Effect of Thermal Oxidation Coating on the Hot Forging Process of High Strength Ti-6Al-4V Bolt |
Kim, Jeoung-Han
(재료기술연구소)
Lee, Chae-Hoon (한국기계연구원, 재료기술연구소/ 특수합금연구그룹) Hong, Jae-Keun (한국기계연구원, 재료기술연구소/ 특수합금연구그룹) Kim, Jae-Ho (신진볼택, 냉간사업부) Yeom, Jong-Taek (한국기계연구원, 재료기술연구소/ 특수합금연구그룹) |
1 | N. S. Reddy , Y. H. Lee , J. H. Kim , C. S. Lee, 2008, High temperature deformation behavior of Ti-6Al-4V alloy with an equiaxed microstructure: a neural networks analysis. Met. Mater. Int., Vol. 14, pp. 213-222 DOI ScienceOn |
2 | N. Matsukura, 2007, Development of cold forging technology for beta-titanium, in M. Niinomi, S.Akitama, M. Hagiwara, M. Ikeda, and K. Maruyama(eds). Ti-2007 science and technology, Kyoto, pp. 1395-198 |
3 | S. L. Semiatin, R. L. Goetz, E. B. Shell, V. Seetharaman, A. K. Ghosh, 1999, Cavitation and failure during hot forging of Ti-6Al-4V, Metall. Mater. Trans., A Vol. 30, pp. 1411-1424 DOI ScienceOn |
4 | U. Wiklund, I. M. Hutchings, 2001, Investigation of surface treatments for galling protection of titanium alloys, Wear, Vol. 251, pp. 1034-1041 DOI ScienceOn |
5 | M. J. Donarchie Jr., 2000, Titanium-A Technical Guide edition, ASM International, pp. 5-11 |