• Title/Summary/Keyword: $({Al_2}{O_3}-SiC)$- SiC- TiC

Search Result 210, Processing Time 0.029 seconds

Study of $MgB_2$ Films Grown on Various Impurity Layers by using HPCVD Method (혼성물리화학기상 증착법으로 여러가지 불순물층 위에 제조한 $MgB_2$ 박막에 대한 연구)

  • Park, S.W.;Seong, W.K.;Jung, Soon-Gil;Kang, W.N.
    • Progress in Superconductivity
    • /
    • v.10 no.1
    • /
    • pp.35-39
    • /
    • 2008
  • By using the hybrid physical-chemical vapor deposition (HPCVD) technique, we have fabricated $MgB_2$ thick films on $Al_{2}O_3$ substrates with various impurity layers of Ni, Ti, and SiC. We have found a significant enhancement of the critical current density ($J_c$) for $MgB_2$ films grown on impurity layered substrates, indicating that additional impurity layers were provided as possible pinning sites by chemical doping in $MgB_2$ films. All samples doped by Ni, Ti, and SiC were observed to have high superconducting transition temperatures of 39 - 41 K. The $J_c$ of $MgB_2$ films grown on SiC impurity layered substrates showed three times higher than that of undoped films at high magnetic fields above 1 T.

  • PDF

Element Dispersion and Wallrock Alteration from Samgwang Deposit (삼광광상의 모암변질과 원소분산)

  • Yoo, Bong-Chul;Lee, Gil-Jae;Lee, Jong-Kil;Ji, Eun-Kyung;Lee, Hyun-Koo
    • Economic and Environmental Geology
    • /
    • v.42 no.3
    • /
    • pp.177-193
    • /
    • 2009
  • The Samgwang deposit consists of eight massive mesothermal quartz veins that filled NE and NW-striking fractures along fault zones in Precambrian granitic gneiss of the Gyeonggi massif. The mineralogy and paragenesis of the veins allow two separate discrete mineralization episodes(stage I=quartz and calcite stage, stage II-calcite stage) to be recognized, temporally separated by a major faulting event. The ore minerals are contained within quartz and calcite associated with fracturing and healing of veins that occurred during both mineralization episodes. The hydrothermal alteration of stage I is sericitization, chloritization, carbonitization, pyritization, silicification and argillization. Sericitic zone occurs near and at quartz vein and include mainly sericite, quartz, and minor illite, carbonates and chlorite. Chloritic zone occurs far from quartz vein and is composed of mainly chlorite, quartz and minor sericite, carbonates and epidote. Fe/(Fe+Mg) ratios of sericite and chlorite range 0.45 to 0.50(0.48$\pm$0.02) and 0.74 to 0.81(0.77$\pm$0.03), and belong to muscovite-petzite series and brunsvigite, respectiveIy. Calculated $Al_{IV}$-FE/(FE+Mg) diagrams of sericite and chlorite suggest that this can be a reliable indicator of alteration temperature in Au-Ag deposits. Calculated activities of chlorite end member are $a3(Fe_5Al_2Si_3O_{10}(OH)_6$=0.0275${\sim}$0.0413, $a2(Mg_5Al_2Si_3O_{10}(OH)_6$=1.18E-10${\sim}$7.79E-7, $a1(Mg_6Si_4O_{10}(OH)_6$=4.92E-10${\sim}$9.29E-7. It suggest that chlorite from the Samgwang deposit is iron-rich chlorite formed due to decreasing temperature from high temperature(T>450$^{\circ}C$). Calculated ${\alpha}Na^+$, ${\alpha}K^+$, ${\alpha}Ca^{2+}$, ${\alpha}Mg^{2+}$ and pH values during wallrock alteration are 0.0476($400^{\circ}C$), 0.0863($350^{\circ}C$), 0.0154($400^{\circ}C$), 0.0231($350^{\circ}C$), 2.42E-11($400^{\circ}C$), 7.07E-10($350^{\circ}C$), 1.59E-12($400^{\circ}C$), 1.77E-11($350^{\circ}C$), 5.4${\sim}$6.4($400^{\circ}C$), 5.3${\sim}$5.7($350^{\circ}C$)respectively. Gain elements(enrichment elements) during wallrock alteration are $TiO_2$, $Fe_2O_3(T)$,CaO, MnO, MgO, As, Ag, Cu, Zn, Ni, Co, W, V, Br, Cs, Rb, Sc, Bi, Nb, Sb, Se, Sn and Lu. Elements(Ag, As, Zn, Sc, Sb, Rb, S, $CO_2$) represents a potential tools for exploration in mesothermal and epithermal gold-silver deposits.

Electrical Properties of $(Sr_{0.85}Ca_{0.15})TiO_3$ Thin Films with Top Electrodes (상부전극에 따른 $(Sr_{0.85}Ca_{0.15})TiO_3$ 박막의 전기적 특성)

  • Jo, Chun-Nam;Kim, Jin-Sa;Sin, Cheol-Gi;O, Jae-Han;Choe, Un-Sik;Kim, Chung-Hyeok;Lee, Jun-Ung
    • The Transactions of the Korean Institute of Electrical Engineers C
    • /
    • v.49 no.2
    • /
    • pp.107-112
    • /
    • 2000
  • $(Sr_{0.85}Ca_{0.15})TiO_3$(SCT) thin films were deposited on Pt-coated $TiO_2/SiO_2/Si$ wafer by the rf sputtering method. Experiments were conducted to investigate the electrical properties of SCT thin films with various top electrodes. Various top electrodes as Pt, Al, Ag, Cu were deposited on SCT thin films by sputter and thermal evaporator. The characteristics of C-F and C-V of SCT thin films were not obviously varied with various top electrodes, SCT thin films annealed at $600^{\circ}C$ represents as favorable capacitance characteristics than SCT thin films not annealed, and Pt top electrode have the most high capacitance. The characteristic of I-V of SCT thin films showed that Pt top electrode revealed more less leakage current density than other electrodes, had a leakage current density below 10-8$[A/cm^2]$ until 25[V] applied voltage.

  • PDF

Evaluation of wear chracteristics for $Al_{2}O_{3}-40%TiO_{2}$ sprayed on casting aluminum alloy (주조용 알루미늄합금의 $Al_{2}O_{3}-40%TiO_{2}$ 용사층에 대한 마멸특성 평가)

  • 채영훈;김석삼
    • Proceedings of the Korean Society of Tribologists and Lubrication Engineers Conference
    • /
    • 1997.10a
    • /
    • pp.183-190
    • /
    • 1997
  • The wear behaviors of $Al_2O_3-40%TiO_2$ deposited on casting aluminum alloy(ASTM A356) by plasma spray against SiC ball have been investigated experimentally. Friction and wear tests are carried out at room temperature. The friction coefficient of $Al_2O_3-40%TiO_2$ coating is lower than that of pure $Al_2O_3$ coating(APS). It is found that low friction correspond to low wear and high friction to high wear in the experimental result. The thickness of $Al_2O_3-40%TiO_2$ coatings indicated the existence of the optimal coating thickness. It is found that a voids and porosities of coating surface result in the crack generated. As the tensile stresses in coating increased with the increased friction coefficient. The columnar grain of coating will be fractured to achieve the critical stress. It is found that the cohesive of splats and the porosity of surface play a role in wear characteristics. It is suggested that the mismatch of thermal expansion of substrate and coating play an important role in wear performance. Tensile and compressire under thermo-mechanical stress may be occurred by the mismatch between thermal expansion of substrate and coating. This crack propagation above interface is observed in SEM.

  • PDF

Evaluation of Wear Chracteristics for $Al_2O_3-40%TiO_2$Sprayed on Casted Aluminum Alloy (주조용 알루미늄 합금의 $Al_2O_3-40%TiO_2$ 용사층에 대한 마멸특성 평가)

  • 채영훈;김석삼
    • Tribology and Lubricants
    • /
    • v.15 no.1
    • /
    • pp.39-45
    • /
    • 1999
  • The wear behavior of $Al_2$O$_3$-40%TiO$_2$deposited on casted aluminum alloy (ASTM A356) by APS (Air Plasma Spray) against SiC ball has been investigated in this work. Wear tests were carried out at room temperature. The friction coefficient of $Al_2$O$_3$-40%TiO$_2$coating is lower than that of pure $Al_2$O$_3$coating(APS). $Al_2$O$_3$-40%TiO$_2$coating indicated the existence of the optimal coating thickness. It is found that voids and pores of coating surface resulted in the generation of cracks, and the cohesive of splats and the porosity of surface play a role in wear characteristics. It is suggested that the mismatch of thermal expansion of substrate and coating play an important role in wear performance. Tension and compression under thermo-mechanical stress may be occurred by the mismatch between thermal expansion of substrate and coating. The crack propagation above interface is observed in SEM.

Fabrication of $BaTiO_3-PTCR$ Ceramic Resister Prepared by Direct Wet Process (습식 직접합성법을 이용한 PTCR 소자개발 연구)

  • 이경희;이병하;이희승
    • Journal of the Korean Ceramic Society
    • /
    • v.22 no.4
    • /
    • pp.61-65
    • /
    • 1985
  • $BaTiO_3$ powders doped with $BaTiO_3$ and $Nb_2O_5$ at 9$0^{\circ}C$ for 1hr. were synthesized by Direct Wet Process. These powders were very homogeneous and fine particle size. To obtain the highe PTCR effect AST($1/3Al_2O_3$.$3/4SiO_2$.$1/4TiO_2$) and $MnO_2$ were added in the semiconduc-ting $BaTiO_3$. In this case $Bi_2O_3$ and $MnO_2$ were used in the form of $Bi(NO)_3$ and $MnCl_2$.$4H_2O$ solution for Direct Wet Process. $BaTiO_3$ doped Nb2O5 and $MnO_2$ demostrated greater PTCR effect than $BaTiO_3$ doped $Nn_2O_5$ only.

  • PDF

The effect of additive on $SnO_2$ gas sensor for improving stability ($SnO_2$계 가스 센서의 안정성 향상을 위한 산화물의 첨가 효과)

  • Park, Kwang-Mook;Min, Bong-Ki;Choi, Soon-Don;Nam, Hyo-Duk
    • Proceedings of the Korean Institute of Electrical and Electronic Material Engineers Conference
    • /
    • 2002.07b
    • /
    • pp.865-868
    • /
    • 2002
  • $SnO_2$ powders were prepare by precipitating $Sn(OH)_4$ from an aqueous solution of $SnCl_4{\cdot}5H_2O$, pH 9.5. The effects of stability and sensitivity of $SnO_2$ thick film sensors added with various amounts, $SiO_2$, $Al_2O_3$, $ZrO_2$, $TiO_2$ have been investigated. It is shown that the 3wt% $Al_2O_3$ or $SiO_2$ can improve the stability of $SnO_2$ gas sensor at an operating temperature of $350^{\circ}C$.

  • PDF

A Comparison of Structural Characterization of Composite Alumina Powder Prepared by Sol-Gel Method According to the Promoters (졸-겔법으로 제조된 복합 알루미나 미분체의 첨가제에 의한 구조적 특성 비교)

  • Lee, Jung-Woon;Yoon, Ho-Sung;Chae, U-Suk;Park, Han-Jin;Hwang, Un-Yeon;Park, Hyung-Sang;Park, Dal-Ryung;Yoo, Seung-Joon
    • Korean Chemical Engineering Research
    • /
    • v.43 no.4
    • /
    • pp.503-510
    • /
    • 2005
  • In this research, composite alumina was prepared to add the various promoters by sol-gel method and examined its thermal stability. After sintering at $1,200^{\circ}C$, the thermal stability resulted in following order, $Si{\fallingdotseq}La$ > Ti > $Ba{\fallingdotseq}Ce$ > Y > $Zr{\fallingdotseq}Mg$, in accordance with adding the promoters. Especially in case of silica-added alumina, a phase transformation temperature to ${\alpha}$-alumina increased about $150^{\circ}C$ and after sintering at $1,200^{\circ}C$, it showed to maintain in ${\gamma}$-form and ${\delta}$-form alumina phase. Also it showed an increase of surface area from $3m^2/g$ to $71m^2/g$ compared with pure ${\alpha}$-alumina. In the case of silicaadded alumina, the characterization change of this alumina particle resulted in a delay of phase transformation because Si-O-Al bond was increased when sintered at high temperature. In case of lanthanum-added alumina, there was a sintering delay phenomenon in inter-particles as $LaAlO_3$ structure existed. The existence of lanthanum structure was confirmed by XRD and XPS analysis. It appeared on the alumina surface as $La_2O_3$ structure when it was sintered under $1,000^{\circ}C$, as the perovskite structure of $LaAlO_3$ at above $1,000^{\circ}C$ and as the magneto-plumbite structure of $LaAl_{11}O_{18}$ at above $1,300^{\circ}C$.

Effects of Additives on the Characteristics and Microstructure of $UO_2$ Pellet ($UO_2$ 소결체의 특성 및 미세구조에 미치는 첨가제의 영향)

  • 유호식;이신영;이승재;강권호;김형수
    • Journal of the Korean Ceramic Society
    • /
    • v.37 no.7
    • /
    • pp.660-664
    • /
    • 2000
  • Effect of various kinds of additive such as AlOOH, Al(OH)3, Al2Si2O5(OH)4, Nb2O5, TiO2 and MgO on the properties and microstructures of UO2 pellet has been examined. All the tested dopants had played a role to reduce sintered density and open porosity. It was revealed that the addition of TiO2 made pellet more stable thermally. UO2 pellet doped with 0.2wt% TiO2 was swelled rather than densified after annealing for 24 hrs at 1$700^{\circ}C$. It was attributed to large pore with spherical shape. Titinia and silicon coexisted with Al element were more effective to increase grain size than other additives. It could be also revealed that the formation of liquid phase was the main cause of grain growth.

  • PDF

Synthesis of ceramic particles by hydrothermal method (수열법에 의한 세라믹분말 합성)

  • 김판채;최종건
    • Proceedings of the Korea Association of Crystal Growth Conference
    • /
    • 1996.06b
    • /
    • pp.219-222
    • /
    • 1996
  • 수열법은 밀폐용기중에서 10$0^{\circ}C$이상의 가열, 가압된 수용액이 반응에 관여하는 것으로써, 수정, CaCO3, AlPO4, GaPO4 등과 같은 단결정의 육성 뿐만 아니라 균일분산계로부터 균일한 결정성의 미립자 합성에도 폭넓게 이용되고 있다. 세라믹분말의 합성에 있어서, 이 방법은 특히 형상, 입자크기의 제어가 용이할 뿐만 아니라 고상법, 졸-겔법, 공침법에서와 같은 열처리, 분쇄과정이 필요없기 때문에 고순도의 초미립자를 얻을 수 있는 장점이 있다. 근년 미국, 일본에서는 수열법을 이용한 유전, 압전체 등 세라믹분말의 일부가 공업적인 규모로 대량 생산되고 있다. 그러나 이에 대한 국내 기술은 아직 초기단계에 이르고 있는 실정이다. 따라서 본 연구실에서는 수열법에 의한 단결정 육성 (예; 자수정, CaCO3, AlPO4, GaPO4, KTP, Emerald 등), 박막제조 (예; GaP, PbTiO3, BaTiO3 등), 정제 (고령토, 장석, 도석 등), 원석처리 (진주, 인공 emerald, 비취 등) 그리고 각종 세라믹분말의 합성 등과 같은 다양한 기반기술의 축적과 동시에 공업화에 대응한 수열장치를 위하여 반응용기의 대형화, 엄밀한 밀폐방식, 실용적인 수열조건 등을 개발해 오고 있다. 본 발표에서는 현재까지의 연구개발 내용 중에서 결정성 미립자에 관련한 세라믹분말의 합성에 대한 일부의 결과들을 보고한다. 일반적으로 수열장치는 전기로, 반응용기, 온도 및 압력제어계 등을 기본으로 하고 있으며 시판용의 대부분이 교반기가 부착된 수직형 (vertical type)이다. 이와 같은 방식에 있어서는 엄밀한 밀폐가 곤란, 반응온도의 한계성 (25$0^{\circ}C$ 이하), 증진율의 한계성 (소량생산) 등과 같은 점이 있기 때문에 본 연구실에서는 개폐식 전기로내에 엄밀한 밀폐가 가능한 수평식(horizontal type)의 반응용기를 채택한 뒤 이를 회전 또는 시이소(seesaw)식으로 움직일 수 있도록 하여 연속공정화, 온도구배의 자율조절 그리고 보다 저온에서도 인위적인 이온의 확산을 효율적으로 유도할 수 있도록 하였다. 이와 같은 방식은 기존의 방식과 비교하여 반응용기 내에 응집현상과 미반응물이 존재하지 않으며 또한 단분산으로 결정성 미립자를 대량적으로 얻을 수 있는 장점이 있었다. 다음은 이상과 같이 본 연구실에서 자체 개발한 수열장치를 이용하여 PbTiO3, (Pb,La)TiO3Mn, BaTiO3, ZnSiO4:Mn, CaWO4 등과 같은 세라믹분말에 대한 합성 실험의 결과이다. 압전성, 초전성이 우수한 PbTiO3 및 (Pb,La)TiO3:Mn 분말의 수열합성은 PbO, TiO2, La2O3 등의 분말을 출발원료로 하여 합성도도 25$0^{\circ}C$부근의 알카리성 용액중에서 결정성 PbTiO3 및 (Pb,La)TiO3:Mn 미립자를 단상으로 얻었으며 입자의 형상 및 크기는 합성온도와 수열용매의 종류에 의존하였다. 유전체로서 폭넓게 응용되고 있는 BaTiO3 분말은 Ba(OH)2.8H2O, TiO2와 같은 최적의 출발원료를 선택함으로써 15$0^{\circ}C$ 부근의 저온영역에서도 용이하게 합성할 수 있었다. 특히 본 연구에서는 수용성인 Ba(OH)2.8H2O를 사용함으로써 host-guest적인 반응을 유도시키는데 있어 물의 가장 실용적이고 효과적인 수열용매임도 알았다. ZnSiO4:Mn, CaWO4, MgWO4와 같은 형광체 분말은 공업적으로 고상반응 또는 습식법에 의해 얻어지고 있으나 이들 방법에 있어서는 분쇄공정으로 인한 형광특성의 저하와 같은 문제점이 있다. 따라서 본 연구에서는 수열법을 이용하여 이들 화합물의 합성을 시도하였으며 그 결과 합성온도 30$0^{\circ}C$ 부근의 알칼리성 용액중에서 수열적으로 얻어짐을 알았다. 여기서의 합성분말을 이용하여 실제 조명램프로 제조한 결과 녹색, 청색 발광용 형광체로서 우수한 형광특성을 나타내었다. 천연에서 소량 산출되고 있는 고가의 (Li,Al)MnO2(OH)2:Co 분말은 도자기의 전사지용 청색안료로써 이용되고 있다. 본 연구실에서는 LiOH.H2O, Al(OH)3, MnO2 등의 분말을 출발원료로 하고 24$0^{\circ}C$ 온도 부근 그리고 물을 수열용매로 하여 천연산에 필적하는 (Li,Al)MnO2(OH)2:Co 분말을 인공적으로 합성하였다.

  • PDF