• 제목/요약/키워드: $BaTiO_3$ thin film

검색결과 203건 처리시간 0.032초

다양한 기판위에 증착된 BST 박막의 열처리 온도에 따른 마이크로파 유전성질과 미세구조 변화 (Microwave Properties and Microstructures of (Ba,Sr)TiO3 Thin Films on Various Substrates with Annealing Temperature)

  • 조광환;강종윤;윤석진;김현재
    • 한국재료학회지
    • /
    • 제17권7호
    • /
    • pp.386-389
    • /
    • 2007
  • The dielectric properties of $(Ba_{0.5}Sr_{0.5})TiO_3$ ferroelectric thin films have been investigated according to the substrates in order to optimize the their properties. MgO, r-plane sapphire, and poly-crystalline sapphire (Alumina) substrates have been used to deposite $(Ba_{0.5}Sr_{0.5})TiO_3$ ferroelectric thin films by RF magnetron sputtering. The BST thin films deposited on the single crystal (100)MgO substrates have high tunability and low dielectric loss. These results are caused by a low misfit between the lattice parameters of the BST films and the substrate. The BST films deposited on r-plane sapphire have relatively high misfit, and the tunability of 17% and dielectric loss of 0.0007. To improve the dielectric properties of the BST films, the post-annealing methods has been introduced. The BST films deposited on (100)MgO, (1102)r-plane sapphire, and poly-crystalline sapphire substrates have best properties in post-annealing conditions of $1050^{\circ}C$, $1100^{\circ}C$, and $1150^{\circ}C$, respectively. The different optimal post-annealing conditions have been found according to the different misfits between the films and substrates, and thermal expansion coefficients. Moreover, the films deposited on alumina substrate which is relatively cheap have a good tunability properties of 23% by the post-annealing.

Seed-layer 공정을 이용한 Ba0.66Sr0.34TiO3박막의 제조 및 전기적 특성 연구 (Electrical Properties of Ba0.66Sr0.34TiO3 Thin Films Fabricated by a Seed-layer Process)

  • 최덕영;박철호;손영국
    • 한국세라믹학회지
    • /
    • 제40권2호
    • /
    • pp.198-205
    • /
    • 2003
  • R.F. Magnetron Sputtering법을 이용하여 Pt/Ti/ $SiO_2$/Si기판 위에 seed-layers와 $Ba_{0.66}$S $r_{0.34}$Ti $O_3$박막을 제조하였다. 다양한 기판온도에 따른 BST 박막의 전기적인 특성(정전용량과 누설전류)과 seed-layer층이 BST 박막에 미치는 영향을 조사하였다. BST 박막은 seed-layer층을 삽입함으로써 박막의 결정성이 향상되었고, 박막의 기판온도(결정화온도)도 상당히 낮출 수 있었다. 순수한 BST에 비하여 seed-layer를 삽입한 BST는 높은 유전상수와 낮은 유전손실 및 낮은 누설전류를 가지는 우수한 전기적 특성을 나타내었다. BST 박막의 전기적 특성은 기판온도에 따라 영향을 받고, seed-layer에 의해 향상됨을 알 수 있었다.

Preparation and Characterization of $BaTiO_3-CuFe_2O_4$ Bi-Layer Thin Films Prepared By Pulsed Laser Deposition

  • ;;;이희영
    • 한국전기전자재료학회:학술대회논문집
    • /
    • 한국전기전자재료학회 2010년도 하계학술대회 논문집
    • /
    • pp.209-209
    • /
    • 2010
  • Multiferroic properties of $BaTiO_3-CuFe_2O_4$ thin films grown on highly-textured Pt(111)/$TiO_2/SiO_2$/Si(100) substrates were studied. $CuFe_2O_4$ ceramic target was synthesized by mixing oxide powders of CuO, $Fe_2O_03$, $BaTiO_3$ ceramic target was also prepared separately. The film structure was of bi-layer type, where $BaTiO_3$ layer lies underneath of $CuFe_2O_4$ layer, where both layers were grown by pulsed laser deposition technique. We will report the ferroelectric and magnetic properties of $BaTiO_3-CuFe_2O_4$ bi-layer films in some detail.

  • PDF

강유전체 (Ba,Sr)TiO$_3$ 박막을 이용한 분포 정수형 아날로그 위상변위기 설계 및 제작 (Design and Fabrication of Distributed Analog Phase Shifter Using Ferroelectric (Ba,Sr)TiO$_3$ Thin Films)

  • 류한철;김영태;문승언;곽민환;이수재
    • 한국전자파학회:학술대회논문집
    • /
    • 한국전자파학회 2002년도 종합학술발표회 논문집 Vol.12 No.1
    • /
    • pp.370-374
    • /
    • 2002
  • This paper describes the design and fabrication of distributed analog phase shifter circuit. The phase shifter consist of coplanar waveguide(CPW) lines that are periodically loaded with voltage tunable (Ba,Sr)TiO$_3$ thin film interdigital(IDT) capacitors deposited by the pulsed laser deposition(PLD) on (001) MgO single crystals. The phase velocity on these IDT loaded CPW lines is a function of applied bias voltage, thus resulting in analog phase shifting circuits. The measured differential phase shift is 48$^{\circ}$ and the insertion loss decreases from -5㏈ to -3㏈ with increasing bias voltage from 0 to 40 V at 100㎐.

  • PDF

Sputtering 압력에 따른 (Ba,Sr)TiO$_3$[BST] 박막의 구조 및 전기적 특성 (Microstructure Electrical Prperties of (Ba, Sr)TiO$_3$[BST] Thin Films with Sputtering Pressure)

  • 신승창;이문기;류기원;배선기;이영희
    • 한국전기전자재료학회:학술대회논문집
    • /
    • 한국전기전자재료학회 1998년도 춘계학술대회 논문집
    • /
    • pp.379-382
    • /
    • 1998
  • (Ba, Sr)TiO$_3$[BST] thin films were fabricated on Pt/SiO$_2$/Si substrate by RF sputtering technique. The Mic개structure, dielectric and electrical properties of BST thin films were investigated with sputtering pressure. Dielectric constant and dielectric loss of the deposited thin film at sputtering pressure of 5 mTorr were about 91 and 1.9(%), respectively. Increasing sputtering pressure, leakage current was increased. It was found that leakage current of BST thin films was depended on the sputtering pressure.

  • PDF

Orientation Control and Dielectric Properties of Sol-gel Deposited (Ba,Sr)TiO3 Thin Films for Room-temperature Tunable Element Applications

  • Zhai, Jiwei;Chen, Haydn
    • 한국세라믹학회지
    • /
    • 제40권4호
    • /
    • pp.380-384
    • /
    • 2003
  • The effects of the mole concentrations of precursor solution on the microstructure and dielectric properties of sol-gel deposited $Ba_{0.85}$S $r_{0.15}$Ti $O_3$(BST) thin films have been investigated. The films were of single perovskite phase with strong (100) preferred orientation when grown on LaNi0$_3$ buffered Pt/Ti/ $SiO_2$Si substrates using a diluted precursor solution. Variation of the precursor solution concentration resulted in a different microstructure and, in turn, affected the tunability of the sol-gel deposited films. It was observed that leakage currents increased asymmetrically for the negative and positive bias voltage with decreasing thickness. Overall results suggest that those BST films have acceptable properties f3r applications as room-temperature tunable elements.

고밀도 플라즈마에 의한 (Ba,Sr)$TiO_3$막의 식각특성 연구 (A study on the etching properties of (Ba,Sr)$TiO_3$ film by high density plasma)

  • 김승범;김창일;장의구
    • 대한전기학회:학술대회논문집
    • /
    • 대한전기학회 1998년도 추계학술대회 논문집 학회본부 C
    • /
    • pp.798-800
    • /
    • 1998
  • (Ba,Sr)$TiO_3$ thin films were etched with $Cl_2$/Ar gas mixing ratio in an inductively coupled plasma (ICP) by varying the etching parameter such as f power, do bias voltage, and chamber pressure. The etch rate was $560{\AA}/min$ under Cl_2/(Cl_2+Ar)$ gas mixing ratio of 0.2, rf power of 600 W, do bias voltage of 250 V, and chamber pressure of 5 mTorr, At this time, the selectivity of BST to Pt, $SiO_2$ was respectively 0.52, 0.43. The surface reaction of the etched (Ba,Sr)$TiO_3$ thin films was investigated with X-ray photoelectron spectroscopy (XPS).

  • PDF

$BaTiO_3$계 세라믹 박막의 열처리에 따른 미세구조변화 (Varition Microstructure for Heat treatment of Thin Films $BaTiO_3$ System)

  • 박춘배;송민종;김태완;강도열
    • 대한전기학회:학술대회논문집
    • /
    • 대한전기학회 1994년도 추계학술대회 논문집 학회본부
    • /
    • pp.293-295
    • /
    • 1994
  • Barium Titanate ($BaTiO_3$) is one of the few titanateds which is cubic at room temperature. It has the perovskite structure, high dielectric constant (${\varepsilon}_r=300$) and a small temperature coefficient of resistance due to it's Low transition temperature ($Tc=120^{\circ}c$). PTCR (Positive Temperature Coefficient of Resistivity) thermistor in thin film $BaTiO_3$ system was prepared by using radio frequency (13.56MHz) and BC magnetron sputter equipment. Polycrystalline, and surface structure characteristics of the specimens were measured by X-ray diffraction (D-Max3, Rigaku, Japan), SEM(Scanning Electron Microscopy: M. JSM84 01, Japan), respectively. Temperature at below $600^{\circ}C$, $1000^{\circ}C$ to $700^{\circ}C$, and above $1100^{\circ}C$ for spotted $BaTiO_3$ thin films showed the amorphous, degree of crystal growth, and polycrystalline, respectively.

  • PDF

PZT/$BaTiO_3$/PZT 다층 후막의 유전특성 (Electrical Properties of PZT/$BaTiO_3$/PZT Multilayer Thick Films)

  • 남성필;이성갑;배선기;이영희
    • 대한전기학회:학술대회논문집
    • /
    • 대한전기학회 2006년도 추계학술대회 논문집 전기물성,응용부문
    • /
    • pp.123-124
    • /
    • 2006
  • The sandwiched PZT/$BaTiO_3$/PZT thick films were fabricated by two different methods thick films of the PZT by screen printing method on alumina substrateselectrodes with Pt, thin films of $BaTiO_3$ by the spin-coating method on the PZT thick films and once more thick films of the PZT by the screen printing method on the $BaTiO_3$ layer. The structural and the dielectric properties were investigated for effect of various stacking sequence of sol-gel prepared $BaTiO_3$ coating solution at interface of the PZT thick films, The insertion of BaTi03 interlayer yielded the PZT thick films with homogeneous and dense grain structure with the number of $BaTiO_3$ layers. The leakage current density of the $PZT/BaTiO_3-1$ film is less that $4.41{\times}10^{-9}A/cm^2$ at 5 V.

  • PDF

Tunable 소자 응용을 위한 Sol-gel 법으로 제작된 BST 박막의 Bi 첨가에 따른 구조적, 유전적 특성 (Structure and Dielectric properties of BST Thin Films prepared by Sol-gel method for Tunable element application)

  • 김태형;김경태;김창일
    • 한국전기전자재료학회:학술대회논문집
    • /
    • 한국전기전자재료학회 2004년도 하계학술대회 논문집 Vol.5 No.2
    • /
    • pp.565-568
    • /
    • 2004
  • An alkoxide-based sol-gel method was used to fabricate $Ba_{0.6}Sr_{0.4}TiO_3$ thin films doped by Bi from 5 to 20 mol% on a Pt/Ti/SiO2/Si substrate. The structural and dielectric properties of BST thin films were investigated as a function of Bi dopant concentration. The dielectric properties of the Bi doped BST films were strongly dependent on the Bi contents. The dielectric constant and dielectric loss of the films decreased with increasing Bi content. However, the leakage current density of the 10 mol% Bi doped $Ba_{0.6}Sr_{0.4}TiO_3$ thin film showed the lowest value of 5.13 10-7 at 5 V. The figure of merit (FOM) reached a maximum value of 32.42 at a 10 mol% Bi doped $Ba_{0.6}Sr_{0.4}TiO_3$ thin films. The dielectric constant, loss factor, and tunability of the 10 mol% Bi doped $BBa_{0.6}Sr_{0.4}TiO_3$ thin films were 333,0.0095, and 31.1%, respectively.

  • PDF