• 제목/요약/키워드: $BaTiO_3$ thin film

검색결과 203건 처리시간 0.031초

NdBaCuO 초전도박막 합성 (Fabrication of NdBaCuO Superconducting Thin Film)

  • 이상헌;이상근
    • 한국전기전자재료학회:학술대회논문집
    • /
    • 한국전기전자재료학회 2002년도 추계학술대회 논문집 Vol.15
    • /
    • pp.244-247
    • /
    • 2002
  • NdBaCuO thin films were prepared on $SrTiO_{3}$ substrates by RF magnetron sputtering. These as-grown films were classified into 3type. The resistivity of the deposited films are usually lower than of the YBCO film. The Tc (onset) and Tc (R=0) in the optimized thin films are as high as 90 and 80K, respectively. These as-grown films are highly uniform and semi-trans parent and have a room temperature resistivity of $0.3m{\Omega}cm$.

  • PDF

두께 변화에 따른 BST 박막의 특성 (The Properties of BST Thin Films by Thickness)

  • 홍경진;민용기;조재철
    • 한국전기전자재료학회:학술대회논문집
    • /
    • 한국전기전자재료학회 2001년도 추계학술대회 논문집 Vol.14 No.1
    • /
    • pp.455-458
    • /
    • 2001
  • The thin films of high pemitivity in ferroelectric materials using a capacitor are applied to DRAMs and FRAMs. (Ba, Sr)$TiO_3$ thin films as ferroelectric materials were prepared by the sol-gel method and made by spin-coating on the Pt/Ti/$SiO_2/Si$ substrate at 4,000 [rpm] for 10 seconds. The devices of BST thin films to composite $(Ba_{0.7},Sr_{0.3})TiO_3$ were fabricated by changing of the depositing layer number on $Pt/Ti/SiO_2/Si$ substrate. The thin film capacitor to be ferroelectric devices was investigated by structural and electrical properties. The thickness of BST thin films at each coating numbers 3, 4 and 5 times was $2500[\AA]$, $3500[\AA]$, $3800[\AA]$. The dielectric factor of thin film when the coating numbers were 3, 4 and 5 times was 190, 400 and 460 on frequency l[MHz]. The dielectric loss of BST thin film was linearly increased by increasing of the specimen area.

  • PDF

두께 변화에 따른 BST 박막의 특성 (The Properties of BST Thin Films by Thickness)

  • 홍경진;민용기;조재철
    • 한국전기전자재료학회:학술대회논문집
    • /
    • 한국전기전자재료학회 2001년도 추계학술대회 논문집
    • /
    • pp.455-458
    • /
    • 2001
  • The thin films of high permitivity in ferroelectric materials using a capacitor are applied to DRAMs and FRAMs. (Ba, Sr)TiO$_3$ thin films as ferroelectric materials were prepared by the sol-gel method and made by spin-coating on the Pt/Ti/SiO$_2$/Si substrate at 4,700 [rpm] for 10 seconds. The devices of BST thin films to composite (Ba$\_$0.7/Sr$\_$0.3/)TiO$_3$ were fabricated by changing of the depositing layer number on Pt/Ti/SiO$_2$/Si substrate. The thin film capacitor to be ferroelectric devices was investigated by structural and electrical properties. The thickness of BST thin films at each coating numbers 3, 4 and 5 times was 2500[${\AA}$], 3500[${\AA}$], 3800[${\AA}$]. The dielectric factor of thin film when the coating numbers were 3, 4 and 5 times was 190, 400 and 460 on frequency 1[MHz]. The dielectric loss of BST thin film was linearly increased by increasing of the specimen area.

  • PDF

RF Sputtering법에 의한 (Ba,Sr)TiO$_3$ 세라믹 박막의 구조적 특성에 관한 연구 (A study on the structural properties of (Ba,Sr)TiO$_3$ Ceramics Thin Films by RF Sputtering Technique)

  • 신승창;정장호;배선기;이영희
    • 한국전기전자재료학회:학술대회논문집
    • /
    • 한국전기전자재료학회 1997년도 추계학술대회 논문집
    • /
    • pp.217-220
    • /
    • 1997
  • (Ba,Sr)TiO$_3$ thin film capacitors were prepared on SiO$_3$/Si(100)wafer by RF sputtering technique. The structural and crystallographic properties were studied with deposition conditions and annealing temperatures. Microstructural properties of (Ba,Sr)TiO$_3$ thin films were investigated by the SEM, XRD. The thickness and grain size were studied for the varying of RF power and temperature.

  • PDF

$BaTiO_3$ 박막커패시터의 유전특성 (The Characteristics of $BaTiO_3$ Thin Capacitor)

  • 홍경진;이정빈;정우성;김현종;이진;김태성
    • 대한전기학회:학술대회논문집
    • /
    • 대한전기학회 1994년도 하계학술대회 논문집 C
    • /
    • pp.1274-1276
    • /
    • 1994
  • A study on $BaTiO_3$ ceramics have been shown that dielectric properties of $BaTiO_3$ ceramics strongly depend on the size and ferroelectric domain density of the constituting grain. According to rising substrate temperature from $25[^{\circ}C]$ to $600[^{\circ}C]$, the peak intensity and crystal plane in XRD are increased. In this study, $BaTiO_3$ thin film prepared by RF sputtering from room temperature to $600[^{\circ}C]$ of substrate temperature. Therefore, we tried to investigate the relation between the characteristics of ceramics structure and dielectric factor.

  • PDF

$Ar/CF_{4}$ 유도결합 플라즈마로 식각된 $(Ba_{0.6}Sr_{0.4})TiO_{3}$ 박막의 특성분석 (The etching characteristics of $(Ba_{0.6}Sr_{0.4})TiO_{3}$ film Using $Ar/CF_{4}$ Inductively Coupled Plasma)

  • 강필승;김경태;김동표;김창일;이수재
    • 한국전기전자재료학회:학술대회논문집
    • /
    • 한국전기전자재료학회 2002년도 춘계학술대회 논문집 센서 박막재료 반도체재료 기술교육
    • /
    • pp.16-19
    • /
    • 2002
  • (Ba,Sr)TiO3(BST) thin film is an attractive material for the application in high-density dynamic random access memories (DRAMs) because of the high relative dielectric constant and small variation in dielectric properties with frequency. In this study, (Ba0.6,Sr0.4)TiO3 thin films on Pt/Ti/SiO2/Si substrates were deposited by a sol-gel method and the CF4/Ar inductively coupled plasma (ICP) etching behavior of BST thin films had been investigatedby varying the process parameters such as chamber pressure, ICP power, and substrate bias voltage. To analysis the composition of surface residue following etching BST films etched with different Ar/CF4 gas mixing ratio were investigated using x-ray photoelectron spectroscopy (XPS) and secondary ion mass spectrometer (SIMS).

  • PDF

$(Ba_xSr_{1-x})$TiO$_3$박막의 온도 변화에 따른 유전 특성 (Dielectric Properties with Temperature Variation of $(Ba_xSr_{1-x})$TiO$_3$Thin Films)

  • 김덕규;전장배;송민종;박춘배
    • 한국전기전자재료학회:학술대회논문집
    • /
    • 한국전기전자재료학회 1997년도 춘계학술대회 논문집
    • /
    • pp.309-313
    • /
    • 1997
  • (Ba$_{x}$Sr$_{l-x}$)TiO$_3$(BST) thin fi1ms with various Ba/Sr ratios were deposited on Pt(80nm)/SiO$_2$(100nm)/Si by RF magnetron sputtering. BST thin films which have x=0.6, 0.5, 0.4 were studied dielectric properties with temperature variation. The frequency was used from 100Hz to 1MHz for measuring dielectric constant. The measurement conditions of dielectric constant with Temperature Variation were 1KHz and 2$0^{\circ}C$. As a result, the dielectric constant of BST thin film was about 425 and loss factor was 0.013. Also, with increasing Temperature, the dielectric constants of BST thin films were gradually decreased.sed.

  • PDF

Electrical Properties of (Ba, Sr)TiO$_3$ Thin Film Deposited on RuO$_2$Electrode

  • Park, Chi-Sun;Kim, In-Ki
    • Transactions on Electrical and Electronic Materials
    • /
    • 제1권4호
    • /
    • pp.30-39
    • /
    • 2000
  • The variation of electrical properties of (Ba, Sr)TiO$_3$[BST] thin films deposited of RuO$_2$electrode with (Ba+Sr)/Tr ration was investigated. BST thin films with various (Ba+Sr)/Tr ration were deposited on RuO$_2$/Si substrates using in-situ RF magnetron sputtering. It was found that the electrical properties of BST films depends on the composition in the film. The dielectric constant of the BST films is about 190 at the (Ba+Sr)/Tr ration of 1.0, 1,025 and does not change markedly. But , the dielectric constant degraded to 145 as the (Ba+Sr)/Tr ratio increase to 1.0. In particular, the leakage current mechanism of the films shows the strong dependence on the (Ba+Sr)/Tr ration in the films. At the ration (Ba+Sr)/Tr=1,025, the Al/BST/RuO$_2$ capacitor show the most asymmetric behavior in the leakage current density, vs, electric field plot. It is considered that the leakage current of the (Ba+Sr)/Tr=1,025 thin films is controlled by the battier-Iimited process, i,e, Schottky emission.

  • PDF

캐패시터용 강유전체 박막의 제조 및 특성 (Fabrication and Properties of Ferroelectric Thin Film for Capacitor)

  • 소병문;박춘배
    • 대한전기학회:학술대회논문집
    • /
    • 대한전기학회 1999년도 추계학술대회 논문집 전문대학교육위원 P
    • /
    • pp.31-34
    • /
    • 1999
  • In the present study, we fabricated stoichiometric $(Ba_{1-x}Sr_x)TiO_3$ thin films at various substrate temperature and contents using of magnetron sputtering method on optimized Pt-based electrodes (Pt/TiN/$SiO_2$/Si). The substate temperature deposited at 200[ $^{\circ}C$], 400[$^{\circ}C$] and 600[$^{\circ}C$] and crystalline BST thin films show above 400[$^{\circ}C$]. Also, the composition of $(Ba_{1-x}Sr_x)TiO_3$ thin films deposited on Si wafer substrate at 400[$^{\circ}C$] were closed to stoichiometry($1.015{\sim}1.093$ in A/B ratio), but compositional deviation from a stoichiometry is larger as $SrCO_3$ is added. The drastic decrease of dielectric constant and increase of dielectric loss in $(Ba_{1-x}Sr_x)TiO_3$thin films is observed above 100[kHz]. V-I characteristics of $(Ba_{1-x}Sr_x)TiO_3$ thin films show the decrease of leakage current with the increase of $SrCO_3$ contents.

  • PDF