Abstract
Due to tightened environmental regulations on halogen type flame retardants, the portions of those based on phosphorous compounds that are non-halogen type is rising. When producing functional film, the physical and thermal properties become distinctly different depending on the amount of Red-phosphorus(RP) addition which causes flame resistance. The physical properties of resin fall in big scale when too much flame retardants are added, and it is hard to be applied to functional films such as shrink or anticorrosive film. The purpose of this research is to study the effects on mechanical, physical, and other properties of RP-LDPE films by changing the RP-MB contents. The LDPE film used for this study was produced through blow-type injection molding. The flame resistance was VTM-0, and the tear resistance showed inverse trends of MD and TD. Contraction percentage showed no relationship with the amount of RP content, but the anti-corrosive property showed 0.05 % better result than the national anti-corrosion shrink film reliability standard.
Keywords
Flame retardant; LDPE (Low Density Polyethylene); MB (Master Batch); Red phosphorus;
Citations & Related Records
Times Cited By KSCI : 1  (Citation Analysis)
연도 인용수 순위
1 M. Modesti, A. Lorenzetti, "Flame retardancy of polyisocyanurate-polyurethane foams: use of different charring agents", Polym. Degrad. Stab., 78, 341, 2002. DOI: http://dx.doi.org/10.1016/S0141-3910(02)00184-2   DOI
2 W. Y. Chen, Y. Z. Wang, F. C. Chang, "Thermal and Flame Retardation Properties of Melamine Phosphate-Modified Epoxy Resins", J. Polym. Res., 11, 109, 2004. DOI: http://dx.doi.org/10.1023/B:JPOL.0000031069.23622.bc   DOI
3 O. P. Korobeinichev, V. M. Shvartsberg, A. G. Shmakov, D. A. Knyazkov, and I. V. Rybitskaya, Proceedings of the Combustion Institute, 31, 2741, 2007. DOI: http://dx.doi.org/10.1016/j.proci.2006.07.120   DOI
4 M. Liu, Y. Liu, Q. Wang, "Flame-Retarded Poly(propylene) with Melamine Phosphate and Pentaerythritol/Polyurethane Composite Charring Agent", Macromol. Mater. Eng., 292, 206, 2007. DOI: http://dx.doi.org/10.1002/mame.200600353   DOI
5 L. Song, Y. Hu, Y. Tang, R. Zhang, Z. Chen, W. Fan, "Study on the properties of flame retardant polyurethane/organoclay nanocomposite", Polym. Degrad. Stab., 87, 111, 2005. DOI: http://dx.doi.org/10.1016/j.polymdegradstab.2004.07.012   DOI
6 F. Siminoi, M. Chechin, M. Modesti, A. Lorenzetti, "Influence of different flame retardants on fire behaviour of modified PIR/PUR polymers", Polym. Degrad. Stab., 74, 475, 2001. DOI: http://dx.doi.org/10.1016/S0141-3910(01)00171-9   DOI
7 Y. Chen, Q. Wang, W. Yan, H. Tang, "Preparation of flame retardant polyamide composite with melamine cyanurate nanoparticles in situ formed in extrusion process", Polym. Degrad. Stab., 91, 2632, 2006. DOI: http://dx.doi.org/10.1016/j.polymdegradstab.2006.05.002   DOI
8 B. Y. Jo, S. C. Moon, J. K. Choi, "Effect of Waste Ground Tire Rubber on Flame Retardancy and Foaming Properties of the NBR foams", Elast. Compos., 38, 251, 2003.
9 U. Braun, B. Schartel, M. A. Fichera, C. Jager, "Flame retardancy mechanisms of aluminium phosphinate in combination with melamine polyphosphate and zinc borate in glass-fibre reinforced polyamide 6,6", Polym. Degrad. Stab., 92, 1528, 2007. DOI: http://dx.doi.org/10.1016/j.polymdegradstab.2007.05.007   DOI
10 M. Thirumal, D. Khastgir, N. K. Singha, B. S. Manjunath, Y. P. Naik, "Effect of expandable graphite on the properties of intumescent flame-retardant polyurethane foam", J. Appl. Polym. Sci., 110, 2586, 2008. DOI: http://dx.doi.org/10.1002/app.28763   DOI
11 T. M. Jayaweera, C. F. Melius, W. J. Pitz, C. K. Westbrooka, O. P. Korobeinichev, V. M. Shvartsberg, A. G. Shmakov, I. V. Rybitskaya, and H. J. Curran, "Combustion and Flame", 140, 103 2005. DOI: http://dx.doi.org/10.1016/j.combustflame.2004.11.001   DOI
12 G. Kumar and A. Z. Worku, PCT Patent Application WO 00/17268 2000.
13 J. G. Uhlmann, J. D. Oelberg, K. D. Sikkema, and R. G. Nelb, "Plastics Additives and Compounding", May/June, 38 1993.
14 T. Akiyoshi and S. Tamura, European Patent Application 1,055,705 2000.
15 D. Hoang, J. Kim, and B. N. Jang, Polym. Degrad. Stabil., 93, 2042 2008. DOI: http://dx.doi.org/10.1016/j.polymdegradstab.2007.10.020   DOI
16 Korean Standard Association, KS T 1043, KSA, 2011
17 Korean Standard Association, KS M ISO 6383-2, 2010
18 Korean Standard Association, KS M ISO 9773, 2011
19 KRICT, RS-KRICT-006, 2011.