$CF_4$ 분해에 미치는 비열플라즈마 반응기 구조의 영향 (Effect of Non-thermal plasma Reactor construction by $CF_4$ decomposition)

  • 김선호;박재윤;하현진;황보국;김광수;임근회
    • 한국전기전자재료학회:학술대회논문집
    • /
    • 한국전기전자재료학회 2002년도 하계학술대회 논문집 Vol.3 No.2
    • /
    • pp.912-916
    • /
    • 2002
  • In this paper, the $CF_4$ decomposition rate and by-product were investigated for a simulated two plasma reactors which are metal particle reactor and spiral wire reactor as function of mixed gases. The $CF_4$ decomposition rate by plasma reactor with metal particle electrode had a gain of 20~25[%] over that by plasma reactor with spiral wire electrode. The $CF_4$ decomposition efficiency increases with increasing applied voltage up to the critical voltage for spark formation. The $CF_4$ decomposition efficiency of metal particle reactor was about 80[%] at AC 24[kV]. The $CF_4$ decomposition rate used $Ar-N_2$ as base gas was the highest among three base gases of $N_2$, $Ar-N_2$, air. The by-products of the $N_2$, $Ar-N_2$ base as were similar, but in case of air base they were different.

  • PDF

The Effects of CF4 Partial Pressure on the Hydrophobic Thin Film Formation on Carbon Steel by Surface Treatment and Coating Method with Linear Microwave Ar/CH4/CF4 Plasma

  • Han, Moon-Ki;Cha, Ju-Hong;Lee, Ho-Jun;Chang, Cheol Jong;Jeon, Chang Yeop
    • Journal of Electrical Engineering and Technology
    • /
    • 제12권5호
    • /
    • pp.2007-2013
    • /
    • 2017
  • In order to give hydrophobic surface properties on carbon steel, the fluorinated amorphous carbon films were prepared by using linear 2.45GHz microwave PECVD device. Two different process approaches have been tested. One is direct deposition of a-C:H:F films using admixture of $Ar/CH_4/CF_4$ working gases and the other is surface treatment using $CF_4$ plasma after deposition of a-C:H film with $Ar/CH_4$ binary gas system. $Ar/CF_4$ plasma treated surface with high $CF_4$ gas ratio shows best hydrophobicity and durability of hydrophobicity. Nanometer scale surface roughness seems one of the most important factors for hydrophobicity within our experimental conditions. The properties of a-C:H:F films and $CF_4$ plasma treated a-C:H films were investigated in terms of surface roughness, hardness, microstructure, chemical bonding, atomic bonding structure between carbon and fluorine, adhesion and water contact angle by using atomic force microscopy (AFM), nano-indentation, Raman analysis and X-ray photoelectron spectroscopy (XPS).

$Ar/CF_{4}$ 유도결합 플라즈마에서 식각된 $(Ba_{0.6}Sr_{0.4})TiO_{3}$ 박막의 손상 감소 (Study on Damage Reduction of $(Ba_{0.6}Sr_{0.4})TiO_{3}$ Thin Films in $Ar/CF_{4}$ Plasma)

  • 강필승;김경태;김동표;김창일;황진호;김태형
    • 한국전기전자재료학회:학술대회논문집
    • /
    • 한국전기전자재료학회 2002년도 추계학술대회 논문집 Vol.15
    • /
    • pp.171-174
    • /
    • 2002
  • The barium strontium titannate (BST) thin films were etched in $CF_{4}/Ar$ inductively coupled plasma (ICP). The high etch rate obtained at a $CF_{4}(20%)/Ar(80%)$ and the etch rate in pure argon was twice higher than that in pure $CF_{4}$. This indicated that BST etching is sputter dominant process. It is impossible to avoid plasma-induced damages by the energetic particles in the plasma and the nonvolatile etch products. The plasma damages were evaluated in terms of leakage current density, residues on the etched sample, and the changes of roughness. After the BST thin films exposed in the plasma, the leakage current density and roughness increases. In addition, there are appeared a nonvolatile etch byproductsand from the result of X-ray photoelectron spectroscopy (XPS). After annealing at ${600^{\circ}C}$ for 10 min in $O_{2}$ ambient, the increased leakage current density, roughness and nonvolatile etch byproducts reduced. From the this results, the plasma induced damage recovered by annealing process owing to the relaxation of lattice mismatches by Ar ions and the desorption of metal fluorides in high temperature.

  • PDF

Etching Characteristics of Au Thin Films using Inductively Coupled CF4 / Cl2 / Ar Plasma

  • Kim Dong-Pyo;Kim Chang-Il
    • Transactions on Electrical and Electronic Materials
    • /
    • 제4권3호
    • /
    • pp.1-4
    • /
    • 2003
  • The etching of Au thin films has been performed in an inductively coupled $CF_4 / Cl_2 / Ar$ plasma. The etch properties including etch rate and selectivity were examined as $CF_4$ content adds from o to $30\%$ to $Cl_2/Ar$ plasma. The $Cl_2/(Cl_2 + Ar)$ gas mixing ratio was fixed at $20\%$. Other parameters were fixed at an rf power of 700 W, a dc bias voltage of -150 V, a chamber pressure of 15 mTorr, and a substrate temperature of $30^{\circ}C$. The highest etch rate of the Au thin film was 370 nm/min at a $10\%$ additive $CF_4$ into $Cl_2/Ar$ gas mixture. The surface reaction of the etched Au thin films was investigated using x-ray photoelectron spectroscopy (XPS) analysis. The XPS analysis shows that the intensities of Ail peaks are changed, indicating that there is a chemical reaction between Cl and Au. Au-Cl is hard to remove on the surface because of its high melting point. However, etching products can be sputtered by Ar ion bombardment.

Inductively Coupled Plasma를 이용한 lead-zirconate-titanate 박막의 식각 손상 개선 (The reduction of etching damage in lead-zirconate-titanate thin films using Inductively Coupled Plasma)

  • 임규태;김경태;김동표;김창일
    • 한국전기전자재료학회:학술대회논문집
    • /
    • 한국전기전자재료학회 2003년도 춘계학술대회 논문집 센서 박막재료 반도체 세라믹
    • /
    • pp.178-181
    • /
    • 2003
  • In this work, we etched PZT films with various additive gases ($O_2$ and Ar) in $Cl_2/CF_4$ plasmas, while mixing ratio was fixed at 8/2. After the etching, the plasma induced damages are characterized in terms of hysteresis curves, leakage current, retention properties, and switching polarization. When the electrical properties of PZT etched in $O_2$ or Ar added $Cl_2/CF_4$ were compared, the value of remanent polarization in $O_2$ added $Cl_2/CF_4$ plasma is higher than that in Ar. added plasma. The maximum etch rate of the PZT thin films was 145 nm/min for 30% Ar added $Cl_2/CF_4$ gas having mixing ratio of 8/2 and 110 nm/min for 10% $O_2$ added to that same gas mixture. In order to recover the ferroelectic properties of the PZT thin films after etching, we annealed the etched PZT thin films at $550^{\circ}C$ in an $O_2$ atmosphere for 10 min. From the hysteresis curves, leakage current, retention property and switching polarization, the reduction of the etching damage and the recovery via the annealing was turned out to be more effective when $O_2$ was added to $Cl_2/CF_4$ than Ar. X-ray diffraction (XRD) showed that the structural damage was lower when $O_2$ was added to $Cl_2/CF_4$. And the improvement in the ferroelectric properties of the annealed samples was consistent with the increased intensities of the (100) and the (200) PZT peaks.

  • PDF

평면형 PLASMA 시스템에서의 방전 전압에 관한 연구 (A STUDY OF DISCHARGE VOLTAGE IN PLANER PLASMA SYSTEM)

  • 김종식;강봉구;권오대
    • 대한전기학회:학술대회논문집
    • /
    • 대한전기학회 1989년도 하계종합학술대회 논문집
    • /
    • pp.426-428
    • /
    • 1989
  • As a first phase of plasma study intended for semiconductor processing research, we have studied the discharge phenomena. In particular, we have obtained a specific formula for the breakdown voltage as a function of the neutral state pressure of reactive gases. Our experimental results with H2,O2,Ar,CF4 seem ro verify this formula. In addition we find the voltage levels for various gases in the descending order of CF4>O2=Ar>H2 in high pressure region, while H2>CF4>O2>Ar in low pressure region. When H2 and CF4 were mixed, we observe the overall voltage dominated by the gas with lower breakdown volotage.

  • PDF

Ar/$CF_4$ 고밀도 플라즈마에서(Ba,Sr)$TiO_3$ 박막의 식각 메카니즘에 관한 연구 (A Study on Etching Mechanism of (Ba,Sr)$TiO_3$ in Ar/$CF_4$ High Density Plasma)

  • 김승범;김창일
    • 대한전기학회:학술대회논문집
    • /
    • 대한전기학회 1999년도 하계학술대회 논문집 D
    • /
    • pp.1550-1552
    • /
    • 1999
  • In this study, (Ba,Sr)$TiO_3$ thin films were etched with a magnetically enhanced inductively coupled plasma (MEICP) as a function $CF_4$/Ar gas mixing ratio. Experimental was done by varying the etching parameters such as rf power, dc bias and chamber pressure. The maximum etch rate of the BST films was $1700{\AA}$/min under $CF_4/(CF_4+Ar)$ of 0.1, 600W/350V and 5 mTorr. The selectivity of BST to Pt and PR was 0.6, 0.7, respectively. X-ray photoelectron spectroscopy (XPS) studies shows that there are surface reaction between Ba, Sr, Ti and C, F radicals during the (Ba,Sr)$TiO_3$ etching. To analysis the composition of surface residue remaining after the etching, films etched with different $CF_4$/Ar gas mixing ratio were investigated using XPS.

  • PDF

$Ar/CF_{4}/Cl_{2}$ 플라즈마에 의한 $CeO_2$ 박막의 식각 특성 연구 (A study on etch Characteristics of $CeO_2$ thin Film in an $Ar/CF_{4}/Cl_{2}$ Plasma)

  • 장윤성;장의구;김창일;이철인;김태형;엄준철
    • 한국전기전자재료학회:학술대회논문집
    • /
    • 한국전기전자재료학회 2001년도 추계학술대회 논문집 Vol.14 No.1
    • /
    • pp.217-220
    • /
    • 2001
  • The possibility of cerium dioxide $(CeO_2)$ thin films as insulators of metal erroelectric insulator semiconductor (MFIS) structures have been studied. The etching $CeO_2$ thin films have been perfonned in an inductively coupled $Cl_{2}/CF_{4}/Ar$ plasma. The high etch rate of the $CeO_2$ thin film was $250\AA /m$ at a 10 % addition of $Cl_2$ into the $Ar(80)/CF_{4}(20)$. The surface reaction of the etched $CeO_2$ thin films was investigated using X-ray photoelectron spectroscopy (XPS) analysis. There are Ce-Cl and Ce-F bonding by chemical reaction between Cl, F and Ce. These products can be removed by the physical bombardment of incident Ar ions.

  • PDF

자장강화된 유도결합 플라즈마를 이용한 (Ba, Sr) $TiO_3$박막의 식각 특성 연구 (The Etching Characteristics of (Ba, Sr) $TiO_3$Thin Films Using Magnetically Enhanced Inductively Coupled Plasma)

  • 민병준;김창일
    • 한국전기전자재료학회논문지
    • /
    • 제13권12호
    • /
    • pp.996-1002
    • /
    • 2000
  • Ferroelectric (Ba, Sr) TiO$_3$(BST) thin films have attracted much attention for use in new capacitor materials of dynamic random access memories (DRAMs). In order to apply BST to the DRAMs, the etching process for BST thin film with high etch rate and vertical profile must be developed. However, the former studies have the problem of low etch rate. In this study, in order to increase the etch rate, BST thin films were etched with a magnetically enhanced inductively coupled plasma(MEICP) that have much higher plasma density than RIE (reactive ion etching) and ICP (inductively coupled plasma). Experiment was done by varying the etching parameters such as CF$_4$/(CF$_4$+Ar) gas mixing ratio, rf power, dc bias voltage and chamber pressure. The maximum etch rate of the BST films was 170nm/min under CF$_4$/CF$_4$+Ar) of 0.1, 600 W/-350 V and 5 mTorr. The selectivities of BST to Pt and PR were 0.6 and 0.7, respectively. Chemical reaction and residue of the etched surface were investigated with X-ray photoelectron spectroscopy (XPS) and secondary ion mass spectroscopy (SIMS).

  • PDF

The Dry Etching of TiN Thin Films Using Inductively Coupled CF4/Ar Plasma

  • Woo, Jong-Chang;Choi, Chang-Auck;Joo, Young-Hee;Kim, Han-Soo;Kim, Chang-Il
    • Transactions on Electrical and Electronic Materials
    • /
    • 제14권2호
    • /
    • pp.67-70
    • /
    • 2013
  • In this study, we changed the input parameters (gas mixing ratio, RF power, DC bias voltage, and process pressure), and then monitored the effect on TiN etch rate and selectivity with $SiO_2$. When the RF power, DC-bias voltage, and process pressure were fixed at 700 W, - 150 V, and 15 mTorr, the etch rate of TiN increased with increasing $CF_4$ content from 0 to 20 % in $CF_4$/Ar plasma. The TiN etch rate reached maximum at 20% $CF_4$ addition. As RF power, DC bias voltage, and process pressure increased, all ranges of etch rates for TiN thin films showed increasing trends. The analysis of x-ray photoelectron spectroscopy (XPS) was carried out to investigate the chemical reactions between the surfaces of TiN and etch species. Based on experimental data, ion-assisted chemical etching was proposed as the main etch mechanism for TiN thin films in $CF_4$/Ar plasma.