton's process was dependent on concentration of Hydrogen peroxide, Ferrous sulphate, pH, and contact time. A $2^3$ factorial design was used to evaluate the effects of these key factors: pH, Fe(II), and $H_2O_2$ concentration, for a dye concentration of 50 mg/L with COD of 340 mg/L at pH 3.0. The response function was removal of colour under optimised conditions; pH 3.0, [Fe(II)] 40.83 mg/L, [$H_2O_2$] 4.97 mmol/L; 13.6 min. of treatment resulting in 100% colour removal. The final COD of treated wastewater was nil suggesting that AOP is a potentially useful process of color removal and dye degradation/mineralisation of effluent having AO7. Minimum contact time for complete decolourisation was at 5 mmol/l $H_2O_2$ concentration. Increase in $FeSO_4$ (mg/l) concentration resulted in decrease of time for complete decolourisation. Box-Behnken Design was used to optimize the process variables. Maximum and minimum levels of pH (3-5), $H_2O_2$ (4-6 mmol/l), $FeSO_4$ (30-46 mg/l) and contact time (5-15 minutes) were used. The statistical analysis revealed a value of 0.88 for coefficient of regression ($R^2$) indicating a good fit of model. Calculated F-value was found higher than the tabulated value confirming to significance of the model. Based on student's t-test, Ferrous sulphate, pH, and contact time have a positive effect on the percent decolourisation of Acid Orange 7.

The Preparation of Magnetic Chitosan Nanoparticles with GABA and Drug Adsorption-Release (GABA를 담지한 자성 키토산 나노입자 제조와 약물의흡수 및 방출 연구)

  • Yoon, Hee-Soo;Kang, Ik-Joong
    • Korean Chemical Engineering Research
    • /
    • v.58 no.4
    • /
    • pp.541-549
    • /
    • 2020
  • The Drug Delivery System (DDS) is defined as a technology for designing existing or new drug formulations and optimizing drug treatment. DDS is designed to efficiently deliver drugs for the care of diseases, minimize the side effects of drug, and maximize drug efficacy. In this study, the optimization of tripolyphosphate (TPP) concentration on the size of Chitosan nanoparticles (CNPs) produced by crosslinking with chitosan was measured. In addition, the characteristics of Fe3O4-CNPs according to the amount of iron oxide (Fe3O4) were measured, and it was confirmed that the higher the amount of Fe3O4, the better the characteristics as a magnetic drug carrier were displayed. Through the ninhydrin reaction, a calibration curve was obtained according to the concentration of γ-aminobutyric acid (GABA) of Y = 0.00373exp(179.729X)-0.0114 (R2 = 0.989) in the low concentration (0.004 to 0.02 wt%) and Y = 21.680X-0.290 (R2 = 0.999) in the high concentration (0.02 to 0.1 wt%). Absorption was constant at about 62.5% above 0.04 g of initial GABA. In addition, the amount of GABA released from GABA-Fe3O4-CNPs over time was measured to confirm that drug release was terminated after about 24 hr. Finally, GABA-Fe3O4-CNPs performed under the optimal conditions were spherical particles of about 150 nm, and it was confirmed that the properties of the particles appear well, indicating that GABA-Fe3O4-CNPs were suitable as drug carriers.

Removal of Copper Ion with Iron-Oxide-Coated Sand (산화철 피복사에 의한 구리이온제거)

  • 곽명화;우성훈;김익성;박승조
    • Resources Recycling
    • /
    • v.9 no.1
    • /
    • pp.70-75
    • /
    • 2000
  • The sand particle was coated with $Fe_3O_4$ and then $Fe_2O_3$ that adsorption capacity was more excellent than $Fe_3O_4$ was mostly found in 2nd step for preparation of iron-oxide-coated sand (IOCS). The copper removal rate was 74.9 percent by adding 30 gram per liter iron-oxide-coated sand from the solution with 5 mg/l Cu in 20 minute. Breakthrough time occurred in 23 hours and adsorption capacity 0.87$\cdot$Cu/g$\cdot$IOCS in case of breakthrough copper concentration was 1.0 mg/l in the continuous test.

  • PDF

Growth and defect structures of undoped and heavily MgO-doped LiNbO3 single crystals (Undoped and heavily MgO-doped $LiNbO_3$ 결정의 성장 및 결함구조)

  • 김상수
    • Journal of the Korean Crystal Growth and Crystal Technology
    • /
    • v.9 no.5
    • /
    • pp.447-453
    • /
    • 1999
  • Congruent $LiNbO_3$ crystals with doped Mg and codoped with Mn or Fe were grown by the Czochralski method. It is known that the physical properties of $LiNbO_3$ depend strongly on the addition of Mg and transition metals. This is established by studying the following properties; XRD patterns, the phase transition temperature, energy of the fundamental absorption edge, the shape of the absorption band of the $OH^-$ vibration and lines of the ESR of $Fe^{3+},\; Mn^{2+}$. The position of the UV absorption edge and the shape and peak point of the absorption band of the $OH^-$ vibrational band changed monotonously up to a critical concentration of $Mg^{2+}$ ions. The mechanism of the incorporation of Mg ions changes at this concentration. The transition temperature was estimated by measuring the dielectric temperature behavior up to $1230^{\circ}C$ in a frequency range of 100Hz to 10MHz. EPR of $Mn^{2+}\;and\; Fe^{3+}$ ions were employed to investigated the Mg doping effects in the $LiNbO_3$ crystal. The increase of linewidths and the asymmetry of signals were observed in all crystals. New signals of $Fe^{3+}$ arising from the new centers were observed I the heavily Mg-doped crystals.

  • PDF

High Temperature Oxidation of Ti-6Al-4V, Ti-4Fe, Ti-(1,2)Si Alloys (Ti-6Al-4V, Ti-4Fe, Ti-(1,2)Si합금의 고온산화)

  • 박기범;이동복
    • Journal of the Korean institute of surface engineering
    • /
    • v.34 no.2
    • /
    • pp.135-141
    • /
    • 2001
  • Arc-melted Ti-6Al-4V, Ti-4Fe and Ti-(1,2) Si alloys were oxidized at 700, 800, 900 and $1000^{\circ}C$ in air. The oxidation resistance of Ti-4Fe was comparable to that of Ti-6Al-4V, while the oxidation resistance of Ti-(1,2) Si was superior to that of Ti-6Al-4V. Ti-2Si displayed the best oxidation resistance among the four alloys, but failed after oxidation at $1000^{\circ}C$ for 17h. The oxide scale formed on Ti-6Al-4V, Ti-4Fe and Ti-(1,2)Si consisted of ($TiO_2$ and a small amount of $Al_2$$O_3$), ($TiO_2$ and a small amount of dissolved iron), and ($TiO_2$ plus a small concentration of amorphous $SiO_2$), respectively. The oxide grains of the surface scale of the four alloys were generally fine and round.

  • PDF

A Stud on the Catalytic Removal of Nitric Oxide (질소산화물의 촉매반응에 의한 저감기술에 관한 연구)

  • 홍성수;박종원;정덕영;박대원;조경목;오광중
    • Journal of Korean Society for Atmospheric Environment
    • /
    • v.14 no.1
    • /
    • pp.25-33
    • /
    • 1998
  • We have studied the reduction of NO by propane over perovskite-type oxides prepared by malic acid method. The catalysts were modified to enhance the activity by substitution by substitution of metal into A or B site of perovskite oxides. In addition, the reaction conditions, such as temperature, $O_2$ concentration, space velocity have been studed. In the $LaCoO_3$ type catalyst, the partial substitution of Ba, Sr into A site enhanced the catalytic activity in the reduction of NO. In the $La_{0.6}Sr_{0.4}Co_{1-x}Fe_xO_3(x=0 \sim 1.9)$ catalyst, the partial substitution of Fe into B site enhanced the conversion of NO, but excess amount of Fe decreased the conversion of NO. The surface area and catalytic activity of perovskite catalysts prepared by malic acid method showed higher values than those of solid reaction method. In the $La_{0.6}Sr_{0.4}Co_{1-x}Fe_xO_3$ catalyst, the conversion of NO increased with increasing $O_2$ concentration and contact time. The introduction of water into reactant feed decreased the catalytic activity.

  • PDF

Determination of Hydroperoxyl/superoxide Anion Radical (HO2·/O2·-) Concentration in the Decomposition of Ozone Using a Kinetic Method

  • Kwon, Bum-Gun;Lee, Jai H.
    • Bulletin of the Korean Chemical Society
    • /
    • v.27 no.11
    • /
    • pp.1785-1790
    • /
    • 2006
  • A novel kinetic method for determination of $HO_2{^{\cdot}}/O_2{^{{\cdot}-}}$ in ozone decomposition in water is described. In this study, potential interferences of $O_3$ and the hydroxyl radicals, $^{\cdot}OH_{(O3)}$, are suppressed by $HSO_3{^-}/SO_3{^{2-}}$. $HO_2{^{\cdot}}/O_2{^{{\cdot}-}}$ formed in ozone decomposition reduces $Fe^{3+}$-EDTA into $Fe^{2+}$-EDTA and subsequently the well-known Fenton-like (FL) reaction of $H_2O_2$ and $Fe^{2+}$-EDTA produces the hydroxyl radicals, $^{\cdot}OH_{(FL)}$. Benzoic acid (BA) scavenges $^{\cdot}OH_{(FL)}$ to produce OHBA, which are analyzed by fluorescence detection (${\lambda}_{ex}=320nm$ and ${\lambda}_{ex}=400nm$). The concentration of $HO_2{^{\cdot}}/O_2{^{{\cdot}-}}$ in ozone decomposition has been determined by the novel kinetic method using the experimentally determined half-life ($t_{1/2}$). The steady-state concentration of $HO_2{^{\cdot}}/O_2{^{{\cdot}-}}$ is proportional to the $O_3$ concentration at a given pH. However, the steady-state concentration of $HO_2{^{\cdot}}/O_2{^{{\cdot}-}}$ in ozone decomposition is inversely proportional to pH values. This pH dependence is due to significant loss of $O_2{^{{\cdot}-}}$ by $O_3$ at higher pH conditions. The steady-state concentrations of $HO_2{^{\cdot}}/O_2{^{{\cdot}-}}$ are in the range of $2.49({\pm}0.10){\times}10^{-9}M(pH=4.17){\sim}3.01({\pm}0.07){\times}10^{-10}M(pH=7.59)$ at $[O_3]_o=60{\mu}M$.

The Study on the Change of Iron Concentration and the Reaction Mechanism of the 1,4-Dioxane Degradation using Zero Valent Iron and UV (영가철(Fe$^0$)과 UV를 이용한 1,4-dioxane 분해 반응시 철농도의 변화와 반응 메커니즘의 연구)

  • Son, Hyun-Seok;Im, Jong-Kwon;Zoh, Kyung-Duk
    • Journal of Korean Society of Environmental Engineers
    • /
    • v.30 no.3
    • /
    • pp.323-330
    • /
    • 2008
  • The study presents the results of 1,4-dioxane degradation using zero valent (Fe$^0$) or Fe$^{2+}$ ions with and without UV. During the reaction, the change of [Fe$^{2+}$] and [Fe$^{2+}$]/[Fe(t)], the concentration ratio of ferrous ion to total iron ion in solution was measured. Less than 10% degradation of 1,4-dioxane was observed by UV-only, Fe$^0$-only, and Fe$^{2+}$-only conditions, and also the changes of [Fe$^{2+}$] and [Fe$^{2+}$]/[Fe(t)] were minimal in each reaction. However, the oxidation of Fe$^0$ was enhanced with the irradiation of UV by approximately 25% and the improvement of 1,4-dioxane degradation was observed. Fenton reaction ($Fe^{2+}+H_2O_2$) showed higher degradation efficiency of 1,4-dioxane until 90 min, which of the degradation was stopped after that time. In the reaction of Fe$^{2+}$ and UV, the ratio of [Fe$^{2+}$]/[Fe(t)] decreased then slowly increased after a certain time indicating the reduction of Fe3+ to Fe$^{2+}$. In case of Fe$^0$ in the presence of UV, the first-order rate constant was found to be 1.84$\times$10$^{-3}$ min$^{-1}$ until 90 min, and then changed to 9.33$\times$10$^{-3}$ min$^{-1}$ when the oxidation of Fe$^{2+}$ mainly occurred. In this case [Fe$^{2+}$]/[Fe(t)] kept decreasing for the reaction. However, the addition of perchlortae (ClO$_4^-$) in the reaction of Fe$^0$ and UV induced the continuous increase of [Fe$^{2+}$]/[Fe(t)] ratio. The results mean the primary degradation factor of 1,4-dioxane is the oxidation by the radicals generated from the redox reaction between Fe$^{2+}$ and Fe$^{3+}$. Also, both UV and ClO$_4^-$ played the role inducing the reduction of Fe$^{3+}$, which is important to degrade 1,4-dioxane by enhancing the generation of radicals.