Tensile tests were conducted on the GFRP reinforcement exposed to high temperature. The exposure condition for this study was below $200^{\circ}C$ for about 3 minutes. This conditioning is minor compared with that presented in experimental program conducted by other researchers. The residual tensile strength and elastic modulus of GFRP reinforcing bars at high temperature and after exposure to high temperature were compared. In results, tensile properties were decreased at high temperatures, but those after exposure to high temperature were recovered to pre-heating level almost completely. These results could be valuable for evaluating GFRP reinforced structure damaged by fire accident.
Keywords
GFRP reinforcing bar; High temperature; Tensile strength; Tensile elastic modulus;
Citations & Related Records
연도 인용수 순위
  • Reference
1 Abbasi, A. and Hogg, P. J. (2005). "Temperature and environmental effects on glass fibre rebat : Modulus, Strength and Interfacial Bond Strength with Concrete." Compos : Part B., Vol. 36, pp. 394-404.   DOI
2 Alsayed, S., Al-Salloum, Y., Almusallam, T., El-Gamal, S. and Aqel, M. (2012). "Performance of glass fiber reinforced polymer bars under elevated temperatures." Compos : Part B., Vol. 43, pp. 2265-2271.   DOI
3 AL-ZAHRANI, M., AL-DULAIJAN, S. U., AL-IDI, S. H. and AL-METHEL, M. H. (2007). "High temperature effect on tensile strength of GFRP bars and flexural behavior of GFRP reinforced concrete beams." FRPRCS-8, University of Patras. Patras. Greece.
4 Bisby, L. A., Green, M. F. and Kodur, V. K. R. (2005). "Response to fire of concrete structures that incorporate FRP." Prog. Struct. Engng Mater., Vol. 7, pp. 136-149.   DOI
5 Bosze, E. J., Alawar, A., Bertschger, O., Tasai, Y. I. and Nutt, S. R. (2006). "High-temperature strength and storage modulus in unidirectional hybrid composites." Compos. Sci. Tech., Vol. 66, pp. 1963-1969.   DOI
6 Correia, J. R., Gomes, M. M., Pires, J. M. and Branco, F. A. (2013). "Mechanical behaviour of pultruded glass fibre reinforced polymer composites at elevated temperature : Experiments and Model Assessment." Compos. Struct., Vol. 98 pp. 303-313.   DOI
7 Foster, S. K. and Bisby, L. A. (2005). "High temperature residual properties of externally-bonded FRP systerms." Am. Concr. Inst., Vol. ACI-SP230, No. 7, pp. 1235-1252.
8 Fu, Y. N., Zhao, J. and Li, Y. L. (2011). "Research on tensile mechanical properties of GFRP rebar after high temperature." Adv. Mater. Research., Vol. 181-182, pp. 349-354.   DOI
9 Kashwani, G. A. and Al-Tamimi, A. K. (2014). "Evaluation of FRP bars performance under high temperature." Phys. Procedia., Vol. 55, pp. 296-300.   DOI
10 Kumahara, S., Masuda, Y., Tanano, H. and Shimizu, A. (1993). "Tensile strength of continuous fiber bar under high temperature." Spec. Publ., Vol. 138, pp. 731-742.
11 Robert, M. and Benmokrane, B. (2010). "Behavior of GFRP reinforcing bars subjected to extreme temperatures." J. Compos. Constr., Asce., pp. 353-360.
12 Saafi, M. (2002). "Effect of fire on FRP reinforced concrete members." Compos. Struct., Vol. 58, pp. 11-20.   DOI
13 Wang, Y. C. and Kodur, V. (2005). "Variation of strength and stiffness of fibre reinforced polymer reinforcing bars with temperature." Cem. Concr. Compos., Vol. 27, pp. 864-874.   DOI
14 Weber, A. (2008). "Fire-resistance tests on composite rebars." 4th Int. Conf. FRP Compos. Civ. Eng. (CICE 2008), Zurich, Switzerland.