Synthesis of Cobalt Oxide Free Black Color Spinel Pigment (CoO가 첨가되지 않은 스피넬계 흑색안료의 합성)

  • Kim, Jun-Ho;Lee, Seong-Ho;Suh, Man-Chul;Lee, Byung-Ha
    • Journal of the Korean Ceramic Society
    • /
    • v.44 no.11
    • /
    • pp.639-644
    • /
    • 2007
  • Spinel pigments, developing black color in high temperature glazes at oxidation or reduction atmosphere, without CoO because of its high price were synthesized by solid solution method. Ten mixed compositions consisted of NiO, MnO, $Fe_2O_3 and $Mn_2O_3$ were fired at $1250^{\circ}C$ for 1h. The resulting pigments were characterized by using XRD, FT-IR, SEM and UV-vis spectrometer. Structure of the pigments are spinel and particles' shape are spherical or cubic. Glazed tiles containing 5 wt% pigments were fired at $1260^{\circ}C$ and $1240^{\circ}C$ in reduction atmosphere. Color in glazes were analyzed by UV-vis spectrometer. Colors of NiO 0.875 MnO $0.125{\cdot}Fe_2O_3$ $0.4875{\cdot}Cr_2O_3$ $0.50{\cdot}Mn_2O_3$ 0.0125 mole% and NiO 0.875 MnO $0.125{\cdot}Fe_2O_3$ $0.3875{\cdot}Cr_2O_3$ $0.50{\cdot}Mn_2O_3$ 0.1125 mole% in lime glaze showed black in oxidation, in reduction NiO 0.875 MnO $0.125{\cdot}Fe_2O_3$ $0.4875{\cdot}Cr_2O_3$ $0.50{\cdot}Mn_2O_3$ 0.0125 mole% and NiO 0.875 MnO $0.125{\cdot}Fe_2O_3$ $0.4375{\cdot}Cr_2O_3$ $0.55{\cdot}Mn_2O_3$ 0.0125 mole% showed black. In case of lime-barium glaze, NiO 0.875 MnO $0.125{\cdot}Fe_2O_3$ $0.3875{\cdot}Cr_2O_3$ $0.50{\cdot}Mn_2O_3$ 0.1125 mole%, NiO 0.975 MnO $0.075{\cdot}Fe_2O_3$ $0.4375{\cdot}Cr_2O_3$ $0.50{\cdot}Mn_2O_3$ 0.0625 mole% and NiO 0.925 MnO $0.075{\cdot}Fe_2O_3$ $0.4375{\cdot}Cr_2O_3$ $0.50{\cdot}Mn_2O_3$ 0.0625 mole% showed black color in oxidation and NiO 0.875 MnO $0.125{\cdot}Fe_2O_3$ $0.3875{\cdot}Cr_2O_3$ $0.50{\cdot}Mn_2O_3$ 0.1125 mole%, NiO 0.925 MnO $0.075{\cdot}Fe_2O_3$ $0.4375{\cdot}Cr_2O_3$ $0.50{\cdot}Mn_2O_3$ 0.0625 mole% and NiO 0.725 MnO $0.275{\cdot}Fe_2O_3$ $0.4375{\cdot}Cr_2O_3$ $0.50{\cdot}Mn_2O_3$ 0.0625 mole% showed black one in reduction.

A Study of Ferrite Formation by Aerial Oxidation of Fe$(OH)_2$ Suspension of Aqueous Solution Containing Heave Metal Ions (水酸化鐵 懸濁液에서 空氣酸化에 의한 중금속이온의 Ferrite 생성에 관한 연구)

  • Lee, Sung Ho;Hyun, Yong Bum;Kim, Soo Saeng
    • Journal of Environmental Health Sciences
    • /
    • v.12 no.1
    • /
    • pp.1-14
    • /
    • 1986
  • This investigation was carried out on the study of Ferrite formation by aerial oxidation of Fe $(OH)_2$ suspension of aqueous solution containing heavy metal ions. In this study the optimum reactionary condition of the Ferrite formation in Batch reactor wa studied by aerial oxidation which are subjected to various reaction time and temperature, under the different kinds of R(2NaOH/$FeSO_4$) Values, pH, Air flow rate, and $Fe^2+/M^2+$ mole ratio. The optimum condition for the Ferrite formation in Batch reactor was such that residence Time was 90 min., Temperature $65{\circ}$C, pH 11.0, Air flow rate 2.0l/min and $Fe^{2+}/M^{2+}$ mole ratio 4.0, which was observed by X-Ray diffraction analysis. The relation R-value, pH and ORP affecting the formation of Ferrite is that the jump step in pH 11.0, when a amount of NaOH is added, is steady state to the formation of Ferrite. Effect of R-value of $FeSO_4$ and $FeCl_2$ on the formation of Ferrite in different from each other the optimum condition of the in different from each other the optimum condition of the $FeCl_2$ is R-value 0.7, pH 11.0 and the $FeSO_4$ R-value 1.2, pH 11.0.

  • PDF

Crystal Packing of Two Different Tetranuclear Iron(III) Clusters, [(tacn)4Fe4O2(OH)4]2.8Br.9H2O (tacn = 1,4,7-triazacyclononane)

  • Jin, Mi-Kyung;Kim, Yoo-Jin;Jung, Duk-Young;Heu, Min;Yoon, Seok-Won;Suh, Byoung-Jin
    • Bulletin of the Korean Chemical Society
    • /
    • v.26 no.2
    • /
    • pp.253-259
    • /
    • 2005
  • [$(tacn)_4Fe_4O_2(OH)_4]_2{\cdot}8Br{\cdot}9H_2O$ (tacn = 1,4,7-triazacyclononane), a tetranuclear iron(III) complex was synthesized by the hydrolysis of (tacn)FeCl3 and crystallizes in the orthorhombic space group, Pca2(1), with cell parameters, a = 37.574(3) $\AA$, b = 16.9245(12) $\AA$, c = 14.2830(11) $\AA$, V = 9082.9(12) ${\AA}^3$. [$(tacn)_4Fe_4O_2(OH)_4]^{4+}$ cations approach S4 point symmetry containing an adamantane skeleton. Four Fe(III) atoms have distorted octahedral environments with two hydroxo and an oxo bridges. Two [$(tacn)_4Fe_4O_2(OH)_4]^{4+}$ clusters having different Fe…Fe distances are connected to each other by the networked hydrogen bonds. The electrochemical behavior reveals irreversible three cathodic and two anodic peaks. Magnetic properties are characterized by antiferromagnetic (AF) interactions between Fe(III) ion spins. However, the low-lying states are still magnetic and exhibit a blocking behavior and a magnetic hysteresis at low temperatures.

Al-Fe Partitioning between Coexisting Garnet and Epidote from Metamorphic Rocks

  • Kim, Hyung-Shik;Kim, Young-Kyum;Jang, Young-Nam
    • The Journal of the Petrological Society of Korea
    • /
    • v.2 no.2
    • /
    • pp.63-73
    • /
    • 1993
  • The assemblage epidote and grandite garnet occurs in low-to medium-grade metabasites and calc schists of various geotectonic settings and in hydrothermally altered calcareous rocks in skarn deposits. The compositions of sixteen epidote-garnet paris have been analysed by means of electron microprobe. Al-Fe partitioning between coexisting grandite garnet and epidote is considered and measured at the grain boundaries on the supposition that the surface equilibrium was maintained in the following exchange reaction: 2$Ca_2Al_3Si_3O_12$(OH)+$Ca_3Fe_2Si_3O_12$=2$Ca_2A_l2FeSi_3O_12$(OH)+$Ca_3Al_2Si_3O_12$ Partition coefficients confirms the differences in thermal conditions between low-grade and medium-grade metamorphic rocks. $K_D$ values ($X_{$CO_2$}$=($Fe^{+3}$/Al)$^{Ep}$/($Fe^{+3}$/Al)$^{Gr}$, where Fe=$Fe^{+3}$) from greenschist facies rocks of the estimated metamorphic temperatures, 330~$390^{\circ}C$, range approximately between 0.02 and 0.17. Epidote-amphibolite facies rocks and calcareous skarns of the estimated temperatures, 400~$550^{\circ}C$, have $K_D$ values between 0.24 and 0.37. $K_D$ values from the rocks of the temperatures, 640~$700^{\circ}C$, range nearly between 0.58 and 0.75. The diagrams in Figs. 2 and 3 can serve as a mineralogic thermometer for relatively shallow rocks, assuming that the pressure dependence of partition coefficients for the iron-exchange reaction in the two minerals can be neglected.

  • PDF

A study on the removal of mixed heavy metal ions using crab shell (게 껍질을 이용한 수중의 복합 중금속 제거에 관한 연구)

  • Kim, Dong-Seog
    • Journal of Environmental Science International
    • /
    • v.11 no.7
    • /
    • pp.729-735
    • /
    • 2002
  • In order to examine the inhibition effect of other heavy metal ions on the removal of heavy metal ions by crab shell in aqueous solution, 10 heavy metal ions $(Cr^{3+},\;Cd^{2+},\;Ni^{2+},\;Zn^{2+},\;Hg^{2+},\;Cu^{2+},\;Mn^{2+],\;Fe^{2+},\;Fe^{3+},\;Pb^{2+})$ were used as single heavy metal ions and mixed heavy metal ions, respectively. In single heavy metal ions, $Pb^{2+},\;Cr^{3+},\;Cu^{2+}$ were well removed by crab shell, however, $Cd^{2+},\;Ni^{2+},\;Zn^{2+},\;Mn^{2+}$ were not. The heavy metal removal increased as the increase of covalent index (Xm$^2$r), and the relationship classified heavy metal ions as 2 heavy metal groups $(Fe^{3+},\;Fe^{2+},\;Cu^{2+},\; Cr^{3+},\;Mn^{2+},\;Ni^{2+},\;Zn^{2+}\;group\;and\;Pb^{2+},\;Hg^{2+},\;Cd^{2+}\;group)$. In mixed heavy metal ions, the removals of $Fe^{2+},\;Fe^{3+},\;Pb^{2+},\;Cu^{2+}$ as 0.49 m㏖/g, regardless of the existence of other heavy metal ions, were similar to the result of single heavy metal ions experiment. The removals of $Mn^{2+},\;Cd^{2+},\;Ni^{2+}$ decreased as the existence of other heavy metal ions, however, the removal of $Zn^{2+},\;Cr^{3+},\;Hg^{2+}$ increased.

Tunable Magnetism by Magnetic Phase in $Fe_3O_4$/ZnO Multilayer

  • Yun, Jong-Gu;Park, Chang-Yeop;Yun, Sun-Gil
    • Proceedings of the Materials Research Society of Korea Conference
    • /
    • 2011.10a
    • /
    • pp.21.2-21.2
    • /
    • 2011
  • $Fe_3O_4$ having half metallic property is one of the efficient spin filtering materials which are widely used in spintronic research field and ZnO is wide band gap semiconductor which can be used by tunnel barrier or semiconductor channel in spin MOSFET. We investigated the magnetic and the electric properties of $Fe_3O_4$/ZnO multilayer fabricated on c-$Al_2O_3$ substrate by pulsed laser deposition (PLD). For multilayer films, PLD was performed at variable temperatures such as $200{\sim}750^{\circ}C$ and at target distance from 40 to 80 mm, KrF eximer laser of 1.5 $J/cm^2$ and a reputation rate of 2Hz. $Fe_3O_4$/ZnO multilayers were deposited at $4{\times}10^{-6}$ Torr. After fabricating $Fe_3O_4$/ZnO multilayers, $Fe_3O_4$/ZnO multilayers were treated by RTA(Rapid Thermal Annealing) at various temperature to change magnetic phase. The magnetism of the multilayer is changed by thickness of the ZnO tunnel barrier. Magnetic phase of FexOy showed a very small magnetism due to $Fe_2O_3$ ${\alpha}$-phase, but large magnetism from $Fe_3O_4$ or $Fe_2O_3$ ${\gamma}$-phase was observed. In the present study, effect of the ZnO thickness on the MR (magnetoresistance) ratio was investigated in detail.

  • PDF

Preparation of Highly Efficient Nd-Fe-B Magnetic Powders by Reduction/Diffusion Process (환원/확산 공정에 의한 고성능 Nd-Fe-B 자성분말의 제조)

  • Kim, Dongsoo;Chen, Chunqiang;Baek, Younkyoung;Choi, Chuljin
    • Journal of Powder Materials
    • /
    • v.20 no.3
    • /
    • pp.197-202
    • /
    • 2013
  • A novel route to prepare Nd-Fe-B magnetic particles by utilizing both spray drying and reduction/diffusion processes was investigated in this study. Precursors were prepared by spray drying method using the aqueous solutions containing Nd salt, Fe salt and boric acid with stoichiometric ratios. Precursor particles could be obtained with various sizes from 2 to $10{\mu}m$ by controlling concentrations of the solutions and the average size of $2{\mu}m$ of precursors were selected for further steps. After heat treatment of precursors in air, Nd and Fe oxides were formed through desalting procedure, followed by reduction processes in Hydrogen ($H_2$) atmosphere and with Calcium (Ca) granules in Argon (Ar) successively. Moreover, diffusion between Nd and Fe occurred during Ca reduction and $Nd_2Fe_{14}B$ particles were formed. With Ca amount added to particles after $H_2$ reduction, intrinsic coercivity was changed from 1 to 10 kOe. In order to remove and leach CaO and residual Ca, de-ionized water and dilute acid were used. Acidic solutions were more effective to eliminate impurities, but Fe and Nd were dissolved out from the particles. Finally, $Nd_2Fe_{14}B$ magnetic particles were synthesized after washing in de-ionized water with a mean size of $2{\mu}m$ and their maximum energy product showed 9.23 MGOe.

The Effect of Post Oxidation on Corrosion Characteristics of Gas Nitrocarburised Carbon Steels (Nitrocarburising 처리된 탄소강의 내식특성에 미치는 Post Oxidation 효과)

  • Kim, Y.H.;Jung, K.H.
    • Journal of the Korean Society for Heat Treatment
    • /
    • v.12 no.1
    • /
    • pp.9-20
    • /
    • 1999
  • The effect of post oxidation, water-quenched after holding in air for 5~420 seconds or cooling or furnace cooling, on corrosion resistance and phase formation characteristics of the surface layer of SM20C and SM45C carbon steels after gas nirtrocarbursing in the $NH_3-5%CO_2-N_2$ gas atmosphere at $580^{\circ}C$ for 3hours is studied. The compound layers of two steels consist of ${\varepsilon}-Fe_{2-3}N$, ${\gamma}^{\prime}-Fe_4N$ and $Fe_3O_4$, phases, however, the quantity of ${\gamma}^{\prime}-Fe_4N$ phase increases for the furnace cooled specimen compared to that of air cooling specimen. With increasing $NH_3$ content in the gas mixture and also increasing the keeping time in the air after gas nitrocarburising, the ${\varepsilon}-Fe_{2-3}N$ phase of compound layer increases, while the decreased current density recognizing the improvement of corrosion resistance are shown. the passive current density of SM45C steel is lower than that of SM20C steel at the same nitrocarburising conditions.

  • PDF

On-Site Corrosion Behavior of Water-Treated Boiler Tube Steel

  • Seo, Junghwa;Choi, Mihwa;He, Yinsheng;Yang, Seok-Ran;Lee, Je-Hyun;Shin, Keesam
    • Applied Microscopy
    • /
    • v.45 no.3
    • /
    • pp.177-182
    • /
    • 2015
  • The boiler tubes of X20CrMoV12.1 used in fossil-fired power plants were obtained and analyzed for the effect of water treatment on the steam corrosion-induced oxide scale in an effort to better understand the oxide formation mechanism, as well as pertinent method of maintenance and lifetime extension. The specimens were analyzed using various microscopy and microanalysis techniques, with focuses on the effect of water treatment on the characters of scale. X-ray diffraction analysis showed that the scales of specimens were composed of hematite ($Fe_2O_3$), magnetite ($Fe_3O_4$), and chromite ($FeCr_2O_4$). Electron backscatter diffraction analysis showed that the oxides were present in the following order on the matrix: outer $Fe_2O_3$, intermediate $Fe_3O_4$, and inner $FeCr_2O_4$. After all volatile treatment or oxygenated treatment, a dense protective $Fe_2O_3$ layer was formed on the $Fe_3O_4$ layer of the specimen, retarding further progression of corrosion.

Synthesis of Magnetic Powder in the Sm-Fe-N System by the Reduction-Diffusion Process (환원-확산법에 의한 Sm-Fe-N계 자성분말 제조)

  • Lee, Jung-Goo;Kang, Seok-Won;Park, Sang-Jun;Oh, Yung-Woo;Choi, Chul-Jin
    • Korean Journal of Metals and Materials
    • /
    • v.48 no.9
    • /
    • pp.842-846
    • /
    • 2010
  • In the present study, the reduction-diffusion method was employed to produce Sm-Fe alloy powder. It was confirmed that the amount of unreacted ${\alpha}-Fe$ in $Sm_2Fe_{17}$ matrix gradually decreased as the percentage of $Sm_2O_3$ increased. $Sm_2Fe_{17}$ single-phase powder was produced by the reduction-diffusion method with 40% excess $Sm_2O_3$. The Ca and Oxygen contents of the powder were approximately 300 ppm and 1600 ppm, respectively, after washing and acid treatment. By a subsequent nitrogenation, $Sm_2Fe_{17}N_x$ magnetic powders were produced. The coercivity of the powder increased with decreasing of the particle size by ball milling, and the highest coercivity of 2850 Oe was obtained after milling for 10 hours.